Search NASA⌕ Search

SEARCH · Search NASA

Results for “particle cracking”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Stochastic 3D reconstruction of cracked polycrystalline NMC particles using 2D SEM data

Li-ion battery performance is strongly influenced by the 3D microstructure of its cathode particles. Cracks within these particles develop during calendaring and cycling, reducing connectivity but increasing reactive surface, making their impact on battery performance complex. Understanding these contradictory effects requires a quantitative link between particle morphology and battery performance. However, informative 3D imaging techniques are time-consuming, costly and rarely available, such that analyses often have to rely on 2D image data. This paper presents a novel stereological approach for generating virtual 3D cathode particles exhibiting crack networks that are statistically equivalent to those observed in 2D sections of experimentally measured particles. Consequently, 2D image data suffices for deriving a full 3D characterization of cracked cathodes particles. Such virtually generated 3D particles could serve as geometry input for spatially resolved electro-chemo-mechanical simulations to enhance our understanding of structure-property relationships of cathodes in Li-ion batteries.

36 MATERIALS SCIENCE↗

Multiscale Modeling of Damage Processes in Aluminum Alloys: Grain-Scale Mechanisms

This paper has two goals related to the development of a physically-grounded methodology for modeling the initial stages of fatigue crack growth in an aluminum alloy. The aluminum alloy, AA 7075-T651, is susceptible to fatigue cracking that nucleates from cracked second phase iron-bearing particles. Thus, the first goal of the paper is to validate an existing framework for the prediction of the conditions under which the particles crack. The observed statistics of particle cracking (defined as incubation for this alloy) must be accurately predicted to simulate the stochastic nature of microstructurally small fatigue crack (MSFC) formation. Also, only by simulating incubation of damage in a statistically accurate manner can subsequent stages of crack growth be accurately predicted. To maintain fidelity and computational efficiency, a filtering procedure was developed to eliminate particles that were unlikely to crack. The particle filter considers the distributions of particle sizes and shapes, grain texture, and the configuration of the surrounding grains. This filter helps substantially reduce the number of particles that need to be included in the microstructural models and forms the basis of the future work on the subsequent stages of MSFC, crack nucleation and microstructurally small crack propagation. A physics-based approach to simulating fracture should ultimately begin at nanometer length scale, in which atomistic simulation is used to predict the fundamental damage mechanisms of MSFC. These mechanisms include dislocation formation and interaction, interstitial void formation, and atomic diffusion. However, atomistic simulations quickly become computationally intractable as the system size increases, especially when directly linking to the already large microstructural models. Therefore, the second goal of this paper is to propose a method that will incorporate atomistic simulation and small-scale experimental characterization into the existing multiscale framework. At the microscale, the nanoscale mechanics are represented within cohesive zones where appropriate, i.e. where the mechanics observed at the nanoscale can be represented as occurring on a plane such as at grain boundaries or slip planes at a crack front. Important advancements that are yet to be made include: 1. an increased fidelity in cohesive zone modeling; 2. a means to understand how atomistic simulation scales with time; 3. a new experimental methodology for generating empirical models for CZMs and emerging materials; and 4. a validation of simulations of the damage processes at the nano-micro scale. With ever-increasing computer power, the long-term ability to employ atomistic simulation for the prognosis of structural components will not be limited by computation power, but by our lack of knowledge in incorporating atomistic models into simulations of MSFC into a multiscale framework.

Hochhalter, J. D.↗

Quantifying precursors to void nucleation and coalescence in aluminum

Ductile rupture is a common failure mode for engineering alloys. It is generally comprised of three mechanisms: void nucleation at secondary particles, void growth, and coalescence of voids. Conventional models for ductile rupture have limited precision for predicting macroscopic failure. This is partially because they have been corroborated using ex-situ observations of these three mechanisms and calibrated by macroscopic strain or stress metrics. In this study, in-situ high-energy X-ray characterization was conducted to correlate sites of void nucleation via particle cracking and sites of void growth with grain-scale metrics. Here it is shown that particle cracking is not predicated by elevated stress metrics, which disagrees with classical models. Instead, particle cracking tended to occur for the largest, least spherical particles. This trend persisted on the aggregate-scale and within individual neighborhoods around particles. Furthermore, an Eshelby analysis illuminated a statistically significant increase in maximum principal stress within a cracked particle, compared to an uncracked particle. In-situ observations also revealed two separate examples of intragranular void growth comprised of flat, crack-like features that grew showing alignment with slip systems of the highest resolved shear stress. Post-mortem fractography revealed a secondary population of dimples on these crack-like features, implying that void sheeting may be occurring during this crack-like void growth. Furthermore, these in-situ observations imply that classical models for void growth, that assume a homogenous medium, should be extended to account for the anisotropic grain-level behavior to correctly capture distinct features of void nucleation and growth.

Al-2219↗

Degradation Pathways of Cobalt–Free LiNiO 2 Cathode in Lithium Batteries

Electrode-electrolyte reactivity (EER) and particle cracking (PC) are considered two main causes of capacity fade in high-nickel layered oxide cathodes in lithium-based batteries. However, whether EER or PC is more critical remains debatable. Herein, the fundamental correlation between EER and PC is systematically investigated with LiNiO 2 (LNO), the ultimate cobalt-free lithium layered oxide cathode. Specifically, EER is found more critical than secondary particle cracking (SPC) in determining the cycling stability of LNO; EER leads to primary particle cracking, but mitigates SPC due to the inhibition of H2-H3 phase transformation. Two surface degradation pathways are identified for cycled LNO under low and high EERs. A common blocking surface reconstruction layer (SRL) containing electrochemically-inactive Ni 3 O 4 spinel and NiO rock-salt phases is formed on LNO in an electrolyte with a high EER; in contrast, an electrochemically-active SRL featuring regions of electron- and lithium-ion-conductive LiNi 2 O 4 spinel phase is formed on LNO in an electrolyte with a low EER. These findings unveil the intrinsic degradation pathways of LNO cathode and are foreseen to provide new insights into the development of lithium-based batteries with a minimized EER and a maximized service life.

25 ENERGY STORAGE↗

Coupling of multiscale imaging analysis and computational modeling for understanding thick cathode degradation mechanisms

Here, using a thick NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ) electrode as an example, we present a macro- to nanoscale 2D and 3D imaging analysis approach coupled with 4D (space + time) computational modeling to probe its degradation mechanism in a lithium-ion battery cell. Particle cracking increases and contact loss between particles and carbon-binder domain are observed to correlate with the cell degradation. This study unravels that the reaction heterogeneity within the thick cathode caused by the unbalanced electron conduction is the main cause of the battery degradation over cycling. The increased heterogeneity in the system will entail more cathode regions where the degree of active material utilization is uneven, leading to higher probabilities of particle cracking. These findings shed light on the crucial role of the electronic and ionic transportation networks in the performance deterioration of the thick cathode. They also provide guidance for cathode architecture optimization and performance improvement.

25 ENERGY STORAGE↗

Deconstructing the High Voltage Degradation Mechanisms in Na 2/3 Ni 1/3 Mn 2/3 O 2 with Single Crystals and Advanced Electrolyte

Abstract Sodium layered oxide cathodes can uniquely benefit from the existing lithium‐ion battery industry as sodium‐ion batteries gain traction as a potential low‐cost, drop‐in replacement. However, achieving relevant energy density with a suitable cycle life remains a challenge for sodium layered oxides. At high operating potentials, several competing degradation mechanisms prevent P2‐type Na 2/3 Ni 1/3 Mn 2/3 O 2 (≈550 Wh kg −1 ) from achieving meaningful cycle life—with bulk structural instability and surface reactivity being the primary retractors. Herein, the issue of particle cracking is addressed through detailed synthesis methods of “single‐crystal” materials. By comparison to a polycrystalline baseline, the single‐crystal materials quantify the capacity loss due to isolation of active material caused by intergranular particle cracking. The single crystal materials are then employed in cells with an advanced, “localized saturated electrolyte” (LSE) to demonstrate the magnitude of capacity loss due to electrolyte decomposition at the cathode surface. Mitigation of the surface reactivity through the LSE electrolyte effectively demonstrates the elevated importance of surface reactivity at high voltages despite the onset of egregious particle cracking. This work aims to guide future research into understanding molten‐salt assisted syntheses and advance the debate on surface versus bulk degradation.

Darga, Joe↗

Rational design of mechanically robust Ni-rich cathode materials via concentration gradient strategy

Mechanical integrity issues such as particle cracking are considered one of the leading causes of structural deterioration and limited long-term cycle stability for Ni-rich cathode materials of Li-ion batteries. Indeed, the detrimental effects generated from the crack formation are not yet entirely addressed. Here, applying physicochemical and electrochemical ex situ and in situ characterizations, the effect of Co and Mn on the mechanical properties of the Ni-rich material are thoroughly investigated. As a result, we successfully mitigate the particle cracking issue in Ni-rich cathodes via rational concentration gradient design without sacrificing the electrode capacity. Our result reveals that the Co-enriched surface design in Ni-rich particles benefits from its low stiffness, which can effectively suppress the formation of particle cracking. Meanwhile, the Mn-enriched core limits internal expansion and improve structural integrity. The concentration gradient design also promotes morphological stability and cycling performances in Li metal coin cell configuration.

36 MATERIALS SCIENCE↗

Cracking vs. surface reactivity in high-nickel cathodes for lithium-ion batteries

High-nickel layered oxide cathodes LiNi x Mn y Co z O 2 (NMC) experience microcracks during cycling. This can expose fresh cathode surfaces for parasitic reactions and isolate active cathode material from the conductive electrode matrix, resulting in impedance increase and capacity fade. The commonly held belief attributes microcracks to anisotropic lattice volume changes of primary particles during cycling. Nevertheless, recent reports suggest that certain electrolytes might reduce microcracks in NMC cathodes during deep cycling. This raises a crucial question on the origin of microcracks: do microcracks exacerbate surface stability, or does poor surface stability contribute to microcrack formation? This perspective aims to provide context and expound this “chicken or egg” dilemma. We contend that the consequence of surface reactivity on the cycle life of high-Ni cathodes is more pronounced than that of particle cracking. Here, we hypothesize that particle cracking is more of a symptom of severe surface reactivity rather than a cause of capacity fade.

25 ENERGY STORAGE↗

Investigation of the plastic fracture of high-strength aluminum alloys

In a study of plastic fracture in five high-strength aluminum alloys (2014, 2024, 2124, 7075, and 7079), it has been shown that fracture toughness is affected primarily by the size and volume fraction of the larger (2 to 10 microms) second-phase particles. Certain of these particles crack at small plastic strains, nucleating voids which, with further plastic strain, coalesce to cause fracture. Not all second-phase particles crack at small plastic strains, and qualitative analysis of those which are primarily responsible for void nucleation shows that they contain iron or silicon or both. This result suggests that a reduction in the iron and silicon impurity content of the alloys should improve fracture toughness without loss of strength.

Van Stone, R. H.↗

Effects of aging condition on the fracture toughness of 2XXX and 7XXX series aluminum alloy composites

Results are presented on the effects of matrix aging condition (i.e., matrix temper) on the fracture toughness of 2XXX and 7XXX Al matrix alloys reinforced with SiC particulates, and the results are compared with the mechanical behavior. Fracture toughness testing was conducted on fatigue precracked bend specimens, and fracture surfaces were examined using SEM. Results revealed dramatic differences in the effect of matrix microstructure on the fracture properties of the two composite series. In the 7XXX material, the toughness values decreased from the underaged (UA) condition to the overaged (OA) condition by approximately 40 percent, while in the 2XXX series composite, the effect of matrix microstructure was marginal. In the 7XXX series composites, a transition in fracture mode from particle cracking (in UA) to matrix and linear-interface failure (in OA) was observed, while the 2XXX series composite failed predominantly by particle cracking.

Manoharan, M.↗

Surface Stabilization with Fluorine of Layered Ultrahigh-Nickel Oxide Cathodes for Lithium-Ion Batteries

High-nickel layered oxide cathodes are key to meet the demands of the electric vehicle industry because of their high specific capacity. However, commercialization of these materials is hindered by critical challenges, such as phase transitions, particle cracking, aggressive surface reactivity, and thermal instability. Cation doping along with surface coating has proven to be an effective way to circumvent some of these issues to a large extent. Herein, fluorine coating is employed on a high-nickel Li[Ni 0.95 Mn 0.015 Co 0.02 Al 0.01 Mg 0.005 ]O 2 (NMCAM) cathode via a solution route. Detailed structural and electrochemical analyses indicate fluorine largely decorates the surface at low enough calcination temperatures. The cathode with 1 mol % fluorine coating exhibits a capacity retention of 71% after 500 cycles as compared to 59% for the control sample when cycled to a high cutoff voltage of 4.3 V in a full cell configuration with graphite anode. Post-mortem analysis of cycled electrodes reveals that surface reactivity is a major contributor to capacity fade as compared to particle cracking. Fluorine coating reduces surface reactivity and the depth to which rock-salt phase is formed on the surface during cycling. The thermal stability is also enhanced after fluorine coating as the material shows less heat release at high states of charge. Furthermore, this work demonstrates an effective, economical, and scalable way to stabilize the surface with fluorine and enhance the electrochemical performance of high-nickel cathodes.

25 ENERGY STORAGE↗

Intralattice-bonded phase-engineered ultrahigh-Ni single-crystalline cathodes suppress strain evolution

Single crystallization remains a debated strategy for advancing Ni-rich cathode materials. While it mitigates particle cracking and improves tap density by eliminating particle boundaries, extended diffusion pathways introduce volumetric and lattice distortions, compromising electrochemical and structural stability. These challenges hinder the commercialization of high-Ni single-crystal cathodes, calling for a reassessment of their viability. Here, in this study, we report a structural design: intralattice-bonded phase single-crystal LiNi 0.92 Co 0.03 Mn 0.05 O 2 (IBP-SC92). This architecture maintains structural integrity while shortening diffusion pathways, resulting in almost zero electrochemical degradation during cycling. The robust structure and fast ion transport mitigate lattice strain, as confirmed by multiscale high-resolution diffraction and imaging techniques, preventing intragranular cracks and irreversible phase transitions. As a result, IBP-SC92 shows outstanding cycling stability, with nearly 100% capacity retention after 100 cycles in half cells and 94.5% retention after 1,000 cycles in full cells. This redefined single-crystal cathode represents a significant step towards the industrial adoption of high-energy-density materials.

36 MATERIALS SCIENCE↗

Maximizing Calendering Effects Through the Mechanical Pulverization of Co-Free Nickel-Rich Cathodes in Lithium-Ion Cells

Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles.

25 ENERGY STORAGE↗

Effect of Si impurities on microstructure and tensile properties of a cast Al-Mg-Fe alloy

Al-Mg alloys are attractive for structural castings owing to their superior strength and ductility in the as-cast state. However, given the tight tolerance for impurities, Al-Mg alloys produced from secondary sources still face multiple challenges. Here, we report the effect of increased Si impurity (0.05–1.6 wt%), which is commonly found in secondary Al sources, on microstructure and tensile properties of a cast Al-4.3Mg-1.6Fe (wt%) alloy, commercially referred to as Castaduct-42 alloy. Microstructural characterization revealed that Si addition increased the volume fraction, size, and aspect ratio of primary Al13Fe4 intermetallic particles as well as the volume fraction of other binary and ternary eutectic phases. Tensile testing results demonstrated that increasing Si impurities from 0.05 to 1.6 wt% reduced ductility from 14.3 ± 1.4 % to 2.2 ± 1.0 %. A particle cracking damage accumulation model coupled with failure analysis indicated primary Al13Fe4 intermetallic particles to be the major contributing factor to the deterioration in ductility with increasing Si content. Additionally, the stabilizing effect of Si on primary Al 13 Fe 4 was inconsistent with the CALPHAD calculation results based on existing CALPHAD databases which predict a slightly decreasing primary Al13Fe4 phase fraction with increasing Si concentration. This work provides new insights into the phase stability and mechanical behavior of the lesser studied Al-Mg-Fe-Si alloy system that will contribute to the development of sustainable cast Al-Mg based alloys.

36 MATERIALS SCIENCE↗

The Mars Environmental Compatibility Assessment MECA Abrasion Tool

The Mars Environmental Compatibility Assessment (MECA) experiment, an instrument suite to be flown on Mars Surveyor 2001, will include a tool for doing simple mineralogical scratch and streak tests on particles from the Martian regolith. The Abrasion Tool will be applied to particles that adhere to highly polished substrates of various hardnesses. Granular soil components will be subjected to a compressive force of about 3 N using a leaf spring. The spring will be applied with a paraffin actuator capable of a 0.76 mm throw to achieve a maximum displacement of about 7.5 mm at the tip of the tool. The pressure per grain will be dependent on the grain size, the number of grains that adhere to the substrate and the number of grains in compression. The pressure per particle is expected to be on the order of 100 MPa - 1 GPa. The MECA sample wheel containing the substrates will be rotated after the particles are placed in compression to produce scratches or pits. A primary goal of the Abrasion Tool is to identify quartz (Mohs' hardness = 7) using substrates of varying hardnesses. Quartz is considered hazardous to future human explorers of Mars because it can cause silicosis of the lungs if it is of respirable size. It is also hazardous to machinery, structures, and space suits because of its ability to abrade and scratch surfaces. Since large quantities of minerals harder than quartz are not expected, any scratches produced on polished quartz substrates might be reasonably attributed to quartz particles, although there may be minerals such as impact metamorphic diamond in the soils. Careful calibration of the tool will be necessary to ensure that grains are not overloaded; for example, a steel ball pressed into glass will produce a Hertzian fracture, even though it is softer than glass. Other minerals, such as magnetite (Mohs'hardness = 6.5) have been shown to scratch glass ceramics such as Zerodur (Mohs' hardness = 6.5). Thus, minerals can be differentiated: note that regardless of the mineral species, if any particle is harder than 6.5 it will certainly be an interesting discovery for both planetary geology and human exploration concerns. The scratches will be identified using the 6X optical microscope and profiled with the atomic force microscope included in the MECA instrument suite. Analysis of the scratch morphology will yield evidence concerning the shape of the particle responsible for producing each scratch. For example, angular grains should leave vertical cracks with microconchoidal lateral chipping, while rounded grains might leave chattermarks, or nested partial Hertzian cracks. Particle shape can thus be inferred from these indentation modes, as well as material hardness. In addition, particle size information may also be available if pits caused by rolling particles can be identified. Converse to scratching, the minerals may be crushed at their contact points, and be smeared onto the target substrates to leave what geologists refer to as "streaks". These are coldwelded trails of mineral material that have structure and color indicative of mineral composition. The AFM will determine the morphology of these streaks, while the microscope will ascertain the color. On the harder substrates, we might expect streaking to dominate; on the softer substrates, scratching may dominate. Progressions of material interactions across the substrate selection will be a valuable source of data for mineral discrimination. It should also be noted that many minerals have coatings (such as iron oxides), and these will have to be differentiated from the host mineral grains; laboratory tests will establish the effects of such coatings on the scratch results. Finally, we note that the microscope will provide corroborative data regarding likely mineral species by grain shapes, fracture patterns, surface textures, colr, and UV fluorescence reactions.

Kuhlman, K. R.↗

The Mars Environmental Compatibility Assessment (MECA) Abrasion Tool

The Mars Environmental Compatibility Assessment (MECA) experiment, an instrument suite to be flown on Mars Surveyor 2001, will include a tool for doing simple mineralogical scratch and streak tests on particles from the Martian regolith. The Abrasion Tool will be applied to particles that adhere themselves to highly polished substrates of various hardnesses. Granular soil components will be subjected to a compressive force of about 3 N using a leaf spring. The spring will be applied with a paraffin actuator capable of a 0.76 mm throw to achieve a maximum displacement of about 7.5 mm at the tip of the tool. The pressure per grain will be dependent on the grain size, the number of grains that adhere to the substrate and the number of grains in compression. The pressure per particle is expected to be on the order of 100 MPa - 1 GPa. The MECA sample wheel containing the substrates will be rotated after the particles are placed in compression to produce scratches or pits. A primary goal of the Abrasion Tool is to identify quartz (Mohs' hardness = 7) using substrates of varying hardnesses. Quartz is considered hazardous to future human explorers of Mars because it can cause silicosis of the lungs if it is of respirable size. It is also hazardous to machinery, structures, and space suits because of its ability to abrade and scratch surfaces. Since large quantities of minerals harder than quartz are not expected, any scratches produced on polished quartz substrates might be reasonably attributed to quartz particles, although there may be minerals such as impact metamorphic diamond in the soils. Careful calibration of the tool will be necessary to ensure that grains are not overloaded; for example, a steel ball pressed into glass will produce a Hertzian fracture, even though it is softer than glass. Other minerals, such as magnetite (Mohs' hardness = 6.5) have been shown to scratch glass ceramics such as Zerodur (Mohs' hardness = 6.5). Thus, minerals can be differentiated: note that regardless of the mineral species, if any particle is harder than 6.5 it will certainly be an interesting discovery for both planetary geology and human exploration concerns. The scratches will be identified using the 6X optical microscope and profiled with the atomic force microscope included in the MECA instrument suite. Analysis of the scratch morphology will yield evidence concerning the shape of the particle responsible for producing each scratch. For example, angular grains should leave vertical cracks with microconchoidal lateral chipping, while rounded grains might leave chatter marks, or nested partial Hertzian cracks. Particle shape can thus be inferred from these indentation modes, as well as material hardness. In addition, particle size information may also be available if pits caused by rolling particles can be identified. Converse to scratching, the minerals may be crushed at their contact points, and be smeared onto the target substrates to leave what geologists refer to as "streaks". These are cold-welded trails of mineral material that have structure and color indicative of mineral composition. The AFM will determine the morphology of these streaks, while the microscope will ascertain the color. On the harder substrates, we might expect streaking to dominate; on the softer substrates, scratching may dominate. Progressions of material interactions across the substrate selection will be a valuable source of data for mineral discrimination. It should also be noted that many minerals have coatings (such as iron oxides), and these will have to be differentiated from the host mineral grains; laboratory tests will establish the effects of such coatings on the scratch results. Finally, we note that the microscope will provide corroborative data regarding likely mineral species by grain shapes, fracture patterns, surface textures, color, and UV fluorescence reactions. Additional information is contained in the original extended abstract.

Kuhlman, K. R.↗

Microstructurally based model of fatigue initiation and growth

A model to calculate fatigue life is developed based on the assumption that fatigue life is entirely composed of crack growth from an initial microstructural inhomogeneity. Specifically, growth is considered to start from either an ellipsoidal void, a cracked particle, or a debonded particle. The capability of predicting fatigue life from material microstructure is based on linear elastic fracture mechanics principles, the sizes of the crack-initiating microstructural inhomogeneities, and an initiation parameter that is proportional to the cyclic plastic zone size. A key aspect of this modeling approach is that it is linked with a general purpose probability program to analyze the effect of the distribution of controlling microstructural features within the material. This enables prediction of fatigue stress versus life curves for various specimen geometries using distributional statistics obtained from characterizations of the microstructure. Results are compared to experimental fatigue data from an aluminum alloy.

Brockenbrough, J. R.↗

Ni-Rich Li[Ni x MnyCo 1– x – y ]O 2 Single Crystals as Superior Fast Charge Cathodes for Lithium-Ion Batteries

The utilization of single-crystal (SC) Li[Ni x MnyCo 1-x-y ]O 2 (NMC) cathodes has facilitated unparalleled performance in commercial high-energy lithium-ion batteries (LIBs). In the current study, we evaluate the application of SC cathodes in fast charge (FC)-LIBs where particle cracking is a predominant failure mechanism. Ni-rich SC-NMC samples with various compositions, sizes, and shapes are synthesized and investigated for their influence on FC performance. We reveal the necessity of utilizing smaller SCs (<1 μm) as larger sizes (>2 μm) experience significant particle-level lithium concentration gradients under FC conditions. To improve lithium transport and minimize side reactivities, we strategically expose the (104) crystal facets on the surface. Exceptional performance was observed on an optimized SC-LiNi 0.80 Mn 0.05 Co 0.15 O 2 , delivering a discharge capacity of 165 mAh/g even after 150 cycles at 6C charge. Our study not only demonstrates the promise of SC-NMC but also provides the key insights for the design and optimization of advanced cathodes for FC-LIBs.

25 ENERGY STORAGE↗