Search NASA⌕ Search

SEARCH · Search NASA

Results for “mesophase pitch”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Scale up production of carbon fibers from petroleum mesophase pitch

This work investigates the scale-up of pitch precursors for the carbon fiber market using mesophase pitch formulated and produced by Advanced Carbon Products Technologies’ (ACPT’s) patented mesophase pitch processing technology. Through use of its patented process, ACPT developed strategic materials by converting petroleum-based pitch into a high-value, low-cost, carbon-rich feedstock for carbon fiber and other materials critical to our national security. The team successfully developed processing criteria for the tailored mesophase pitch material that can be processed further into precursor and carbon fiber. Processability of the mesophase pitch into precursor and carbon fiber was demonstrated at scale. The resulting materials sequester the carbon that would otherwise be burned and released into the atmosphere, making this an environmentally friendly way to produce these materials in the United States.Pitch-based carbon fibers offer a promising pathway toward cost-effective, high-performance materials for structural and high-modulus composite applications; however, adoption has been limited by challenges in precursor processability and scale-up. In this work, tailored isotropic and mesophase petroleum-derived pitch materials were developed and evaluated for precursor and carbon fiber production through a collaborative effort between Oak Ridge National Laboratory (ORNL) and ACPT. Processing conditions were established at ORNL’s Carbon Fiber Technology Facility to enable stable melt-blowing of pitch-based precursors under continuous operation. Mesophase pitch precursor fibers were produced following oxidation and carbonization, corresponding to a diameter shrinkage of approximately 12%–13% and an estimated mass yield of about 75%–80%. Continuous melt-blowing steady-state operation was demonstrated over time, indicating robust process stability. Melt-blowing was achieved at throughput rates of approximately 20 lb/h⁻¹, validating the commercial viability of petroleum-derived pitch feedstocks for fiber production. Further studies are required to tailor carbon fiber microstructure and properties for specific composite applications.

99 GENERAL AND MISCELLANEOUS↗

Preparation of Mesophase Pitch Feedstock for Carbon Fiber

A filtration process of the low cost mesophase pitch developed by Advanced Carbon Products, LLC (ACP) was developed. The mesophase pitch was melt spun into fiber at the University of Kentucky Center for Applied Energy Research (UKY), and converted to carbon fiber. The melt spinning process was moderately stable, but resulted in some void structure in the green fibers. The tensile properties of the resulting carbon fibers, after graphitization heat treatment, were tested yielding a modulus value of approximately 560 GPa or 81 MSI. This demonstrated that a high modulus graphitic carbon fiber is certainly possible from the ACP 20 mesophase pitch. For future work, a better balance between the softening point temperature, the spinning temperature, and filtering must be met to reduce the volatiles generated in the pitch during spinning. This would reduce voids in the fiber, facilitate spinning, and generate finer, higher performance graphitic fiber.

36 MATERIALS SCIENCE↗

Molecular origin of viscoelasticity and influence of methylation in mesophase pitch

The viscoelastic and thermomechanical properties of pitches are responsible for their melt-spinning behavior, which is a critical step for manufacturing high-performance pitch-based carbon fibers. Here, we systematically explore the impact of methyl group modifications on the viscoelastic and thermal properties of mesophase pitches. We employ a range of atomistic modeling approaches, including Density Functional Theory (DFT), Density Functional Tight Binding (DFTB), and Classical Molecular Mechanics (MM), to provide detailed insights into the molecular interactions and structural changes. Further, our results revealed the molecular mechanisms that promote layered structures leading to the anisotropic nature of the viscoelastic behavior of mesophase pitch. Furthermore, we propose a modified molecular representation of naphthalene-based mesophase pitch based on the analysis of x-ray diffraction measurements. This study provides fundamental insights into the molecular structures of mesophase pitch and the role of methyl groups controlling its viscosity, which offer valuable insights into mesophase-based carbon fiber production.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploration of fibers produced from petroleum based-mesophase pitch and pet blends for carbon fiber production

Petroleum-derived mesophase pitch and polyethylene terephthalate (PET) were blended and melt-extruded to create precursor fibers. The raw blends, heat treated bulk materials, and fibers were all examined to determine compatibility between petroleum-derived mesophase pitch and PET. Thermal investigation of the raw blends showed the presence of both the pitch and PET in separate phases suggesting no interactions had occurred during mixing. Here, the heat-treated bulk material also showed multiple phases under polarized light while Fourier-transform infrared spectroscopy indicated that the two materials did not fully separate during extrusion. Elemental scans of the precursor fibers showed areas of high oxygen concentrations averaging 11.7% as compared to a 2% oxygen concentration across the majority of the cross-section. Tensile tests of the precursor fibers showed a decrease in average modulus as compared to pure pitch fibers; however, the depressed modulus of the blended fibers was found to be independent of the PET weight percentage. Fibers created from 5 wt.% PET had a strength value within 10% of pure pitch and a 200% increase in modulus and were therefore found to be the most promising for carbon fiber production. Pure pitch and the 5 wt.% PET fibers were stabilized and carbonized to 1000 °C. Both types of fibers were tensile tested to determine their strength and stiffness. Pure pitch carbon fibers maintained a higher strength while the carbon fibers produced from 5 wt.% PET possessed a stiffer modulus which can be attributed to their radial microstructure.

36 MATERIALS SCIENCE↗

On the role of methyl groups in the molecular architectures of mesophase pitches

The role of methyl groups on the liquid–crystal structure of mesophase pitches was investigated by combining experimental characterizations and atomic-scale computational modeling, using three pitches synthesized from different precursors. Of the three pitches, C-9 alkyl benzene and naphthalene-based pitches have 13 and 7 methyl groups per average polyaromatic hydrocarbon, respectively. By contrast, mesophase produced from a coal-tar pitch has about one methyl group. The coal tar–based mesophase pitch is hydrogen deficient or more aromatic compared with C-9 alkyl benzene- and naphthalene-based pitches. Additionally, X-ray diffraction data showed that average coherent domain sizes of C-9 alkyl benzene (3.7 nm) and naphthalene-based (3.6 nm) pitches with more methyl groups are larger than that of coal tar–based mesophase (2.4 nm). Based on the identified features, the influence of the methyl group on the layering structures was investigated via molecular dynamics simulations. The results revealed that methyl groups are critical in mesophase layering in C-9 alkyl benzene- and naphthalene-based pitches, by reducing CH-π interaction. However, similar alignment could be achieved without the same degree of methyl substitutions for the coal tar-based pitch because of stronger π-π interaction than the other precursors. The insights from this study contribute to our understanding of the formation of conventional mesophase pitch and have implications for the processing of coal-derived materials. In conclusion, this knowledge is vital to produce valuable products like carbon fiber and graphite from pitches.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tuning Microstructure of Mesophase Pitch Carbon Fiber by Altering the Carbonization Ramp Rate

The microstructure of mesophase pitch carbon fibers (CFs) are tuned by varying ramp rates from 1 to 50 °C min –1 up to 1000 °C to study the effect of ramp rate on CFs’ microstructure, thermal and mechanical properties with the goal of offsetting the cost by decreasing cycle time. The ramp rates represent carbonization times ranging from 16.4 to 1.17 h, not including cool down. Differential scanning calorimetry, thermogravimetric analysis, and derivative thermogravimetry are used to investigate the impact ramp rate has on the thermal properties of mesophase pitch. It is found that lower ramp rates are endothermic in nature with a lower temperature onset and maximum weight loss. Higher ramp rates possess an exothermic nature with higher temperatures resulting in maximal weight loss over a smaller range of temperatures. Mechanical testing shows varying CF strengths and moduli dependent on ramp rate and an optimized process is developed to produce the strongest CF. Furthermore, microstructural characterization revealed that faster ramp rates lead to smaller interplanar spacings and larger crystallites but possessed greater disorder.

36 MATERIALS SCIENCE↗

Compatibility of mesophase pitch and linear low-density polyethylene for low-cost carbon fiber

Mesophase pitch and linear low-density polyethylene (LLDPE) were blended by shear mixing and extruded producing precursor fibers which were then converted to carbon fibers (CFs). LLDPE additives agglomerate within the isotropic spheres rather than uniformly dispersing throughout the entire matrix. The blends possess different thermal properties and precursor tensile properties evident by two-phase tensile stress nature not present in precursor fibers produced from pure pitch. The resultant CFs were oxidized at 280 °C for 4 h and carbonized at 1000 °C for 15 min. This process created pitch CFs with a tensile strength of 1.23 GPa and a Young’s modulus of 99 GPa. All CFs produced from blends of pitch and LLDPE possessed a tensile strength of 0.63 GPa and less. These CFs showed a microstructure slightly different from the pure pitch CFs with fractured CF cross sections revealing voids present in all blended CFs due to burnt off LLDPE stemming from carbonization. Further study into compatibilizers and new conversion processes is required to successfully blend LLDPE with mesophase pitch for the purpose of producing a new low-cost CF.

36 MATERIALS SCIENCE↗

The effect of inhomogeneities in coal-based mesophase pitch on filament formation and melt spinning for carbon fiber

Mesophase pitch-based carbon fibers excel as high specific strength and modulus materials, but challenges in stable, continuous melt spinning processing are a serious limiting factor. Inhomogeneities in the pitch may result in flow instabilities that can lead to filament breakage. This work aims to characterize and offer mitigation strategies for the negative effects that inhomogeneities such as isotropic binder, gels, and other inclusions impart on melt spinning of mesophase pitch. The effect of inhomogeneities on spinning stability are analyzed using capillary rheometry, borescope imaging of elongating filaments, and filtration. With no filter, immediate blockage of the spinning capillary occurred. Improvement in melt spinning duration was observed when a porous metal filter (20 μm nominal pore size) was utilized, but no significant further improvement in spinning duration was found upon decreasing the filter nominal pores size to 10, 5 and 2 μm. Moreover, flow instabilities that disrupted melt spinning stability were observed by capillary rheometry when the size of included isotropic pitch domains were larger than approximately 10 μm. Resultant carbon fiber properties and SEM imaging of fracture surfaces are reported.

01 COAL, LIGNITE, AND PEAT↗

Filament Formation and Melt Spinning of Coal-Based Mesophase Pitch for Carbon Fiber Production

High-performance carbon fibers excel as high specific strength and modulus materials, and are utilized in composites applications ranging across aerospace, automotive, energy, infrastructure, and sports equipment sectors. Compared to PAN-based carbon fiber, mesophase pitch-based carbon fiber has lower tensile strength but provides a higher modulus, higher thermal conductivity, and a lower cost potential. However, challenges in stable, continuous melt spinning processing are a serious limiting factor. Unlike typical melt spinning of long, linear chain polymers, mesophase pitch is a comprised of relatively shorter polycyclic aromatic hydrocarbons which form a liquid crystal. In its ‘green’ or ‘as-spun’ state, the fibers are very fragile. Moreover, its temperature of processing is quite high, often approaching 400ºC. Complex flow dynamics combined with short length and time scale heat transfer render its melt spinning a formidable processing challenge. Improved understanding of the root causes for nascent filament breakage and spinning instabilities are needed. This work aims to determine fundamental phenomena that govern mesophase pitch filament formation by comparison of required draw force and uninterrupted spinning minutes with applied draw down ratio. The effect of perturbations on spinning stability are analyzed using capillary rheometry, microscopy of elongating filaments, and filtration.

01 COAL, LIGNITE, AND PEAT↗

Comparative Analysis of Radial and Random Microstructures of Mesophase Pitch Carbon Fibers

Carbon fibers (CF) with radial and random microstructures are produced. Here, these fibers are subjected to identical treatment before being mechanically tested and analyzed with Weibull analysis, with the results revealing a statistically significant difference in tensile strengths of 2.23 GPa for random CF and 1.69 GPa for radial CF. Raman mapping probed the crystalline structure perpendicular to the fiber axis and found a uniform structure, while wide‐angle X‐ray diffraction showed a significant difference of 7.5 Å in the crystallites’ basal lengths parallel to the fiber. Small‐angle X‐ray scattering is completed parallel to the fiber for the first time. A cross‐section Guinier plot of the 1D azimuthal integration is generated assuming symmetric scattering, and the parallel scatterers are found to have a similar length scale to the crystallite's length, validating the testing method. Finally, transmission electron microscopy is completed on the longitudinal cross‐section of each fiber. The radial carbon fiber is found to have a core–shell structure, as evidenced further by fast Fourier transform images. Through all studies, it is shown that the structure developed during mesophase pitch spinning altered the microstructure, thus impacting the mechanical properties, confirming a direct relationship between processing, structure, and properties.

Scherschel, Alexander [Univ. of Virginia, Charlott↗

Development of coal-derived carbon-based structural unit as a potential new building material

Coal combustion for energy has not only wasted the hydrogen-rich volatile matters but also results in CO 2 emission causing serious environmental issues. An integrated coal pyrolysis and solvent extraction process under elevated temperatures in an inert atmosphere is implemented to convert as-mined coal from Wyoming Powder River Basin to functional carbon elements such as pyrolysis char (PC). This paper presents the development and fabrication of new carbon-based structural unit (CSU) using pulverized PC and two coal-derived pitches (mesophase pitch and tar pitch) to attain high compressive strength greater than 30 MPa, low thermal conductivity less than 0.30 W/m.K, and low density less than 1.25 g/cm 3 . CSUs have the potential to overcome the current challenges with cement and concrete through pressurized fabrication followed by carbonization. This study aims to develop CSU with nearly 100% coal-derived carbon material for structural application in buildings. The effects of pressing pressures, carbonization temperatures, and binder contents on the density and mechanical and thermal properties of CSU samples are investigated. The study concludes that mesophase pitch produces a better performance of CSU samples, a combination of 100 MPa pressing pressure and carbonization temperature of 900 ⁰C yields the highest compressive strength, and a 25% MP content is recommended for low-cost CSU fabrication. Furthermoer, CSU has a much lower density, lower thermal conductivity, higher compressive strength, and higher strength-to-density ratio than normal concrete.

36 MATERIALS SCIENCE↗

Mesophase pitch-based high performance carbon fiber production using coal extracts from mild direct coal liquefaction

Mild direct coal liquefaction (autogenous pressure, no catalyst, no H2 gas) of Springfield coal in fluid catalytic cracking decant oil is shown to effectively produce coal extract precursors to spinnable mesophase pitch. Here this work demonstrates that the coal extract can be thermally treated to obtain mesophase pitch in a facile one-step process, bypassing the production of an intermediate isotropic pitch. Furthermore, the presence of 25 wt.% coal in the initial slurry can increase the yield to mesophase pitch nearly twofold and yield to carbon fiber by approximately 70%. The coal extract-derived mesophase pitch was melt-spun and heat treated to produce carbon fiber with graphitic texture, high modulus (>400 GPa) and tensile strength up to 943 MPa. Overall, this work demonstrates that coal can be effectively utilized to markedly amplify the mesophase pitch and carbon fiber yield from fluid catalytic cracking decant oil by relatively simple processing, while conserving utility as a precursor to high performance carbon fiber and potentially other high value graphitic products.

36 MATERIALS SCIENCE↗

Coal to Carbon Fiber (C2CF) Continuous Processing for High Value Composites (Final Report)

Coal tar is a condensed and recovered by-product of the coking of metallurgical coal for steel production. The heaviest fraction of distilled coal tar is an isotropic pitch largely used as a binder in the manufacturing of carbonaceous electrodes for primary aluminum smelting and in electric arc furnaces. Coal tar pitch offers high carbon yield upon carbonization. In this project, a process to convert the domestically sourced isotropic coal tar pitch, containing very low particulates (QI = 0.32 wt.%), to form flow-domain mesophase pitch amenable for melt spinning into precursor (green) fibers for carbon fiber, was developed and optimized. The final reproducible processing developed is reviewed in this report, along with several characterizations of the mesophase pitch. A final definition of the characteristics of a ‘spinnable’ mesophase pitch is presented. With this mesophase pitch, reproducible and stable multifilament melt spinning was developed, producing green fiber tows with filament diameters of approximately 20 m. The multifilament melt spinning was the most challenging aspect of the project and required the most effort. The best practices learned from this project for melt spinning are reviewed in this report. Once spun, the green fibers were oxidatively stabilized, carbonized and graphitized under inert gas atmosphere to form the final carbon fibers. Given the relatively high softening point of the mesophase pitch, no issues of interfilament fusion were observed during batch oxidation, and subsequent batch carbonization and graphitization went smoothly in all cases. An ~ 80 wt.% conversion of the green fiber mass to final carbon fiber was achieved. After graphitization, the carbon fibers showed high tensile moduli (most were ~ 600 GPa, or 87 Msi) consistent with commercially-available high-performance pitch-based carbon fiber. However, tensile strength and strain to failure were comparatively low. Further work to reduce defects in and on the fiber surfaces would increase these properties. SEM imaging of the graphitic fiber textures is presented herein. Rudimentary composites were fabricated from the carbon fibers and characterized showing similar modulus to baseline composites fabricated with commercial carbon fiber. Finally, a basic economic analysis was done showing the potential to increase the value of the isotropic coal tar pitch by up to 13.6 to 136 times based on a carbon fiber value of $\$$5/lb to $\$$50/lb, respectively. Moreover, the site case study suggests that the coal tar from the single integrated steel mill could supply production of up to 16 kt/yr of carbon fiber. Finally, a technological gap analysis was done which shed light on remaining technical challenges. These challenges included: recovery and utilization of condensates from the mesophase pitch processing, further advancing and increasing stability of the multifilament melt spinning processing, optimization of the oxidation processing, defect reduction for increased carbon fiber strength, and the development of a weaving process towards carbon fiber fabrics. To maximize the coal value chain, the primary objectives of this project were to (a) develop and scale efficient processing technology for producing melt-spinnable mesophase pitch from isotropic coal tar pitch, (b) clarify and simplify tedious continuous fiber processing technologies (particularly multifilament melt spinning of mesophase pitch) towards the efficient production of high performance carbon fiber, and (c) demonstrate and characterize representative composite parts derived from the final carbon fiber. Immense progress was made on all 3 objectives and is detailed in this report.

01 COAL, LIGNITE, AND PEAT↗

Technoeconomic and life cycle energy analysis of carbon fiber manufactured from coal via a novel solvent extraction process

Coal is a versatile energy resource and was a driver of the industrial revolution that transformed the economies of Europe and North America and the trajectory of civilization. In this work, a technoeconomic analysis was performed for a coal-to-carbon-fiber manufacture process developed at the University of Kentucky’s Center for Applied Energy Research. According to this process, coal, with decant oil as the solvent, was converted to mesophase pitch via solvent extraction, and the mesophase pitch was subsequently converted to carbon fiber. The total cost to produce carbon fibers from coal and decant oil via the solvent extraction process was estimated to be $\$$11.50/kg for 50,000-tow pitch carbon fiber with a production volume of 3750 MT/year. The estimated carbon fiber cost was significantly lower than the current commercially available PAN-based carbon fiber price ($\$$20–$\$$30/kg). With decant oil recycling rates of 50% and 70% in the solvent extraction process, the manufacturing cost of carbon fiber was estimated to be $\$$9.90/kg and $\$$9.50/kg of carbon fiber, respectively. A cradle-to-gate energy assessment revealed that carbon fiber derived from coal exhibited an embodied energy of 510 MJ/kg, significantly lower than that of conventionally produced carbon fiber from PAN. This notable difference is primarily attributed to the substantially higher conversion rate of coal-based mesophase pitch fibers into carbon fiber, surpassing PAN fibers by 1.6 times. These findings indicate that using coal for carbon fiber production through solvent extraction methods could offer a more energy-efficient and cost-competitive alternative to the traditional PAN based approach.

01 COAL, LIGNITE, AND PEAT↗

Interpretation of wide-angle x-ray diffraction patterns from mesophase pitch-based carbon fibers – a simulation and experimental study

Carbon fiber is a critical material in a wide range of industries, where it is highly valued for its high specific strength/stiffness, excellent wear resistance, efficient electrical and thermal transport properties, chemical resistance, and low coefficient of thermal expansion. The properties of a specific carbon fiber are closely tied to its structural characteristics at all length scales. Here, in this work, we applied wide-angle x-ray diffraction to a set of heat-treated mesophase pitch-based carbon fibers, with the goal of elucidating the crystalline structures as a function of fiber orientation. To assist with analysis and interpretation of the experimental data, we employed diffraction pattern simulations using the scalar and vector forms of the Debye scattering equation to determine the influence of basal plane orientation, crystalline ordering (turbostratic-graphitic), and basal plane asymmetry on the diffraction patterns. The results presented here suggest that growth of the transverse crystallites in mesophase pitch-based carbon fiber is fixed until graphitization temperatures are reached. The work completed here provides a framework for the analysis of carbon fiber and other oriented carbon-based materials via diffraction.

36 MATERIALS SCIENCE↗

Evaluating consumer 3D printing nozzles as a low cost alternative for mesophase pitch-derived carbon fiber production

Synthetic fibers, such as Kevlar fibers, SiC fibers, and carbon fibers, are essential components for constructing high performance structures. Whether for engineering, sports, energy storage (batteries and supercapacitors), or aerospace applications, fiber microstructure plays a critical role in fiber properties and functionalities. However, studying fiber nozzle configurations and spinning parameters to achieve the desired microstructure remains challenging, costly, and time consuming. Here, mesophase pitch-derived fibers were used as an example to demonstrate that low cost, commercially available 3D printer nozzles can “print” fibers. Four different nozzles were used to “print” fibers and the effects of their features on fiber properties were observed and compared to other lab spun and commercial pitch- derived CF. A longer orifice length resulted in higher modulus fiber whereas a larger draw-down ratio yielded a stronger fiber. Furthermore, the findings provide a new opportunity for 3D printer hardware application and open up opportunities for developing low-cost fibers.

36 MATERIALS SCIENCE↗

Experimental Validation and Continuous Testing of an On-Purpose High-Yield Pitch Synthesis Process for Producing Carbon Fiber from US Domestic Coal

This project aims to develop technology that converts domestic United States (US) raw coal to high quality, high value, and marketable carbon fiber. More specifically, the project aims to significantly improve the selectivity and yield of carbon fiber produced per ton of coal over conventional coal pitch-based production by using low-severity direct coal conversion technology to maximize the yield of pitch from coal, suitable for production of carbon fiber. To meet the stated objective of developing a technology platform, capable of producing high quality, high-value and marketable carbon fiber from domestic US coal, the proposed scope of work involves testing of a low-severity direct coal liquefaction (LS-DCL) process approach. The isotropic pitch produced from the LS-DCL process will be thermally treated using conventional processes to convert to a liquid crystal or “mesophase” pitch as a precursor for structural carbon fibers. This mesophase pitch will then be melt-spun into fiber, oxygen stabilized, and carbonized using conventional processes. The resulting carbon fiber will be evaluated for mechanical properties and suitability for structural applications such as automotive parts and spars for wind turbine blades. The overall process is expected to significantly lower the cost of fiber compared to state of the art fibers produced from polyacrylonitrile (PAN) precursors.

01 COAL, LIGNITE, AND PEAT↗

Low-Cost, High-Performance Carbon Fiber for Compressed Natural Gas Storage Tanks (Final Technical Report – Down Select Report)

The aim of this project is to reduce the cost of Type IV, carbon fiber (CF) composite overwrap compressed gas storage tanks by reducing the cost of CF and CF composites. The project team worked to reduce the cost of CF by exploring and testing opportunities for a low-cost alternative precursor material for CF production to supplant market-dominant and costly polyacrylonitrile (PAN). Concurrently, the team aimed to reduce the cost of the tanks at the composite level by improving the interfacial adhesion between the fibers and the matrix resin through the incorporation of low-cost nanoparticles recycled from waste materials, which would reduce the volume of costly CF required to achieve the same tank performance. At the end of the first year, the project team selected mesophase pitch as the primary precursor candidate from a field of materials based on the superior mechanical performance and cost-saving potential. During the second year, the team produced CFs derived from mesophase pitch achieving an average tensile strength of 365.6 ksi and average tensile modulus of 40.74 Msi. Facility availability for spinning and converting these fibers at greater scale has hindered scale-up demonstration, but the team has identified opportunities to conduct this work in the near term. Cost modeling shows that these mesophase pitch-derived CFs can be up to 40% less expensive than PAN-derived CFs due to the lower cost of the feedstock material, higher throughput, greater conversion yield, and lower cost spinning method and compared to PAN. Additionally, the team has demonstrated at lab-scale that nanoparticle coating CFs can significantly increase the interfacial shear strength and load transfer efficiency of CFs in a matrix. Single filament pull-out testing showed a 27% average increase in max interfacial shear strength due to this coating. A continuous method of applying these coatings to a tow of CF has been developed for scale-up. 26 m tows of coated CFs were produced using this system and formed into composite ring samples for ASTM ring burst testing. Issues with the testing protocol have limited assessment of these results. A prototype Type IV tank was designed to meet ANSI HGV2 standards, and the design criteria set out by DOE, using the CF properties developed by the team paired with a proprietary resin matrix, a polyamide liner, and aluminum end bosses. The tank weighs 153.1 kg and with a total capacity of 5.8 kg H2 (5.6 kg usable), which yields a gravimetric capacity of 1.17 kWh/kg. Cost modeling predicts that the tank will have a projected cost of $15.73/kWh. Tank performance modeling does not include considerations for fiber-matrix load transfer efficiency improvements offered by nanoparticle coating method.

08 HYDROGEN↗