Search NASA⌕ Search

SEARCH · Search NASA

Results for “surface finish”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Surface finishing

A surface of an article adapted for relative motion with a fluid environment is finished by coating the surface with a fluid adhesive. The adhesive is covered with a sheet of flexible film material under tension, and the adhesive is set while maintaining tension on the film material.

Kinzler, J. A.↗

Surface finishing

A surface of an article adapted for relative motion with a fluid environment is finished by coating the surface with a fluid adhesive, covering the adhesive with a sheet of flexible film material under tension on the film material whereby the tensioned film material is bonded to the surface by the adhesive.

Kinzler, J. A.↗

Evaluation of the Effect of Surface Finish on High-Cycle Fatigue of SLM-IN718

The surface finish of parts produced by additive manufacturing processes is much rougher than the surface finish generated by machining processes, and a rougher surface can reduce the fatigue strength of a part. This paper discusses an effort to quantify that reduction of strength in high-cycle fatigue for selective laser melt (SLM) coupons. A high-cycle fatigue (HCF) knockdown factor was estimated for Inconel 718, manufactured with the SLM process. This factor is the percentage reduction from the maximum stress in fatigue for low-stress ground (LSG) specimens to the maximum stress of those left with the original surface condition at the same fatigue life. Specimens were provided by a number of vendors, free to use their "best practice"; only one heat treat condition was considered; and several test temperatures were characterized, including room temperature, 800F, 1000F, and 1200F. The 1000F data had a large variance, and was omitted from consideration in this document. A first method used linear approximations extracted from the graphs, and only where data was available for both. A recommended knockdown factor of the as-built surface condition (average roughness of approximately 245 micro-inches/inch) versus low-stress ground condition (roughness no more than 4 micro-inches/inch) was established at approximately 1/3 or 33%. This is to say that for the as-built surface condition, a maximum stress of 2/3 of the stress for LSG can be expected to produce a similar life in the as-built surface condition. In this first evaluation, the knockdown factor did not appear to be a function of temperature. A second approach, the "KP method", incorporated the surface finish measure into a new parameter termed the pseudo-stress intensity factor, Kp, which was formulated to be similar to the fracture mechanics stress intensity factor. Using Kp, the variance seemed to be reduced across all sources, and knockdown factors were estimated using Kp over the range where data occurred. A plot of the results suggests that the knockdown factor is a function of temperature, and that for low lives the knockdown might be lower than the knockdown observed above about one million cycles, where it tended to stabilize. This was not universal for all temperatures tested. The higher temperature tests are thought to be influenced by the test temperature, which perhaps continued the aging process. Further evaluation of the method is suggested.

Lambert, D. M.↗

The Effect of Composition on the Surface Finish of PS400: A New High Temperature Solid Lubricant Coating

A new composite, multi-constituent, solid lubricant coating, NASA PS400, developed for high temperature tribological applications, exhibits a smoother surface finish after grinding and polishing than its predecessors PS200 and PS300. In this paper, the baseline composition of PS400 is modified to investigate each individual constituent s role on the achievable surface finish through a series of coating deposition, grinding, and polishing experiments. Furthermore, to explore the limits of compositional tailoring for improved tribological performance, several PS400 coatings were doped with additional solid lubricants (graphite, MoS2 and BN) and tribologically tested. The test results clearly showed that, compared to PS300 coatings, PS400 achieves a smoother surface finish via a reduced lubricant content. Coatings prepared with higher than the baseline level (10 wt%) of lubricants exhibited higher final surface roughness than the earlier generation PS300 coatings. Reducing or eliminating the one or both lubricants (fluorides or silver) did not further improve the surface finish suggesting that the current composition of PS400 is near optimal with respect to surface finish. Lastly, attempts to improve the poor initial room temperature tribological behavior of PS400 via the addition of traditional solid lubricants were unsuccessful. Based upon this work and earlier results it is expected that future research will concentrate on developing methods to produce a lubricious glaze on the rubbing surface during break in to ensure that low friction and wear are rapidly achieved.

DellaCorte, Christopher↗

The effect of rotor blade thickness and surface finish on the performance of a small axial flow turbine

An experimental investigation was conducted to determine the effect of blade profile inaccuracies and surface finish on the aerodynamic performance of a 11.13 cm tip diameter turbine. The as-received cast rotor blades had a significantly thicker profile than the design intent and a fairly rough surface finish. Stage test results showed an increase of one point in efficieny by smoothing the surface finish and another three points by thinning the blade profiles to near the design profile. Most of the performance gain between the as-cast thick and the thinned rotor blades both with the same surface finish, was attributed to reduced trailing edge losses of the recontoured blades.

Roelke, R. J.↗

Effect of Blade-surface Finish on Performance of a Single-stage Axial-flow Compressor

A set of modified NACA 5509-34 rotor and stator blades was investigated with rough-machine, hand-filed, and highly polished surface finishes over a range of weight flows at six equivalent tip speeds from 672 to 1092 feet per second to determine the effect of blade-surface finish on the performance of a single-stage axial-flow compressor. Surface-finish effects decreased with increasing compressor speed and with decreasing flow at a given speed. In general, finishing blade surfaces below the roughness that may be considered aerodynamically smooth on the basis of an admissible-roughness formula will have no effect on compressor performance.

COMPRESSORS - AXIAL FLOW↗

Surface Fatigue Lives of Case-Carburized Gears With an Improved Surface Finish

Previous research provides qualitative evidence that an improved surface finish can increase the surface fatigue lives of gears. To quantify the influence of surface roughness on life, a set of AISI 93 10 steel gears was provided with a nearmirror finish by superfinishing. The effects of the superfinishing on the quality of the gear tooth surfaces were determined using data from metrology, profilometry, and interferometric microscope inspections. The superfinishing reduced the roughness average by about a factor of 5. The superfinished gears were subjected to surface fatigue testing at 1.71 -GPa (248-ksi) Hertz contact stress, and the data were compared with the NASA Glenn gear fatigue data base. The lives of gears with superfinished teeth were about four times greater compared with the lives of gears with ground teeth but with otherwise similar quality.

Krantz, T. L.↗

An improved evaluation of surface finish with a three dimensional tester

The design and programming of an automated three dimensional surface finish tester is described. The device produces a three dimensional image of the microscopic texture of the examined surface. The surface finish tester presents the following advantages over conventional profilometry: (1) more complete exploration of surface texture by successive probe sweeps; (2) automation of measuring and calculating; (3) more accurate representation of the derived parameters; (4) analysis of the degree of homogeneity of the surface; (5) three dimensional graphic representation accurately depicting the state of the surface; (6) detection of local imperfections; and (7) detection of scoring that occurred during machining.

GRANDADAM↗

Effects of Strain Rate and Surface Finish on Tensile Properties in High Pressure Hydrogen — A Case Study for LP-DED NASA HR-1

NASA has advanced NASA HR-1 as a solution for liquid rocket engine components that operate in hydrogen rich environments using various AM techniques. The NASA HR-1 for AM applications was specifically formulated for high ductility in high pressure gaseous hydrogen environment in addition to high strength and low cycle fatigue (LCF) resistance. NASA HR-1 meets materials requirements for liquid rocket engine components, including good hydrogen resistance, high conductivity, good LCF performance, and high elongation and strength for components in medium heat flux environments. NASA has completed fabrication of several subscale and full-scale channel wall nozzles in LP-DED NASA HR-1 and completed hot-fire testing. This includes refinement of the process to produce thin-walls and various channel geometries to meet the requirements for channel wall nozzle applications. The main objective of this investigation is to better understand the effects of tensile test strain rate and specimen surface finish on the amount of tensile ductility degradation in high pressure gaseous hydrogen environments. Performing smooth tensile tests in high pressure hydrogen and nitrogen environments can serve as a rapid and economical screening method to determine the relative susceptibility of materials to HEE. This paper presents the tensile test results for LP-DED NASA HR-1 in hydrogen and details the material evaluation on the effects of strain rate and surface finish condition on surface cracking behavior and fracture characteristics. The resistance to HEE for LP-DED NASA HR-1 and the wrought alloy is compared under the same testing conditions. Loss of tensile ductility is quantified in terms of changes in elongation at failure in hydrogen to compare HEE susceptibility. The most suitable strain rate and specimen surface finish condition for future HEE screening testing at MSFC are recommended.

Additive manufacturing↗

Portable flooring protects finished surfaces, is easily moved

To protect curved, finished surface and provide support for workmen, portable flooring has been made from rigid plastic foam blocks, faced with aluminum strips. Held together by nylon webbing, the flooring can be rolled up for easy carrying.

Carmody, R. J.↗

Surface finish measurement studies

The performance of stylus instruments for measuring the topography of National Transonic Facility (NTF) model surfaces both for monitoring during fabrication and as an absolute measurement of topography was evaluated. It was found that the shop-grade instruments can damage the surface of models and that their use for monitoring fabrication procedures can lead to surface finishes that are substantially out of range in critical areas of the leading edges. The development of a prototype light-scattering instrument which would allow for rapid assessment of the surface finish of a model is also discussed.

Teague, E. C.↗

Experimental Investigation of the Heat-Transfer Rate to a Series of 20 deg Cones of Various Surface Finishes at a Mach Number of 4.95

The heat-transfer rates were measured on a series of cones of various surface finishes at a Mach number of 4.95 and Reynolds numbers per foot varying from 20 x 10(exp 6) to 100 x 10(exp 6). The range of surface finish was from a very smooth polish to smooth machining with no polish (65 micro inches rms). Some laminar boundary-layer data were obtained, since transition was not artificially tripped. Emphasis, however, is centered on the turbulent boundary layer. The results indicated that the turbulent heat-transfer rate for the highest roughness tested was only slightly greater than that for the smoothest surface. The laminar-sublayer thickness was calculated to be about half the roughness height for the roughest model at the highest value of unit Reynolds number tested.

Jones, Jim J.↗

Effect of longitudinal surface finish on elastohydrodynamic lubrication

The effect of longitudinal-lay surface finish on the elastohydrodynamic film thickness and the percentage of film between rolling disks in contact were evaluated using a rolling disk apparatus. Film thickness was measured by transmitted X-rays, and percentage of film was monitored by an alternating-current continuity circuit. Disk finish was varied on both the crowned upper disk and the cylindrical lower disk. A type-2 ester and a synthetic paraffinic oil were used as lubricants. It was shown that the roughness with longitudinal lay has a deleterious effect on both film thickness and percentage of film. Measured film thicknesses for the two lubricants were comparable at equivalent test conditions. The percentage of film where a change in surface topography was observed was approximately 20 percent for the synthetic paraffinic oil and 10 percent for the type-2 ester.

Dow, T. A.↗

Surface finish effects and the strength-grain size relation in SiC

The effect of surface finish on the strength-grain size relation was investigated for dense hot-pressed SiC. Failure initiated predominantly via the propagation of extrinsic machining-induced flaws for the range of grain sizes and machining grit sizes studied. These results are consistent with the region of large-grain-size flaw control as delineated by Prochazka and Charles. The severity of machining-induced flaws, relative to the machining grit size, decreased with increasing machining grit size and decreasing SiC grain size.

Cranmer, D. C.↗