Non-contact Current-Voltage (I-V) Tracer for Photovoltaics

This report presents a non-contact approach to simultaneously obtain current-voltage (I-V) curves of photovoltaic (PV) substrings and modules in a string without the need of disconnecting the individual modules from the string. There are two types of I-V curve tracers currently available in the marketplace, capacitor-based and electronic load-based. The primary requirement of these conventional I-V tracers is the disconnection of individual modules in the string so the individual modules contacted through the connectors of the individual modules. These contact-tracers have three major limitations in the utility scale power plants: First limitation – Weather and Accuracy: The mass-produced commercial contact-tracers cannot obtain the I-V curves of both string and its modules (as high as 30 modules), almost simultaneously (within about 5 minutes) at, practically, a single irradiance level, a single module temperature, a single spectrum and a single AOI (angle of incidence). This inability of the contact-tracers forces the testing personnel to wait for an extended or multiple sunny (>800 W/m 2 ) duration(s) of a cloudy day. This is a serious limitation as waiting for the sunny conditions or days is a huge practical challenge in almost all locations, except desert locations. Also, since the I-V curves are obtained at different prevailing weather conditions, it becomes critical to translate all the measured I-V curves of 30 modules in the string to a single test condition, for example STC (standard test conditions), so the underperforming modules can be identified. The accuracy of translation equations is heavily influenced by the irradiance level and temperature, spectral and AOI ranges; Second limitation - Safety: The second limitation is related to the high voltage electrical safety of the test personnel during disconnecting and reconnecting of individual modules or cable connectors from the string under daylight conditions and damaging of the original module connectors (especially the field aged connectors) during the disconnecting and reconnecting process; Third limitation – Labor: The third limitation is related to the enormous amount of time and hardship for the test personnel under prevailing (often harsh) protracted field conditions. This project was executed by Arizona State University in collaboration with its industry partner, PV Measurements Inc. (PVM). To mitigate all the three challenges of the state-of-the-art equipment indicated above, we utilized a non-contact I-V (NCIV) tracer approach. In this approach, we utilized an electrostatic voltmeter (ESV) and voltage sensor/probe combination to obtain I-V curves. The ESV units are extensively used in the high voltage industry but not in the PV industry. To obtain the simultaneous I-V curves of the substrings and modules within a string, we utilized multiple commercial ESV-Probe sets. In this approach, we utilized a non-contact voltage sensor (called, Probe) placed on the glass surface of the module (above the last cell of the module). This probe senses the module voltage (with respect to ground) through measured capacitance which is dictated by the surface charges (which in turn is dictated by the module voltage) and transmits the sensed voltage to the voltmeter (called, ESV or NCV, non-contact voltmeter). The current is sensed by a non-contact hall sensor. In a 30-module string, the 30th probe obtains the entire string I-V along with the string I-V obtained by the electronic load. so that the I-V curves of the substrings and modules can be obtained by NCIV without the need of disconnecting the individual modules in the string. The string I-V curves obtained by the electronic load and NCIV can be compared for the accuracy determination. One can use 30 ESV units and 30 Probes to obtain 30 I-V curves of a 30-module string or use just 5 ESV units and 30 Probes in conjunction with 5 six-channel switchboxes (called, 6:1 switchboxes). To reduce the equipment cost, we utilized the 6:1 switchbox approach so the number of ESV units is reduced from 30 to 5. The approaches, achievements and challenges of this project are detailed in this report.

14 SOLAR ENERGY↗

Outdoor Deployment Data for a Four-Terminal GaAs//Si Tandem Solar Mini-Module

This dataset contains the complete outdoor measurement and analysis data for a mechanically stacked, four-terminal (4T) gallium arsenide (GaAs)//silicon (Si) tandem solar mini-module deployed from October 2019 to January 2021 at the Solar Radiation Research Laboratory (SRRL) in Golden, Colorado, USA. The data support a performance modeling and degradation analysis framework for tandem photovoltaic devices, as described in the accompanying publication. The dataset includes: (1) current–voltage (J–V) characteristics of each sub-cell measured approximately every five minutes, with extracted performance parameters; (2) spectral irradiance from an EKO MS-710 WISER spectroradiometer, along with derived spectral mismatch ratios (SMR) and average photon energy (APE); (3) one-minute resolution meteorological data from the co-located SRRL weather station and GPS-derived precipitable water vapor (PWV); (4) pre-deployment laboratory characterization (external quantum efficiency, J–V curves, standard test conditions parameters); (5) outdoor-extracted temperature and PWV correction coefficients; and (6) PVcircuit equivalent-circuit simulation outputs used for model validation. Degradation rates of −4.1 ± 0.2 %/year (GaAs) and −2.5 ± 0.9 %/year (Si) were determined using a filtering and normalization methodology adapted for fixed-tilt tandem modules. All data are provided in open, portable formats (Apache Parquet, CSV, JSON) to enable full reproducibility of the published analysis.

14 SOLAR ENERGY↗

Performance Modeling of Tandem Photovoltaics: A Yearlong Outdoor Degradation Analysis of a Ga⁢As//Si Minimodule

We present a performance modeling and degradation analysis framework for tandem photovoltaic modules, building upon established procedures for crystalline silicon devices and adapting them to account for the spectral sensitivity of multijunction technologies. The methodology employs filter criteria to select outdoor measurements close to standard test conditions (STC) under stable spectral and ambient conditions, followed by normalization of power production data with corrections for temperature, irradiance, and precipitable water vapor. We demonstrate this framework using a mechanically stacked four-terminal gallium arsenide (Ga⁢As) // silicon (Si) tandem solar minimodule deployed outdoors from October 2019 to January 2021 in Golden, Colorado, USA. We determined degradation rates of −4.1 ±0.2%/year for the Ga⁢As subcell and −2.5 ±0.9%/year for the Si subcell, with analysis of individual performance metrics indicating that packaging degradation, particularly delamination, was the dominant failure mode. Simulations using PVcircuit, an open-source equivalent-circuit solver, confirmed these findings. The presented methodology provides a reproducible foundation for performance modeling and degradation analysis of emerging tandem technologies.

14 SOLAR ENERGY↗

NREL's Improved Linearity Testing of Photovoltaic Reference Cells

Photovoltaic devices are characterized under standard testing conditions that include a defined reference spectrum and total irradiance. International standards for reference cell calibrations require that reported reference cell response (typically Isc) vs. total irradiance must be linear. How can linearity be efficiently determined? In 2006 NREL developed a test bed, based on the "two-lamp method" that provided a low cost, but low accuracy method for determining whether cell response was linear with irradiance. This paper describes very simple changes to NREL's historical method [1] for determining linearity that yield greatly improved results. It also describes a method that can be used to quantify and correct for non-linearity.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Impact of undoped substrates on high performance silicon solar cells

Today's highest-efficiency silicon solar cells typically operate near the threshold between low-level and high-level injection. It is not well understood if pushing further into a regime in which the cell operating point is solidly in high-level injection at all times of the day has further benefits for the solar cell performance. From a reliability perspective, cells fabricated on lower doped silicon have a larger breakdown voltage. This advantage can affect the design of modules allowing higher voltages and a relaxation of the number of bypass diodes needed. In this project, we present a comprehensive assessment, both experimental and using simulation, of how bulk resistivity, light intensity, and operation temperature impact the performance of the silicon solar cell. This work incorporates a comprehensive device physics analysis assisted by numerical simulation. The source code is now available under General Public License (GPL3), and to further leverage the findings of this project and outreach people outside of the scientific community, we are working with www.pveducation.org (which receives >1 million visitors a year) to create interactive content using our simulation results. The simulation results indicate that high bulk resistivity wafers (>>10 Ωcm) require bulk Shockley-Read-Hall (SRH) lifetimes in the millisecond range to outperform wafers with standard bulk resistivities (<10 Ωcm). Additionally, above bulk resistivities of 10 Ωcm (the exact value depends on the bulk characteristics of the wafer), the cell efficiency is weakly dependent on the bulk resistivity. As a result, ingot manufactures may have an opportunity to further reduce wafer cost by growing higher resistivity ingots that are more tolerant to resistivity variations. This project is particularly relevant today, as solar cell architectures with improved surface passivation and milliseconds lifetimes wafers are commercially available, leveraging potential benefits of using higher bulk resistivities. Outside of interdigitated back contact (IBC) cell, reported studies on high resistivity silicon (>100 Ωcm) are very limited. To the best of our knowledge, this project provides for the first-time experimental insight on solar cells fabricated on wafers with bulk resistivities up to several thousand Ωcm, delivering a comprehensive vision of their performance under real-world temperature and light intensity operation conditions. We manufactured and characterized solar cells with bulk resistivities in the range of 1 Ωcm to >15k Ωcm. Under standard testing conditions (STC), we measured solar cells efficiencies over 20% over the entire range of bulk resistivities, using our baseline cell processing. To evaluate the cell performance in real-world operation conditions, the solar cells were measured at different temperatures (25-80°C) and at different light intensities (0.1-1 suns). The measurements show that the bulk resistivity does not impact the solar cell response to temperature and light intensity. Similar thermal coefficients (TC) were measured for standard and high bulk resistivities, and they are comparable with the TC values reported in the literature for standard bulk resistivities <10 Ωcm. After light soaking, the solar cell didn’t show signs of light-induced degradation (LID). This result was expected since n-type float zone (FZ) wafers were used in this work, i.e. low traces of boron and low concentration of oxygen (oxygen is typically found in the seed end of Czochralski (CZ) ingots). We measured for high bulk resistivities (>10 Ωcm) extremely high breakdown voltages (>1000V). In conclusion, the insight provided by this project can positively impact the levelized cost of energy (LCOE) of the photovoltaic systems through its effect on cell and ingot manufacturing yield, silicon cell power output, and module reliability.

14 SOLAR ENERGY↗

GeoMelt{sup R} In-Container Vitrification (ICV){sup TM} for Fukushima Daiichi Water Treatment Secondary Wastes - 20212

The Japanese government is supporting development work implemented jointly by Veolia subsidiaries Kurion Japan, K.K., Veolia Nuclear Solutions (VNS), Inc., and Veolia Nuclear Solutions Federal Services, LLC for treating radioactive waste generated from Fukushima Daiichi Nuclear Power Station (NPS) water treatment using the GeoMelt{sup TM} In-Container Vitrification (ICV){sup TM} technology. The initial work consisted of glass formulation and engineering-scale testing which was completed in 2018, in the frame of an IRID (International Research Institute for Nuclear Decommissioning) program as part of a project subsidized by Japan's Ministry of Economy, Trade and Industry (METI). The Fukushima Daiichi NPS Mid- and Long-Term Road-map requires investigation of methods to stabilize solid wastes (and to immobilize radioisotopes in the wastes) generated as a result of emergency response and decommissioning activities. Cooling water treatment has resulted in a significant amount of solid and slurry secondary wastes (mostly adsorbents and ion-exchange materials) which will require processing at some point. GeoMelt{sup R} ICV{sup TM} is a joule-heated melter technology which uses a refractory-lined single-use container combining the melter and disposal container. There is no pouring required nor concerns with refractory corrosion which allows the process to accommodate a wide range of waste chemistries and high waste loadings. The testing described here consisted of three engineering-scale melts, each processing between 212 kg and 240 kg of waste simulants, glass formers, and non-radioactive cesium (Cs) and strontium (Sr) tracers. Continuous isokinetic stack sampling of off-gas emissions was performed for each test in order to calculate Cs and Sr retention in the glass wasteform. Single-pass retention of Cs in the final glass wasteform ranged from 91.46 to 99.30%, and single-pass retention of Sr ranged from 99.76 to 100%. Planned particulate recycle will increase these retention levels. Melt 1 processed a mixture of KUR-EH (a zeolite-based ion-exchange material), simulated Advanced Liquid Processing System (ALPS) Carbonate and Iron Slurries, and glass additives. Melt 2 processed a mixture of KUR-EH, KUR-TSG (a titanate-based adsorbent), and glass additives. Melt 3 processed a mixture of KUR-EH, simulated barium sulfate/iron ferrocyanide sludge (AREVA sludge), and glass additives. Waste loadings for these melts ranged from 70 weight percent (wt%) to 82 wt%. Vitrification produces a waste form much denser than the stored water treatment secondary waste wastes, resulting in significant volume reduction. Volume reductions for the three tests ranged from 74 to 79 vol%. Vitrification produces a chemically durable wasteform. Pacific Northwest National Laboratory (PNNL) tested three glass samples from each engineering-scale melt) by the Materials Characterization Center 1 (MCC-1) test, an international standard leach test of the chemical durability of nuclear waste glasses. PNNL also obtained one U.S. reference glass (EA Glass) and two Japan reference glasses P0798) and tested these under the same MCC-1 conditions (90 deg. C, 10 m-1, DIW, and 7, 14, 28-day) as the GeoMelt{sup R} ICV{sup TM} glasses. The GeoMelt{sup R} ICV{sup TM} glasses exhibited lower total normalized releases and 14- to 28-day normalized release rates than the three reference glasses. These results suggest that the GeoMelt{sup R} ICV{sup TM} glasses have durabilities on par with high-level waste glasses under standard test conditions. Post-melt process sampling and analysis indicated no Cs migration into the melter refractory materials and very little deposition of Cs or Sr onto the melter hood or off-gas piping internals. The results of the testing indicated good Cs retention in the glass, high volume reduction and waste loadings, and excellent chemical durability. These factors are important to minimize treatment costs and to protect workers and the environment. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Methods for In Situ Electroluminescence Imaging of Photovoltaic Modules Under Varying Environmental Conditions

Electroluminescence (EL) imaging is a powerful tool used to identify defects in photovoltaic solar cells. Typically, this type of characterization is performed in the dark using a current injection that equals short-circuit current measured at standard test conditions (STC). Restricting imaging to such a temperature range limits the information obtained about the module and cells. However, it is not trivial to develop a tool that would allow for EL imaging to be performed under a wider range of temperatures. Here we demonstrate an in situ EL imaging capability developed within an environmental chamber that allows for control of sample temperatures between –40 and 90 °C. Additionally, we demonstrate EL imaging of 4-cell mini-modules (MiMo) under front-side mechanical loading. A Raspberry Pi-connected camera with short-pass filter removed is used for EL imaging. The camera is low-cost with a small form-factor, appropriate for use in a harsh, enclosed environment. The camera is installed within a thermally isolating housing mounted within the environmental chamber. Three example cases are given for MiMos that exhibit various forms of degradation including solder fatigue and cell cracking. It is shown that by measuring at conditions above and below STC, different behaviors may be identified. In some cases, restricting characterization to STC may lead to a failure to detect damage existing in the sample.

14 SOLAR ENERGY↗

Comprehensive Performance Calibration Guidance for Perovskites and Other Emerging Solar Cells

Emerging photovoltaic (PV) technologies (e.g., organic, perovskite, and solution processed quantum dot) have attracted remarkable attention with the rapid growth of their efficiencies, and their transition toward commercialization. Accurate and reliable efficiency measurements of these PV technologies are crucial, yet much more complicated than for conventional PV technologies due to the former's pronounced dynamic responses to changes in measurement conditions (e.g., current–voltage (I–V) scan rate and preconditioning) and their susceptibility to degradation. Adjustments to the measurement procedures are therefore necessary so that a reproducible “steady state” is reached during measurement. Furthermore, given the small size of many emerging cells, inappropriate device area definition and solar simulator setup can lead to measurement errors. Here, comprehensive efficiency calibration guidance is offered for emerging solar cells, including area measurement; spectral irradiance translation to standard test conditions; and steady-state electrical performance. The necessity of reporting steady-state efficiency is justified with a statistical performance comparison between conventional and steady-state I–V scans over hundreds of cells the group has received globally for efficiency certifications. The procedures described here do not require specialized measurement instrumentation; what matters most are changes to the measurement protocols. These described changes aim to enable better comparisons between reported efficiencies.

14 SOLAR ENERGY↗

Spectral Effects on the Energy Harvesting Efficiency of Two- and Four-Terminal Tandem Photovoltaics

In this work, the effect of a varying spectral irradiance and top cell bandgap on the energy harvesting efficiency of two-terminal (2T) and four-terminal (4T) perovskite//silicon tandem solar cells under outdoor operating conditions is investigated. For the comparison, an optoelectronic model employing a 1 year outdoor data set for a 4T mechanical stacked gallium arsenide (GaAs) on crystalline silicon (Si) tandem device is first validated. Then, the verified model is used to simulate perovskite//silicon tandem devices with a varying perovskite top cell bandgap for a location in Golden, Colorado, USA. Here, a spectral binning method to efficiently reduce and improve the visualization of the 1 min-resolved environmental data while maintaining the simulation accuracy is introduced. The findings reveal that, for a device that is current matched under standard testing conditions, the annual spectral deviation reduces the energy harvesting efficiency by only 2% rel . When additional realistic losses for the 4T are taken into account, 2T devices are shown to have an energy-harvesting efficiency that is at parity or higher. Deviations in the top cell bandgap are more than 0.1 eV from current matching result in a reduced energy harvesting efficiency of more than 5% rel for the 2T tandem device.

14 SOLAR ENERGY↗

Investigation of the Semicoa 2N7616 and 2N7425 and the Microsemi 2N7480 for Single-Event Gate Rupture and Single-Event Burnout

Single-event-effect test results for hi-rel total-dose-hardened power MOSFETs are presented in this report. The 2N7616 and the 2N7425 from Semicoa and the 2N7480 from International Rectifier were tested to NASA test condition standards and requirements. The 2N7480 performed well and the data agree with the manufacture's data. The 2N7616 and 2N7425 were entry parts from Semicoa using a new device architecture. Unfortunately, the device performed poorly and Semicoa is withdrawing power MOSFETs from it line due to these data. Vertical metal-oxide-semiconductor field-effect transistors (MOSFETs) are the most commonly used power transistor. MOSFETs are typically employed in power supplies and high current switching applications. Due to the inherent high electric fields in the device, power MOSFETs are sensitive to heavy ion irradiation and can fail catastrophically as a result of single-event gate rupture (SEGR) or single-event burnout (SEB). Manufacturers have designed radiation-hardened power MOSFETs for space applications. See [1] through [5] for more information. The objective of this effort was to investigate the SEGR and SEB responses of two power MOSFETs recently produced. These tests will serve as a limited verification of these parts. It is acknowledged that further testing on the respective parts may be needed for some mission profiles.

Scheick, Leif↗

Susceptibility to polarization type potential induced degradation in commercial bifacial p-PERC PV modules

Potential induced degradation (PID) is a reliability issue affecting photovoltaic (PV) modules, mainly when PV strings operate under high voltages in hot/humid conditions. Polarization-type PID (PID-p) has been known to decrease module performance quickly. PID-p can be reduced or recovered under the light in some cases, but this effect, as expected, would be less pronounced on the rear side of bifacial PV modules receiving lower irradiance. As bifacial PV modules are projected to dominate the PV market within the next 10 years, it is crucial to understand the PID-p issue in bifacial modules better. In this study, we performed indoor PID testing to induce PID-p on 14 commercial bifacial p-PERC modules with three different module constructions from three manufacturers. Here, four rounds (+ve and –ve polarities for front and rear sides) of PID testing are done at 25°C, 54% relative humidity (RH) for 168 h using the aluminum foil method. Each module side (front cell side and back cell side) is tested individually under both negative and positive voltage bias. The results show that the highest degradation of 32% in maximum power (Pmax) at standard test conditions (1000 W/m 2 ) and 51% at low irradiance (200 W/m 2 ) has been observed in some cases. Recovery under sunlight is also done, and outcomes show a near-complete recovery in Pmax. This study presents an extensive experimental methodology and a detailed analysis to systematically and simultaneously/sequentially evaluate multiple construction types of bifacial modules to the PID-p susceptibility and recovery.

14 SOLAR ENERGY↗

How Should Researchers Measure Perovskite-Based Monolithic Multijunction Solar Cells’ Performance? A Calibration Lab's Perspective

Perovskite multijunctions (PVSK MJs) have made remarkable progress with monolithic PVSK/PVSK tandems surpassing the efficiency of single-junction (1 J) PVSK cells and PVSK/Si cells reported to exceed the 30% efficiency mark. These efficiencies are reported at standard test conditions (STC), established by the photovoltaic (PV) community to facilitate comparison between devices and technologies. Herein, it is discussed why an accurate STC performance measurement for a MJ is more complicated than for a 1 J cell and the special aspects to be considered when measuring the current-voltage characteristics and the performance of PVSK-containing MJ cells are emphasized. It is discussed why a spectrally adjustable solar simulator is needed and the sequence of accurate performance measurement, namely measurement of the spectral response of each junction, adjustment of the spectrum, and appropriate protocols for measuring the power output of the device at STC, is presented. For all these, common errors and pitfalls that sometime lead to misleading interpretation of the results are presented, and the methods to evaluate the accuracy of the data when a spectrally adjustable solar simulator is not available are recommended. Finally, first step is taken toward recommending performance measurement approaches when high throughput is required as will eventually be in a production line.

14 SOLAR ENERGY↗

Thermal model to quantify the impact of sub-bandgap reflectance on operating temperature of fielded PV modules

Minimizing module heating is an effective way to increase the lifetime energy output of photovoltaic systems. Maximizing the reflection of light that is unusable for energy conversion is one of the most promising ways to reduce the operating temperature of fielded modules. We derive a model based on a steady-state energy balance to quantify the temperature benefit of cell or module optical modifications aimed at improving reflection of light with photon energies below the photovoltaic cell bandgap energy. This more detailed model is then simplified so that, from outdoor measured data, temperature differences arising from reflectance can be isolated from those arising from irradiance, wind speed, and module standard-test-condition efficiency.

14 SOLAR ENERGY↗

Polarization-type potential-induced degradation in bifacial PERC modules in the field

This study examines the susceptibility of bifacial glass/glass passivated emitter and rear cell (PERC) modules to potential-induced degradation-polarization (PID-p) in the field. While there are several studies showing PID-p occurring on both front and back faces of bifacial PERC in accelerated tests, we address the yet unclarified behavior in fielded modules. We examine the effects of mounting configuration; specifically, comparing modules mounted near ground and in elevated ground rack configurations. Modules with the cell circuit in -1500 V system voltage configuration, whether mounted on racks about 30 cm above the ground or elevated 2 m high showed mean degradation of 4.5% to 6% in power under standard test conditions over about 2.5 weeks as measured from the front side of the module. This extent of degradation remained sustained for a duration of about 6 months analyzed. Average daytime temperatures of modules in the various mounting configurations were similar and therefore judged to be insufficient to be a primary influence for the modest PID-p rate differences that we observed among mounting configurations. Increased leakage current in the morning suggests morning dew was sustained longer on modules near the ground measured over six months which would be expected to increase the PID-p rate over the long term. However, the main difference seen between the modules on the various mountings during the initial period with up to 6% mean degradation by PID-p was the approximately two times the irradiance from albedo on the rear of modules mounted in elevated ground rack compared to those on the near ground rack. This difference in incident albedo led to a modestly reduced rate of the development of PID-p of the modules on the elevated ground rack. The difference is attributed to the dissipation of PID-p-causing electrical charge by the albedo incident on the module rear. The behavior could be modeled by a sigmoidal equation with consideration of the differences in the insolation on the module rear.

14 SOLAR ENERGY↗

Evaluation of an LED Simulator for Single- and Multi-Junction PV Cell Performance Testing

We present the evaluation of a solar simulator comprising a Light Emitting Diode (LED) array as its light source. While multiple applications can be envisioned for such a light source, here we focus on its use for performance testing of solar cells at Standard Test Conditions. With this in mind, we present characterization of the spatial uniformity of the irradiance and its temporal stability as well as the spectral range and spectral class. For a multisource simulator, the spectral uniformity across the test plane should also be evaluated and we discuss a method for performing this evaluation that is well suited to a solar cell performance testing application. One major advantage of this simulator is the ability to easily adjust the spectral output as needed in multijunction PV cell measurements and we also discuss this application here.

LED↗

PV Lifetime Project (2021 NREL Annual Report)

DOE's PV Lifetime project was initiated in 2016 with the goal of accurately characterizing the early-life evolution of photovoltaic (PV) field performance. Different PV cell and module technologies result in different initial performance loss rates due to effects like light-induced degradation (LID) and light & elevated temperature-induced degradation (LeTID). To accurately characterize the initial field performance loss requires the use of high-accuracy indoor IV curve measurements at standard test conditions. Therefore, PV modules involved in this study are removed from the field once or twice per year and brought indoors for measurement. Current samples deployed and monitored in this way include Jinko Solar (2016), Trina Solar (2016), Hanwha Q-Cells (2017), Panasonic (2018), LG (2018), Canadian Solar (2018), Mission Solar (2019). More recently, modules from Sunpreme (2019), and LONGi (2020) have been deployed but not yet analyzed. Overall annual performance loss rates are as follows: our first modules to be deployed (Jinko and Trina) have annual median performance loss rate between -0.4%/yr and -0.9%/yr, mainly concentrated in the first year. The QCells mono-PERC and multi-PERC modules have an annual degradation rate of -0.76%/yr and -0.69%/yr respectively, also concentrated in the first year of operation. Panasonic and LG modules displayed negligible performance loss in the past two years, at 0.1%/yr and -0.0%/yr respectively. They also were the only modules with initial IV curve measurements consistently above the nameplate rating. Possibly relatedly, these are also the only two N-type silicon module types analyzed so far. Canadian Solar multi-PERC modules demonstrated a -1.3%/yr degradation rate which actually accelerated in the past year, so this will be a module type to monitor in future years. Mission Solar modules exhibited strong recoverable performance loss, consistent with LeTID susceptibility. (The same is true for the Jinko JKM260 module type). Annual performance loss actually showed improvement in time at +0.3%/yr after 2 years in the field, although the module initially was measured at 3% below nameplate rating. These modules could therefore be experiencing a form of post-LeTID recovery. Initial measurements have been conducted on the next two module types - Sunpreme n-HIT and LONGi bifacial mono-PERC. We will report on initial year-1 performance change for these modules in the next PV Lifetime annual report. For the remaining modules, an additional year of field exposure will provide greater certainty in annual degradation rates, particularly for those with degradation concentrated in the initial year of field deployment.

14 SOLAR ENERGY↗

Solar Canopy Expansion Project (Final Technical Report)

This project is a parking-lot canopy solar photovoltaic system, consisting of four canopy structures and 1,080 470-watt (W) modules. The nameplate rating of the project is 507.6 kilowatts direct current (kWDC) at Standard Test Condition (STC), and 448 kilowatts alternating current (kWAC). It is interconnected to the existing Tribe-owned medium-voltage micro-grid generation system via a step-up transformer and short medium-voltage line. This project offsets energy usage from more expensive existing sources, specifically the Tribe-owned gas-fired engine generators providing the primary power source for existing Tribal facilities and the electric utility, which provides an alternate source. The solar photovoltaic system is a renewable source, which has the benefit of reducing reliance on fossil-fuel burning sources. By reducing demand on existing Tribe-owned conventional generators, the project has avoided the need to add more conventional generation and has prolonged the lifespan of existing gas-fired engine generators. The project reduced energy costs and reliance on fossil-fuel burning power sources, increasing Tribe-owned generating sources and self-reliance, and prolonging the lifespan of existing generators. A side benefit to the project is the production of dozens of covered parking spaces in the existing parking lot.

14 SOLAR ENERGY↗