Search NASA⌕ Search

SEARCH · Search NASA

Results for “surface morphologies”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Surface Morphology and Surface Stability against Oxygen Loss of the Lithium-Excess Li 2 MnO 3 Cathode Material as a Function of Lithium Concentration

There is a growing appreciation for the role of surface reactivity and subsequent reconstruction affecting the performance of high-voltage, high-capacity Li-ion cathode materials. In particular, the promising Li-excess materials are known to exhibit significant vulnerability toward oxygen release, which can cause surface densification and impede Li intercalation. In this work, we focus on the end member, Li 2 MnO 3 , as a Li-excess, Mn-rich representative of this class of materials and systematically elucidate all possible stoichiometric low Miller index surfaces with various cation ordering on each surface. We apply surface cation reconstruction rules that depend on the local environment, including target Mn-Li site exchanges, and optimize the resulting surface Li configurations using metadynamics. The equilibrium Wulff shape shows dominant (001), (010) surface facets, and almost all facets exhibit favorable Mn reconstruction. Most importantly, we find that while all equilibrium Li x MnO 3 surfaces become unstable toward oxygen release for x < 1.7, some facets are consistently more resistant than others which may provide a design metric for more stable particle morphologies and enhanced surface oxygen retention.

36 MATERIALS SCIENCE↗

Periodic Surface Morphology Characteristics of Tungsten Under Simultaneous Helium and Deuterium Bombardment at 30 keV

The ITER divertor will feature tungsten monoblocks as the plasma-facing component (PFC) that will be subject to extreme temperature and radiation environments. This paper reports the development of surface morphologies on tungsten under helium bombardment at high temperatures, which has important implications for safety, retention, and PFC erosion. Polycrystalline tungsten samples were implanted in the Dual Advanced Ion Simultaneous Implantation Experiment dual-beam ion implantation experiment at the University of Wisconsin-Madison with He-only and simultaneous He-D implantation at incidence angles of 55 deg, ion energies of 30 keV, and surface temperatures of 900°C to 1100°C. Morphologies resulting from angled incidence conditions differed from those produced under normal incidence bombardment at similar energy and temperature conditions in previous work. A variety of ordered and disordered morphologies dependent on grain orientation were observed for fluences up to 6 × 10 18 He cm –2 . These morphologies displayed dependencies on crystal orientation at low fluences and incident beam directions at higher fluences. Furthermore, these structures appeared, with variation, under both single-species He and mixed He-D implantations.

36 MATERIALS SCIENCE↗

Surface Morphology and Transport Studies of Epitaxial Graphene on SiC(000-1)

Annealing conditions are critical to the properties of epitaxial graphene formed by thermal decomposition of silicon carbide. Here, we report the evolution of coherent electronic transport with increasing anneal temperatures, combined with low energy electron micrographs of equivalent surfaces showing corresponding structural coherence. Ultrahigh vacuum conditions and temperatures in the range of 1250-1300 C produce granular films with a lateral grain size of {approx}20 nm, while temperatures of 1400 C or higher result in grains with progressively larger lateral dimensions in the micron range. Transport measurements show how the electronic coherence length increases as a result of the more coherent physical structure, with a crossover from two-dimensional variable range hopping to the weak localization regime. Here, we show that while the duration of the anneal affects coverage and clustering of grains, the size of individual grains is determined by anneal temperature, with evidence of coalescence of smaller grains into larger domains, suggesting that multistage anneals at different temperatures may yield high-quality graphene.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Epitaxial Ag(001) grown on MgO(001) and TiN(001): Twinning, surface morphology, and electron surface scattering

Epitaxial Ag(001) layers were deposited on MgO(001) in order to study electron surface scattering. X-ray reflection indicates 3D layer nucleation with a high rms surface roughness of 1.0 nm for a layer thickness d = 3.5 nm. X-ray diffraction shows that {l_brace}111{r_brace} twins form at d < 11 nm, followed by 2nd generation twinning for 11 nm < d < 120 nm. Increasing the growth temperature from 25 to 150 deg. C suppresses 2nd generation twinning and reduces the twin density by 2 orders of magnitude. In situ deposition of epitaxial 2.5-nm-thick TiN(001) underlayers prior to Ag deposition results in twin-free single-crystal Ag(001) with 10 x smoother surfaces for d = 3.5 nm. This is attributed to a better wetting on the higher energy TiN(001) than MgO(001) surface, resulting in the absence of 3D nuclei with exposed {l_brace}111{r_brace} facets, which facilitate twin nucleation. The twinned Ag/MgO layers have a higher resistivity {rho} than the single crystal Ag/TiN layers at both 298 and 77 K, due to electron scattering at grain and twin boundaries. The {rho} for single-crystal Ag layers increases with decreasing d, which is well explained with known surface scattering models and provides specularity parameters for the Ag-vacuum and the Ag-air interfaces of p = 0.8 {+-} 0.1 and 0.4 {+-} 0.1, respectively. A comparison with corresponding epitaxial Cu(001) layers shows that {rho}{sub Ag} < {rho}{sub Cu} for d > 50 nm, consistent with known bulk values. However, {rho}{sub Ag} > {rho}{sub Cu} for d < 40 nm. This is attributed to the larger electron mean free path for electron-phonon scattering and a correspondingly higher resistivity contribution from surface scattering in Ag than Cu. In contrast, air exposure causes {rho}{sub Ag} < {rho}{sub Cu} for all d, due to diffuse scattering at the oxidized Cu surface and the correspondingly higher Cu resistivity.

36 MATERIALS SCIENCE↗

Nanopatterning of Si surfaces by normal incident ion erosion: Influence of iron incorporation on surface morphology evolution

The surface morphology of Si(100) induced by 1200 eV Ar{sup +} ion bombardment at normal incidence with and without Fe incorporation is presented. The formation of nanodot patterns is observed only when the stationary Fe areal density in the surface is above a threshold value of 8x10{sup 14} cm{sup -2}. This result is interpreted in terms of an additional surface instability due to locally nonuniform sputtering in connection with the presence of a Fe rich amorphous phase at the peak of the nanodots. At Fe concentrations below the threshold, smoothing dominates and pattern formation is inhibited. The transition from a k{sup -2} to a k{sup -4} behavior in the asymptotic power spectral density function supports the conclusion that under these conditions ballistic smoothing and ion-enhanced viscous flow are the two dominant mechanisms of surface relaxation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Different Cutting Techniques on the Surface Morphology and Composition of Niobium

The surface morphology and chemical purity of superconducting radio frequency (SRF) niobium cavities are very important for proper accelerator operation. Typically on the order of 120 micrometers of niobium (Nb) is removed from cavities to remove damage done during the forming of Nb sheets and cavities. A study was done to find the effect of cutting or finishing Nb with a band saw, diamond saw, electrical discharge machining (EDM) wire, garnet water jet, sheer, and mill. Surface contamination of the samples was measured before and after buffered chemical polish (BCP) by secondary ion mass spectroscopy (SIMS), energy dispersive spectroscopy (EDS), and by measuring relative resistivity ratios (RRRs). Surface morphology was examined with a digital microscope, a surface profilometer and scanning electron microscope (SEM). It was found that all techniques altered the top 3-5 micrometers of the Nb. It was also found by SIMS that the water jet technique introduced the most hydrogen and oxygen to the Nb in the first 2.5 micrometers of the sample. The EDM wire cutting technique introduced the least amount of hydrogen to the Nb. After 5 micrometers were etched away by BCP on the various samples, no contaminants were found except on the water jet cut samples. Even after 20 micrometers of Nb removal silica could be seen on the surface with EDS. The water jet produced the roughest surface with 50-100 micrometer deep pits made from embedded garnet particles. It was found that the garnet water jet damages the surface to the point where even the typical 120 micrometers of BCP etching may not remove all the defects created.

43 PARTICLE ACCELERATORS↗

Surface Morphology Diagram for Cylinder-Forming Block Copolymer Thin Films

We investigate the effect of annealing temperature (T), film thickness (hf) on the surface morphology of flow coated films of a cylinder forming block copolymer, poly (styrene-block-methyl methacrylate) (PS-b-PMMA). Surface morphology transitions from a perpendicular to a parallel cylinder orientation with respect to the substrate with increasing hf are observed in these model frustrated-interaction films where the substrate interaction is preferential for one of the blocks (PMMA) and nearly neutral for the other interface (polymer-air). In these films a transition occurs from cylinders oriented parallel to the substrate to a mixed or hybrid state where the two orientations coexist followed by a transition to cylinders oriented perpendicularly to the polymer-air interface for larger hf. The characteristic values of hf defining these surface morphological transitions depend on T and we construct a surface morphology diagram as a function of hf and T. The surface morphology diagram is found to depend on the method of film formation (flow coated versus spun cast films) so non-equilibrium effects evidently have a large effect on the surface pattern morphology. In particular, the residual solvent within the film (quantified by neutron reflectivity measurements) in the context of physics of glass-formation can have a large effect on the surface morphology diagram.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Effects of surface vacancy-adatom pair formation on PFC tungsten surface morphological response

Abstract We report a simulation study of the effect of He-irradiation-induced surface vacancy-adatom pair formation on the surface morphological evolution of plasma-facing component (PFC) tungsten and examine a number of factors that impact such evolution. Our analysis is based on self-consistent dynamical simulations according to an atomistically-informed, continuum-scale surface evolution model that has been developed following a hierarchical multiscale modeling strategy and can access the spatiotemporal scales of relevance to fuzz formation. The model accounts for the flux of surface adatoms generated as a result of the surface vacancy-adatom pair formation effect upon He implantation, which contributes to the anisotropic growth of surface nanostructural features due to the different rates of adatom diffusion along and across step edges of islands on the tungsten surface. We have carried out atomic-scale computations of optimal diffusion pathways along and across island step edges on the W(110) surface and calculated Ehrlich–Schwoebel (ES) barriers in adatom diffusion along and across such step edges. This aspect of surface adatom diffusion contributes to anisotropic surface atomic fluxes, terrace and step diffusive currents, and has been incorporated into our PFC surface evolution model, which predicts the formation of preferentially aligned nanoridge stripe patterns on the PFC surface. We establish that these anisotropic diffusive currents accelerate nanotendril growth on the PFC surface and the onset of surface nanostructure pattern formation. We also explore systematically the dependence of the PFC surface morphological response on the surface temperature and He ion incident flux, characterize in detail the resulting surface topographies and growth kinetics, and compare the predicted surface morphologies with experimental observations. Our simulation predictions for the emerging surface nanostructure patterns under certain plasma exposure conditions are consistent with experimental findings in the literature.

36 MATERIALS SCIENCE↗

Phosphonium-Containing Block Copolymer Anion Exchange Membranes: Effect of Quaternization Level on Bulk and Surface Morphologies at Hydrated and Dehydrated States

Diblock copolymers of isoprene and chloromethylstyrene were synthesized by nitroxide-mediate polymerization. The polychloromethylstyrene block was quaternized with tris(trimethoxyphenyl)phosphine (P(Ph(OMe) 3 ) 3 ) or triphenyl-phosphine (P(Ph) 3 ). Membranes with ion-exchange capacity (IEC) ranging from 0.87 to 2.35 mmol/g were prepared. The bulk morphology was investigated via small-angle X-ray scattering and transmission electron microscopy, where hexagonal and body-centered cubic morphologies were observed. The surface morphology was revealed by atomic force microscopy where both parallel and perpendicular alignments were observed. Compared to P(Ph(OMe) 3 ) 3 , P(Ph) 3 exhibits higher quaternization efficiency due to less steric hindrance. Partially quaternized membranes were prepared using P(Ph) 3 , and the dependence of domain size on the quaternization level is discussed. The morphologies as a function of relative humidity were investigated. For high IEC membranes, although bulk scattering showed small changes in d -spacing, large changes in domain size on the surface occurred between hydrated and dehydrated conditions. Finally, further investigations of morphological reversibility by humidity cycling showed good recovery between humid and dry conditions, indicating that the expansion and contraction of channels is a reversible process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Control of Surface Morphology during the Growth of (110)-Oriented GaAs by Hydride Vapor Phase Epitaxy

We present a study of the effect of hydride vapor phase epitaxy (HVPE) growth conditions on the morphology of GaAs grown on vicinal and nominally exact (110) GaAs substrates. We evaluate epilayer surfaces using a combination of Nomarski microscopy and atomic force microscopy. The surface morphology strongly depends on the growth conditions employed, as well as the substrate orientation. On substrates offcut 3° toward (111)A, faceting generally develops under conditions in which the growth is Ga-limited, although Ga-limited growth is not the only requirement for faceting. Low growth temperatures lead to a faceted morphology, while higher growth temperatures favor smooth growth and facet-free morphology. We show that the surface morphology is kinetically controlled and that the tendency to facet correlates with the growth rate. 3D growth occurs on nominally exact substrates, resulting in hillock formation, but reduction of the group V precursor partial pressure results in smooth morphology. Overall, our results are consistent with models for step-bunching-induced surface faceting that invoke a negative Ehrlich–Schwoebel step-edge barrier.

(110) oriented GaAs↗

Hole formation effect on surface morphological response of plasma-facing tungsten

We report simulation results on the effect of helium (He) bubble bursting-mediated surface hole formation on the surface morphological response of tungsten plasma-facing components (PFCs) in nuclear fusion devices. Our analysis is based on an atomistically informed, continuum-scale model, which is capable of accessing the spatiotemporal scales relevant to the fuzz nanostructure formation process on the surface of PFC tungsten. Our simulations account, in an empirical fashion, for two types of subsurface bubble dynamical phenomena in the nanobubble region of PFC tungsten during He plasma irradiation, involving bubble bursting and surface crater formation. We demonstrate that the hole formation effect on the PFC tungsten surface accelerates the growth rate of nanotendrils and the onset of fuzz formation. As a result, the predicted incubation time for surface nanotendril growth is shortened, in agreement with experimental data of incubation fluence at comparable plasma exposure conditions. We also explore systematically the dependence of the PFC surface morphological response on the areal density of holes introduced at regular time intervals onto the He-implanted tungsten surface, a parameter in our analysis that serves as a proxy for the rate of He bubble bursting. More importantly, our simulations capture fine surface features in the PFC tungsten surface morphology and predict that the average spacing between nanotendrils is on the order of 100 nm, consistent with the experimental findings.

Chen, Chao-Shou (ORCID:0000000307910042)↗

Surface morphological evolution during annealing of epitaxial Cu(001) layers

Single crystal Cu(001) layers were grown on MgO(001) by ultrahigh vacuum magnetron sputtering at T{sub s}=100 deg. C. Quantitative surface morphological analyses by in situ scanning tunneling microscopy show that the surfaces exhibit self-affine mound structures with a scaling exponent of 0.82{+-}0.03 and a mound radius r{sub c} that increases from 31{+-}8 to 39{+-}6 nm for increasing layer thickness t=24-120 nm. In situ annealing at 200 and 300 deg. C leads to a thermodynamically driven mass transport that minimizes the surface step density, resulting in broader mounds and a smaller root mean square surface roughness {sigma}. This effect is most pronounced for t=24 nm, for which r{sub c} increases from 31{+-}8 to 70{+-}20 nm and {sigma} decreases from 1.3{+-}0.1 to 0.74{+-}0.08 nm, resulting in a decrease in the average surface slope from {chi}=7 deg. to 2 deg. and an increase in the average terrace width w{sub T} by more than a factor of 4. In contrast, w{sub T} increases by only 20% for t=120 nm. This remarkable difference between 'thin' and 'thick' layers is attributed to diverging surface morphological pathways during annealing: The strong smoothening for t=24 nm is due to a competitive coalescence process where some mounds grow laterally at the expense of their smaller neighbors, which die out. In contrast, the initially wider mounds of thicker layers (t=120 nm) combine to form a quasistable surface morphology that exhibits anisotropic mound structures, which limit mass transport and stabilize the surface step density.

36 MATERIALS SCIENCE↗

He-Ion and Self-Atom Induced Damage and Surface-Morphology Changes of a Hot W Target

We report results of measurements on the evolution of the surface morphology of a hot tungsten surface due to impacting low-energy (80 12,000 eV) He ions and of simulations of damage caused by cumulative bombardment of 1 and 10 keV W self-atoms. The measurements were performed at the ORNL Multicharged Ion Research Facility (MIRF), while the simulations were done at the Kraken supercomputing facility of the University of Tennessee. At 1 keV, the simulations show strong defect-recombination effects that lead to a saturation of the total defect number after a few hundreds impacts, while sputtering leads to an imbalance of the vacancy and interstitial number. On the experimental side, surface morphology changes were investigated over a broad range of fluences for both virgin and pre-damaged W-targets. At the lowest accumulated fluences, small surface-grain features and near-surface He bubbles are observed. At the largest fluences, individual grain characteristics disappear in FIB/SEM scans, and the entire surface is covered by a multitude of near-surface bubbles with a broad range of sizes, and disordered whisker growth, while in top-down SEM imaging the surface is virtually indistinguishable from the nano-fuzz produced on linear plasma devices. These features are evident at progressively lower fluences as the He-ion energy is increased.

Meyer, Fred W↗