Search NASA⌕ Search

SEARCH · Search NASA

Results for “subcritical crack growth”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

A study of the effect of subcritical crack growth on the geometry dependence on nonlinear fracture toughness parameters

The effect of subcritical crack growth on the geometry dependence of nonlinear fracture toughness parameters was studied by comparing the toughness values for different specimen geometries at the onset of subcritical crack growth and at the initiation of unstable crack propagation. Center-cracked thin sheet specimens of 2024-T3 and 7075-T6 aluminum alloys were tested by varying the specimen length L, width w, and crack length-to-width ratio c/w. When the onset of unstable crack propagation was selected as the critical point, the nonlinear energy toughness and the R curve toughness increased with increasing w and decreasing L and c/w. However, when the onset of subcritical crack growth was taken as the critical point, energy toughness and the linear toughness values were independent of these geometrical variables.

Jones, D. L.↗

Subcritical crack growth in soda-lime glass in combined mode I and mode II loading

Subcritical crack growth under mixed-mode loading was studied in soda-lime glass. Pure mode I, combined mode I and mode II, and pure mode II loadings were achieved in precracked disk specimens by loading in diametral compression at selected angles with respect to the symmetric radial crack. Crack growth was monitored by measuring the resistance changes in a microcircuit grid consisting of parallel, electrically conducting grid lines deposited on the surface of the disk specimens by photolithography. Subcritical crack growth rates in pure mode I, pure mode II, and combined mode I and mode II loading could be described by an exponential relationship between crack growth rate and an effective crack driving force derived from a mode I-mode II fracture toughness envelope. The effective crack driving force was based on an empirical representation of the noncoplanar strain energy release rate. Stress intensities for kinked cracks were assessed using the method of caustics and an initial decrease and a subsequent increase in the subcritical crack growth rates of kinked cracks were shown to correlate with the variations of the mode I and the mode II stress intensities.

Singh, Dileep↗

Subcritical crack growth in two titanium alloys.

Measurement of subcritical crack growth during static loading of precracked titanium alloys in salt water using samples too thin for plane strain loading to predominate was examined as a method for determining the critical stress intensity for crack propagation in salt water. Significant internal crack growth followed by arrest was found at quite low stress intensities, but crack growth rates were relatively low. Assuming these techniques provided a reliable measurement of the critical stress intensity, the value for annealed Ti-4Al-1.5Mo-0.5V alloy was apparently about 35 ksi-in. to the 1/2 power, while that for annealed Ti-4Al-3Mo-1V was below 45 ksi-in. to the 1/2 power. Crack growth was also observed in tests conducted in both alloys in an air environment. At 65 ksi-in. to the 1/2 power, the extent of crack growth was greater in air than in salt water. Ti-4Al-3Mo-1V showed arrested crack growth in air at a stress intensity of 45 ksi-in. to the 1/2 power.

Williams, D. N.↗

Effects of subcritical crack growth on fracture toughness of ceramics assessed in chevron-notched three-point bend tests

A numerical computational study was carried out to assess the effects of subcritical crack growth on crack stability in the chevron-notched three-point bend specimens. A power-law relationship between the subcritical crack velocity and the applied stress intensity were used along with compliance and stress-intensity relationships for the chevron-notched bend specimen to calculate the load response under fixed deflection rate and a machine compliance. The results indicate that the maximum load during the test occurs at the same crack length for all the deflection rates; the maximum load, however, is dependent on the deflection rate for rates below the critical rate. The resulting dependence of the apparent fracture toughness on the deflection rate is compared to experimental results on soda-lime glass and polycrystalline alumina.

Chao, L. Y.↗

Hydrogen adsorption and diffusion, and subcritical-crack growth in high strength steels and nickel base alloys

Embrittlement, or the enhancement of crack growth by gaseous hydrogen in high strength alloys, is of primary interest in selecting alloys for various components in the space shuttle. Embrittlement is known to occur at hydrogen gas pressures ranging from fractions to several hundred atmospheres, and is most severe in the case of martensitic high strength steels. Kinetic information on subcritical crack growth in gaseous hydrogen is sparse at this time. Corroborative information on hydrogen adsorption and diffusion is inadequate to permit a clear determination of the rate controlling process and possible mechanism in hydrogen enhanced crack growth, and for estimating behavior over a range of temperatures and pressures. Therefore, coordinated studies of the kinetics of crack growth, and adsorption and diffusion of hydrogen, using identical materials, have been initiated. Comparable conditions of temperature and pressure will be used in the chemical and mechanical experiments. Inconel 718 alloy and 18Ni(200) maraging steel have been selected for these studies. Results from these studies are expected to provide not only a better understanding of the gaseous hydrogen embrittlement phenomenon itself, but also fundamental information on hydrogen adsorption and diffusion, and crack growth information that can be used directly for design.

Wei, R. P.↗

Subcritical crack growth and other time- and environment-dependent behavior in crustal rocks

Stable crack growth strongly influences both the fracture strength of brittle rocks and some of the phenomena precursory to catastrophic failure. Quantification of the time and environment dependence of fracture propagation is attempted with the use of a fracture mechanics technique. Some of the difficulties encountered when applying techniques originally developed for simple synthetic materials to complex materials like rocks are examined. A picture of subcritical fracture propagation is developed that embraces the essential ingredients of the microstructure, a microcrack process zone, and the different roles that the environment plays. To do this, the results of (1) fracture mechanics experiments on five rock types, (2) optical and scanning electron microscopy, (3) studies of microstructural aspects of fracture in ceramics, and (4) exploratory tests examining the time-dependent response of rock to the application of water are examined.

Swanson, P. L.↗

Subcritical crack growth of selected aerospace pressure vessel materials

This experimental program was undertaken to determine the effects of combined cyclic/sustained loads, stress level, and crack shape on the fatigue crack growth rate behavior of cracks subjected to plane strain conditions. Material/environment combinations tested included: 2219-T87 aluminum plate in gaseous helium, room air, and 3.5% NaCl solution at room temperature, liquid nitrogen, and liquid hydrogen; 5Al-2.5 Sn (ELI) titanium plate in liquid nitrogen and liquid hydrogen and 6AL-4V (ELI) STA titanium plate in gaseous helium and methanol at room temperature. Most testing was accomplished using surface flawed specimens instrumented with a clip gage to continuously monitor crack opening displacements at the specimen surface. Tapered double cantilever beam specimens were also tested. Static fracture and ten hour sustained load tests were conducted to determine fracture toughness and apparent threshold stress intensity values. Cyclic tests were performed using sinusoidal loading profiles at 333 MHz (20 cpm) and trapezoidal loading profiles at both 8.3 MHz (0.5 cpm) and 3.3 MHz (0.2 cpm). Data were evaluated using modified linear elastic fracture mechanics parameters.

Hall, L. R.↗

Hydrogen adsorption and diffusion, and subcritical-crack growth in high-strength steels and nickel base alloys

Coordinated studies of the kinetics of crack growth and of hydrogen adsorption and diffusion were initiated to develop information that is needed for a clearer determination of the rate controlling process and possible mechanism for hydrogen enhanced crack growth, and for estimating behavior over a range of temperatures and pressures. Inconel 718 alloy and 18Ni(200) maraging steel were selected for these studies. 18Ni(250) maraging steel, 316 stainless steel, and iron single crystal of (111) orientation were also included in the chemistry studies. Crack growth data on 18Ni(250) maraging steel from another program are included for comparison. No sustained-load crack growth was observed for the Inconel 718 alloy in gaseous hydrogen. Gaseous hydrogen assisted crack growth in the 18Ni maraging steels were characterized by K-independent (Stage 2) extension over a wide range of hydrogen pressures (86 to 2000 torr or 12 kN/m2 to 266 kN/m2) and test temperatures (-60 C to +100 C). The higher strength 18Ni(250) maraging steel was more susceptible than the lower strength 200 grade. A transition temperature was observed, above which crack growth rates became diminishingly small.

Wei, R. P.↗

Equivalence of macroscopic and microscopic Griffith conditions for subcritical crack growth

Exact relations are derived for a simple bond-snapping model of fracture and numerical results from a previous work are presented. A lattice model with a nonlinear cohesive force law is then considered. In both cases, the results confirm the equivalence of the microscopic and macroscopic Griffith conditions. The Griffith stress intensity is to be identified with the quiescent stress intensity.

Esterling, D. M.↗

Damage Mechanisms and Controlled Crack Propagation in a Hot Pressed Silicon Nitride Ceramic

The subcritical growth of cracks from pre-existing flaws in ceramics can severely affect the structural reliability of a material. The ability to directly observe subcritical crack growth and rigorously analyze its influence on fracture behavior is important for an accurate assessment of material performance. A Mode I fracture specimen and loading method has been developed which permits the observation of stable, subcritical crack extension in monolithic and toughened ceramics. The test specimen and procedure has demonstrated its ability to generate and stably propagate sharp, through-thickness cracks in brittle high modulus materials. Crack growth for an aluminum oxide ceramic was observed to be continuously stable throughout testing. Conversely, the fracture behavior of a silicon nitride ceramic exhibited crack growth as a series of subcritical extensions which are interrupted by dynamic propagation. Dynamic initiation and arrest fracture resistance measurements for the silicon nitride averaged 67 and 48 J/sq m, respectively. The dynamic initiation event was observed to be sudden and explosive. Increments of subcritical crack growth contributed to a 40 percent increase in fracture resistance before dynamic initiation. Subcritical crack growth visibly marked the fracture surface with an increase in surface roughness. Increments of subcritical crack growth loosen ceramic material near the fracture surface and the fracture debris is easily removed by a replication technique. Fracture debris is viewed as evidence that both crack bridging and subsurface microcracking may be some of the mechanisms contributing to the increase in fracture resistance. A Statistical Fracture Mechanics model specifically developed to address subcritical crack growth and fracture reliability is used together with a damaged zone of material at the crack tip to model experimental results. A Monte Carlo simulation of the actual experiments was used to establish a set of modeling input parameters. It was demonstrated that a single critical parameter does not characterize the conditions required for dynamic initiation. Experimental measurements for critical crack lengths, and the energy release rates exhibit significant scatter. The resulting output of the model produces good agreement with both the average values and scatter of experimental measurements.

Calomino, Anthony Martin↗

Complex Dependence of Calcite Crack Kinetics on Salinity: The Role of DLVO and Hydration Forces

Abstract Subcritical crack growth (SCG) plays an important role in many geological processes such as delayed earth rupture and rock weathering. The complex dependency of SCG on the in‐crack fluid chemistry, however, is still poorly understood. In this study, we utilize the newly developed surface force‐based fracture theory (SFFT) to elucidate the relative contributions of surface forces and solute transport to the crack growth kinetics of calcite in NaCl solutions. Expanding on Barenblatt's cohesive crack model, SFFT introduces an effective stress intensity at the crack tip that encompasses all the relevant intermolecular forces across the crack in addition to the external far‐field stresses. The nonlinear system of equations portraying the crack opening profile, the solute distribution in a propagating crack, and the crack growth velocity are numerically solved via an implicit scheme. After carefully calibrating the model for calcite‐water systems, the SFFT is used to predict the SCG response of calcite at different NaCl concentrations, based on various hypotheses. These predictions are then compared to existing SCG data from the literature. We demonstrate that the experimentally observed variation of SCG rate with NaCl concentration cannot be explained solely by DLVO forces (electrostatic and Van der Waals interactions). This can be remediated by introducing an exponentially decaying hydration force with a nonlinear, nonmonotonic dependence on NaCl concentration. Furthermore, we demonstrate that accounting for both diffusive and advective transport of ions is important in explaining the absence of a stage‐II SCG response for calcite in electrolyte solutions. Plain Language Summary Subcritical crack growth (SCG) refers to the slow propagation of cracks in materials under a stress below the threshold for catastrophic failure. SCG is a key process in many geological events, for example, delayed earth ruptures and rock weathering. New initiatives such as underground CO 2 and H 2 storage in carbonate reservoirs further call for better understanding of SCG in carbonate minerals subjected to varying fluid chemistry. This study examines the SCG of calcite, a key mineral found in carbonate rocks, intergranular cement in sandstones, and filling material in mineral veins and faults, determining their deformation and strength. A mathematical model is developed to describe how the crack opens and propagates, how solutes (like salts) distribute within the crack, and how the crack surfaces interact with each other. We used the model to predict calcite SCG in water at different salt concentrations and compared it with experimental data. Our results revealed that the hydration force is the dominating factor in determining the complex, non‐linear dependency of SCG on salinity. We also found that both the movement of ions by diffusion and by bulk water flow are crucial for explaining the SCG rates, especially when the cracks grow quickly. Key Points Surface Force‐Based Fracture Theory predicts the complex subcritical crack growth patterns of calcite crystals immersed in NaCl solutions Results highlight the dominant role of hydration forces in altering the fracture behavior of calcite compared to VdW and electric double‐layer forces Advective solute transport explains the absence of stages‐II and ‐III subcritical crack growth responses in solid‐liquid systems

DLVO↗