Search NASA⌕ Search

SEARCH · Search NASA

Results for “siloxanes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Siloxane Deposition on the Ni-YSZ Solid Oxide Fuel Cell Anode Exposed to Bio-Syngas

Siloxane, a common contaminant present in biogas, is known for adverse effects on cogeneration prime movers. In this study, the siloxane deposition products and mechanism in the solid oxide fuel cell nickel-yttria stabilized zirconia (Ni-YSZ) anode are investigated analytically and experimentally. An SOFC with Ni-YSZ anode and pure Ni/YSZ pellets were exposed to a simulated biogas-reformate fuel with octamethylcyclotetrasiloxane (D4) contamination at 750 °C. The electrochemical characterization results show that the SOFCs performance degradation caused by D4 contamination is irreversible. Morphology and XRD results illustrate that silicon and carbon deposition can both be detected in the anode and pellets. Graphite, SiC and SiO2 are all possible products based on the results of XRD test. Here, according to the formation of graphite and SiC, the new mechanism suggests that carbon is also an essential factor in siloxane contamination of Ni-YSZ anodes besides silicon, which can be explained by the catalytic and electrochemical analysis.

25 ENERGY STORAGE↗

Copoly(imide siloxane) Abhesive Materials with Varied Siloxane Oligomer Length

In this work, low surface energy copoly(imide siloxane)s were synthesized with various siloxane segment lengths. Characterization of these materials revealed that domain formation of the low surface energy component within the matrix was more prevalent for longer siloxane segments as indicated by increased opacity, decreased mechanical properties, and variation of the Tg. Incorporation of siloxanes lowered the polymer s surface energy as indicated by water contact angle values. Topographical modification of these materials by laser ablation patterning further reduced the surface energy, even generating superhydrophobic surfaces. Combined, the contact angle data and particle adhesion testing indicated that copoly(imide siloxane) materials may provide greater mitigation to particulate adhesion than polyimide materials alone. These enhanced surface properties for abhesive applications did result in a reduction of the tensile moduli of the copolymers. It is possible that lower siloxane loading levels would result in retention of the mechanical properties of the polyimide while still affording abhesive surface properties. This hypothesis is currently being investigated. Laser ablation patterning offers further reduction in particle retention as the available surface area for particle adhesion is reduced. Pattern variation and size dependencies are currently being evaluated. For the purposes of lunar dust adhesion mitigation, it is likely that this approach, termed passive due to the lack of input from an external energy source, would not be sufficient to mitigate surface contamination or clean contaminated surfaces for some lunar applications. It is feasible to combine these materials with active mitigation strategies - methods that utilize input from external energy sources - would broaden the applicability of such materials for abhesive purposes. Collaborative efforts along these lines have been initiated with researchers at NASA Kennedy Space Center where experiments are being conducted involving a series of embedded electrodes within polymeric matrices.

Wohl, Christoper J.↗

Copoly(Imide Siloxane) Abhesive Materials with Varied Siloxane Oligomer Length

Incorporation of PDMS moieties into a polyimide matrix lowered the surface energy resulting in enhanced adhesive interactions. Polyimide siloxane materials were generated using amine-terminated PDMS oligomers of different lengths to study changes in surface migration behavior, phase segregation, mechanical, thermal, and optical properties. These materials were characterized using contact angle goniometry, tensile testing, and differential scanning calorimetry. The surface migration behavior of the PDMS component depended upon the siloxane molecular weight as indicated by distinct relationships between PDMS chain length and advancing water contact angles. Similar correlations were observed for percent elongation values obtained from tensile testing, while the addition of PDMS reduced the modulus. High fidelity topographical modification via laser ablation patterning further reduced the polyimide siloxane surface energy. Initial particulate adhesion testing experiments demonstrated that polyimide siloxane materials exhibited greater abhesive interactions relative to their respective homopolyimides.

Wohl, Christopher J.↗

Kinetic Separation of Siloxanes in Metal–Organic Frameworks

We present an in silico assessment of metal–organic frameworks (MOFs) for the kinetic separation of linear and cyclic siloxanes. We employed molecular dynamics simulations investigating both rigid and flexible 1D MOF frameworks to identify a specific range of pore parameters that enables the diffusion of linear siloxanes but leads to slow diffusion of cyclic siloxanes. We then extended our analysis to flexible 3D MOFs to select adsorbents for the kinetic separation of cyclic and linear siloxanes. Based on synthesizability metrics we identified four 3D MOFs capable of discriminating between cyclic and linear siloxanes. One of the MOFs with structure code WIYFAM stood out with the ability to distinguish between cyclic and linear siloxanes and facilitate the diffusion of all linear siloxanes investigated in this study. One of the other MOFs, IRMOF-6, is found to be capable of not only discriminating between cyclic and linear siloxanes, but even between shorter and longer linear siloxanes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Equilibrium Separation of Siloxanes in Metal–Organic Frameworks

We present an in silico assessment of metal–organic frameworks (MOFs) for the equilibrium separation of linear and cyclic siloxanes. Using a combination of configurational bias/continuous fractional component Monte Carlo (CB/CFCMC) simulations and Ideal Adsorbed Solution Theory (IAST), we investigated the adsorption of both equimolar and nonequimolar mixtures of linear and cyclic siloxanes in a selection of synthesizable MOFs with medium to large pore volumes. We showed that configurational entropy effects drive the preferential adsorption of linear siloxanes over cyclic siloxanes. Based on synthesizability metrics we identified ZIF-70 as a promising adsorbent for the separation of linear and cyclic siloxanes. Self-diffusivities of linear and cyclic siloxanes in ZIF-70 calculated from molecular dynamics simulations show that equilibrium can be reached on reasonable time scales. We explored vacuum-temperature swing adsorption (VTSA) as a potential method for the recovery of adsorbed linear siloxanes from ZIF-70, achieving a 75% reduction in adsorbed phase concentration. Additionally, we demonstrated that supercritical CO 2 offers an alternative desorption strategy by displacing adsorbed linear siloxanes in ZIF-70 at pressures above 200 bar driven by entropy effects.

Adsorption↗

Separation of Linear and Cyclic Siloxanes in Pure Silica Zeolites

We present a computational assessment of pure-silica zeolites for separating linear and cyclic siloxanes. We developed a force field (FF) for pure silica zeolites, when combined with our previously developed FF for siloxanes using standard Lorentz–Berthelot combining rules, shows good agreement with dispersion-corrected density functional theory calculations. We used molecular dynamics simulations to investigate diffusion of siloxanes in pure silica zeolites and identified a pure silica zeolite with the structure code FAU that enables kinetic separation of linear and cyclic siloxanes. FAU allows the diffusion of linear siloxanes (L2–L6) while excluding cyclic siloxanes. D4 siloxane does not diffuse in any of the investigated zeolites, eliminating the potential of pure silica zeolites to achieve equilibrium-based separations of linear and cyclic siloxanes.

adsorption↗

Degradation Comparison of Cyclic and Linear Siloxane Contamination on Solid Oxide Fuel Cells Ni-YSZ Anode

The solid oxide fuel cell (SOFC) nickel-yttria stabilized zirconia (Ni-YSZ) anode degradation due to different types of siloxane contamination is investigated. A cyclic structure siloxane, octamethylcyclotetrasiloxane (D4), and a linear structure siloxane, decamethyltetrasiloxane (L4), are mixed with H 2 +N 2 as the fuel for SOFCs at 750°C. The electrochemical characterization results after stability experiments suggest that the SOFC contaminated with cyclic siloxane, D4, had higher degradation. Pure YSZ pellets with different surface hydroxylation extents were also tested to investigate the D4/L4 adsorption and deposition process. Postmortem SEM/WDS, XRD and Raman analysis all indicate that cyclic siloxane has more deposition than linear siloxane on the anode. Further analysis demonstrates that high adsorption and low desorption rates of cyclic siloxane on YSZ are linked to the degradation. Besides the silicon deposition, SiC and amorphous carbon deposition were also observed from the XRD and Raman analysis.

25 ENERGY STORAGE↗

Investigating the Influence of Ni, ZrO 2 , and Y 2 O 3 from SOFC Anodes on Siloxane Deposition

Siloxanes, as a type of impurity in biogas, can poison the Ni-YSZ anode of SOFCs. However, the influence of individual components of the anode, such as Ni, ZrO 2 , and Y 2 O 3 , on the siloxane deposition process has not been investigated extensively. In this study, Ni, ZrO 2 , and Y 2 O 3 pellets were exposed to H 2 + N 2 + H 2 O + D4 (octamethylcyclotetrasiloxane, 2.5 ppmv) and H 2 + N 2 + D4 (2.5 ppmv siloxane) gas mixtures at 750 °C to investigate their affinity and tolerance for siloxane degradation. Surface morphology analysis and electrochemical analysis including electrochemical impedance spectroscopy (EIS), related distribution of relaxation times (DRT) analysis and equivalent circuit modeling with complex nonlinear least square (CNLS) fitting were conducted. Here, a microstructure parameter—tortuosity factor to porosity ratio $\tau /\varepsilon $ calculated by diffusion polarization resistance was utilized for siloxane deposition evaluation. After comparing pellets surface morphology changes before and after experiments and $\tau /\varepsilon $ change following the contamination, Ni is considered as a major factor in siloxane deposition reactions in Ni-YSZ anode.

25 ENERGY STORAGE↗

Silylsilane‐Substituted Polymers: Fluorine‐Free, Liquid Repellent, and Hydrolytically Stable Alternatives to Siloxanes

Abstract Per‐ and polyfluoroalkyl substances (PFAS) are omniphobic and exceptionally stable, making them ideal for a wide range of materials applications. However, as “forever chemicals”, their exceptional persistence and bioaccumulation have generated an increasing amount of environmental and health concerns, prompting the search for fluorine‐free alternatives. Siloxane‐based materials are therefore interesting to examine as PFAS alternatives due to their low surface energy and hydrophobicity but suffer from hydrolytic instability of Si─O linkages. To address this challenge, a novel methacrylate monomer, 3‐[tris(trimethylsilyl)silyl]propyl methacrylate (M‐silyl), is designed containing Si─Si bonds rather than Si─O bonds of siloxanes. Polymers derived from M‐silyl (P‐silyl) is prepared by controlled free radical polymerization and compared with their siloxane analogues after coating on silicon wafers. Contact angle (CA) measurements confirmed P‐silyl to be hydrophobic (advancing/receding water CA = 109.7°/83.0°), with a low‐hysteresis for oil (lyophobic) (hexadecane CA hysteresis = 2.0°), comparable to its siloxane‐based counterpart. Importantly, P‐silyl maintained these surface properties after exposure to acidic or basic conditions, while siloxane analogues lost hydrophobicity. Consequently, the incorporation of Si ─ Si linkages into the design of the polymer enables chemically stable, fluorine‐free alternatives for water‐repellent and low hysteresis surface coatings and advances the design of fluorine‐free functional materials.

fluorine-free↗

Siloxane containing polyimides with improved processability

Siloxane containing polyimides were prepared in an effort to improve processability of linear aromatic polyimides and toughness of addition curing imide oligomers. Linear aromatic polyimides were endcapped with varying proportions of a silane; a diaminosiloxane was copolymerized with an aromatic diamine; polyimide oligomers were endcapped with reactive groups; and acetylene terminated siloxane-containing oligomers were blended with linear siloxane-containing polyimides. The resins were used to prepare moldings, titanium to titanium adhesive bonds, and graphite reinforced composites. In each case, physical properties and other characteristics were compared to those of chemically similar polyimides with no siloxane incorporation. The resins, in most cases, performed better at room temperature than the corresponding polyimide. At elevated temperatures, for high siloxane content, the performance deteriorated.

Maudgal, Shubha↗

Failure analysis of solid oxide fuel cells nickel-yttria stabilized zirconia anode under siloxane contamination

In this study, the failure process of the solid oxide fuel cell (SOFC) Ni-yttria-stabilized zirconia (YSZ) anode is investigated with D4 siloxane (octamethylcyclotetrasiloxane) contamination. In order to evaluate the influence of the electrochemical reaction on the siloxane deposition process, the SOFC experiments were operated at open circuit voltage (OCV) and 50 mA cm -2 conditions at 800°C. During the failure process, electrochemical, morphology and exhaust gas component analysis testing are conducted at the critical points. An equivalent circuit model and corresponding microstructure parameter calculations for separated physicochemical processes were utilized for the quantitative analysis of the failure process. Further, the results confirm the siloxane chemical adsorption deposition mechanism proposed in previous work. As a result, the failure of the anode was attributed to the gas diffusion blockage by dense silicon dioxide layer formation. The anode failure process with siloxane contamination is faster when the anode is operated under polarization.

25 ENERGY STORAGE↗

Quantitative Simulations of Siloxane Adsorption in Metal–Organic Frameworks

We present a transferable force field (FF) for simulating the bulk properties of linear and cyclic siloxanes and the adsorption of these species in metal–organic frameworks (MOFs). Unlike previous FFs for siloxanes, our FF accurately reproduces the vapor–liquid equilibria of each species in the bulk phase. The quality of our FF combined with the Universal Force Field using standard Lorentz–Berthelot combining rules for MOF atoms was assessed in a wide range of MOFs without open metal sites, showing good agreement with dispersion-corrected density functional theory calculations. Predictions with this FF show good agreement with the limited experimental data for siloxane adsorption in MOFs that is available. As an example of using the FF to predict adsorption properties in MOFs, we present simulations examining entropy effects in binary linear and cyclic siloxane mixture coadsorption in the large-pore MOF with structure code FOTNIN.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling and Analysis of Polarization Losses in Solid Oxide Fuel Cells with Siloxane Contamination

In this study, the degradation of the solid-oxide fuel cell (SOFC) nickel-yttria stabilized zirconia anode under decamethyltetrasiloxane (L4) contamination is examined with experiments and modeling. A model is developed for the polarization losses based on the charge transfer coefficient,α, and diffusion layer thickness,δ, and fitted to the experimental data to understand how the siloxane degrades the SOFC performance with time. The results of the model indicate that the total polarization losses increase approximately 44% over the course of the 180 min experiment at 350 mA cm −2 . Activation losses dominate the polarization losses initially but decrease in their total contribution while concentration losses increase. Scanning electron microscopy (SEM) with wavelength dispersive X-ray spectroscopy (WDS) elemental mapping indicates that silicon deposition is highest at the outer edge of the anode and forms a barrier layer to fuel diffusion, increasing concentration losses. When the model is applied to other previous D4 and L4 siloxane experiments conducted over a period of 40 h, similar trends in polarization losses are observed. Polarization losses increase more rapidly with D4 compared to L4 siloxane contamination, with concentration losses increasing the fastest with both types of siloxane.

Electrochemistry↗

Structure property behavior of polyimide siloxane segmented copolymers

Procedures were developed for preparing soluble fully imidized polyimide-polydimethyl siloxane segmented copolymers of wide ranging compositions. At low siloxane levels, the materails behave as modified polyimides. At higher concentrations, the materials are analogous to thermoplastic elastomers. Characterization by dynamic mechanical and thermal analysis methods will be reported along with an assesment of the bulk mechanical properties and the surface behavior. The surface behavior is particularly interesting since the materials can be tailored to have siloxane surfaces even at rather low siloxane contents. This influences a number of properties such as the coefficient of friction and, importanly, the degradation of these materials under aggressive oxygen environments (e.g., atomic oxygen, oxygen plasma).

Arnold, C. A.↗

Poly(imide-siloxane) segmented copolymer structural adhesives prepared by bulk and solution thermal imidization

The improved properties that have been demonstrated through thermal solution imidization in the case of polyimides and poly(imide-siloxane) segmented copolymers suggests significant potential for application of these new materials. Specifically, the enhancement in solubility, moisture reduction, and processability observed through this solution technique is quite dramatic. Previous work has shown that the presence of low amounts of siloxane does not detract significantly from the lap shear strength of these materials to titanium in the case of bulk thermal imidization synthesis. In addition, the siloxane incorporation results in the added advantage of resistance to hot, wet environments. This added durability is presumably due to the hydrophobic siloxane segments preventing the uptake of water at the critical interphase between the adhesive and the adherend. This paper discusses the extension of this work to the solution imidization synthesis technique recently developed in our laboratory. Results dealing with the absolute bond strengths as well as durability and failure surface analysis will be presented.

Bott, R. H.↗

Polyimides containing pendent siloxane groups

The incorporation of siloxane units into the backbone of aromatic polyimides has been shown to impart certain advantages over the unmodified polyimides. These include enhanced solubility, lower moisture adsorption, lower dielectric constant, improved toughness and surface modification. Also, when exposed to an atomic oxygen environment these materials form an in-situ silicate (SiO2) surface coating which protects the underlying material from further erosion. These unique advantages make polyimide-siloxanes useful in a variety of electronic and aerospace applications. As part of an effort on high performance polymeric materials for potential aerospace applications, polyimides containing pendent siloxane groups are under study. These materials were prepared by reacting a functionalized siloxane compound with polyimides containing benzhydrol groups. Thin films of the polymers exhibited glass transition temperatures ranging from 167 to 235 C. Tensile strengths and moduli measured at 23 C ranged from 11 to 14 ksi and 250 to 450 ksi, respectively. The dielectric constant was lowered substantially from that of the unmodified polyimide.

Connell, John W.↗

Polyimides containing pendent siloxane groups

Novel polyimides containing pendent siloxane groups (PISOX) were prepared by the reaction of functionalized siloxane compounds with hydroxy containing polyimides (PIOH). The pendent siloxane groups on the polyimide backbone offer distinct advantages such as lowering the dielectric constant and moisture resistance and enhanced atomic oxygen resistance. The siloxane containing polyimides are potentially useful as protective silicon oxide coatings and are useful for a variety of applications where atomic oxygen resistance is needed.

Connell, John W.↗