Search NASA⌕ Search

SEARCH · Search NASA

Results for “offgas”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Measurement of Offgas Species from Thermal Decomposition of Simulated DWPF Melter Feed

A better understanding of the decomposition process in the DWPF melter is desired to improve the melter offgas flammability model. Antifoam in DWPF is of interest because its presence contributes to the flammability of the melter offgas via formation of flammable gas species. Simulant formic/nitric and glycolic/nitric flowsheet SRAT/SME (melter feed) products were studied at several antifoam concentrations. In addition, redox measurements were compared to the offgas generation data to aid in the overall understanding of the feed decomposition process in the DWPF. A new method for quantitatively measuring the offgas species from simulated DWPF melter feed during heating was used to measure the offgas as a function of temperature. Results indicated that the form of the antifoam (degraded, pristine, or a surrogate) had a negligible effect on the offgas composition (including H 2 generation) or glass redox for the SB8 formic/nitric flowsheet. Antifoam concentration in the glycolic/nitric flowsheet feed had a negligible effect on the offgas composition (including H 2 generation) and glass redox. The glycolic/nitric flowsheet feed had significantly less (~ ¼) total H 2 generation in the offgas during melting compared to the formic/nitric flowsheet and is thought to be related to different reaction paths among the flowsheets.

antifoam↗

LAW Melter Offgas System Design Basis Flowsheets (11/15/2019)

The overall objective of this calculation is to develop design basis flowsheets for confirmation of equipment and piping design associated with the LAW melter offgas system (Systems LOP and LVP). Three flowsheet cases are developed. Minimum, maximum, and nominal offgas cases are developed assuming two melters in operation. The minimum, maximum, and nominal cases are expected during normal operation of the offgas system. An additional minimum case is developed assuming one melter is operating.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

A Predictive Model for Offgas Composition in Waste Glass Melters - Spring 2021 SULI General Audience Abstract

Approximately 56 million gallons of nuclear waste are currently stored in 177 underground storage tanks at the Hanford site in Washington state. A portion of the tank waste is targeted for immobilization by converting the nuclear waste to borosilicate glass through a process called vitrification. During vitrification, emissions are produced in addition to the intended glass product. These emissions, contained in a volume above the molten glass called the plenum, are composed of water vapor, air components, aerosols, particulates, and other gaseous species that result from evaporation, reactions, and air influx. The formation of these gasses causes the surface of the glass to foam. To reduce foaming, sucrose is added to the waste stream before the conversion to glass. Sucrose also reduces the formation of hazardous gasses in the plenum including nitrous oxides, NOx, and carboxides, COx. However, if excess sucrose is present, the reactions that produce the gasses in the plenum will be incomplete, and increased levels of NOx and COx can be observed. The Waste Treatment and Immobilization Plant at the Hanford site is equipped with the technology to treat the plenum emissions. Though many tests have been run to determine the presence of particulates in the plenum emissions, there is does not exist an established method to confidently predict the composition of the gaseous species in the plenum prior to treatment without physical testing. A model was created in the process modeling software Aspen Plus to predict the composition of NOx and COx in the plenum. The model employs a constant stirred tank reactor and user-defined reaction chemistry to determine the plenum composition. To verify the model, the offgas predicted by the model were compared to available offgas data for ten different feed compositions. It is demonstrated that the developed Aspen Plus model is capable of predicting the composition of NOx and COx in the plenum.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

H-Canyon Dissolver Offgas Monitoring Using Raman Spectroscopy

This report describes the development and in facility demonstration of a Raman spectrometer to monitor known aluminum offgas components generated during the dissolution of Spent Nuclear Fuel at the Savannah River Site H-Canyon facility. The presence of these gases is an indicator that material is actively being dissolved. This process monitoring technique, which measures the offgas in real time, has the potential to improve the efficiency of facility operations. If the dissolution time is too short, time is wasted due to extended dissolution periods with additional probing of the dissolver pot to confirm that fragment levels are below the thresholds for continuing to the next charge or moving the dissolvent to a receiving tank. If the dissolution time is too long, time and energy are wasted.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

LAW Primary Offgas Process (LOP) and LAW Secondary Offgas/Vessel Vent Process (LVP) System Design Description

This system design description (SDD) defines the technical, functional, and performance requirements of the Low-Activity Waste (LAW) Facility primary offgas process system (LOP) and the LAW Facility secondary offgas/vessel vent process system (LVP). This document details waste treatment requirements, environmental compliance requirements, and authorization basis requirements of the LOP and LVP systems as they are currently known and understood.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

AP-105 Melter Offgas Condensate and EMF Evaporator Concentrate Raman and LIBS Qualitative Evaluation for the use of In-Line Monitoring (Rev. 0)

The Pacific Northwest National Laboratory (PNNL) was tasked to perform Raman spectroscopy and laser induced breakdown spectroscopy (LIBS) testing on the melter off-gas condensate generated during low-activity waste process testing of a sample from Hanford Site tank AP-105 and/or evaporate from evaporation of the condensate. This was a proof-of-principle demonstration that Raman spectroscopy and LIBS have the potential to be used as analytical tools for in-line process analysis of key aqueous phase analytes in radioactive process streams associated with the Hanford Waste Treatment and Immobilization Plant. The work completed under this project complements work completed for WRPS with the development of in-line monitoring systems to characterize and quantify constituents of tank waste following Cs removal and filtration. The WRPS work is currently limited to Raman sensors and utilizes chemometric models for quantification of several anionic species in the sample system. It should be noted that while this approach can be applied to off-gas condensate streams, new chemometric models are needed to accurately quantify analytes under off-gas condensate conditions. The work completed under this project makes timely use of available samples and equipment at PNNL. The project utilized the opportunity to collect off-gas samples from planned AP-105 processing work and included the direct condensate and the evaporate from the DFLAW Radioactive Waste Test Platform. Samples were characterized by instruments already in place at PNNL including a Raman spectrometer optimized for in-line monitoring of flowing and stationary samples as well as a LIBS instrument, which was optimized for static liquid droplet analysis. The ultimate objective was to determine if these techniques could be used to qualitatively characterize analytes present within the off-gas samples. The testing confirmed the use of the Raman as an in-line monitoring system was able to qualitatively observe NO 3 - , NO 2 - , aluminum (as aluminate, Al(OH) 4 - ), SO 4 2- , CrO 4 2- , CO 3 2- , and PO 4 3- in the AP-105 melter feed evaporator condensate samples. The testing also confirmed LIBS as a potential useful technique for in-line monitoring, able to qualitatively detect Na, N, Al, and tentatively Cr and Cl in a simulant stock evaporate solution.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Permanganate Oxidation of Actual Defense Waste Processing Facility (DWPF) Slurry Mix Evaporator Condensate Tank (SMECT) and Offgas Condensate Tank (OGCT) Samples to Remediate Glycolate

Savannah River Remediation (SRR) tasked Savannah River National Laboratory (SRNL) to examine glycolate destruction in radioactive samples emulating the proposed process. Experiments with radioactive Defense Waste Processing Facility (DWPF) condensates were performed to demonstrate the oxidation of glycolate using sodium permanganate. One test each was performed for Off-Gas Condensate Tank (OGCT) and Slurry Mix Evaporator Condensate Tank (SMECT) samples received. Condensates were blended with Recycle Collection Tank (RCT) heel simulant and Slurry Mix Evaporator (SME) product containing glycolate to represent typical RCT compositions with estimated nominal entrainment of glycolate. A permanganate to glycolate (P/G) molar ratio targeting 5.7 decreased sample glycolate concentration below Ion Chromatography (IC), glycolate method reporting limits in less than 2 hours for the OGCT sample and in less than 8 hours for the SMECT sample.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Enabling System Technologies to Improve the Economies and Performance of Existing LWRs and Advanced BWR Plants: Improving Offgas System Performance. Final CRADA Report

The project goal is to study adsorbent materials and adsorption conditions in order to develop recommendations to improve the current BWR off-gas treatment operations with respect to cost savings. ANL tasks included a literature survey on relevant information for the adsorption of radionuclides (e.g., Xe and Kr), including adsorption coefficients on various charcoals, the effect of radionuclide concentration and moisture, and alternative sorption materials; participate in meetings and teleconferences as needed; prepare reports and support efforts INL and other organization Team Members.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Biocrude and Offgas Data from Hydrothermal Liquefaction of 50-50 Mix of Primary and Secondary Sludge [Slides]

This presentation provides flowrate and compositional information on process off gas generated from a Hydrothermal Liquefaction test conducted with sludge. Density and viscosity data as a function of temperature on biocrude properties from this test are also provided. Data can be used for comparisons, preliminary estimates, modeling and as preliminary data for stakeholders

09 BIOMASS FUELS↗

Behavior of Mercury During DWPF Chemical Process Cell Processing

The Defense Waste Processing Facility has experienced significant issues with the stripping and recovery of mercury in the Chemical Processing Cell (CPC). The stripping rate has been inconsistent, often resulting in extended processing times to remove mercury to the required endpoint concentration. The recovery of mercury in the Mercury Water Wash Tank has never been high, and has decreased significantly since the Mercury Water Wash Tank was replaced after the seventh batch of Sludge Batch 5. Since this time, essentially no recovery of mercury has been seen. Pertinent literature was reviewed, previous lab-scale data on mercury stripping and recovery was examined, and new lab-scale CPC Sludge Receipt and Adjustment Tank (SRAT) runs were conducted. For previous lab-scale data, many of the runs with sufficient mercury recovery data were examined to determine what factors affect the stripping and recovery of mercury and to improve closure of the mercury material balance. Ten new lab-scale SRAT runs (HG runs) were performed to examine the effects of acid stoichiometry, sludge solids concentration, antifoam concentration, form of mercury added to simulant, presence of a SRAT heel, operation of the SRAT condenser at higher than prototypic temperature, varying noble metals from none to very high concentrations, and higher agitation rate. Data from simulant runs from SB6, SB7a, glycolic/formic, and the HG tests showed that a significant amount of Hg metal was found on the vessel bottom at the end of tests. Material balance closure improved from 12-71% to 48-93% when this segregated Hg was considered. The amount of Hg segregated as elemental Hg on the vessel bottom was 4-77% of the amount added. The highest recovery of mercury in the offgas system generally correlated with the highest retention of Hg in the slurry. Low retention in the slurry (high segregation on the vessel bottom) resulted in low recovery in the offgas system. High agitation rates appear to result in lower retention of mercury in the slurry. Both recovery of mercury in the offgas system and removal (segregation + recovery) from the slurry correlate with slurry consistency. Higher slurry consistency results in better retention of Hg in the slurry (less segregation) and better recovery in the offgas system, but the relationships of recovery and retention with consistency are sludge dependent. Some correlation with slurry yield stress and acid stoichiometry was also found. Better retention of mercury in the slurry results in better recovery in the offgas system because the mercury in the slurry is stripped more easily than the segregated mercury at the bottom of the vessel. Although better retention gives better recovery, the time to reach a particular slurry mercury content (wt%) is longer than if the retention is poorer because the segregation is faster. The segregation of mercury is generally a faster process than stripping. The stripping factor (mass of water evaporated per mass of mercury stripped) of mercury at the start of boiling were found to be less than 1000 compared to the assumed design basis value of 750 (the theoretical factor is 250). However, within two hours, this value increased to at least 2000 lb water per lb Hg. For runs with higher mercury recovery in the offgas system, the stripping factor remained around 2000, but runs with low recovery had stripping factors of 4000 to 40,000. DWPF data shows similar trends with the stripping factor value increasing during boiling. These high values correspond to high segregation and low retention of mercury in the sludge. The stripping factor for a pure Hg metal bead in water was found to be about 10,000 lb/lb. About 10-36% of the total Hg evaporated in a SRAT cycle was refluxed back to the SRAT during formic acid addition and boiling. Mercury is dissolved as a result of nitric acid formation from absorption of NO x . The actual solubility of dissolved mercury in the acidic condensate is about 100 times higher than the actual concentrations measured. Mercury metal present in the MWWT from previous batches could be dissolved by this acidic condensate. The test of the effect of higher SRAT condenser temperature on recovery of mercury in the MWWT and offgas system was inconclusive. The recovery at higher temperature was lower than several low temperature runs, but about the same as other runs. Factors other than temperature appear to affect the mercury recovery. The presence of chloride and iodide in simulants resulted in the formation of mercurous chloride and mercurous iodide, respectively, in the offgas system. Actual waste data shows that the chloride content is much less than the simulant concentrations. Future simulant tests should minimize the addition of chloride. Similarly, iodine addition should be eliminated unless actual waste analyses show it to be present; currently, total iodine is not measured on actual waste samples.

36 MATERIALS SCIENCE↗

DISSOLUTION OF PLUTONIUM METAL IN 8-10 M NITRIC ACID

The H-Canyon facility will be used to dissolve Pu metal for subsequent purification and conversion to plutonium dioxide (PuO 2 ) using Phase II of HB-Line. To support the new mission, the development of a Pu metal dissolution flowsheet which utilizes concentrated (8-10 M) nitric acid (HNO 3 ) solutions containing potassium fluoride (KF) is required. Dissolution of Pu metal in concentrated HNO 3 is desired to eliminate the need to adjust the solution acidity prior to purification by anion exchange. The preferred flowsheet would use 8-10 M HNO 3 , 0.015-0.07 M KF, and 0.5-1.0 g/L Gd to dissolve the Pu up to 6.75 g/L. An alternate flowsheet would use 8-10 M HNO 3 , 0.05-0.2 M KF, and 1-2 g/L B to dissolve the Pu. The targeted average Pu metal dissolution rate is 20 mg/min-cm 2 , which is sufficient to dissolve a “standard” 2250-g Pu metal button in 24 h. Plutonium metal dissolution rate measurements showed that if Gd is used as the nuclear poison, the optimum dissolution conditions occur in 10 M HNO 3 , 0.04-0.05 M KF, and 0.5-1.0 g/L Gd at 112 to 116 °C (boiling). These conditions will result in an estimated Pu metal dissolution rate of ~11-15 mg/min-cm 2 and will result in dissolution times of 36-48 h for standard buttons. The recommended minimum and maximum KF concentrations are 0.03 M and 0.07 M, respectively. The data also indicate that lower KF concentrations would yield dissolution rates for B comparable to those observed with Gd at the same HNO 3 concentration and dissolution temperature. To confirm that the optimal conditions identified by the dissolution rate measurements can be used to dissolve Pu metal up to 6.75 g/L in the presence of representative concentrations of Fe and Gd or B, a series of experiments was performed to demonstrate the flowsheets. In three of the five experiments, the offgas generation rate during the dissolution was measured and samples were analyzed for hydrogen gas (H 2 ). The use of 10 M HNO 3 containing 0.03-0.05 M KF, 0.5-1.0 g/L Gd, and 1.9 g/L Fe resulted in complete dissolution of the metal in 2.0-3.5 h. When B was used as the neutron poison, 10 M HNO 3 solutions containing 0.05-0.1 M KF, 1.9 g/L Fe, and 1 g/L B resulted in complete dissolution of the metal in 0.75-2.0 h. Dissolution rates estimated using data from the flowsheets demonstrations agreed reasonably well with the measured rates; although, a discrepancy was observed in the Gd system. The presence of 1 g/L Gd or B in the dissolving solution had about the same effect on the dissolution rate. The predominant Pu valence in the dissolving solution was Pu(IV). The concentration of Pu(VI) was evaluated by UV-visible spectroscopy and was estimated to be significantly less than 1 wt %. The offgas generation rates and H 2 concentrations measured in the offgas from experiments performed using 10 M HNO 3 containing 0.05 M KF, 1.9 g/L Fe and either 1 g/L Gd or B were approximately the same. These data support the conclusion that the presence of either 1 g/L Gd or B had the same general effect on the dissolution rate. The calculated offgas generation during the dissolutions was 0.6 mol offgas/mol of Pu. The H 2 concentration measured in the offgas from the dissolution using Gd as the neutron poison was approximately 0.5 vol %. In the B system, the H 2 ranged from nominally 0.8 to 1 vol % which is about the same as measured in the Gd system within the uncertainty of the analysis. The offgas generation rate for the dissolution performed using 10 M HNO 3 containing 0.03 M KF, 0.5 g/L Gd, and 1.9 g/L Fe was approximately a factor of two less than produced in the other dissolutions; however, the concentration of H 2 measured in the offgas was higher. The adjusted concentration ranged from 2.7 to 8.8 vol % as the dissolution proceeded. Higher concentrations of H 2 occur when the Pu dissolution proceeds by a metal/acid reaction rather than nitrate oxidation. The higher H 2 concentration could be attributed to the reduced activity of the fluoride due to complexation with Pu as the dissolution progressed. Dissolution of Pu metal at 20 °C in 10 M HNO 3 containing 0.05 M KF showed that the Pu metal dissolves slowly without any visible gas generation. As the Pu metal dissolves, it forms a more-dense Pu-bearing solution which sank to the bottom of the dissolution vessel. The dissolved Pu did not form a boundary layer around the sample and failed to distribute homogeneously due to minimal (thermally-induced) mixing. This indicates that in the H-Canyon dissolver insert, the Pu will diffuse out of the insert into the bulk dissolver solution where it will disperse. At 35 °C, the Pu metal dissolved without visible gas generation. However, due to thermal currents caused by maintaining the solution at 35 °C, the dissolved Pu distributed evenly throughout the dissolver solution. It did not form a boundary layer around the sample.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of Changes to the MTR Fuel Dissolution Flowsheet to Increase the Number of L-Bundles Charged to a Dissolver

Material Test Reactor (MTR) fuels are dissolved in the H-Canyon facility using a Hg-catalyzed, HNO₃ dissolution flowsheet. The flowsheet is based on experimental work in which laboratory-scale experiments were used to provide bounding values for both offgas and H₂ generation rates. The generation of H₂ gas, primarily from the dissolution of Al, is controlled by limiting the surface area exposed to the solution. The number of L-Bundles charged and their submergence level defines the exposed surface area which is directly proportional to the H₂ generation rate. For the MTR fuel dissolution flowsheet, the maximum number of L-Bundles which can be charged to a dissolver was specified as a function of the Al concentration in the solution and the submergence level of the bundle. The MTR fuels are currently dissolved in the 6.1D dissolver. To reach the desired terminal Al concentration, a total of 12 L-Bundles of fuel are dissolved per batch. Depending on the submergence level being used in the dissolver, the 12 bundles are dissolved in three charges of four bundles per charge or in a sequence of three, four, and five bundles. However, if six L-Bundles could be dissolved in the initial charge, a dissolver batch could be completed in two dissolutions instead of three. To assess the feasibility of dissolving six bundles in the first charge, the Savannah River National Laboratory evaluated changes to the MTR flowsheet which increase the number of bundles which can be charged to a dissolver. Since the development of the existing MTR fuel dissolution flowsheet, improved offgas measurement methods have been developed to more accurately calculate the offgas composition and generation rate during laboratory-scale dissolutions. In the first part of this study, improvements in the calibration model for the Raman spectrometer (used for offgas characterization) and a more effective data smoothing routine were applied to existing data. The uncertainty in the offgas composition data used to define the MTR fuel dissolution flowsheet were subsequently re-evaluated which resulted in an approximate 50% reduction in the uncertainty of the H₂ gas concentration measurements. The reduced uncertainty was used in new calculations to define the maximum number of L-Bundles which can be charged to either the 6.1D or 6.4D dissolver as a function of the Al concentration. With the reduced uncertainty in the H₂ concentration measurements, a flowsheet was defined which supported initially charging 6 bundles to a dissolver. This flowsheet is based on the use of 0.002 M Hg, an L-Bundle immersion depth of 54 in., an air sparge/purge flowrate of 40 scfm, an iodine reactor operating temperature of 200 °C, and not exceeding 60% of the H₂ LFL in the dissolver offgas. In the second phase of this study, calculations were performed to assess the impact of changing various operating parameters to increase the number of L-Bundles charged to an H-Canyon dissolver. Applying the improved offgas measurement techniques including the reduced uncertainty in the H₂ concentration measurements to the existing data, the number of bundles of MTR fuel which can be charged to either the 6.1D or 6.4D dissolver were calculated based on varying the bundle immersion depth (44-60 in.), air sparge/purge flowrate (40-60 scfm), iodine reactor operating temperature (150-200 °C), and the percentage of the H₂ LFL which must not be exceeded (60-76%). Qualitatively, the percentage of the LFL had the largest influence on the maximum number of bundles which can be charged to a dissolver followed by the air sparge/purge flowrate, L-Bundle immersion depth, and the iodine reactor operating temperature. During the evaluation of each variable, the other variables were held at the baseline flowsheet conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Modeling and Analysis of Coupled Flow Through Packed Beds as a Diagnostic Tool for Packed Bed Reactor Health - 17172

The US Department of Energy, Office of River Protection, is building the Waste Treatment and Immobilization Plant (WTP) in Richland, Washington, to immobilize the hundreds of millions of liters of radioactive waste stored at the Hanford Site in Washington state. The offgas generated during vitrification of these wastes requires treatment to remove and/or destroy chemical and radioactive hazardous components before release to the atmosphere. In particular, volatile and semi-volatile hydrocarbon components are to be catalytically oxidized to carbon dioxide and water, whereas nitrogen oxides (NOx) are to be catalytically reduced to nitrogen and water. These tasks are accomplished in a series of packed bed reactors. Achieving the requisite Destruction/Removal Efficiency (DRE) for each of the tracked components is highly dependent on the flow characteristics of the offgas through the packed beds. The flow kinetics may be monitored and characterized during the initial warm-up of the system. The gases, initially at 76 deg. C (169 deg. F), (a) flow through one side of a countercurrent heat exchanger to recover heat from the exiting gases (which have already passed through the catalytic beds), (b) are then further heated electrically to approximately 400 deg. C (750 deg. F; the preferred operating temperature of the Thermo Catalytic Oxidizer (TCO)), (c) pass through the TCO where the reduced components of the offgas are oxidized over a supported Pt catalyst bed, (d) are partially cooled to approximately 315 deg. C (600 deg. F) by addition of approximately 25% (by weight) diluted ammonia/air mixture, (e) pass through the Selective Catalytic Reducer (SCR) where the NOx components are converted to N{sub 2} and H{sub 2}O over a supported V2O{sub 5}/TiO{sub 2} catalyst bed, and (f) exit through the hot side of the countercurrent heat exchanger. The electrical heater is not powerful enough to raise the temperature of the offgas to the desired 400 deg. C without the contribution of the heat recovered in the heat exchanger. Moreover, the thermal mass of the beds and housings of the TCO and SCR require a significant input of thermal energy to reach the desired operating temperatures; the better part of a day is required to bring the unit from ambient temperatures to operating temperatures. Therefore, the temperature of the stream during the initial warm-up of the system at each point in the system is dependent upon the thermal mass, flow dispersion, and permeability of the components, quantified as characteristic/representative volumes and residence times. By monitoring the temperature of the offgas as it enters and exits each portion of the system during this warm-up period one may model the system as a series of small Continuously Stirred Tank Reactors (CSTR)s (referred to as 'CSTRlets') to explain the flow kinetics through the catalyst beds. These component CSTRlets are adjustable in size and number, that one may model the flow profile of the gases through the catalyst beds. For example, a single large CSTR will present an effluent temperature profile with a simple exponential decay shape. Concatenating more CSTRlets generate more complex sigmoidal responses. Concatenating one CSTRlet significantly larger than the others in the train also alters the shape of the effluent temperature profile, in a fashion not replicable by a train of equal-sized CSTRlets. The ultimate goal is to accurately emulate the entire system as a representative CSTRlet train. Once accomplished, this characterization may be used in subsequent warm-ups (following shutdown for catalyst maintenance, for example) or by an intentional step change in inlet offgas temperature to detect/diagnose anomalies in flow through the beds (e.g., channeling or partial blockage.) This work presents development of this model through analytical, calculational, and empirical means. - The analytic model is accomplished by Laplace transform analysis of each component to recover component process transfer functions. - The calculational portion is performed via brute force finite element calculation. - Fitting empirical data from the warm-up of the TCO skid allows one to select the hypothetical CSTRlet trains which best fit the TCO and SCR beds for the analytical and finite element calculations. The first portion of this paper presents the development of the analytical (Laplace space) model of the coupled system. Estimated values for the initial temperature, mass, specific heat, electrical heat, and relative quantities of the offgas, catalyst beds, stainless steel housings, and ammonia dilution stream are used to generate expected temperature profiles at several selected junctures of the system. The number and size of the component hypothetical CSTRlets are calculated from the analytical model and are used to predict temperature profiles at the exit of the system and at intermediate junctions between system components (where thermocouples are present in the actual unit.) The finite element calculations employ a series of CSTRlet volumes to produce a similar suite of temperature profiles, for comparison with the analytical model results. Finally, empirical data from the Factory Acceptance Test system warm-up are used to select and compare the results from each modeling strategy to select the CSTRlet train(s) which best model the behavior of the actual system. This work presents a novel method of system component characterization, of value to the WTP plant and similar vitrification facilities as well as chemical process industries unrelated to waste management. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Tracking the Key Constituents of Concern of the WTP LAW Stream

The testing results presented in the present report were also obtained on a DM10 melter system operated with the primary WTP LAW offgas system components with recycle, as specified in the statement of work (SOW) [6] and detailed in the Test Plan for this work [7]. The primary offgas system components include the SBS, the WESP, and a recycle system that allows recycle of liquid effluents back to the melter, as in the present baseline for the WTP LAW vitrification. The partitioning of technetium and other key constituents between the glass waste form, the offgas system liquid effluents, the offgas stream that exits the WESP, and the liquid condensate from the vacuum evaporator were quantified in this work. The tests employed three different LAW streams spanning a range of waste compositions anticipated for WTP. Modifications to the offgas system and operational strategy were made to expedite the approach to steady state concentrations of key constituents in the glass and offgas effluent solutions during each test.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nitric-glycolic flowsheet evaluation with the slurry-fed melt rate furnace

The Savannah River National Laboratory (SRNL) was tasked to support validation of the Defense Waste Processing Facility (DWPF) melter offgas flammability model for the nitric-glycolic (NG) flowsheet. The work supports Deliverable 4 of the DWPF & Saltstone Facility Engineering Technical Task Request (TTR)1 and is supplemental to the Cold Cap Evaluation Furnace (CEF) testing conducted in 2014.2 The Slurry-fed Melt Rate Furnace (SMRF) was selected for the supplemental testing as it requires significantly less resources than the CEF and could provide a tool for more rapid analysis of melter feeds in the future. The SMRF platform has been used previously to evaluate melt rate behavior of DWPF glasses, but was modified to accommodate analysis of the offgas stream. Additionally, the Melt Rate Furnace (MRF) and Quartz Melt Rate Furnace (QMRF) were utilized for evaluations. MRF data was used exclusively for melt behavior observations and REDuction/OXidation (REDOX) prediction comparisons and will be briefly discussed in conjunction with its support of the SMRF testing. The QMRF was operated similarly to the SMRF for the same TTR task, but will be discussed in a separate future report. The overall objectives of the SMRF testing were to; 1) Evaluate the efficacy of the SMRF as a platform for steady state melter testing with continuous feeding and offgas analysis; and 2) Generate supplemental melter offgas flammability data to support the melter offgas flammability modelling effort for DWPF implementation of the NG flowsheet.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Vitrification of Hanford Tank 241-AP-101 Waste and Simulant

Hanford tank 241-AP-101 (referred to herein as AP-101) is the second Hanford radioactive tank waste planned to be processed and vitrified. A simulant version of AP 101 waste was formulated from the best-basis inventory (BBI) for the Hanford Tank 241-AP-101 liquid with an assumed target dilution of the waste from the BBI sodium molarity of 8.61 M to the desired 5.5 M Na. After the addition of glass-forming chemicals (GFCs), the simulant melter feed was processed in a non-radioactive, continuous laboratory-scale melter (CLSM) system. The AP-101 simulant melter feed was charged into the CLSM for 6.11 h of processing, which produced 6.55 kg of glass, for an average glass production rate of 2275 kg m 2 d -1 . Since there were no processing issues with the AP-101 simulant melter feed, AP-101 melter feed made with actual waste was then processed in a CLSM system built into a contamination area in a radioactive environment. The melting behavior characteristics appeared similar for both the simulant and waste melter feeds. The AP-101 waste melter feed was charged into the CLSM for 12.14 h of processing, which produced 8.75 kg of glass, for an average glass production rate of 1530 kg m 2 d -1 . During the AP-101 waste melter feed charging, the pump used to move the feed reached a maximum and it is believed that if the pump had a greater capacity, a greater average glass production rate could have been achieved. A constituent of interest present in low quantities in the AP-101 waste is 99 Tc or its non-radioactive surrogate, Re, added to the AP-101 simulant. Analysis for the quantities of 99 Tc and Re in the AP-101 glass product resulted in an average single-pass retention from the melter feed during relative chemical steady state of 55 ± 2 % for 99 Tc and 45 ± 2 % for Re. Compared to the processing of other melter feeds, the retention of 99 Tc in the AP-101 glass was greater than in both AP-107 and AP-105 glass, while the retention of Re in the AP-101 was less than in the AP-107 glass, but greater than in the AP-105 glass. A spike of I was added into the AP-101 melter feed that could be detected above the analysis detection limits. However, the iodine was only detectable above the ~6 ppm limit in one glass pour: the pour immediately following the burn off of the cold cap, where the I level reached ~30 ppm. This event was significant because the glass was poured immediately after burn off and thus it is presumed that the iodine had yet to volatilize from the glass melt while idling. It is recommended to perform future tests with I spikes at greater levels so that it can be detected in additional glass pours to determine if the expected 50 % retention of I used in the Kim et al. glass models can be confirmed. Offgas liquid samples were analyzed for acetonitrile, which was present at greater concentrations in CLSM liquids than in other scaled melter systems. This result was expected based on unique conditions with the CLSM system including a small plenum space leading to low residence time for offgas and the rapidity of offgas cooling upon exiting the CLSM vessel due to the location and environment. About 90 % of the total acetonitrile captured during both the AP-101 simulant and waste CLSM runs was found in the offgas condensate and demister liquids, thus it is recommended that only those liquids be sent for analysis if future testing to study the presence of acetonitrile in offgas products is desired.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Dissolution Flowsheet for High Flux Isotope Reactor Fuel

As part of the Spent Nuclear Fuel (SNF) processing campaign, H-Canyon is planning to begin dissolving High Flux Isotope Reactor (HFIR) fuel in late FY17 or early FY18. Each HFIR fuel core contains inner and outer fuel elements which were fabricated from uranium oxide (U 3 O 8 ) dispersed in a continuous Al phase using traditional powder metallurgy techniques. Fuels fabricated in this manner, like other SNF’s processed in H-Canyon, dissolve by the same general mechanisms with similar gas generation rates and the production of H 2 . The HFIR fuel cores will be dissolved and the recovered U will be down-blended into low-enriched U. HFIR fuel was previously processed in H-Canyon using a unique insert in both the 6.1D and 6.4D dissolvers. Multiple cores will be charged to the same dissolver solution maximizing the concentration of dissolved Al. The objective of this study was to identify flowsheet conditions through literature review and laboratory experimentation to safely and efficiently dissolve the HFIR fuel in H-Canyon. Laboratory-scale experiments were performed to evaluate the dissolution of HFIR fuel using both Al 1100 and Al 6061 T6 alloy coupons. The Al 1100 alloy was considered a representative surrogate which provided an upper bound on the generation of flammable (i.e., H 2 ) gas during the dissolution process. The dissolution of the Al 6061 T6 alloy proceeded at a slower rate than the Al 1100 alloy, and was used to verify that the target Al concentration in solution could be achieved for the selected Hg concentration. Mass spectrometry and Raman spectroscopy were used to provide continuous monitoring of the concentration of H 2 and other permanent gases in the dissolution offgas, allowing the development of H 2 generation rate profiles. The H 2 generation rates were subsequently used to evaluate if a full HFIR core could be dissolved in an H-Canyon dissolver without exceeding 60% of the calculated lower flammability limit (LFL) for H 2 at a given Hg concentration. Complete dissolution of the Al 1100 and Al 6061 T6 alloys up to a final Al concentration of 2 M was obtained using a 7 M HNO 3 solution containing a 0.002 M Hg catalyst. However, following the dissolutions, solids were observed in the solution. The solids were amorphous, but likely originated from the Si present in the alloys. No crystalline materials, such as Al(NO 3 ) 3 were observed. During the course of the dissolution experiments, it was determined that delaying the addition of Hg once the HNO 3 solution reached the boiling point can reduce the total offgas and H 2 generation rates. The delay in starting the Hg addition is not necessary for HFIR fuel dissolution, but could be useful in other research reactor dissolution campaigns. The potential to generate flammable concentrations of H 2 in the offgas during a HFIR fuel dissolution was evaluated using the experimental data. The predicted H 2 concentration in the dissolver offgas stream was compared with 60% of the calculated H 2 LFL at 200 °C using several prototypical experiments. The calculations showed that a full HFIR core can be dissolved using nominally 0.002 M Hg to catalyze the dissolution. The margin between the predicted H 2 concentration and the calculated LFL was greater when the solution was allowed to boil for 45 min prior to initiating the Hg addition. When the Hg was increased to 0.004 M, the predicted H 2 concentration exceeded the calculated LFL early in the dissolution. The dissolution experiments also demonstrated that additional Hg (beyond the initial 0.002 M) could be added as the Al concentration increases. The ability to add more Hg during a HFIR fuel dissolution could be beneficial if slow dissolution rates are observed at high Al concentrations. Experimental data were used to demonstrate that the predicted H 2 concentration in a dissolver was below 60% of the calculated LFL at 200 °C when 0.004 M Hg was used to catalyze the dissolution if the Al concentration is conservatively greater than 0.5 M. Data also show that the Hg concentration during a HFIR fuel dissolution can be increased from 0.002 to 0.008 M at an Al concentration of 1.3 M.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Antifoam Development for Eliminating Flammability Hazards and Decreasing Cycle Time in the Defense Waste Processing Facility

The Savannah River National Laboratory (SRNL) was requested to develop a new antifoam control method for the Defense Waste Processing Facility’s (DWPF) Chemical Process Cell (CPC). SRNL completed testing of both chemical and nonchemical foam controls. The nonchemical foam controls were either ineffective (or worse, created more foam) or impractical (a water spray can control foam, but excessive water is needed). As a result, the focus of this study was on finding a superwetter or commercial antifoam for controlling foam. Thirty potential antifoams were tested as part of this study. A series of tests were developed to help screen out ineffective alternatives including: 1. Spreading testing of superspreaders, 2. Foam column testing with physical simulants, 3. Boiling testing with physical and chemical simulants, 4. Days-only Sludge Receipt and Adjustment Tank (SRAT) process simulations with sludge (containing noble metals and mercury), Precipitate Reactor Feed Tank (PRFT), and Slurry Mix Evaporator Feed Tank (SEFT) simulants in the RC1 Reaction Calorimeter (purchased for antifoam testing), and 5. Around-the-clock SRAT and Slurry Mix Evaporator (SME) process simulations with sludge(containing noble metals and mercury), PRFT, and SEFT simulants in the RC1 Reaction Calorimeter. Evonik Surfynol® MD20, a commercially available defoamer, was relatively effective in controlling foam, while remaining chemically stable in SRAT and SME processing across the pH range of 4 to 13. No degradation products were detected in the offgas, in the condensate or in the SRAT and SME products. In nitric-glycolic acid flowsheet testing, 250 mg/kg Evonik Surfynol® MD20 was needed for foam control compared to 1,625 mg/kg for Antifoam 747, DWPF’s current antifoam. In nitric-formic acid flowsheet testing, 1,125 mg/kg of Evonik Surfynol® MD20 was needed to control foam throughout the SRAT and SME cycles. The commercially available superspreader Momentive™ Y-17112 was even more effective than Evonik Surfynol® MD20 as both a defoamer and an antifoam. Not only was the foam destroyed upon addition but also was less persistent between additions. It was the most effective antifoam in testing using both the nitric-glycolic acid flowsheet and the nitric-formic acid flowsheet. In nitric-glycolic acid flowsheet testing, only 100 mg/kg Momentive™ Y-17112 was needed to control foam throughout the SRAT and SME cycles. In nitric-formic acid flowsheet testing, 300 mg/kg Momentive™ Y-17112 was needed to control foam throughout the SRAT and SME cycles. Momentive™ Y-17112 is also resistant to hydrolysis as demonstrated by its chemical stability in SRAT and SME processing across the pH range of 4 to 13 and lack of degradation products in offgas or condensate. Both candidates were effective as potential replacements for Antifoam 747, with Y-17112 demonstrating superior foam control. During nitric-glycolic flowsheet testing 50% less antifoam was needed when using Momentive™ Y-17112 compared to MD20. During nitric-formic flowsheet testing 75% less antifoam was needed when using Momentive™ Y-17112 compared to MD20. Foam remediated with Momentive™ Y-17112 was less persistent throughout testing. In addition, no degradation products were detected in the offgas, in the condensate or in the SRAT and SME products. Based on this testing, Momentive™ Y-17112 is clearly superior to Evonik Surfynol® MD20 and Antifoam 747, especially for the nitric-formic acid flowsheet processing; it is recommended that Momentive™ Y-17112 replace Antifoam 747 in DWPF. An antifoam addition strategy is recommended for both the nitric-glycolic acid flowsheet and the nitric-formic acid flowsheet. Implementation of Momentive™ Y-17112 is expected to decrease SRAT and SME boiling times by up to 50%, eliminate the issues resulting from Antifoam 747 degradation products, and minimize foamovers. To validate the effectiveness of these defoaming agents, SRNL recommends irradiation of a SRAT or SME product simulant containing fresh antifoam. The goal of this testing is to determine whether the irradiation causes decomposition of the antifoam that would make it less effective or produce new species in the offgas or slurry. This testing began in April 2020. An evaluation should be completed to determine the thermolytic hydrogen and methane generation rate in downstream equipment, including the High-Level Waste evaporators.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗