At least 19 records

Reduced Recombination and Improved Performance of CdSe/CdTe Solar Cells due to Cu Migration Induced by Light Soaking

The performance of CdTe solar cells has advanced impressively in recent years with the incorporation of Se. Instabilities associated with light soaking and copper reorganization have been extensively examined for the previous generation of CdS/CdTe solar cells, but instabilities in Cu-doped Se-alloyed CdTe devices remain relatively unexplored. In this work, we fabricated a range of CdSe/CdTe solar cells by sputtering CdSe layers with thicknesses of 100, 120, 150, 180, and 200 nm on transparent oxide-coated glass and then depositing CdTe by close-spaced sublimation. After CdCl 2 annealing, Cu-doping, and back metal deposition, a variety of analyses were performed both before and after light soaking to understand the changes in device performance. The device efficiency was degraded with light soaking in most cases, but devices fabricated with a CdSe layer thickness of 120 nm showed reasonably good efficiency initially (13.5%) and a dramatic improvement with light soaking (16.5%). Here, the efficiency improvement is examined within the context of Cu ion reorganization that is well known for CdS/CdTe devices. Low-temperature photoluminescence data and V oc versus temperature measurements indicate a reduction in nonradiative recombination due to the passivation of defects and defect complexes in the graded CdSe x Te 1–x layer.

CdSexTe1−x↗

Modeling delayed thermal runaway in nitric acid-soaked cat litter mixed with radioactive waste

Thermal ignition of radioactive waste within a 55-gallon drum was simulated by using a pressure-dependent waste decomposition model (Hobbs et al. in Process Saf Environ Prot https://doi.org/10.1016/j.psep.2022.09.047, 2022) calibrated with data from full-scale drum experiments (Parker et al. in The thermolytic response of a surrogate RNS waste mixture at the drum scale. Los Alamos National Laboratory Report LA-UR-16-21760, 2016) and validated with experiments from multiple laboratories (Hobbs et al. in Thermal analysis of aged nitric acid-soaked kitty litter in TRU waste drums-23370.WM2023 Conference, Phoenix, AZ, 2023). The acceleration of nitric acid chemistry reacting with an organic cat litter leading to thermal ignition was likely triggered by a restricted vent in the drum. Here, we address whether the form of the rate equation in (Hobbs et al. in Process Saf Environ Prot https://doi.org/10.1016/j.psep.2022.09.047, 2022) is sufficient to extrapolate thermal ignition within aged drums of similar content that have been stored in Texas for over nine years by investigating four different reaction rate forms for waste decomposition. A critical reaction rate reduction analysis is performed on each of these models to determine if delayed thermal runaway within vented aged waste is possible after nine years. We found that a pressure-dependent first-order rate expression not only predicted the accidental ignition of the waste drum, but the form also matches multiple experiments from different laboratories. Even though the waste composition decreases over time, the model predicts that acceleration leading to thermal runaway is possible if the waste is confined, even after 9 years. In conclusion, waste containing oxidizers such as nitric acid should not be mixed with organic adsorbents, especially if the waste is confined.

cookoff↗

Austenite Formation and Manganese Partitioning during Double Soaking of an Ultralow Carbon Medium‐Manganese Steel

Double soaking (DS) is a thermal processing route intended to produce austenite–martensite microstructures in steels containing austenite‐stabilizing additions and consists of intercritical annealing (primary soaking), followed by heating and brief isothermal holding at an increased temperature (secondary soaking), and quenching. Herein, experimental dilatometry during DS of a medium‐manganese (Mn) steel with nominally 7 wt% Mn and an ultralow residual carbon concentration, in combination with phase‐field simulations of austenite formation during secondary soaking, is presented. The feasibility of maintaining heterogeneous Mn distributions during DS is demonstrated and insight is provided on the effects of the secondary soaking temperature and prior Mn distribution on the ferrite‐to‐austenite phase transformation during the secondary soaking portion of the DS treatment.

36 MATERIALS SCIENCE↗

Tempering and Austempering of Double Soaked Medium Manganese Steels

The addition of a tempering or austempering step to the double soaking of a 0.14C–7.17Mn (wt pct) steel was investigated in the present contribution. The double soaking heat treatment is a two-step intercritical annealing heat treatment, which generates microstructures of athermal martensite, retained austenite and ferrite when applied to medium manganese steels. Microstructures following double soaking and (aus)tempering contained a combination of retained austenite, athermal or tempered martensite, and blocky or bainitic ferrite. X-ray diffraction, dilatometry and transmission Kikuchi diffraction were utilized to investigate microstructural changes which occurred during tempering or austempering. The resulting mechanical properties were measured using uniaxial tensile testing. The double soaking plus tempering heat treatment was shown to generate an ultimate tensile strength of 1,340 MPa in combination with 28 pct total elongation while the double soaking plus austempering heat treatment resulted in an ultimate tensile strength of 1,675 MPa and total elongation of 22 pct. Overall, both novel heat treatments produced a combination of strength and ductility desired for the third generation of advanced high strength steels.

36 MATERIALS SCIENCE↗

Effect of Liquid Electrolyte Soaking on the Interfacial Resistance of Li 7 La 3 Zr 2 O 1 2 for All-Solid-State Lithium Batteries

In this work, the impact of liquid electrolyte soaking on the interfacial resistance between the garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte and metallic lithium has been studied. Lithium carbonate (Li 2 CO 3 ) formed by inadvertent exposure of LLZO to ambient conditions is generally known to increase interfacial impedance and decrease lithium wettability. Soaking LLZO powders and pellets in the electrolyte containing lithium tetrafluoroborate (LiBF 4 ) shows a significantly reduced interfacial resistance and improved contact between lithium and LLZO. Raman spectroscopy, X-ray diffraction, and soft X-ray absorption spectroscopy reveal how Li 2 CO 3 is continuously removed with increasing soaking time. On-line mass spectrometry and free energy calculations show how LiBF 4 reacts with surface carbonate to form carbon dioxide. Using a very simple and scalable process that does not involve heat-treatment and expensive coating techniques, we show that the Li–LLZO interfacial resistance can be reduced by an order of magnitude.

25 ENERGY STORAGE↗

Universal and versatile morphology engineering via hot fluorous solvent soaking for organic bulk heterojunction

After explosive growth of efficiency in organic solar cells (OSCs), achieving ideal morphology of bulk heterojunction remains crucial and challenging for advancing OSCs into consumer market. Herein, by utilizing the amphiphobic nature and temperature-dependent miscibility of fluorous solvent, hot fluorous solvent soaking method is developed to optimize the morphology with various donor/acceptor combinations including polymer/small-molecule, all-polymer and all-small-molecule systems. By immersing blend film into hot fluorous solvent which is utilized as liquid medium with better thermal conductivity, the molecular reorganization is accelerated. Furthermore, fluorous solvent can be miscible with the residue of chloroform and chloronaphthalene above upper critical solution temperature. This mixed solvent diffuses around inside the active layer and selectively promotes molecular reorganization, leading to optimized morphology. Compared to widely-used thermal annealing, this approach processed under mild conditions achieves superior photovoltaic performance, indicating the practicality and universality for morphological optimization in OSCs as well as other optoelectronic devices.

14 SOLAR ENERGY↗

In-Situ Luminescence Imaging of Perovskite Solar Cells Demonstrates Increasing Spatial Nonuniformity Upon Light-Soaking Degradation

In this work we investigate degradation rates of triplecation mixed-halide perovskite p-i-n solar cells. We present an accelerated stress testing procedure using periodic blue light-soaking at elevated temperatures until devices reach ~80% of their initial efficiency. We track light-induced degradation via in-situ: photoluminescence (PL), current-voltage (I-V) curves, and transient photovoltage. Devices underwent 165 hours of light bias at 65degrees C. Results suggest that spatial uniformity in PL intensity decreases as device degradation increases. This investigation lays the groundwork to address the current gap in understanding the interplay between device performance and the evolution of macroscopic features in perovskite solar cells. Thus, we believe spatial characterization techniques will play a crucial role in the commercialization of perovskite solar cells.

imaging↗

Recovery of DNA from fired and unfired cartridge casings: comparison of two DNA collection methods

For over 10 years, various studies have attempted to increase the recovery of DNA from ammunition by modifying the DNA collection, extraction, purification, and amplification procedures, with varying levels of success. This study focused on the “soaking” method of Montpetit & O’Donnell [1] and the “rinse-and-swab" method of Bille et al. [2]. First, testing for the presence of exogenous DNA, 210 boxed cartridges (brass, steel, and nickel-plated) from nine manufacturers were swabbed and DNA was extracted, concentrated, and quantified. Extracts that quantified > 0 ng/µL (44 of 210) were amplified and genotyped with GlobalFiler™. Of those, only one extract yielded two alleles indicating that the manufacturing and packaging of ammunition was virtually DNA free. Next, to obtain a baseline comparison of two DNA collection methods on a non-metallic substrate and identify a suitable number of cells to spot on cartridges, different DNA input amounts of primary human adult epidermal keratinocytes (HEKa) were tested. Thereafter, 300 brass and 300 nickel-plated, cartridges were spotted with HEKa cells containing ~5 ng of DNA, fired or unfired, and processed with either method. Finally, five methods representing hybrids of the soaking and rinse-and-swab methods were tested to determine if variations of those methods could be used to increase DNA yield and recovery. The results show that the soaking method consistently yielded more DNA than the rinse-and-swab method from a non-metallic substrate. However, the comparison study demonstrated that both methods performed comparably for cartridges. On average, the soaking method recovered 0.25 ng of DNA (5.1% recovery) and the rinse-and-swab method recovered 0.28 ng (5.8% recovery). However, average recoveries were significantly different among three analysts and considerable variation in yields were observed, possibly due to storage time. Furthermore, consistent with prior reports, the DNA recovered from brass casings was only 16% of that recovered from nickel-plated casings and the average yield of DNA from fired casings was reduced to 67% of unfired casings. Moreover, DNA extracts from brass or nickel-plated casings did not appear to contain amplification inhibitors and only 30/596 appeared severely degraded. Finally, both the published rinse-and-swab and soaking methods yielded more DNA than all modifications of the two methods. Overall, both methods yielded equivalent DNA quantities. Additionally, recovery of DNA from any given cartridge casing may be dependent on storage time as well as the skill, proficiency, and experience of the analyst and may reflect stochastic effects, particularly for casings containing low copy and/or degraded DNA.

59 BASIC BIOLOGICAL SCIENCES↗

Sealability Qualification of Material Extruded Zytel Gaskets at Extreme Temperatures

In this work, an in-depth qualification of additively manufactured Zytel for gasketing proton exchange membrane fuel cells (PEMFC’s) subject to extreme temperature conditions. The temperature cycling of the PEMFC from 55°C to 100°C accelerates the deterioration of these gaskets compared to that of conventional operation. The additive manufacturing process employed to print these gaskets is material extrusion using Zytel filament. In order to see the effects of the temperature of interest on the printed specimen, each specimen was thermally soaked and then charactered and tested according to ASTM standard F37B. ASTM F37B tests a materials ability to seal and maintain it while bearing both a compressive load and internal pressure load to simulate being in static operation. This process of thermally soaking and sealability testing is shown to show the validity of both this material and additive manufactured components for other applications as well. It is observed that soaking the gaskets at 100°C corrects some of the defects that are present after printing such as missing layers and small voids on the surface of the samples. This allowed for the hot soaked materials to perform better than the samples at room temperature and cold soaked.

Sealability↗

Behavior of Na and RbF-Treated CdS/Cu(In,Ga)Se 2 Solar Cells with Stress Testing under Heat, Light, and Junction Bias

In this work, the effects of Na and RbF alkali treatment on the metastability behavior of CdS/Cu(In,Ga)Se 2 solar cells are investigated with stress factors of heat, junction bias, and illumination. Four device types with and without Na or RbF treatments are subjected to heat- and light-soaking under open- and short-circuit (OC, SC) junction bias. Low-Na devices show a higher bandgap due to increased minimum Ga content, higher recombination current, and lower open-circuit voltage (V OC ). Devices with RbF post-deposition treatment (PDT) show an improvement in net doping density ≈10 16 cm –3 , V OC , and efficiency. Heat- and light-soaking under OC junction bias provokes an increase in net carrier concentration and V OC irrespective of the alkali treatments. After SC stress, a decrease in V OC and net carrier concentration is observed, which can be stabilized by RbF-PDT. An increase in Na and oxygen concentration in CIGS is observed for baseline and low-Na devices, respectively, after OC stress. The oxygen concentration in CdS decreases after heat- and light-soaking for devices without RbF-PDT, whereas it remains unchanged for devices with RbF-PDT. The atomic concentration profiles in CIGS significantly stabilize as a function of stress with the addition of RbF-PDT.

14 SOLAR ENERGY↗

Electrical Potential Investigation of Reversible Metastability and Irreversible Degradation of CdTe Solar Cells

In this paper, we report on the stability of CdTe devices with a structure of TCO/MZO/CdSeTe/CdTe/back-contact. The device showed reversible transitions between the light-soak state (LSS) with the best device efficiency and the dark-soak state (DSS) with an inferior efficiency. However, it showed an irreversible degradation state (DgS) driven by long-hour light soaking at an elevated temperature. We have investigated transitions between these three states from the perspective of the electric field by nm-resolution potential imaging across the devices using Kelvin probe force microscopy (KPFM). The results exhibit different anomalous electric field profiles. At the LSS, the electric field exhibits a main peak inside the CdSeTe layer instead of the MZO/CdSeTe heterointerface, illustrating a buried homojunction (BHJ) of the device. At the DSS, a large electric field peak at the MZO/CdSeTe interface was measured, which probably resulted in the inferior fill factor at the DSS. At the DgS, the electric field peak at the MZO/CdSeTe interface increased further and a third electric field was measured at the back contact of the device. Device modeling using COMSOL software, in alignment with both the electric field and device current-voltage curves, elucidates that a low n-doped CdSeTe in the region near the MZO/CdSeTe interface caused the BHJ in the LSS and a loss of MZO doping and/or increase of the conduction band offset spike due to long-term stress caused the increased electric field near the MZO/CdSeTe interface at the DgS.

CdTe solar cell↗

Heavy-Duty Vehicle Activity Updates for MOVES Using NREL Fleet DNA and CE-CERT Data

The U.S. Environmental Protection Agency's (EPA's) Motor Vehicle Emission Simulator (MOVES) is a publicly available tool used by researchers and policymakers to help understand motor vehicle emission sources at a national, county, and project level. Estimates of heavy-duty activity in the most recent version of the model at the time this work was conducted, MOVES2014, was identified as an area in need of improvement. The start activity in MOVES2014 is based on a limited and dated data set. In addition, MOVES2014 relies on drive cycles that represent on-network activity but do not account for idling activity that occurs on off-network roads, such as at a distribution center, while the truck is queuing or during loading and unloading. As a result, MOVES2014 may currently underestimate the number of starts and idle and soak time for heavy-duty trucks in real-world operation. The National Renewable Energy Laboratory (NREL) has previously leveraged its expansive Fleet DNA database of heavy-duty vehicles to idle and start activity for six of the nine heavy-duty vehicle source types of classes in the MOVES model. The data available in Fleet DNA from 416 conventional, diesel-powered vehicles provided activity estimates from more than 120,000 hours of operation throughout 14,682 vehicle days between October 2006 and January 2016. NREL calculated start fraction, starts per day, soak fraction, and idle fraction by hour of the day for each vehicle type, state, and vocation, and provided results in .CSV files that can be translated to MOVES table inputs. The idle and start activity from this initial analysis of Fleet DNA data was used to develop default idle and start data for heavy-duty vehicles in MOVES3. Satisfied with the results from the Fleet DNA data used for MOVES3, the EPA asked NREL to extend this start/soak/idle analysis using additional data from a larger number of vehicles for a potential future update to the MOVES model. Such a data set was achieved from a project led by the University of California at Riverside, College of Engineering, Center for Environmental Research & Technology (CE-CERT) and funded by California Air Resources Board. Specifically, this data set consists of 90 heavy-duty vehicles operated mainly in California, which can be separated into five of the nine heavy-duty vehicle classes in the MOVES model. In addition, the heavy-duty activity database collected by CE-CERT provided activity estimates from more than 44,000 hours of operation throughout 4,724 vehicle days between November 2014 and September 2016. This report details the analysis of the heavy-duty activity database collected from the University of California at Riverside by providing graphical analysis and context for the start, soak, and idle distributions. The comparison of the related results from both the Fleet DNA and CE-CERT data sets are documented as well.

33 ADVANCED PROPULSION SYSTEMS↗

Metastability and Degradation of CdTe Solar Cells Investigated by nm-Scale Electrical Potential Imaging

We report on investigations of reversible metastability and irreversible degradation of MZO/CdSeTe/CdTe devices from the perspective of electric field across the device using Kelvin probe force microscopy (KPFM). The device showed reversible transitions between the light-soak state (LSS) with the best device efficiency and the dark-soak state (DSS) with an inferior efficiency. However, it showed an irreversible degradation state (DgS) driven by long-hour light soaking at an elevated temperature. The nm-scale KPFM electric field imaging on cross-sections of the devices revealed different anomalous electric field profiles. The electric field at the LSS exhibits a main peak inside the CdSeTe layer but not at the MZO/CdSeTe heterointerface, demonstrating that working junction of the device is a buried homojunction (BHJ). At the DSS, a second electric field peak was observed at the MZO/CdSeTe interface with a similar strength to the main BHJ, which probably caused the decrease in fill factor at the DSS. At the DgS, the electric field peak at the MZO/CdSeTe interface increased significantly and a third electric field was measured at the back contact of the device. Device modeling using COMSOL and in alignment with both the electric field and device current-voltage curves suggest that a slightly low n-doped CdSeTe in the region near the MZO/CdSeTe interface caused the BHJ, and that either a loss of MZO doping or increase of the conduction band offset spike due to long-term stress caused the fill factor-dominated degradation and the increased electric field near the MZO/CdSeTe interface at the DgS. The former, MZO doping decrease, is more plausible by referring the related literature.