Search NASA⌕ Search

SEARCH · Search NASA

Results for “selenization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Understanding the Effect of Single Atom Cationic Defect Sites in an Al 2 O 3 (012) Surface on Altering Selenate and Sulfate Adsorption: An Ab Initio Study

Adsorption is a promising under-the-sink selenate remediation technique for distributed water systems. Recently it was shown that adsorption induced water network rearrangement control adsorption energetics on the α-Al 2 O 3 (012) surface. Here, we aim to elucidate the relative importance of the water network effects and surface cation identity on controlling selenate and sulfate adsorption energy using density functional theory calculations. Density functional theory (DFT) calculations predicted the adsorption energies of selenate and sulfate on nine transition metal cations (Sc–Cu) and two alkali metal cations (Ga and In) in the α-Al 2 O 3 (012) surface under simulated acidic and neutral pH conditions. We find that the water network effects had a larger impact on the adsorption energy than the cationic identity. However, cation identity secondarily controlled adsorption. Most cations decreased the adsorption energy, weakening the overall performance, the larger Sc and In cations enabled inner-sphere adsorption in acidic conditions because they relaxed outward from the surface, providing more space for adsorption. Additionally, only Ti induced Se selectivity over S by reducing the adsorbing selenate to selenite but not reducing the sulfate. Altogether, this study indicates that tuning water network structure will likely have a larger impact than tuning cation–selenate interactions for increasing adsorbate effectiveness.

Adsorption↗

Topologically and geometrically flexible structural units in seven new organically templated uranyl selenates and selenite–selenates

Single crystals of seven novel uranyl oxysalts of selenium with protonated methylamine molecules, [C{sub 2}H{sub 8}N]{sub 2}[(UO{sub 2})(SeO{sub 4}){sub 2}(H{sub 2}O)] (I), [C{sub 2}H{sub 8}N]{sub 2}[(UO{sub 2}){sub 2}(SeO{sub 4}){sub 3}(H{sub 2}O)] (II), [C{sub 4}H{sub 15}N{sub 3}][H{sub 3}O]{sub 0.5}[(UO{sub 2}){sub 2}(SeO{sub 4}){sub 2.93}(SeO{sub 3}){sub 0.07}(H{sub 2}O)](NO{sub 3}){sub 0.5} (III), [C{sub 2}H{sub 8}N]{sub 3}[H{sub 5}O{sub 2}][(UO{sub 2}){sub 2}(SeO{sub 4}){sub 3}(H{sub 2}O){sub 2}]{sub 2}(H{sub 2}O){sub 5} (IV), [C{sub 2}H{sub 8}N]{sub 2}[H{sub 3}O][(UO{sub 2}){sub 3}(SeO{sub 4}){sub 4}(HSeO{sub 3})(H{sub 2}O)](H{sub 2}SeO{sub 3}){sub 0.2} (V), [C{sub 4}H{sub 12}N]{sub 3}[H{sub 3}O][(UO{sub 2}){sub 3}(SeO{sub 4}){sub 5}(H{sub 2}O)] (VI), and [C{sub 2}H{sub 8}N]{sub 3}(C{sub 2}H{sub 7}N)[(UO{sub 2}){sub 3}(SeO{sub 4}){sub 4}(HSeO{sub 3})(H{sub 2}O)] (VII) have been prepared by isothermal evaporation from aqueous solutions. Their crystal structures have been solved by direct methods and their uranyl selenate and selenite–selenate units investigated using black-and-white graphs from the viewpoints of topology of interpolyhedral linkages and isomeric variations. The crystal structure of IV is based upon complex layers with unique topology, which has not been observed previously in uranyl selenates. Investigations of the statistics and local distribution of the U–O{sub br}–Se bond angles demonstrates that shorter angles associate with undulations, whereas larger angles correspond to planar areas of the uranyl selenite layers. - Graphical abstract: Crystal structures of the seven novel Se-contaning uranyl oxysalts that contain protonated organic molecules as interlayer species have been investigated from the viewpoints of topology of interpolyhedral linkages, isomeric variations and flexibility of structural units. - Highlights: • Single crystals of seven novel uranyl oxysalts were prepared by evaporation method. • The graph theory was used for investigation of topologies of structural units. • The method of orientation matrices was applied to distinguish geometrical isomers. • The flexibility of structural complexes specifies the undulation of layered structural units.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Near Quantitative Removal of Selenate and Sulfate Anions from Wastewaters by Cocrystallization with Chelating Hydrogen-Bonding Guanidinium Ligands

Selenium (Se) has become an environmental contaminant of aquatic ecosystems as a result of human activities, particularly mining, fossil fuel combustion, and agricultural activities. By leveraging the high sulfate concentrations relative to Se oxyanions (i.e., SeO n 2– , n = 3, 4) present in some wastewaters, we have developed an efficient approach to Se-oxyanion removal by cocrystallization with bisiminoguanidinium (BIG) ligands that form crystalline sulfate/selenate solid solutions. The crystallization of the sulfate, selenate and selenite, oxyanions and of sulfate/selenate mixtures with five candidate BIG ligands are reported along with the thermodynamics of crystallization and aqueous solubilities. Oxyanion removal experiments with the top two performing candidate ligands show a near quantitative removal (>99%) of sulfate or selenate from solution. When both sulfate and selenate are present, there is near quantitative removal (>99%) of selenate, down to sub-ppb Se levels, with no discrimination between the two oxyanions during cocrystallization. Reducing the selenate concentrations by 3 orders of magnitude or more relative to sulfate, as found in many wastewaters, led to no measurable loss in Se removal efficiencies. This work offers a simple and effective alternative to selective separation of trace amounts of highly toxic selenate oxyanions from wastewaters, to meet stringent regulatory discharge limits.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sorption of Arsenate, Selenate, and Molybdate on the Barite (001) Surface

Interactions of ions with ionically bonded minerals such as barite (BaSO 4 ) influence the fate and transport of the ions, while the factors that control the sorption of toxic oxyanions on barite remain elusive. In this study, the sorption of arsenate, selenate, and molybdate on the barite (001) surface was examined at pH ~5 using in situ crystal truncation rod analysis, resonant anomalous X-ray reflectivity, and atomic force microscopy. The results show that arsenate and selenate mainly incorporate into the top monolayer of barite, while molybdate primarily adsorbs above the surface. The sorption coverage of arsenate is greater (by ~100%) than that of selenate but similar to that of molybdate. The different incorporation coverages between arsenate and selenate can be explained by their different protonation states at pH 5. The incorporated arsenate may be stabilized by hydrogen bonds between arsenate and oxygen atoms of neighboring sulfate compared to selenate, which exists predominantly in the deprotonated state. The adsorption of molybdate above the surface probably stems from a surface-induced oligomerization, as the anion and the oligomer may be too large for incorporation. Our observation of these different sorption mechanisms demonstrates how the physicochemical properties of the anions control the selective uptake of the toxic metals on the dominant surface of the ionically bonded mineral barite.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of heterocyclic N-donors on the structural topologies and vibrational spectra of uranyl selenate phases

Uranyl (U(VI)O 2 2+ ) selenate compounds represent a well-studied family of structures with diverse structural arrays. Differences in the overall topology and bonding with the uranyl cation combined with additional intermolecular interactions can lead to variation in the resulting spectroscopic signals. Here, in the current study, we evaluated the structural chemistry and vibrational spectroscopy for uranyl selenates crystallized with heterocyclic N-donors. Five compounds ((C 4 H 12 N 2 )[(UO 2 )(SeO 4 ) 2 (H 2 O)]·H 2 O (USe_pip), (C 4 H 5 N 2 ) 2 [(UO 2 )(SeO 4 ) 2 (H 2 O)] (USe_pyrdz), (C 5 H 5 N) 2 [(UO 2 ) 2 (SeO 4 ) 3 (H 2 O)] ∙ 3H 2 O (USe_pyrmd), (H 3 O) 2 (C 4 H 5 N 2 ) 2 [(UO 2 ) 3 (SeO 4 ) 5 (H 2 O)]·H 2 O (USe_pyrz), and (C 5 H 6 N) 2 [(UO 2 ) 2 (SeO 4 ) 3 (H 2 O)] ∙ 3H 2 O (USe_pyr)) were characterized using X-ray diffraction (single-crystal and powder) and vibrational (Raman and IR) spectroscopy. Two one-dimensional (1-D) chain and three two-dimensional sheet (2-D) topologies were identified and classified based upon previous graphical representations. Overall, the arrangement of the heteroatoms could be linked to the hydrogen bonding network associated with the heterocycles and selenate anions. Vibrational spectra of the solid-state compounds were complex, with multiple bands associated with the uranyl cation, selenate anion, and heteroatoms. The ν 1 symmetric stretching band of the uranyl was relatively consistent across all compounds, whereas differences were observed for the ν 3 asymmetric band between the 1-D and 2-D structural topologies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dehydration-driven evolution of topological complexity in ethylamonium uranyl selenates

Single crystals of four novel uranyl selenate and selenite-selenate oxysalts with protonated ethylamine molecules, (C{sub 2}H{sub 8}N){sub 2}[(UO{sub 2})(SeO{sub 4}){sub 2}(H{sub 2}O)](H{sub 2}O) (I), (C{sub 2}H{sub 8}N){sub 3}[(UO{sub 2})(SeO{sub 4}){sub 2}(HSeO{sub 4})] (II), (C{sub 2}H{sub 8}N)[(UO{sub 2})(SeO{sub 4})(HSeO{sub 3})] (III), and (C{sub 2}H{sub 8}N)(H{sub 3}O)[(UO{sub 2})(SeO{sub 4}){sub 2}(H{sub 2}O)] (IV) have been prepared by isothermal evaporation from aqueous solutions. Uranyl-containing 1D and 2D units have been investigated using topological approach and information-based complexity measurements that demonstrate the evolution of structural units and the increase of topological complexity with the decrease of H{sub 2}O content. - Graphical abstract: Single crystals of four novel uranyl selenate and selenite-selenate oxysalts with protonated ethylamine molecules have been prepared by isothermal evaporation from aqueous solutions. Structural analysis and information-based topological complexity calculations points to the possible sequence of crystalline phases formation, showing both topological and structural branches of evolution. - Highlights: • Single crystals of four novel uranyl oxysalts were prepared by evaporation method. • The graph theory was used for investigation of topologies of structural units. • Dehydration processes drives the evolution of topological complexity of 1D and 2D structural units.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

ADSORPTION MECHANISMS AND TRANSPORT BEHAVIOR BETWEEN SELENATE AND SELENITE ON DIFFERENT SORBENTS

Adsorption of different oxidation species of selenium (Se), selenate (SeO42-) and selenite (SeO32-), with varying pHs (2 - 10) and ionic strengths (I = 0.01 M, 0.1 M and 1.0 M NaNO3) was measured on quartz, aluminum oxide, and synthetic iron oxide (ferrihydrite) using batch reactors to obtain a more detailed understanding of the adsorption mechanisms (e.g., inner- and outer-sphere complex). In addition to the batch experiments with single minerals contained in native Hanford Site sediment, additional batch adsorption studies were conducted with native Hanford Site sediment and groundwater as a function of 1) total Se concentration (from 0.01 to 10 mg L-1) and 2) soil to solution ratios (1:20 and 1:2 grams per mL). Results from these batch studies were compared to a set of saturated column experiments that were conducted with natural Hanford sediment and groundwater spiked with either selenite or selenate to observe the transport behavior of these species. Both batch and column results indicated that selenite adsorption was consistently higher than that of selenate in all experimental conditions used. These different adsorption mechanisms between selenite and selenate result in the varying mobility of Se in the subsurface environment and explain the dependence on the oxidation species.

adsorption↗

ADSORPTION MECHANISMS AND TRANSPORT BEHAVIOR BETWEEN SELENATE AND SELENITE ON DIFFERENT SORBENTS

Adsorption of different oxidation species of selenium (Se), selenate (SeO42-) and selenite (SeO32-), with varying pHs (2 - 10) and ionic strengths (I = 0.01 M, 0.1 M and 1.0 M NaNO3) was measured on quartz, aluminum oxide, and synthetic iron oxide (ferrihydrite) using batch reactors to obtain a more detailed understanding of the adsorption mechanisms (e.g., inner- and outer-sphere complex). In addition to the batch experiments with single minerals contained in native Hanford Site sediment, additional batch adsorption studies were conducted with native Hanford Site sediment and groundwater as a function of 1) total Se concentration (from 0.01 to 10 mg L-1) and 2) soil to solution ratios (1:20 and 1:2 grams per mL). Results from these batch studies were compared to a set of saturated column experiments that were conducted with natural Hanford sediment and groundwater spiked with either selenite or selenate to observe the transport behavior of these species. Both batch and column results indicated that selenite adsorption was consistently higher than that of selenate in all experimental conditions used. These different adsorption mechanisms between selenite and selenate result in the varying mobility of Se in the subsurface environment and explain the dependence on the oxidation species.

selenite: selenate: inner-sphere complex: outer-sp↗

Selenization of CIS and CIGS layers deposited by chemical spray pyrolysis

Cu(In1-xGax)Se2 (CIGS) thin films with x=0 (CIS) and x=0.3 (CIGS) were prepared on Mo-coated glass substrate by using chemical spray pyrolysis at a substrate temperature of 350 degrees C, followed by selenization treatment at 550 degrees C in selenium environment under N2 gas flow. X-ray diffraction patterns of as-deposited CIGS layers on Mo showed polycrystalline chalcopyrite phase with an intense (112) plane. Splitting of (204)/(220) and (116)/(312) planes for the film with x=0.3 reveals deviation of tetragonal nature. Field emission scanning electron microscopy cross-sectional images of selenized films showed clear re-crystallization of grains. During the selenization process of the CIGS absorber, a thin interface layer of MoSe2 is formed. Line mapping of Mo/CIGS layer showed more gallium segregation at the interface of back contact resulting in band gap grading. Chemical composition and mapping of the as-deposited and selenized samples were determined by energy dispersive analysis of X-rays. This work leads to fabrication of low cost and large scale Mo/CIGS/CdS/ZnO/ZnO:Al device structure.

14 SOLAR ENERGY↗

Dynamics of the phase formation process upon the low temperature selenization of Cu/In-multilayer stacks

Phase reactions occurring during a low temperature selenization of thin In/Cu-multilayer stacks were investigated by ex-situ x-ray diffraction (XRD) and energy dispersive x-ray spectroscopy (EDS). Therefore, dc-sputtered In/Cu-multilayers onto molybdenum coated soda lime glass were selenized in a high vacuum system at temperatures between 260 and 340 °C with different dwell times and selenium supply. The combination of the results of the phase analysis by XRD and the measurements of the in-depth elemental distribution by EDS allowed a conclusion on the occurring reactions within the layer depth. We found two CuInSe{sub 2} formation processes depending on the applied temperature. Already, at a heater temperature of 260 °C, the CuInSe{sub 2} formation can occur by the reaction of Cu{sub 2−x}Se with In{sub 4}Se{sub 3} and Se. At 340 °C, CuInSe{sub 2} is formed by the reaction of Cu{sub 2−x}Se with InSe and Se. Because both reactions need additional selenium, the selenium supply during the selenization can shift the reaction equilibria either to the metal binaries side or to the CuInSe{sub 2} side. Interestingly, a lower selenium supply shifts the equilibrium to the CuInSe{sub 2} side, because the amount of selenium incorporated into the metallic layer is higher for a lower selenium supply. Most likely, a larger number of grain boundaries are the reason for the stronger selenium incorporation. The results of the phase formation studies were used to design a two stage selenization process to get a defined structure of an indium selenide- and a copper selenide-layer at low temperatures as the origin for a controlled interdiffusion to form the CuInSe{sub 2}-absorber-layer at higher temperatures. The approach delivers a CuInSe{sub 2} absorber which reach total area efficiencies of 11.8% (13.0% active area) in a CuInSe{sub 2}-thin-film solar cell. A finished formation of CuInSe{sub 2} at low temperature was not observed in our experiments but is probably possible for longer dwell times.

36 MATERIALS SCIENCE↗

Spectroscopic Investigation of Arsenate and Selenate Incorporation into Hydroxylapatite

The mechanism(s) of arsenate and selenate incorporation into hydroxylapatite (HAP) using extended X-ray absorption fine structure (EXAFS) spectroscopy was investigated for As- and Se-doped HAP samples with concentrations between 200 and 2500 ppm. EXAFS data on As and Se K-edges have shown similar local coordination environments and are similar to that of P in HAP, suggesting the substitution of arsenate or selenate tetrahedra on the phosphate sites. EXAFS best-fitting for As-doped samples shows that the first shell is fitted with approximately 4 O atoms at {approx}1.68 {angstrom}, showing As(V) in tetrahedral coordination, and Se K-edge EXAFS data are characterized by the backscattering contributions an oxygen shell at 1.2 {angstrom} in the Fourier transform, which can be fit with 4 O atoms at {approx}1.65 {+-} 0.01 {angstrom}. This is characteristic of Se-O distances in SeO{sub 4} tetrahedron. These findings suggest that arsenate and selenate substitute for phosphate groups with local distortions during the incorporation of these metals into the structure of HAP.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Influence of the Organic Species and Oxoanion in the Synthesis of two Uranyl Sulfate Hydrates, (H 3 O) 2 [(UO 2 ) 2 (SO 4 ) 3 ­(H 2 O)]·7H 2 O and (H 3 O) 2 [(UO 2 ) 2 (SO 4 ) 3 (H 2 O)]·4H 2 O, and a Uranyl Selenate-Selenite [C 5 H 6 N][(UO 2 )(SeO 4 )(HSeO 3 )]

Two uranyl sulfate hydrates, (H3O)2[(UO2)2(SO4)3(H2O)]·7H2O (NDUS) and (H3O)2[(UO2)2(SO4)3(H2O)]·4H2O (NDUS1), and one uranyl selenate-selenite [C5H6N][(UO2)(SeO4)(HSeO3)] (NDUSe), were obtained and their crystal structures solved. NDUS and NDUSe result from reactions in highly acidic media in the presence of L-cystine at 373 K. NDUS crystallized in a closed vial at 278 K after 5 days and NDUSe in an open beaker at 278 K after 2 weeks. NDUS1 was synthesized from aqueous solution at room temperature over the course of a month. NDUS, NDUS1, and NDUSe crystallize in the monoclinic space group P21/n, a = 15.0249(4) Å,b = 9.9320(2) Å, c = 15.6518(4) Å, β = 112.778(1)°, V = 2153.52(9) Å3,Z = 4, the tetragonal space group P43212, a = 10.6111(2) Å,c = 31.644(1) Å, V = 3563.0(2) Å3, Z = 8, and in the monoclinic space group P21/n, a = 8.993(3) Å, b = 13.399(5) Å, c = 10.640(4) Å,β = 108.230(4)°, V = 1217.7(8) Å3, Z = 4, respectively.The structural units of NDUS and NDUS1 are two-dimensional uranyl sulfate sheets with a U/S ratio of 2/3. The structural unit of NDUSe is a two-dimensional uranyl selenate-selenite sheets with a U/Se ratio of 1/2. In-situ reaction of the L-cystine ligands gives two distinct products for the different acids used here. Where sulfuric acid is used, only H3O+ cations are located in the interlayer space, where they balance the charge of the sheets, whereas where selenic acid is used, interlayer C5H6N+ cations result from the cyclization of the carboxyl groups of L-cystine, balancing the charge of the sheets.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High Efficiency Adsorption and Removal of Selenate and Selenite from Water Using Metal–Organic Frameworks

A series of zirconium-based, metal organic frameworks (MOFs) were tested for their ability to adsorb and remove selenate and selenite anions from aqueous solutions. MOFs were tested for adsorption capacity and uptake time at different concentrations. NU-1000 was shown to have the highest adsorption capacity, and fastest uptake rates for both selenate and selenite, of all zirconium-based MOFs studied here. Herein, the mechanism of selenate and selenite adsorption on NU-1000 is explored to determine the important features that make NU-1000 a superior adsorbent for this application.

Howarth, Ashlee J.↗

The role of interparticle heterogeneities in the selenization pathway of Cu-Zn-Sn-S nanoparticle thin films: A real-time study

Real-time energy dispersive x-ray diffraction (EDXRD) analysis has been utilized to observe the selenization of Cu-Zn-Sn-S nanoparticle films coated from three nanoparticle populations: Cu- and Sn-rich particles roughly 5 nm in size, Zn-rich nanoparticles ranging from 10 to 20 nm in diameter, and a mixture of both types of nanoparticles (roughly 1:1 by mass), which corresponds to a synthesis recipe yielding CZTSSe solar cells with reported total-area efficiencies as high as 7.9%. The EDXRD studies presented herein show that the formation of copper selenide intermediates during the selenization of mixed-particle films can be primarily attributed to the small, Cu- and Sn-rich particles. Moreover, the formation of these copper selenide phases represents the first stage of the CZTSSe grain growth mechanism. The large, Zn-rich particles subsequently contribute their composition to form micrometer-sized CZTSSe grains. In conclusion, these findings enable further development of a previously proposed selenization pathway to account for the roles of interparticle heterogeneities, which in turn provides a valuable guide for future optimization of processes to synthesize high quality CZTSSe absorber layers.

36 MATERIALS SCIENCE↗

Thin film solar cells by selenization sulfurization using diethyl selenium as a selenium precursor

A method of forming a CIGSS absorber layer includes the steps of providing a metal precursor, and selenizing the metal precursor using diethyl selenium to form a selenized metal precursor layer (CIGSS absorber layer). A high efficiency solar cell includes a CIGSS absorber layer formed by a process including selenizing a metal precursor using diethyl selenium to form the CIGSS absorber layer.