At least 19 records

Fastener joint and associated method for avoiding corrosion of dissimilar material fastener joints

A fastener for use in joining dissimilar materials manufactured by the process of producing the fastener with an external surface that forms an electrically insulating oxide layer when subjected to oxidation and, after manufacture and prior to use, subjecting the fastener to a pre-oxidation process to grow the desired oxide layer in situ on the external surface of the fastener. The present invention also provides a dissimilar material joint in which the pre-oxidized fastener is used to mechanically join dissimilar materials with the oxide layer electrically insulating the fastener from at least one of the dissimilar materials. The fastener may be a rivet used in friction self-piercing riveting (F-SPR). The fastener may be fabricated from an alloy capable of forming Al 2 O 3 or Cr 2 O 3 by thermal oxidation. The fastener may be pre-coated with Al or Cr that functions as a seed layer to form Al 2 O 3 or Cr 2 O 3 .

Lim, Yong Chae↗

Tensile Deformation of DED Graded IN718-René41 Superalloy at 650°C by in-situ Neutron Diffraction and Digital Image Correlation

A compositionally graded material comprised IN718 (718, γ'/γ" strengthened superalloy) and René41 (R41, a medium γ' strengthened superalloy) was fabricated using laser blown-powder directed energy deposition (DED/LB-M). Hot gas path components that require high and low temperature capabilities at different locations may benefit from such graded superalloy, potentially eliminating the use of welded or mechanically joined components and reducing cost. In the present work, microstructure and 650°C tensile behavior of 718-R41 graded superalloy in as-built and heat-treated states are investigated by Digital Image Correlation (DIC), in-situ neutron diffraction, coupled with conventional characterization techniques. The applied heat treatment generates static recrystallization and equiaxed grains in 718 rich compositions, while R41 rich compositions remain partially or un-recrystallized. Yield strengths of 718 and R41 sections in heat-treated state are comparable to wrought forms but the graded compositions show weakness. From neutron experiment, diffraction elastic constants and single crystal elastic constants are calculated, which show small difference between the as-built and heat-treated states and between the γ and γ' phases. Grain-level load transfer from the (220) grains to (200) grains is found to be composition dependent, and qualitatively agrees with DIC measured macroscopic yield strength. Within the (200) grains, the γ/γ' phases deform elastically until the γ phase yields and afterwards the γ' phase takes load from γ phase.

digital image correlation↗

Nonhomologous end-joining uses distinct mechanisms to repair each strand of a double strand break

Abstract Nonhomologous end-joining repairs chromosomal double strand breaks, but it is unknown whether both strands are repaired by this pathway, and if one strand break’s repair path impacts the other. Here, we show that nonhomologous end-joining employs both of two a priori possible strategies. Strand breaks that can be directly ligated are joined near-simultaneously, with no effect of one strand break’s repair path on the other. More complex end structures require obligatorily ordered repair. The first strand to be repaired is used as template for repair of the opposite/second strand break, with the latter repair reaction occurring fastest when also coupled to nonhomologous end-joining. Enforced asymmetry in repair of each strand break can extend to the gap-filling polymerase employed, and whether the polymerases incorporate RNA or DNA. Our results resolve questions about pathway mechanism and identify a requirement for flexibility of the nonhomologous end-joining machinery for efficient repair of both strand breaks within diverse cellular double strand breaks.

Luthman, Adam J.↗

Macro-level mechanical interlocking: A rapid joining approach for additively manufactured compression molded composite panels

Composite joining typically involves multiple steps, such as drilling and surface treatment, as part of the manufacturing process, which leads to low throughput and long cycle times. In the present study, we demonstrated a macro-level mechanical interlocking (MI) based, rapid joining technique to assemble additively manufactured compression molded (AMCM) panels, enabling the production of parts larger than the mold dimensions. Composite panels made of 20 wt% short carbon fiber reinforced acrylonitrile butadiene styrene (CF/ABS) were joined using MI features of various geometries, namely tree (TR), dovetail (Dov), rectangle 2 (Rect2), and rectangle 1 (Rect1), and their in-plane strength was evaluated. The resultant strength of the tested MI joints reached up to 74 % of the baseline tensile strength (i.e., the ‘no joint’ case). Observations from optical and scanning electron microscopy revealed inadequate polymer diffusion between the adherends, indicating that the joint strength was primarily derived from mechanical interlocking. Additionally, the fracture surfaces exhibited stress-whitening marks, which were characterized using differential scanning calorimetry (DSC). The increase in melting enthalpy suggested local stretching of polymer chains due to MI. Finite element analysis (FEA) indicated that the Rect1 MI feature, which generated the lowest stress concentration, outperformed the others in terms of joint strength, achieving 42 MPa. As a demonstration of the MI joining method, a battery box tray measuring 108 cm × 34 cm using a mold with an effective dimension of 36 cm × 34 cm successfully manufactured, resulting in a part with an area three times larger than the mold. In conclusion, this study presents a promising approach to improving composite joining techniques while minimizing production complexities.

In-plane joining↗

Spectra and characteristics of somatic mutations induced by ionizing radiation in hematopoietic stem cells

Spectra and frequencies of spontaneous and X-ray-induced somatic mutations were revealed with mouse long-term hematopoietic stem cells (LT-HSCs) by whole-genome sequencing of clonal cell populations propagated in vitro from single isolated LT-HSCs. SNVs and small indels were the most common types of somatic mutations, and increased up to twofold to threefold by whole-body X-irradiation. Base substitution patterns in the SNVs suggested a role of reactive oxygen species in radiation mutagenesis, and signature analysis of single base substitutions (SBS) revealed a dose-dependent increase of SBS40. Most of spontaneous small deletions were shrinkage of tandem repeats, and X-irradiation specifically induced small deletions out of tandem repeats (non-repeat deletions). Presence of microhomology sequences in non-repeat deletions suggested involvement of microhomology mediated end-joining repair mechanisms as well as nonhomologous end-joining in radiation-induced DNA damages. We also identified multisite mutations and structural variants (SV), i.e., large indels, inversions, reciprocal translocations, and complex variants. The radiation-specificity of each mutation type was evaluated from the spontaneous mutation rate and the per-Gy mutation rate estimated by linear regression, and was highest with non-repeat deletions without microhomology, followed by those with microhomology, SV except retroelement insertions, and multisite mutations; these types were thus revealed as mutational signatures of ionizing radiation. Further analysis of somatic mutations in multiple LT-HSCs indicated that large fractions of postirradiation LT-HSCs originated from single LT-HSCs that survived the irradiation and then expanded in vivo to confer marked clonality to the entire hematopoietic system, with varying clonal expansion and dynamics depending on radiation dose and fractionation.

63 RADIATION, THERMAL, AND OTHER ENVIRON. POLLUTAN↗

Fast-rate joining of thermoplastic composites using integrated additive manufacturing and compression molding process

The integration of additive manufacturing (AM) technology with compression molding (CM), has emerged as a high-performance composite manufacturing technology in recent years. In the AM-CM process, quickly deposited AM preform on a mold undergoes a rapid compaction cycle to fabricate structurally robust composite parts due to highly controlled fiber alignment (from AM) and reduced porosity (from CM). Currently, AMCM-based part size is limited by the size of the mold volume, thus posing a challenge to manufacture scalable parts. Here, this work focuses on joining techniques developed to enable fast rate joining of short fiber-reinforced thermoplastic composite parts using the AM-CM process. Acrylonitrile butadiene styrene resin reinforced with 20 wt% short carbon fiber composites was printed onto a flat mold and pressed under a hydraulic press. Fabricated panels were joined by the (a) mechanical impression at the joining interface and (b) over-molded continuous carbon fiber (CCF) sheet. Tensile tests were performed to characterize the joining strength of both mechanical impression-based joints and CCF over molded joints. Among the mechanical impression-based joints, a U-shape channel allowed the fibers to flow between two joint parts, and 280 % increased mechanical properties were observed. The continuous carbon fiber-based over molded joint CCF showed 350 % increase in tensile strength compared to the butt joints.

36 MATERIALS SCIENCE↗

Roles for epigenetics in wood formation and stress response intrees–from basic biology to forest management

Annual model and crop species have been the subject of most epigenetic studies for plants. In contrast to annuals, forest trees persist on natural landscapes and experience environmental variation within and across seasons, years, and decades or even centuries. Most forest trees species are undomesticated and typically grown on variable landscapes with no irrigation or application of agricultural chemicals. Forest trees must thus rely on their inherent ability to alter growth and physiology to mitigate the effects of changing abiotic and biotic stressors. Like other plants, trees have mechanisms encoded in their genomic DNA sequence that can respond directly to stress events such as drought or heat. Hypothetically, it would be highly advantageous to join these mechanisms with a dynamic “memory” of past exposure to stress. It is now well established that annual model and crop plants can establish epigenetic-based memory of stress events that support more rapid and robust response to stress in the future. Here, evidence is discussed for epigenetic regulation and “memory” in two fundamental biological processes in trees, wood formation and abiotic stress response. Wood formation is an ideal trait for epigenetic research in trees, as wood formation is highly responsive to environmental conditions and includes multiple rapid developmental changes as cells adopt distinct fates within complex tissues. This is followed by a discussion of research needs that would provide the foundation for new epigenetic applications for forestry.

Groover, Andrew↗

A study of adhesive bonding in metal–metal, metal–CFRP, and CFRP–CFRP material combinations under shear deformation: Fracture morphologies and damage mechanisms

Safe design of adhesive joining in multi-materials in engineered structures requires the accumulation of numerous experimental data on the failure behavior of various adhesively-bonded material combinations under different loading conditions. The deep understanding of mechanical performance, fracturing morphologies, and main damage mechanisms is also quintessential for accelerating the development of proper physics-based and multi-scale models for assisting the design. Towards this goal, this work presents a comprehensive characterization of the failure behavior of adhesively-bonded metal–metal, metal–CFRP, and CFRP–CFRP material combinations under global shear deformation via single lap shear testing. Thanks to a synergistic combination of measurement methods by using Digital Imaging Correlation (DIC) and 3D optical profilometry, adhesive features on the adherend after failure were quantified and the main progressive damage mechanisms were identified. The characterization performed in this work provides quantitative data that contributes to a better understanding of shear failure in adhesive bonding across different bi-material combinations. Finally, the obtained results have practical implications, including the potential to enhance adhesive bonding design, identify failure causes in adhesive joints, and develop or validate computational models capable of capturing the observed behavior in various adhesively-bonded materials under global shear deformation.

36 MATERIALS SCIENCE↗

A Multiscale Investigation of the Mechanisms Controlling Materials Degradation in the Fusion Energy Environment (DE-SC0006661: Final Report)

Realizing the promise of fusion as a commercially attractive energy source requires the development of advanced structural materials capable of sustained operation in an incredibly hostile environment. The fusion environment presents many challenges associated with high cyclic thermal-mechanical loadings, welding and joining disparate materials, and achieving chemical compatibility with coolants and tritium breeders. Yet, the overarching concern is the degradation of physical and mechanical properties, resulting from a neutron energy spectrum peaked at 14 MeV. The high-energy fusion neutron irradiation produces both displacement damage and high levels of hydrogen and helium through transmutation reactions. Advanced materials development for use in such a hostile environment is predicated on understanding the underlying mechanisms responsible for physical and material property degradation. This project has closely combined computational, theoretical and experimental techniques within a multiscale materials science paradigm to determine the mechanisms controlling material degradation in the fusion environment.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Scale-Up of Friction Self-piercing Riveting Process for Multi-material Joints

A single-class joining process known as “friction self-piercing riveting (F-SPR)” has been developed for joining various low-ductility lightweight materials on a laboratory scale. The frictional heat generated during the F-SPR process improved local ductility, resulting in crack-free joints and robust mechanical performance. This innovative joining technology was further advanced through the scale-up of the process using a new system with several key features (e.g., automatic rivet feeding and clamping system, vacuum system) toward industry readiness. The new integrated F-SPR systems were effectively demonstrated for joining different material combinations (e.g., carbon fiber composite to 7075 Al alloy, 7075 Al alloy to 7075 Al alloy, and 7075 Al alloy to casting Al Aural 5) with a unified technique. Crack-free joint with adequate mechanical interlocking resulted in good mechanical joint strength for each material combination. Then, the process was successfully scaled up by producing multiple joints without any cracks on larger CFC-Al and Al-Al components by the new integrated system, bringing it closer to industrial application.

Lim, Yong Chae [ORNL] (ORCID:0000000321773988)↗

Elucidating microstructural evolution and hardness variation across friction self-piercing riveted Al-7055 using synchrotron X-ray scattering and advanced microscopy techniques

Friction self-piercing riveting (FSPR) is a unique hybrid joining technique that combines the advantages of mechanical interlocking, frictional heat, and solid-state joining (if metallurgically compatible) to produce crack free joints in high strength and/or low-ductility alloys at room temperature. Here, in the current study, Al-7055 sheets were joined using FSPR for lightweight automotive applications and significant microhardness variations were observed across the joint cross-section. A detailed microstructural characterization at multiple length scales was carried out using advanced electron microscopy and X-ray scattering techniques to provide a fundamental understanding of the process-structure-property relationships. The relative contributions of microstructural characteristics at various length scales (i.e., grain size, dislocation density, solute concentration, precipitate nature) to strengthening were estimated using existent formulations (i.e., Hall-Petch, Taylor, precipitate bypass/shear equations) and correlated to the observed microhardness values across different regions. Small-angle X-ray scattering and scanning transmission electron microscopy revealed significant changes in the size and volume fraction of precipitate species, i.e., GP-I Zones, η′, and Mg/Zn solute co-clusters, depending on the process region. It was observed that the dissolution of the small η′/GP-I zones (T ∼ 150–200 °C) in the heat-affected zone were the key reason for the hardness drop. Further, it was shown that solid-solution, dislocation, grain size and solute co-cluster strengthening played a key role in the thermo-mechanically affected zone and grain-refined zone (GRZ). Finally, these observations were leveraged along with the Zener-Holloman relationship and grain size in the GRZ to estimate the peak joining temperature of the GRZ (∼ 350 °C) near the steel rivet.

aluminum 7xxx alloy↗

Bio-inspired interlocking metasurfaces

Interlocking metasurfaces (ILMs) are patterned arrays of mating features that enable the joining of bodies by constraining motion and transmitting force. They offer an alternative to traditional joining solutions such as mechanical fasteners, welds, and adhesives. This study explores the development of bio-inspired ILMs using a problem-driven bioinspired design (BID) framework. We develop a taxonomy of attachment solutions that considers both biological and engineered systems and derive conventional design principles for ILM design. We conceptualize two engineering implementations to demonstrate concept development using the taxonomy and ILM conventional design principle through the BID framework: one for rapidly assembled bridge truss members and another for modular microrobots. These implementations highlight the potential of BID to enhance performance, functionality, and tunability in ILMs.

attachment↗

Friction Self-piercing Riveting Process for 3T Configuration of AA7075-AA7075-AA6022

Friction self-piercing riveting (F-SPR), as a solid-state joining process that generates frictional heat during the process, was utilized to join a 3 T configuration of low-ductility AA7075-AA7075-AA6022 sheets. A multi-step F-SPR process was employed to precisely control the mechanical interlocking and solid-state joining, ensuring a strong joint formation. With control of the plunge depth when the transition from rivet penetration to rivet flaring, two joining conditions were developed to assess mechanical joint integrity: one bearing deep penetration with a smaller interlock, and the other yielding a shallow penetration with a larger interlock. Both strategies met the criteria for a sound rivet joint. Customized lap shear tensile configurations were designed to assess the joint strength at interface between first and second layers, as well as between second and third layers. Both conditions demonstrated great joint strength between the first and second layers, while deeper penetration approach showed stronger solid-state joint, leading to improved joint strength between the second and third layers.

Wang, Tianzhao [ORNL] (ORCID:0000000315337602)↗

Evaluation of Corrosion and Its Impact on the Mechanical Performance of Al–Steel Joints

Aluminum–steel joints are increasingly used in the automotive industry to meet the requirements for energy saving and emission reduction. Among various joining technologies, self-pierce riveting (SPR) and resistance spot welding (RSW) are two well-established technologies for fabricating dissimilar joints with stable and high mechanical performance. However, corrosion will occur in these joints inevitably due to different electrochemical properties, which can degrade the surface quality and the mechanical performance, such as strength. This paper presents a method of understanding the corrosion mechanisms in joining aluminum and steel. For this understanding, a hybrid method combining experimental observations, mechanical properties identification, and analytical approaches was used to assess the evolution of the impact of corrosion on the joining performance, such as traction separation curves. The study was conducted on common combinations used in the vehicles, e.g., a 1.2 mm thickness aluminum alloy (AA 6022) and 2.0 mm thickness hot deep galvanized steel (HDG HSLA 340) joined by SPR and RSW. After the fabrication of these joints, accelerated cyclic corrosion tests of up to 104 cycles were performed, which reproduced the environmental conditions to which a vehicle was exposed. By investigating the microstructural evolution within the joints, the corrosion mechanisms of SPR and RSW joints were revealed, including the initiation and propagation. Moreover, the intrinsic impact of the corrosion on the mechanical performance, including the strength, axial stiffness, and crashworthiness, was analyzed by performing a lap-shear test. It showed that as corrosion proceeds, the fracture modes and mechanical performance are affected significantly.

Chemistry↗

Evaluation of Tungsten—Steel Solid-State Bonding: Options and the Role of CALPHAD to Screen Diffusion Bonding Interlayers

Critical aspects of innovative design in engineering disciplines like infrastructure, transportation, and medical applications require the joining of dissimilar materials. This study investigates the literature on solid-state bonding techniques, with a particular focus on diffusion bonding, as an effective method for establishing engineering bonds. Welding and brazing, while widely used, may pose challenges when joining materials with large differences in melting temperature and can lead to mechanical property degradation. In contrast, diffusion bonding offers a lower temperature process that relies on solid-state interactions to develop bond strength. The joining of tungsten and steel, especially for fusion reactors, presents a unique challenge due to the significant disparity in melting temperatures and the propensity to form brittle intermetallics. Here, diffusion characteristics of tungsten–steel interfaces are examined and the influence of bonding parameters on mechanical properties are investigated. Additionally, CALPHAD modeling is employed to explore joining parameters, thermal stability, and diffusion kinetics. The insights from this research can be extended to join numerous dissimilar materials for specific applications such as aerospace, automobile industry, power plants, etc., enabling advanced and robust design with high efficiency.

36 MATERIALS SCIENCE↗

Vibration mitigation in interlocking metasurfaces

Interlocking metasurfaces (ILMs) are a new class of mechanical metamaterials with patterned surface features that enable joining of two adjacent bodies, serving as an alternative to welds, fasteners, or adhesives. While the strength of ILMs has been explored previously, it is also possible to envision ILMs that possess the ability to dampen vibration or tailor energy transmission across the interface. In this study, we explore the vibration transmission under frequency sweep and random excitation of three ILM designs. This is the first study to characterize the response of ILMs under vibration. We find that ILMs which are tightly coupled (e.g., small interference fit) behave as a linear system and depart only marginally from the behavior of a solid body. However, through strategic manipulation of the ILM topology, and in particular the fit clearances, we show that vibrations can be damped by over an order of magnitude. Design strategies to employ ILMs for vibration mitigation are developed using a first-order model.

Bolmin, O. [Carnegie Mellon Univ., Pittsburgh, PA ↗

Effect of die design on microstructure and mechanical joint strength in friction self-piercing riveted AA7055-T76 and AA7055-T76

In the present study, a unique friction self-piercing riveting (F-SPR) was applied to join high-strength, low-ductility aluminum alloy (AA) 7055-T76 and AA7055-T76 to mitigate a cracking issue. Also, the effect of die design on both joint formation and the mechanical joint performance were investigated. A crack-free joint was achieved when joining AA7055-T76 and AA7055-T76 by F-SPR. As the bottom diameter of the die increased, the mechanical interlocking distance initially increased then became almost saturated. At the same time, the solid-state bonding gradually disappeared, and the lap-shear fracture changed from bottom aluminum fracture to rivet pull-out with partial bottom aluminum fracture. The average maximum lap-shear joint strength of 11.57 kN and cross tension of 5.65 kN were achieved from the D2 die design owing to the combined contributions from high mechanical interlocking distance and good solid-state bonding at the joint interface. Ultrafine grain refinement was observed at the region next to the rivet shank outer surface and along the materials flow line between the top and bottom aluminum sheet in the rivet cavity. Further, because of the same joint-process parameters, the hardness profile at the joints made by different dies did not show obvious differences. As the distance from the base metal to the rivet outer surface decreased, frictional heat caused the hardness to initially decrease from 190 to 150 HV in the heat-affected zone. Hardness increased up to 175 HV in the thermomechanical affected zone (TMAZ-I) owing to large plastic deformation.