Search NASA⌕ Search

SEARCH · Search NASA

Results for “non-flammable electrolyte”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Investigation of electrode-electrolyte interfaces to enable non-flammable Li-ion batteries operating up to 125°C with liquid electrolyte

Non-flammable and high-temperature stable ionic liquid (IL)-based electrolytes could eliminate catastrophic battery failures and improve battery safety, but their poor electrochemical interaction with the LiNi x Mn y Co z O 2 (NMC) family of cathodes is a long-standing problem due to severe parasitic reactions at high temperature. Understanding surface and bulk structural mechanisms of NMC-type cathodes at elevated operational temperature is of paramount importance to facilitate stable electrochemical performance. Here, we report a non-flammable phosphonium IL-based cell chemistry that offers stable electrode-electrolyte interfaces, leading to electrochemical performance up to 125°C and high-temperature safety. We combine electrochemistry with multimodal X-ray spectroscopy methods to understand interfaces at elevated temperature (100°C). This nanoscale understating enables a proof-of-concept high-temperature cylindrical cell (14500), and the design achieves an average Coulombic efficiency of ≈99.5% up to 300 cycles at 100°C. The results ascertain the significance of depth-dependent degradation at the interface, guiding room-temperature Li-ion technology toward extreme-temperature applications.

36 MATERIALS SCIENCE↗

Bridging the gap between academic research and industrial development in advanced all-solid-state lithium–sulfur batteries

The energy storage and vehicle industries are heavily investing in advancing all-solid-state batteries to overcome critical limitations in existing liquid electrolyte-based lithium-ion batteries, specifically focusing on mitigating fire hazards and improving energy density. All-solid-state lithium–sulfur batteries (ASSLSBs), featuring earth-abundant sulfur cathodes, high-capacity metallic lithium anodes, and non-flammable solid electrolytes, hold significant promise. Despite these appealing advantages, persistent challenges like sluggish sulfur redox kinetics, lithium metal failure, solid electrolyte degradation, and manufacturing complexities hinder their practical use. Further, to facilitate the transition of these technologies to an industrial scale, bridging the gap between fundamental scientific research and applied R&D activities is crucial. Our review will address the inherent challenges in cell chemistries within ASSLSBs, explore advanced characterization techniques, and delve into innovative cell structure designs. Furthermore, we will provide an overview of the recent trends in R&D and investment activities from both academia and industry. Building on the fundamental understandings and significant progress that has been made thus far, our objective is to motivate the battery community to advance ASSLSBs in a practical direction and propel the industrialized process.

25 ENERGY STORAGE↗

Non‐Flammable Ester Electrolyte with Boosted Stability Against Li for High‐Performance Li Metal Batteries

Abstract In traditional non‐flammable electrolytes a trade‐off always exists between non‐flammability and battery performance. Previous research focused on reducing free solvents and forming anion‐derived solid‐electrolyte interphase. However, the contribution of solvated anions in boosting the stability of electrolyte has been overlooked. Here, we resolve this via introducing anions into Li + solvation sheaths using anions with similar Gutmann donor number (DN) to that of solvents. Taking trimethyl phosphate fire‐retardant (DN=23.0 kcal mol −1 ) and NO 3 − (DN=22.2 kcal mol −1 ) as an example, NO 3 − is readily involved in the Li + solvation sheath and reduces the polarity of solvent. This results in boosted stability of electrolyte against Li. The developed non‐flammable electrolyte has low viscosity, high ionic conductivity and is low cost. The reversibility of Li‐Cu cell was improved to 99.49 % and the lifespan of practical LMBs was extended by >100 %.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Is Nonflammability of Electrolyte Overrated in the Overall Safety Performance of Lithium Ion Batteries? A Sobering Revelation from a Completely Nonflammable Electrolyte

It has been widely assumed that the flammability of the liquid electrolyte is one of the most influential factors that determine the safety of lithium-ion batteries (LIBs). Following this consideration, a completely nonflammable electrolyte is designed and adopted for graphite||LiFePO 4 (Gr||LFP) batteries. Contrary to the conventional understanding, the completely nonflammable electrolyte with phosphorus-containing solvents exhibits inferior safety performance in commercial Gr||LFP batteries, in comparison to the flammable conventional LiPF 6 -organocarbonate electrolyte. Mechanistic studies identify the exothermic reactions between the electrolyte (especially the salt LiFSI) and the charged electrodes as the “culprit” behind this counterintuitive phenomenon. The discovery emphasizes the importance of reducing the electrolyte reactivity when designing safe electrolytes, as well as the necessity of evaluating safety performance of electrolytes on a battery level.

25 ENERGY STORAGE↗

A Comparative Study of Degradation Behaviors of LiFePO 4 , LiMn 2 O 4 , and LiNi 0.8 Mn 0.1 Co 0.1 O 2 in Different Aqueous Electrolytes

Aqueous Li-ion batteries (ALIBs) are an important class of battery chemistries owing to the intrinsic non-flammability of aqueous electrolytes. However, water is detrimental to most cathode materials and could result in rapid cell failure. Identifying the degradation mechanisms and evaluating the pros and cons of different cathode materials are crucial to guide the materials selection and maximize their electrochemical performance in ALIBs. Here, in this study, we investigate the stability of LiFePO 4 (LFP), LiMn 2 O 4 (LMO) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC) cathodes, without protective coating, in three different aqueous electrolytes, i.e., salt-in-water, water-in-salt, and molecular crowding electrolytes. The latter two are the widely reported "water-deficient electrolytes." LFP cycled in the molecular crowding electrolyte exhibits the best cycle life in both symmetric and full cells owing to the stable crystal structure. Mn dissolution and surface reduction accelerate the capacity decay of LMO in water-rich electrolyte. On the other hand, the bulk structural collapse leads to the degradation of NMC cathodes. LMO demonstrates better full-cell performance than NMC in water-deficient aqueous electrolytes. LFP is shown to be more promising than LMO and NMC for long-cycle-life ALIB full cells, especially in the molecular crowding electrolyte. However, none of the aqueous electrolytes studied here provide enough battery performance that can compete with conventional non-aqueous electrolytes. This work reveals the degradation mechanisms of olivine, spinel, and layered cathodes in different aqueous electrolytes and yields insights into improving electrode materials and electrolytes for ALIBs.

36 MATERIALS SCIENCE↗

Lithium Dendrite-Free Li 7 N 2 I-LiOH Solid Electrolytes for High Energy Lithium Batteries

All-solid-state lithium batteries (ASSLBs) hold great potential to improve the safety and energy density of today’s lithium-ion batteries by using non-flammable inorganic solid electrolytes. Solid electrolytes (SEs) are believed to prevent Li dendrite growth because of high mechanical strength and high Li+ transference numbers. Significant advances in SE have been achieved, among which, Li7La3Zr2O12 (LLZO) and Li2S–P2S5 (LPS) are the most promising SEs for bulk-type solid-state lithium batteries because of high ionic conductivities (>10-4 S/cm2). However, in contrast to our expectations, the growth of lithium dendrites is not suppressed but is facilitated in LLZOs and LPSs regardless of dopants, porosity, and crystallinity of the electrolytes. Despite the unity Li transference number and over two-times of shear modulus than that of Li metal, the critical current densities for Li plating and stripping in these SEs are less than 1.0 mA cm-2, which is one-fourth to one-tenth of that in liquid electrolytes at room temperature. The incompatibility between LLZO and LPS with Li metal seriously limits the energy density of all-solid-state batteries. The mechanism for lithium dendrite formation and growth in SEs are still disputable. Lack of understanding of the Li dendrite formation mechanism seriously impeded the development of solid-state lithium batteries. The development of the criterion for Li dendrite suppression is essential for the success of solid electrolyte lithium batteries. In this project, a criterion for Li dendrite suppression will be developed through thermodynamics and kinetics analysis of lithium dendrite nucleation/growth, which will guide the solid-state electrolyte design. Li7N2I-LiOH, Li5NI2-LiOH and Li3YCl6 solid electrolyte with high ionic conductivity and low electronic conductivity were used to validate the criterion for lithium dendrite suppression. Different surface modifications were also explored to enhance the dendrite suppression capability of SSEs.

25 ENERGY STORAGE↗

Enabling selective zinc-ion intercalation by a eutectic electrolyte for practical anodeless zinc batteries

Abstract Two major challenges hinder the advance of aqueous zinc metal batteries for sustainable stationary storage: (1) achieving predominant Zn-ion (de)intercalation at the oxide cathode by suppressing adventitious proton co-intercalation and dissolution, and (2) simultaneously overcoming Zn dendrite growth at the anode that triggers parasitic electrolyte reactions. Here, we reveal the competition between Zn 2+ vs proton intercalation chemistry of a typical oxide cathode using ex-situ/ operando techniques, and alleviate side reactions by developing a cost-effective and non-flammable hybrid eutectic electrolyte. A fully hydrated Zn 2+ solvation structure facilitates fast charge transfer at the solid/electrolyte interface, enabling dendrite-free Zn plating/stripping with a remarkably high average coulombic efficiency of 99.8% at commercially relevant areal capacities of 4 mAh cm −2 and function up to 1600 h at 8 mAh cm −2 . By concurrently stabilizing Zn redox at both electrodes, we achieve a new benchmark in Zn-ion battery performance of 4 mAh cm −2 anode-free cells that retain 85% capacity over 100 cycles at 25 °C. Using this eutectic-design electrolyte, Zn | |Iodine full cells are further realized with 86% capacity retention over 2500 cycles. The approach represents a new avenue for long-duration energy storage.

25 ENERGY STORAGE↗

Electrolyte design for Li-ion batteries under extreme operating conditions

The ideal electrolyte for the widely used LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)||graphite lithium-ion batteries is expected to have the capability of supporting higher voltages (≥4.5 volts), fast charging (≤15 minutes), charging/discharging over a wide temperature range (±60 degrees Celsius) without lithium plating, and non-flammability. No existing electrolyte simultaneously meets all these requirements and electrolyte design is hindered by the absence of an effective guiding principle that addresses the relationships between battery performance, solvation structure and solid-electrolyte-interphase chemistry. Here we report and validate an electrolyte design strategy based on a group of soft solvents that strikes a balance between weak Li+-solvent interactions, sufficient salt dissociation and desired electrochemistry to fulfil all the aforementioned requirements. Remarkably, the 4.5-volt NMC811||graphite coin cells with areal capacities of more than 2.5 milliampere hours per square centimetre retain 75 per cent (54 per cent) of their room-temperature capacity when these cells are charged and discharged at -50 degrees Celsius (-60 degrees Celsius) at a C rate of 0.1C, and the NMC811||graphite pouch cells with lean electrolyte (2.5 grams per ampere hour) achieve stable cycling with an average Coulombic efficiency of more than 99.9 per cent at -30 degrees Celsius. The comprehensive analysis further reveals an impedance matching between the NMC811 cathode and the graphite anode owing to the formation of similar lithium-fluoride-rich interphases, thus effectively avoiding lithium plating at low temperatures. Additionally, this electrolyte design principle can be extended to other alkali-metal-ion batteries operating under extreme conditions.

25 ENERGY STORAGE↗

Selecting the Optimal Fluorinated Ether Co-Solvent for Lithium Metal Batteries

To guide the selection of a suitable fluorinated ether (FE) co -solvent for lithium metal batteries, it is crucial to understand the relationship between the organic structures of the FEs and the electrochemical performance of an FE-containing electrolyte. In this work, 1,1,2,2-tetrafluoro-1-(2,2,2-trifluoroethoxy)ethane (FEE), 1,1,2,2-tetrafluoro-3-(1,1,2,2-tetrafluoroethoxy)-propane (TTE), and 1,2-bis(1,1,2,2-tetrafluoroethoxy)ethane (OFDEE) were chosen as representative FE co-solvents because of their distinct structural properties. The structure-activity relationship between the FEs and the electrochemical performance of Li||LiNi 0.6 Mn 0.2 Co 0.2 O 2 (Li||NMC622) cells was correlated and quantified by Fourier-transform infrared and multi-dimensional nuclear magnetic resonance techniques. Sand's model was also employed to assess the extent of lithium dendrite formation in the cells using various FE electrolytes. The cycling performance of Li||NMC622 cells using different FE co-solvents follows the order FEE > TTE > OFDEE. Further, since the direct measurement of Sand's time is difficult, we introduced relative Sand's time to probe the diffusion behavior of each electrolyte, and the results showed that the best performance was obtained in the electrolyte with the longest relative Sand's time. Moreover, the lithium metal cell using the electrolyte with FEE co-solvent showed similar capacity retention compared with the baseline electrolyte at room temperature, but it demonstrated significantly improved low-temperature performance. The results indicate that FEE is a promising co-solvent candidate for improving the low-temperature performance of lithium metal batteries because it possesses not only non-solvating behavior but also very low viscosity and non-flammability. The advanced electrolyte LiPF 6 -FEC-DMC-FEE enables very stable cycling of lithium metal batteries at various temperatures.

25 ENERGY STORAGE↗

Tuning the solvation structure with salts for stable sodium-metal batteries

Sodium-metal batteries are an appealing, sustainable, low-cost alternative to lithium metal batteries due to the high abundance and theoretical specific capacity (1,165 mA h g -1 ) of sodium. However, the poor compatibility of the electrolyte with the cathode and anode leads to unstable electrode-electrolyte interphases. Here we introduce the concept of using a salt as a diluent, which enables the use of a single non-flammable solvent, such as trimethyl phosphate. By using sodium nitrate (NaNO 3 ) salt as a model diluent, we report a 1.1 M NaFSI-NaNO 3 -trimethyl phosphate electrolyte that forms a stable interface with sodium-metal anode. In addition, the formation of robust cathode-electrolyte interphases on Na(Ni 0.3 Fe 0.4 Mn 0.3 )O 2 cathode facilitates smooth phase transitions, thus leading to stable cycle life with a capacity retention of 80% over 500 cycles at C/5 rate in Na||Na(Ni 0.3 Fe 0.4 Mn 0.3 )O 2 cells. Further, the work demonstrates a promising approach towards the development of safe, low-cost, sustainable high-performance sodium-metal batteries. Electrolytes with non-flammable solvents are important for the safe operation of sodium-metal batteries. Here the authors report an electrolyte engineering approach, employing salts as a diluent, to enhance interfacial stability and overall safety.

25 ENERGY STORAGE↗

Influence of Ether-Functionalized Pyrrolidinium Ionic Liquids on Properties and Li + Cation Solvation in Solvate Ionic Liquids

Ionic liquids are tunable solvents composed entirely of ions that have properties desirable as electrolytes for lithium batteries such as non-flammability and a large electrochemical stability window. Solvate ionic liquids are a subclass of ionic liquids that consist of a glyme-based solvent and lithium salt in an equimolar ratio, where Li + cation-glyme solvation interactions result in ionic liquid-like properties. LiG4TFSi is a well-studied solvate ionic liquid consisting of equimolar amounts of lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) and tetraglyme (G4). In this work, pyrrolidinium ionic liquids with ether-functionalized side chains were synthesized containing either one ether (EO1) moiety or three ether (EO3) moieties and mixed with LiG4TFSI to form a new class of electrolyte mixtures. Their physical and transport properties, as well as ion solvation structures, were characterized by electrochemical, thermal, rheological, and spectroscopic measurements. The conductivity of the electrolyte mixture composed of EO1:LiTFSI:G4 in a 1:1:1 molar ratio is 2.54 mS/cm at 30 °C, compared to 1.53 mS/cm for LiG4TFSI, an increase of 67%. A significant decrease in the conductivity to 0.279 mS/cm is observed for the EO3:LiTFSI:G4 mixture in a 1:1:0.4 molar ratio. Pulsed-field gradient nuclear magnetic resonance (PFG-NMR) measurements revealed that the EO1 cation diffuses significantly faster than the EO3 cation in their respective mixtures. Liquid-state 13 C NMR experiments indicate that Li + cations preferentially coordinate with tetraglyme. Li + cations do not coordinate with the EO1 cation and only coordinate with EO3 ether side chains at lower concentrations of tetraglyme. We hypothesize that the oligoether EO3 cation competes with G4 and TFSI - for lithium cation solvation in G4 deficient compositions, leading to a largely adverse effect on the mass transport properties of the electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Green, Fire–Retarding Ether Solvent for Sustainable High–Voltage Li–Ion Batteries at Standard Salt Concentration

Lithium-ion batteries (LIBs) are increasingly encouraged to enhance their environmental friendliness and safety while maintaining optimal energy density and cost-effectiveness. Although various electrolytes using greener and safer glyme solvents have been reported, the low charge voltage (usually lower than 4.0 V vs Li/Li + ) restricts the energy density of LIBs. Herein, tetraglyme, a less-toxic, non-volatile, and non-flammable ether solvent, is exploited to build safer and greener LIBs. It is demonstrated that ether electrolytes, at a standard salt concentration (1 m), can be reversibly cycled to 4.5 V vs Li/Li + . Anchored with Boron-rich cathode-electrolyte interphase (CEI) and mitigated current collector corrosion, the LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode delivers competitive cyclability versus commercial carbonate electrolytes when charged to 4.5 V. Synchrotron spectroscopic and imaging analyses show that the tetraglyme electrolyte can sufficiently suppress the overcharge behavior associated with the high-voltage electrolyte decomposition, which is advantageous over previously reported glyme electrolytes. The new electrolyte also enables minimal transition metal dissolution and deposition. NMC811||hard carbon full cell delivers excellent cycling stability at C/3 with a high average Coulombic efficiency of 99.77%. In conclusion, this work reports an oxidation-resilient tetraglyme electrolyte with record-high 4.5 V stability and enlightens further applications of glyme solvents for sustainable LIBs by designing Boron-rich interphases.

36 MATERIALS SCIENCE↗

Rational Electrolyte Design for Elevated-Temperature and Thermally Stable Lithium-Ion Batteries with Nickel-Rich Cathodes

As the energy density of lithium-ion batteries (LIBs) increases, the shortened cycle life and the increased safety hazard of LIBs are drawing increasing concerns. To address such challenges, a series of localized high-concentration electrolytes (LHCEs) based on a solvating-solvent mixture of tetramethylene sulfone and trimethyl phosphate and a high flash-point diluent 1H,1H,5H-octafluoropentyl 1,1,2,2-tetrafluoroethyl ether were designed. The LHCEs exhibited non-flammability and greatly suppressed heat release at high temperatures, which would potentially improve the safety performance of the LIBs. Moreover, the optimal LHCE achieved capacity retentions of 87.1% and 81.7% in graphite||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells after 500 cycles at 25 °C and 45 °C, respectively, which were significantly better than the conventional electrolyte, whose capacity retentions were only 75.2% and 38.5% under the same condition. Mechanistic studies revealed that the LHCE not only formed a more robust solid electrolyte interphase, but also exhibited improved anodic stability, compared with the conventional electrolyte. Further, this work sheds light in rational electrolyte design for high energy density LIBs with high battery performance and low safety concerns.

25 ENERGY STORAGE↗

Highly Loaded Sulfur Cathode, Coated Separator and Gel Electrolyte for High Rate Li-Sulfur Batteries

As one of DOE Battery 500 Seedling projects, Cornell University and EIC Labs investigated and developed i) highly loaded sulfur cathodes (> 3 mg/cm 2 ), ii) hybrid separators, and iii) gel ceramic electrolytes (GCE) to mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries. Scalable nanomanufacturing processes such as air-controlled electrospray (ACES) and gas-assisted electrospinning (GAES) have been utilized to develop directly deposited electrodes and polymer/ceramic hybrid separators. First, in the development of highly loaded cathodes, alternating layers of sulfur impregnated mesoporous carbon and graphene were fabricated via ACES and the resulting layered cathodes and coated separators exhibit higher capacity and capacity retention (about 1,000 mAh/g capacity with less than 0.02% fade/cycles) than single layer cathode or cathode prepared by conventional slurry cast. Alternating layer approach via ACES has been applied to high loading systems (3 - 5 mg S/cm 2 ), demonstrating the potential to increase sulfur utilization and capacity retention. We have also incorporated iron oxides (Fe 3 O 4 ) into S/mesoporous carbon/graphene cathodes to enhance sulfur utilization and mitigation of polysulfide shuttling. and the effect of Fe 3 O 4 in mesoporous carbon and Gr is highly pronounced at high C rates of 1C and 2C cycling performance. To further improve the cathodes at high rates, graphene nanoribbons (GNR) which can promote ion transport were incorporated in the cathode, resulting in 550 mAh/g at 5C/5C rates. Hybrid Li-ion/Li-S cathodes has also been explored to better engage unreacted polysulfides during charge/discharge. S/LFP hybrid cathodes offer higher sulfur utilization and enhanced rate capability, as well as higher areal loading. This study suggests inclusion of iron phosphide (Fe2P) which can chemically interact with polysulfides can further enhance sulfur utilization and mitigation of soluble polysulfides at high rates. Secondly, in the development of hybrid separators, we first employed graphene coating on the commercial polyolefin separators, which exhibits higher capability, better capacity retention and enhanced rate capability. To improve the rate capability with enhanced safety features such as thermal stability and nonflammability, we developed polymer/ceramic hybrids based on thermally stable polyimide (PI) and room temperature curable ceramic precursors such as organopolysilazane (OPSZ) or polysilsesquioxanes (PSSQ), which exhibit no shrinkages up to 300 ºC and non-flammability. To improve mechanical properties and electrochemical stability, polybenzimidazole (PBI) and alumina have been incorporated in polymer/ceramic hybrid separator, replacing PI and OPSZ/PSSQ, respectively. Finally, the gel ceramic electrolyte (GCE) based on ceramic cross linkers have been applied to make Li-S cells even safer and also to mitigate the polysulfide shuttling further. The resulting gel ceramic electrolyte offers improved capacity retention and rate capability, and also effectively mitigates polysulfide shuttling which was also confirmed by modeling. Inclusion of high ion conducting additives into GCE together with polymer/ceramic hybrid separators exhibit the higher ionic conductivity than liquid electrolyte with commercial polyolefin separator. We demonstrated that the developed highly loaded sulfur cathodes, polymer/ceramic hybrid separators and gel ceramic electrolyte can effectively mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries with improved safety.

25 ENERGY STORAGE↗

Nuclear Magnetic Resonance Dynamics of LiTFSI–Pyrazole Eutectic Solvents

Deep Eutectic Solvents (DESs) have emerged as promising candidates to replace conventional organic solvents in various technological applications due to their low vapor pressure, non-flammability, and ease of preparation at low costs. In particular, Type IV DESs, which are composed of metal salts and hydrogen bond donors, are possible replacements for lithium-ion battery electrolytes. In this study, we investigate the molecular dynamics of solvents of lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) and pyrazole (PYR) at varying LiTFSI:PYR molar ratios (1:2, 1:3, 1:4, 1:5) using Nuclear Magnetic Resonance Dispersion (NMRD) and Pulsed Field Gradient (PFG) Nuclear Magnetic Resonance (NMR). PFG NMR reveals composition-dependent diffusion trends, while NMRD provides molecular-level insights into the longitudinal relaxation rate (R 1 = 1/T 1 ). Notably, the LiTFSI:PYR (1:2) sample shows distinct behavior across both techniques, exhibiting enhanced relaxation rates and lower self-diffusion for 1 H compared to the other nuclei ( 19 F and 7 Li), suggestive of stronger and more efficient Li + –pyrazole interactions, as confirmed by the modeling of the relaxation profiles. Our study advances understanding of ion dynamics in azole-based eutectic solvents, supporting their potential use in safer battery electrolytes.

FFC-NMR↗

Heat Transfer Fluids as Co‐Diluents in Localized High‐Concentration Electrolytes for High‐Rate Lithium Metal Batteries With Enhanced Safety

Localized high-concentration electrolytes (LHCEs) have been identified as promising electrolyte formulations for lithium metal batteries, due to their effective interphase formation and promotion of compact Li deposition, yet their practical implementation is often limited by reduced ion transport kinetics. In this study, two industrially established fluorinated ethers are identified for the first time in battery research as effective co-diluents as they combine a broad electrochemical stability window with a low viscosity and intrinsic non-flammability. Incorporating these components, commonly used as heat transfer fluids, yields safer, less flammable electrolyte formulations with enhanced ion mobilities. In particular, the ternary co-diluent formulation shows improved ion mobility by reducing the electrolyte's viscosity while limiting excessive ion clustering. Based on the improved electrolyte transport kinetics, lower overvoltages and higher Coulombic efficiencies at current densities ≥ 1 mA cm −2 are achieved with the ternary co-diluent blend, resulting in markedly extended cycle life in an application-oriented zero-excess pouch cell compared with the baseline system. Complementary electrochemical and ex situ analysis of harvested electrodes at moderate current densities reveals no discernible differences in interphase morphology and composition, suggesting enhanced ion mobility as the primary cause of the improved high-rate performance.

electrolyte diluent↗

Unveiling the thermite-driven lithium fire ignition in solid-state batteries

Here, this study challenges the assumption of the non-flammability of lithium metal all-solid-state batteries (LiSSBs) and other lithium metal batteries without flammable electrolytes. Through thermodynamic calculations and ex situ experiments, we reveal for the first time the risk of thermite reactions between lithium metal and LiFePO 4 in both charged and discharged states. Reactivity is worsened by excess lithium metal in the cell, reaching final maximum adiabatic temperatures of 2,500°C in the charged state, which is hot enough to boil lithium. The thermite reaction triggers spontaneously at 500°C, with poor surface contact, while increasing surface contact through mixing initiates the reaction at room temperature in an inert environment. Despite its fast kinetics, this reaction is transport limited due to lithium passivation, leading to long burn times and reignition risks. Given the risk of lithium metal contacting the cathode during failure, understanding these reactions is crucial for ensuring the safe deployment of LiSSBs.