Compositional evolution of microalloy carbonitrides in a Mo-bearing microalloyed SAE 4120 steel
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Highlights: • Sn microalloying contributes to the enhancement in cold rolling texture intensity and the acceleration in cold rolling texture transformation. • Sn microalloying promotes the recrystallization process, and recrystallization occurs preferentially in steel with Sn compared with Sn-free steel. • Sn microalloying inhibits the growth of recrystallized grains, and the finer grains are obtained in steel with Sn. - Abstract: We investigated the effects of Sn microalloying on cold rolling and recrystallization textures and microstructure of a ferritic stainless steel. The as-received hot rolled sheets were cold rolled at 10%–90% reductions; the sheets cold rolled up to an 80% reduction were annealed at 740–880 °C for 5 min. For comparison, the cold rolling and recrystallization textures of the steel sheets with and without Sn were determined with the conventional X-ray diffraction method. The cold rolling and recrystallization metallographic microstructures were measured by scanning electron microscope and optical microscope, and the crystal orientation maps of the cold rolled and annealed samples were observed by electron backscattered diffraction. The micro-hardness was determined using a digital micro-hardness tester. Our results show that Sn microalloying in a medium chromium ferritic stainless steel plays multiple roles in the cold rolling and recrystallization processes. Sn micrcoalloying contributes to the enhancement in cold rolling texture intensity and the acceleration in cold rolling texture transformation. Sn microalloying is beneficial in promoting the recrystallization process. Recrystallization occurs preferentially in the ferritic stainless steel with Sn. Sn microalloying plays an important role in inhibiting the growth of recrystallized grains. The finer grains are obtained in ferritic stainless steel with Sn when annealing at high temperatures.
Herein, three final cooling temperatures were employed to achieve high strength and toughness communication in the V-N-Cr microalloyed steels. This study shows that V-N-Cr microalloyed steel primarily consisted of ferrite, granular bainite, acicular ferrite, and a small quantity of M/A phase at the final cooling temperature of 600 °C, while the polygonal ferrite, lamellar bainite, granular bainite, and a small fraction of acicular ferrite were obtained at 450 °C. The width of lamellar bainite was ~ 200-400 nm, and acicular ferrite was composed of fine non-parallel ferrite platelet structures with high dislocations densities. As the final cooling temperature decreased further, the microstructure included granular bainite and lath bainite at 350 °C. The nanoscale precipitates of V-N-Cr microalloyed steel were divided into two types, large-scale precipitates near the grain boundary that precipitated at high temperatures and small precipitates of diameter 5-10 nm at low temperatures, which significantly contributed toward strength. The hot rolled low-carbon V-N-Cr microalloy steel exhibited optimal mechanical properties at the final rolling temperature of 830 °C, as well the final cooling temperature was 450 °C. The highest yield strength and tensile strength of V-N-Cr microalloyed steel were 835 MPa and 989 MPa, respectively. The outstanding impact toughness of 161 J tested at − 60 °C was received. The transformation strengthening and precipitation hardening played a crucial role in affecting the thermo-mechanical properties.
In the present study, the influence of cooling rates (low to ultrafast) on diffusion controlled and displacive transformation of Ti-Nb IF and microalloyed steels has been thoroughly investigated. Mechanisms of nucleation and formation of non-equiaxed ferrite morphologies (i.e., acicular ferrite and bainitic ferrite) have been analyzed in details. The continuous cooling transformation behavior has been studied in a thermomechanical simulator (Gleeble 3800) using the cooling rates of 1-150 °C/s. On the basis of the dilatometric analysis of each cooling rate, continuous cooling transformation (CCT) diagrams have been constructed for both the steels to correlate the microstructural features at each cooling rate in different critical zones. In the case of the IF steel, massive ferrite grains along with granular bainite structures have been developed at cooling rates > 120 °C/s. On the other hand, a mixture of lath bainitic and lath martensite structures has been formed at a cooling rate of ~ 80 °C/s in the microalloyed steel. A strong dependence of the cooling rates and C content on the microstructures and mechanical properties has been established. The steel samples that were fast cooled to a mixture of bainite ferrite and martensite showed a significant improvement of impact toughness and hardness (157 J, for IF steel and 174 J for microalloyed steel) as compared to that of the as-received specimens (133 J for IF steel and 116 J for microalloyed steel). Thus, it can be concluded that the hardness and impact toughness properties are correlated well with the microstructural constituents as indicated by the CCT diagram. Transformation mechanisms and kinetics of austenitic transformation to different phase morphologies at various cooling rates have been discussed in details to correlate microstructural evolution and mechanical properties.
Enhancement of thermal stability in Al-Ni alloys through microalloying with slow-diffusing elements, specifically Zr, has been previously reported which is attributed to Zr segregation at the Al/Al 3 Ni interface. In this study, we explore the influence of microalloying Al-Ni alloys with Zr, Ti, V, and Fe on microstructural evolution, hardness, and electrical and thermal conductivity across a range of heat-treatment temperatures from 300 to 450 °C. The distribution of microalloying elements and precipitates after heat treatment is characterized using atom probe tomography (APT). Our investigation confirms Zr segregation to the Al/Al 3 Ni interface, while similar interfacial segregation is absent with the addition of Ti, V, and Fe. Additionally, our analysis of the Al 3 Ni microfiber morphology reveals that their coarsening and spheroidization rates are similar with and without interfacial segregation; thus, retaining the fiber reinforcement through interfacial segregation of slow diffusing elements may not be an effective strategy. Precipitation of L1 2 nanoparticles was found to be the dominant mechanism affecting enhanced hardness and electrical conductivity in Al-Ni-Zr alloys, attributed to precipitation strengthening and solute depletion, respectively. Similar precipitation was not observed for additions of Ti, V, and Fe following heat treatment. We provide a thermodynamic explanation for this limitation. Furthermore, the findings of this study suggest that an effective approach for designing Al-Ni alloys should involve prioritizing microalloying elements to maximize L1 2 precipitation and minimize solute content in the FCC-Al matrix post heat treatment, rather than focusing on Al/Al3Ni interfacial segregation.
Quantification of nanometer-size precipitates in microalloyed steels has been traditionally performed using transmission electron microscopy (TEM), in spite of its complicated sample preparation procedures, prone to preparation errors and sample perturbation. In contrast to TEM procedures, atomic force microscopy (AFM) is performed on the as-prepared specimen, with sample preparation requirements similar to those for optical microscopy (OM), rendering three-dimensional representations of the sample surface with vertical resolution of a fraction of a nanometer. In AFM, contrast mechanisms are directly related to surface properties such as topography, adhesion, and stiffness, among others. Chemical etching was performed using 0.5% nital, at time intervals between 4 and 20 s, in 4 s steps, until reaching the desired surface finish. For the present application, an average surface-roughness peak-height below 200 nm was sought. Quantification results of nanometric precipitates were obtained from the statistical analysis of AFM images of the microstructure developed by microalloyed Nb and V-Mo steels. Topography and phase contrast AFM images were used for quantification. The results obtained using AFM are consistent with similar TEM reports. - Highlights: Black-Right-Pointing-Pointer We quantified nanometric precipitates in Nb and V-Mo microalloyed steels using AFM. Black-Right-Pointing-Pointer Microstructures of the thermo-mechanically treated microalloyed steels were used. Black-Right-Pointing-Pointer Topography and phase contrast AFM images were used for quantification. Black-Right-Pointing-Pointer AFM results are comparable with traditionally obtained TEM measurements.
The effects of a homogenization treatment and microalloying with Mn on the evolution of the microstructure and hot workability of AA6060 aluminum alloys were investigated. Various homogenization treatments with temperatures ranging from 520 to 610 °C and soaking times from 2 to 16 h were conducted. The results revealed that β-AlFeSi intermetallic was the dominant phase in the as-cast microstructure of the experimental alloys. During the homogenization, the fragmentation of intermetallics occurred and plate-like β-AlFeSi transformed into rod-like α-AlFeSi. In addition, a number of dispersoids precipitated in the 0.1Mn alloy in the temperature range of 520-580 °C. The flow stress behavior of the homogenized AA6060 alloys was mainly determined by the solid solution level. Increasing homogenization temperatures resulted in higher flow stresses owing to the increase in solute atoms in the aluminum matrix. The incremental Mn addition from 0 to 0.1% moderately increased the flow stress by up to 3%. Grain growth occurred in the alloys with low Mn contents (< 0.03Mn) during the high-temperature homogenization (580-610 °C), which resulted in a sudden decrease in the flow stresses and an irregular sample shape after the deformation. Microalloying with Mn (> 0.06%) can effectively prevent grain growth at such temperatures. For an alloy with Mn (0.1%) microalloying, homogenization at 550-580 °C for 6 h could be the optimal condition to balance the flow stress and desirable microstructure.
While L1 2 -Al 3 Zr nanoprecipitates provide a balance between strengthening and good electrical conductivity, the precipitation of L1 2 -Al 3 Zr in aluminum requires aggressive heat treatments. An improved age-hardening response was observed during isochronal aging of an Al-0.24Zr (wt%) alloy when microalloyed with Sn. A new mechanism termed Low melting point Element-Assisted Nucleation (LEAN) is proposed to explain the lower temperature nucleation of L1 2 -Al 3 Zr precipitates observed in this alloy based on the addition of a low melting point element, such as Sn. Characterization verified the first-principles density functional theory prediction that Zr and Sn atoms cluster during homogenization owing to the favorable binding energy of Zr-Sn-vacancy triplets. Direct microstructural observations revealed these clusters form Sn nanoprecipitates that assist the nucleation of L1 2 -Al 3 Zr at 200°C, where L1 2 -Al 3 Zr precipitation is not expected due to the low diffusivity of Zr atoms in Al. At higher temperatures (≳350°C), the acceleration of L1 2 -Al 3 Zr precipitation is driven by faster Zr diffusion in Al with Sn microalloying and the nuclei formed via the LEAN mechanism. In conclusion, this combination of mechanisms explains the improvement in age hardening through L1 2 -Al 3 Zr precipitation with Sn microalloying.
The effects of combined silicon and molybdenum alloying additions on microalloy precipitate formation in austenite after single- and double-step deformations below the austenite no-recrystallization temperature were examined in high-strength low-alloy (HSLA) steels microalloyed with titanium and niobium. The precipitation sequence in austenite was evaluated following an interrupted thermomechanical processing simulation using transmission electron microscopy. Large (~ 105 nm), cuboidal titanium-rich nitride precipitates showed no evolution in size during reheating and simulated thermomechanical processing. The average size and size distribution of these precipitates were also not affected by the combined silicon and molybdenum additions or by deformation. Relatively fine (< 20 nm), irregular-shaped niobium-rich carbonitride precipitates formed in austenite during isothermal holding at 1173 K. Based upon analysis that incorporated precipitate growth and coarsening models, the combined silicon and molybdenum additions were considered to increase the diffusivity of niobium in austenite by over 30% and result in coarser precipitates at 1173 K compared to the lower alloyed steel. Deformation decreased the size of the niobium-rich carbonitride precipitates that formed in austenite. - Highlights: • We examine combined Si and Mo additions on microalloy precipitation in austenite. • Precipitate size tends to decrease with increasing deformation steps. • Combined Si and Mo alloying additions increase the diffusivity of Nb in austenite.
In this study, the microalloying effect on glass-forming ability (GFA) has been investigated from the structural aspect, by performing synchrotron radiation x-ray diffraction and absorption measurements coupled with simulations in the NiNbZr ternary system. We propose a new parameter which counts the fraction of the fivefold symmetries in all clusters and find it is strongly associated with the GFA. In particular, this structural parameter has the highest value in a composition where the best GFA is achieved. The present work provides an in-depth understanding of microalloying-induced high GFAs in multicomponent alloys.
Mechanical Performance of traditional gas-shielded arc welded joints of 700 MPa grade microalloyed C-Mn steel cannot meet service requirements. Laser welding, with its characteristic high energy density, is known to improve the welding performance of experimental steels. In the present study, Nb-Ti microalloyed steel with a thickness of 4.5 mm was welded using a 4 kW fiber laser. The microstructure, precipitation, and mechanical properties of the welded joints were studied. The hardness and tensile strength of the welded joints were higher than those of the base metal (BM). The microstructure of the fusion zone (FZ) and coarse grain heat affected zone (CGHAZ) was lath martensite (LM), while the microstructure of the fine grain HAZ and mixed grain HAZ consisted of ferrite and martensite/austenite islands. Although LM was observed in both the FZ and CGHAZ, the hardness and calculated tensile strength of the FZ were lower than those of the CGHAZ, due to a reduction in solid solution strengthening by element loss and the dissolution of high-hardness precipitates in FZ. Most precipitates such as [(Nb,Ti)C and (Nb,Ti)(C,N)] that were present in the BM were dissolved, which led to an increase in C and N in solid solution in the FZ. Thus, the elastic modulus of the FZ was higher than that of the BM. Similarly, the elastic modulus of the CGHAZ was higher than that of the BM due to the segregation of C and N atoms during the welding process. The toughness of the FZ was superior to that of the BM, and the toughness of the HAZ approached 91% of that of the BM. The change in toughness primarily depended on the microstructural refinement, the increase in the fraction of grains with high misorientation, the residual austenite in the FZ and CGHAZ, and the dissolution of coarse precipitates.
Recrystallization behavior of a Nb-Mo microalloyed steel has been investigated using double-hit compression tests. A suitable reheating temperature and soaking time were established for the complete dissolution of the microalloying precipitates prior to hot deformation. The influence of hot deformation conditions on the flow behavior and the effect of alloying elements, Nb in particular, on austenite recrystallization kinetics are highlighted. The strain-induced precipitation has been found to play an important role in hindering recrystallization kinetics. Post-deformation microstructural analysis indicates that strain-induced grain boundary migration (SIMB) is one of the mechanisms for the formation of recrystallized grains. Retardation of recrystallization has been explained by estimating pinning force of Nb(C, N) precipitates and recrystallization driving force at 1000 °C, which is in good agreement with the experimental observations in the present study as well as other reported data. The study brings out a better understanding on the influence of strain-induced precipitates on recrystallization behavior.
In this investigation, by using continuous cooling torsion (CCT) testing, the transformation behavior of four microalloyed steels under two circumstances of austenite conditioning and non-conditioning was studied. A full scale hot-rolling schedule containing a 13-pass deformation was employed for the conditioning of the austenite. The CCT tests were then employed till temperature of {approx} 540 Degree-Sign C and the flow curves obtained from this process were analyzed. The initial and final microstructures of the steels were studied by optical and electron microscopes. Results show that alloying elements would decrease the transformation temperature. This effect intensifies with the gradual increase of Mo, Nb and Cu as alloying elements added to the microalloyed steels. As well, austenite conditioning increased the transformation start temperature due mainly to the promotion of polygonal ferrite formation that resulted from a pancaked austenite. The final microstructures also show that CCT alone would decrease the amount of bainite by inducing ferrite transformation in the two phase region. In addition, after the transformation begins, the deformation might result in the occurrence of dynamic recrystallization in the ferrite region. This could lead to two different ferrite grain sizes at the end of the CCT. Moreover, the Nb bearing steels show no sign of decreasing the strength level after the transformation begins in the non-conditioned situation and their microstructure is a mix of polygonal ferrite and bainite indicating an absence of probable dynamic recrystallization in this condition. In the conditioned cases, however, these steels show a rapid decrease of the strength level and their final microstructures insinuate that ferrite could have undergone a dynamic recrystallization due to deformation. Consequently, no bainite was seen in the austenite conditioned Nb bearing steels. The pancaking of austenite in the latest cases produced fully polygonal ferrite structures. - Highlights: Black-Right-Pointing-Pointer Adding alloying elements would decrease the transformation temperatures. Black-Right-Pointing-Pointer Austenite conditioning increases the transformation start temperature. Black-Right-Pointing-Pointer Deformation could induce the occurrence of dynamic recrystallization in ferrite region.
The effect of Si on the ultra-low temperature toughness of Nb–Ti microalloyed cryogenic pressure vessel steels was investigated by electron back-scattered diffraction and transmission electron microscope with energy dispersive spectroscopy. Equiaxed ferrite and bainite were obtained in the tempered steels with small Si additions. Nanosized Nb–Ti carbides (< 10 nm) were formed in the steel containing 0.05% Si, whereas much coarser carbides (> 30 nm) were found in the steel containing 0.47% Si. The ultra-low temperature toughness of the Nb–Ti microalloyed cryogenic pressure vessel steel was remarkably enhanced by the reduction in the Si content, which was attributed to the pre-existing iron carbide formation before the precipitation of nanosized Nb–Ti carbides during tempering. - Highlights: • Nanosized Nb-Ti carbides formed in the tempered steel with smaller Si addition. • Coarser Nb-Ti carbides formed in the tempered steel with more Si addition. • Pre-existing cememtites provide nucleation sites for Nb-Ti carbide precipitation. • Ultra-low temperature toughness was remarkably enhanced by Si content reduction.
The precipitation hardening behavior of newly developed Mg−Zn−Ca−Ce alloys, with modified texture and improved ductility, is studied to delineate the microstructural characteristics that lead to effective hardening upon ageing treatments. Advanced electron microscopy and atom probe techniques are used to analyze the structural characteristics in relevance to the hardening potential. It has been found that the formation of a new basal precipitate phase, which evolves from a single atomic layer GP zone, and is finely distributed in both under-aged and peak-aged microstructures, has a significant impact in the improvement of the hardening response compared with the base Mg−Zn alloys. It has also been found that the β′{sub 1} rod precipitates, commonly formed during ageing treatments of Mg−Zn alloys, have their size and distribution significantly refined in the Ca−Ce containing alloys. The role of alloy chemistry in the formation of the fine basal plate GP zones and the refinement in β′{sub 1} precipitation and their relationships to the hardening behavior are discussed. It is proposed that Ca microalloying governs the formation of the GP zones and the enhancement of hardening, particularly in the under-aged conditions, but that this is aided by a beneficial effect from Ce. - Highlights: • Ce−Ca microalloying additions improve hardening in Mg−Zn, over Ce or Ca alone. • Improved hardening is due to refined β′{sub 1} rods, and fine basal plate precipitates. • Atom probe tomography identifies Ca in both β′{sub 1} and the fine basal plates. • The fine basal plates originate as ordered monolayer GP zones with 1:1 Zn:Ca (at.%). • With ageing GP zones become more Zn-rich and transform to the fine basal plates.
Scandium (Sc) is a promising microalloying element that enhances the strength and thermal stability of aluminum (Al) alloys. However, these benefits are not fully realized in aluminum-copper (Al-Cu) systems, and corrosion resistance often declines due to the complex phase evolution and diffusion behavior of Cu and Sc. Here, to clarify this, solute diffusion behavior and Cu-Sc interaction during heat treatment (HT) were investigated using in situ synchrotron-based transmission x-ray microscopy (TXM), wide-angle x-ray scattering (WAXS), and x-ray absorption near-edge structure (XANES) spectroscopy. The results, supported by electron microscopy, reveal strong Cu-Sc bonding that significantly impedes solute diffusion, leading to inhomogeneous solute distribution and non-uniform precipitation. Moreover, the Al-Cu-Sc eutectic phase exhibits high thermal stability, resisting dissolution even near the matrix liquidus. These findings quantitatively elucidate the sluggish diffusion kinetics of Cu and Sc, which can help redesign HT schedules to improve both mechanical properties and corrosion resistance in Sc-microalloyed Al-Cu alloys.
The design of controlled rolling process of microalloyed steel sheets is affected by several factors. In this investigation, effect of the reheating, finishing and coiling temperatures of rolling, which are considered as the most effective parameters on microstructure of hot rolled products has been studied. For this purpose, seven different reheating temperatures between 1000 to 1300 deg. C with 50 deg. C increments, three different finishing temperatures of 950, 900 and 850 deg. C below the non-recrystallization temperature and one temperature of 800 deg. C in the inter critical range and four different coiling temperatures of 550, 600, 650 and 700 deg. C were chosen. By soaking the specimens in furnace, the grain coarsening temperature (T{sub gc}) is obtained about 1250 deg. C. Hence, for these kinds of steels, the reheating temperature 1200 to 1250 deg. C is recommended. Moreover, it is observed that decreasing the coiling and finishing temperatures causes more grain refinement of microstructure and the morphology is changed from polygonal ferrite to acicular one. Findings of this research provide a good connection among reheating, finishing and coiling temperatures and microstructural features of Nb-microalloyed steel sheets.
Binary NiAl suffers from a lack of strength and poor creep properties at and above 1000 K. Poor creep resistance in turn affects low cycle fatigue (LCF) lives at low strain ranges due to the additional interactions of creep damage. One approach for improving these properties involved microalloying with either Zr or N. As an integral part of a much larger alloying program the low cycle fatigue behavior of Zr and N doped nickel aluminides produced by extrusion of prealloyed powders has been investigated. Strain controlled LCF tests were performed in air at 1000 K. The influence of these microalloying additions on the fatigue life and cyclic stress response of polycrystalline NiAl are discussed.