The onset of selective laser flash sintering in undoped and doped lanthanum chromite

Previous studies have shown that selective laser flash sintering (SLFS) can be initiated in dielectrics that exhibit ionic or electronic conduction at high temperature. These materials required high laser powers to reach the temperatures where electrical conduction is sufficient to initiate SLFS. In this study, SLFS in lanthanum chromite (LC), an intrinsic electronic conductor with high conductivity, and lanthanum strontium chromite (LSC), which is doped to further increase electronic conductivity, were investigated with a focus on understanding the initiation mechanisms. Results show that the initiation of SLFS in LC and LSC occurs when electronic charge carriers are activated and flow to the electrode where the current is measured. A combination of carriers produced at the electrode, temperature-activated intrinsic charge carriers, and extrinsic charge carriers present in LSC due to doping are responsible for the facile initiation of SLFS.

36 MATERIALS SCIENCE↗

Solid-State Sintering of Core-Shell Ceramic Powders Fabricated by Particle Atomic Layer Deposition

The properties of technical ceramics are highly dependent on their microstructure, which evolves during sintering. Sintering is the process by which ceramic parts are subjected to high temperatures to activate chemical diffusion and the consumption of porosity. During the initial stage of sintering, interparticle necks between neighboring particles form and subsequently increase in size, consuming porosity as the particle centers move closer together. To experimentally determine how this process depends on particle surface composition, particle atomic layer deposition (ALD) was used to deposit a thin film of amorphous aluminum oxide (Al2O3) onto yttria-stabilized tetragonal zirconia (3YSZ) particles, producing core-shell structured powders. The uniformity of the Al2O3 film was confirmed with transmission electron microscopy and energy dispersive spectroscopy. Scanning electron microscopy was used to observe microstructural evolution during sintering, and the dihedral angles of Al2O3 and 3YSZ grains were measured to determine the ratio of interfacial energies between the 3YSZ|3YSZ, 3YSZ|Al2O3, and Al2O3|Al2O3 interfaces. Analysis of the densification kinetics revealed that the initial stage of densification is dependent on the material at the surface of the particles (ie, the Al2O3 film) and is controlled by the diffusion of Al3+ cations through Al2O3. Once the Al2O3 film has coalesced, the sintering behavior is controlled by the densification of the core material (3YSZ). Thus, core-shell powders fabricated by particle ALD sinter by a two-step process where the kinetics are dependent on the material present at interparticle contacts.

alumina↗

Using in situ UO 2 bicrystal sintering to understand grain boundary dislocation nucleation kinetics and creep

Capillary evolution at bicrystal UO 2 grain boundaries is characterized using in situ transmission electron microscopy. The discontinuous nature of the densification process, both particle rotation and axial strain, along with the large activation stress for densification support a hypothesis that grain boundary strain in UO 2 follows nucleation rate limited kinetics at low to intermediate stresses, that is, less than ≈ 10 8 PA. Further, the temperature dependence of the average activation stress for sintering agrees well with analysis of bulk sintering data and creep data reported within the literature when analyzed in the context of a grain boundary dislocation nucleation rate limited kinetic model.