Search NASA⌕ Search

SEARCH · Search NASA

Results for “polymeric elastomers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Superstretchable, Self-Healing Polymeric Elastomers with Tunable Properties

Utilization of self-healing chemistry to develop synthetic polymer materials that can heal themselves with restored mechanical performance and functionality is of great interest. Self-healable polymer elastomers with tunable mechanical properties are especially attractive for a variety of applications. In this paper, a series of urea functionalized poly(dimethyl siloxane)-based elastomers (U-PDMS-Es) are reported with extremely high stretchability, self-healing mechanical properties, and recoverable gas-separation performance. Tailoring the molecular weights of poly(dimethyl siloxane) or weight ratio of elastic cross-linker offers tunable mechanical properties of the obtained U-PDMS-Es, such as ultimate elongation (from 984% to 5600%), Young's modulus, ultimate tensile strength, toughness, and elastic recovery. The U-PDMS-Es can serve as excellent acoustic and vibration damping materials over a broad range of temperature (over 100 °C). The strain-dependent elastic recovery behavior of U-PDMS-Es is also studied. After mechanical damage, the U-PDMS-Es can be healed in 120 min at ambient temperature or in 20 min at 40 °C with completely restored mechanical performance. Lastly, the U-PDMS-Es are also demonstrated to exhibit recoverable gas-separation functionality with retained permeability/selectivity after being damaged.

36 MATERIALS SCIENCE↗

Recent advances in thermoplastic elastomers from living polymerizations: Macromolecular architectures and supramolecular chemistry

Thermoplastic elastomers (TPEs) have found use in a wide range of applications, such as adhesives, elastomers, coatings, fibers, and in additive manufacturing techniques such as 3D printing. Despite their omnipresence, the need for advanced TPEs with adaptive properties is continuously growing. Along with a brief historical introduction, this review introduces an overview of typical structure-property relationships for various TPEs and discusses the design principles of TPEs from a synthetic chemistry perspective. Recent advances in TPEs with different macromolecular architectures, including linear ABA triblock copolymers, ABC triblock terpolymers, multiblock copolymers, star copolymers, graft copolymers, bottlebrush polymers, and hyperbranched polymers are reviewed. Service temperatures and mechanical properties of the different materials are compared in each section. Incorporating various supramolecular interactions into different macromolecular architectures as a means to further extend the range of TPE applications is also reported on. Further opportunities for TPE research in both academia and industry are proposed as perspectives.

36 MATERIALS SCIENCE↗

The Durability of Piston Seals in Hydraulic Power Take-off Systems in Wave Energy Converters

Hydraulic cylinder seals are a critical component of hydraulic power take-off (PTO) systems in wave energy converters (WECs). Primary hydraulic piston seal wear is a major concern for the longevity of hydraulic PTOs, especially in the context of the effort and expense associated with seal replacement. Piston seals, made from polymeric elastomers, are used to contain and isolate high pressure fluids within PTO systems. A specific challenge for WEC designers is knowing, with confidence, the relative expected lifetimes of commercially available seals and seal materials for the unique long travel and continuous use case of WEC hydraulic systems. This information is critical to accurately determine operating expense (OPEX) and levelized cost of electricity (LCOE). If failures of seals occur earlier than their designed lifetime, the estimated operations, and maintenance (O&M) and LCOE costs may double based on estimation. Unfortunately, information from seal manufacturers on longevity in these applications is not generally available and quantitative performance comparison between different manufacturers is not available, creating significant uncertainty on use of hydraulic PTO system in wave power generation. In this project, PNNL, with advice from different WEC device and seal manufacturers, has created a framework to address the industry need for available, dependable and comparative data for seals and seals materials for WEC hydraulic applications including piston seals, glide rings, and shaft seals. Commonly used and candidate seal materials were identified and available information on the materials such as mechanical and fatigue performance, chemical (fluid) compatibility, and cost has been compiled. Hardware and strategy for bench scale measurement of key materials and seal performance and pathway for publicly available library of hydraulic seal materials, properties, suppliers, and options have also been identified for future implementation. The results of this project were presented at WPTO Seedling Symposium 2023 and OCEANS 2023. The results of the literature review including identified polymer seals and ideal operating conditions were summaried and compiled to a database WEC-SealsDB hosted locally at PNNL.

16 TIDAL AND WAVE POWER↗

Hazards protection for space suits and spacecraft

A flexible multi-layered covering article for protection against the hazards of exposure to the environment of outer space is disclosed. The covering includes an outer layer section comprising an outermost lamina of woven expanded tetrafluoroethylene yarns (Gore Tex) for protecting against abrasion and tearing, an underlying weave of meta-aramid yarns (Nomex) and para-aramid yarns (Kevlar) for particle impart protection, and electrostatic charge dissipation and control system incorporated therein, and a chemical contaminants control barrier applied as a coating. A middle section includes a succession of thermal insulating layers of polymeric thermoplastic or thermoforming material, each of which is coated with a metal deposit of high infra-red emissivity and low solar radiation absorption characteristics and separated from adjacent insulating layers by a low thermal conductance material. The covering further includes a radiation attenuating layer of a tungsten-loaded polymeric elastomer binder for protecting against bremsstrahlung radiation and an inner layer of rip-stop polyester material for abrasion protection. A chloroprene coating may be supplied the polyester-material for added micrometeroid protection. Securing means of low heat conductance material secures the multi-layers together as a laminar composite.

Kosmo, Joseph J.↗

The International Telecommunications Satellite (INTELSAT) Solar Array Coupon (ISAC) atomic oxgyen flight experiment: Techniques, results and summary

Techniques and results of the ISAC flight experiment are presented, and comparisons between flight tests results and ground based testing are made. The ISAC flight experiment, one component of a larger INTELSAT 6 rescue program, tested solar array configurations and individual silver connects in ground based facilities and during STS-41 (Space Shuttle Discovery). In addition to the INTELSAT specimens, several materials, for which little or no flight data exist, were also tested for atomic oxygen reactivity. Dry lubricants, elastomers, polymeric materials, and inorganic materials were exposed to an oxygen atom fluence of 1.2 x 10(exp 20) atoms. Many of the samples were selected to support Space Station Freedom design and decision-making.

Koontz, S.↗

Formation of a Crack-Free, Hybrid Skin Layer with Tunable Surface Topography and Improved Gas Permeation Selectivity on Elastomers Using Gel–Liquid Infiltration Polymerization

Surface modifications of elastomers and gels are crucial for emerging applications such as soft robotics and flexible electronics, in large part because they provide a platform to control wettability, adhesion, and permeability. Current surface modification methods via ultraviolet-ozone (UVO) and/or O2 plasma, atomic layer deposition (ALD), plasmas deposition, and chemical treatment impart a dense polymer or inorganic layer on the surface that is brittle and easy to fracture at low strain levels. This paper presents a new method, based on gel–liquid infiltration polymerization, to form hybrid skin layers atop elastomers. The method is unique in that it allows for control of the skin layer topography, with tunable feature sizes and aspect ratios as high as 1.8 without fracture. Unlike previous techniques, the skin layer formed here dramatically improves the barrier properties of the elastomer, while preserving skin layer flexibility. Furthermore, the method is versatile and likely applicable to most interfacial polymerization systems and network polymers on flat and patterned surfaces.

36 MATERIALS SCIENCE↗

High temperature thermoplastic elastomers synthesized by living anionic polymerization in hydrocarbon solvent at room temperature

We present the synthesis and characterization of a new class of high temperature thermoplastic elastomers composed of polybenzofulvene–polyisoprene–polybenzofulvene (FIF) triblock copolymers. All copolymers were prepared by living anionic polymerization in benzene at room temperature. Homopolymerization and effects of additives on the glass transition temperature (T g ) of polybenzofulvene (PBF) were also investigated. Among all triblock copolymers studied, FIF with 14 vol % of PBF exhibited a maximum stress of 14.3 ± 1.3 MPa and strain at break of 1390 ± 66% from tensile tests. The stress–strain curves of FIF-10 and 14 were analyzed by a statistical molecular approach using a nonaffine tube model to estimate the thermoplastic elastomer behavior. Dynamic mechanical analysis showed that the softening temperature of PBF in FIF was 145 °C, much higher than that of thermoplastic elastomers with polystyrene hard blocks. Microphase separation of FIF triblock copolymers was observed by small-angle X-ray scattering, even though long-range order was not achieved under the annealing conditions employed. Additionally, the microphase separation of the resulting triblock copolymers was examined by atomic force microscopy.

36 MATERIALS SCIENCE↗

Ferroelectric and Piezoelectric Properties of Blends of Poly(Vinylidene-Trifluoroethylene) and Graft Elastomer

A piezoelectric polymeric blend system has been developed. The system contains two components: ferroelectric poly(vinylidene-trifluoroethylene) and graft elastomer. The remanent polarization, Pr, and the piezoelectric strain coefficient, d31, of the blends have been studied as a function of relative composition of the two components, temperature and frequency. Both blended copolymer and graft unit in the elastomer contribute to the total crystallinity of the blend-system, and hence to the remanent polarization and piezoelectricity. The piezoelectric strain coefficient, d31, of the blend systems shows dependence on both the remanent polarization and the mechanical stiffness, which in turn are determined by the fraction of the two components in the blends. This mechanism makes it possible for the piezoelectric strain response of the blend to be tailored by adjusting the relative composition. Although Pr of the copolymer is higher than that of the blends, the blend films containing 75 wt.% copolymer exhibit a higher d31 at room temperature, possibly due to their lower modulus. The blend films containing 50 wt.% copolymer exhibit a constant value of d31, from room temperature to 70 C.

Su, J.↗

Intelsat solar array coupon atomic oxygen flight experiment

A Hughes communications satellite (INTELSAT series) belonging to the INTELSAT Organization was marooned in low-Earth orbit (LEO) on March 14, 1990, following failure of the Titan launch vehicle third stage to separate properly. The satellite, INTELSAT 6, was designed for service in geosynchronous orbit and contains several materials that are potentially susceptible to attack by atomic oxygen. Analysis showed that direct exposure of the silver interconnects in the satellite photovoltaic array to atomic oxygen in LEO was the key materials issue. Available data on atomic oxygen degradation of silver are limited and show high variance, so solar array configurations of the INTELSAT 6 type and individual interconnects were tested in ground-based facilities and during STS-41 (Space Shuttle Discovery, October 1990) as part of the ISAC flight experiment. Several materials for which little or no flight data exist were also tested for atomic oxygen reactivity. Dry lubricants, elastomers, and polymeric and inorganic materials were exposed to an oxygen atom fluence of 1.1 x 10(exp 20) atoms cm(exp 2). Many of the samples were selected to support Space Station Freedom design and decision making. This paper provides an overview of the ISAC flight experiment and a brief summary of results. In addition to new data on materials not before flown, ISAC provided data supporting the decision to rescue INTELSAT 6, which was successfully undertaken in May 1992.

TRT-GENERAL REVIEW↗

Self-healing elastomer system

A composite material includes an elastomer matrix, a set of first capsules containing a polymerizer, and a set of second capsules containing a corresponding activator for the polymerizer. The polymerizer may be a polymerizer for an elastomer. The composite material may be prepared by combining a first set of capsules containing a polymerizer, a second set of capsules containing a corresponding activator for the polymerizer, and a matrix precursor, and then solidifying the matrix precursor to form an elastomeric matrix.

Keller, Michael W.↗

Investigation of the structure, filler interaction and degradation of disulfide elastomers made by Reversible Radical Recombination Polymerization (R3P)

In this paper we report the synthesis and analysis of cyclic polydisulfides, their redox depolymerization as well as their interaction with carbon black. Cyclic poly(3,6-dioxa-1,8-octanedithiol)s (pDODT) were synthesized by Reversible Radical Recombination Polymerization (R3P). R3P is a scalable “green” polymerization process using triethylamine (TEA), H 2 O 2 and air for the polymerization of dithiol monomers. pDODTs were synthesized in 5 and 20 g batches. The effect of peroxide concentration (3, 5, 10, 20, 30%) was investigated. It was found that the molecular weights increased exponentially with increasing peroxide concentrations. At 30% peroxide concentration pDODTs with M n up to 400,000 g/mol and polydispersity of 2 were obtained. 700 and 800 MHz NMR were used for investigating the chemical structure of the polymers. The absence of thiol end group signals in polymers made with > 10wt % H 2 O 2 and M n < 100,000 g/mol, including a sample of a fractionated polymer with starting Mn = 600,000 g/mol, verified cyclic structures. Dithiothreitol reduced the polymers to monomer and a small percentage of oligomers. Carbon black was shown to increase the moduli of high molecular weight pDODTs. Swelling tests in chloroform showed that polymers made with 20 and 30w% peroxide swelled 14 and 10 times of their starting weight without dissolving, indicating chemical interaction between the polymers and carbon black. In conclusion, further analysis of these interesting elastomers, available at the 20 g scale, is in progress.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Constitutive modeling of Radiation effects on the Permanent Set in a silicone elastomer

When a networked polymeric composite under high stress is subjected to irradiation, the resulting chemical changes like chain scissioning and cross-link formation can lead to permanent set and altered elastic modulus. Using a commercial silicone elastomer as a specific example we show that a simple 2-stage Tobolsky model in conjunction with Fricker's stress-transfer function can quantitatively reproduce all experimental data as a function of radiation dosage and the static strain at which radiation is turned on, including permanent set, stress-strain response, and net cross-linking density.

36 MATERIALS SCIENCE↗

Studies on Stress-Strain Relationships of Polymeric Materials Used in Space Applications

A two-year research plan was undertaken in association with Polymers Branch, NASA Glenn Research Center, to carry out experimental and modeling work relating stress and strain behavior of polymeric materials, especially elastomers and vulcanized rubber. An experimental system based on MTS (Mechanical Testing and Simulation) A/T-4 test facility environment has been developed for a broader range of polymeric materials in addition to a design of laser compatible temperature control chamber for online measurements of various strains. Necessary material processing has been accomplished including rubber compounding and thermoplastic elastomer processing via injection molding. A broad suite of testing methodologies has been identified to reveal the complex non-linear mechanical behaviors of rubbery materials when subjected to complex modes of deformation. This suite of tests required the conceptualization, design and development of new specimen geometries, test fixtures, and test systems including development of a new laser based technique to measure large multi-axial deformations. Test data has been generated for some of these new fixtures and has revealed some complex coupling effects generated during multi-axial deformations. In addition, fundamental research has been conducted concerning the foundation principles of rubber thermodynamics and resulting theories of rubber elasticity. Studies have been completed on morphological properties of several thermoplastic elastomers. Finally, a series of steps have been identified to further advance the goals of NASA's ongoing effort.

Jana, Sadhan C.↗

MQ NMR and SPME analysis of nonlinearity in the degradation of a filled silicone elastomer

Radiation induced degradation of polymeric materials occurs via numerous, simultaneous, competing chemical reactions. Though degradation is typically found to be linear in adsorbed dose, some silicone materials exhibit non-linear dose dependence due to dose dependent dominant degradation pathways. We have characterized the effects of radiative and thermal degradation on a model filled-PDMS system, Sylgard 184 (commonly used as an electronic encapsulant and in biomedical applications), using traditional mechanical testing, NMR spectroscopy, and sample headspace analysis using Solid Phase Micro-Extraction (SPME) followed by Gas Chromatography/Mass Spectrometry (GC/MS). The mechanical data and {sup 1}H spin-echo NMR indicated that radiation exposure leads to predominantly crosslinking over the cumulative dose range studies (0 to 250 kGray) with a rate roughly linear with dose. {sup 1}H Multiple Quantum NMR detected a bimodal distribution in the network structure, as expected by the proposed structure of Sylgard 184. The MQ-NMR further indicated that the radiation induced structural changes were not linear in adsorbed dose and competing chain scission mechanisms contribute more largely to the overall degradation process in the range of 50 -100 kGray (though crosslinking still dominates). The SPME-GC/MS data were analyzed using Principal Component Analysis (PCA), which identified subtle changes in the distributions of degradation products (the cyclic siloxanes and other components of the material) as a function of age that provide insight into the dominant degradation pathways at low and high adsorbed dose.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗