At least 19 records

A mechanistic interpretation of Nelson curves for PVP failures under high temperature hydrogen attack

As an empirically established design criterion, Nelson curves that relate the service temperature and the allowable hydrogen partial pressure have been developed and utilized for more than sixty years in pressure vessels and piping (PVP) safety design. Despite a relatively clear thermodynamic understanding of the high-temperature-hydrogen-attack (HTHA) problem, the detailed fracture process on the microstructural length scales, however, remains elusive, and a quantitative assessment of the PVP lifetime under HTHA from the available creep fracture dataset is still not possible. This work develops a microstructure-informed and micromechanics-based model by incorporating a synergy between hydrogen transport and intergranular-cavity-based fracture process. Based on the available creep lifetime data of C-0.5Mo steels, we are able to calibrate material constitutive parameters, and then conduct nonlinear finite element simulations that reveal a real-time stress-induced hydrogen diffusional transport along grain boundaries, coupled with a microstructure-explicit failure process, from which Nelson curves can be computed. Such failure analyses allow us to delineate two distinct regimes on the Nelson curves, i.e., dislocation-creep-controlled or grain boundary diffusion-assisted cavity growth. More importantly, we found that a small change of the pipe thickness and applied stresses can significantly shift these lifetime curves. However, these two parameters are usually not provided in Nelson curves, thus limiting their usage in material selection and safety design. In conclusion, this discrepancy can clearly be mitigated by extensive parametric studies from our micromechanical modeling/simulation framework.

36 MATERIALS SCIENCE↗

Physical-chemical-mechanical quantitative assessment of the microstructural evolution in Portland-limestone cement pastes exposed to magnesium sulfate attack at low temperature

The changes in structural integrity and microstructure of Portland-limestone cement pastes were investigated in the course of magnesium sulfate attack at low temperature. A deterioration front, consisting of three distinct layers (brucite, gypsum, leached cement matrix), swelled in time due to the expansive nature of the deterioration products, generating cracks and subsequently detaching from the sound cement matrix, continuously promoting the process. Gypsum and thaumasite characterized the leached matrix, which experienced extensive cross-linking of the aluminosilicate structures, as a result of decalcification and dealumination of the calcium silicate hydrates (C(A)SH), impairing the overall mechanical performance. CSH of low packing density was most severely affected by the process, as confirmed by the significant drop in nano-mechanical properties. The increased rate of deterioration with limestone content was tentatively attributed to the prevalent morphology of the CSH phase. Results were validated by thermodynamic simulations, indicating that the real systems did not reach equilibrium.

36 MATERIALS SCIENCE↗

Coordinated Thermal Safety Attack and Defense on EV Battery Management Systems

Battery temperature sensor and battery current sensor data which are key sensing inputs to the Battery Management Controllers in electric vehicles, are vulnerable to possible cyber/ physical manipulation due to known vulnerabilities inherited from CAN bus technology that is used for in-vehicle communications between electronic control units that transfer sensing and control data. In this paper, we first create a simulation that enables us to evaluate impact of cyber physical attacks on electric vehicle battery management system in a controlled environment that violates thermal safety. Specifically, we emulate a Level 3 - DC fast charging system with SAE J1772/CCS, integrated with standard charging controls and thermal safety controls on EVs, and various sensing data flows. Second, we propose a coordinated current and battery temperature attack that has crippling economic, and safety impacts. Third, we quantify the usability, economic and safety impacts of such attacks as a function of the extent of data manipulation. Finally, we propose a physics model driven detection technique to detect presence of such attacks.

25 ENERGY STORAGE↗

Experimental and numerical study of the effects of solution concentration and temperature on concrete under external sulfate attack

The work reports on an experimental programme, conducted to validate comprehensively our previously proposed coupled chemo-transport model for external sulfate attack on concrete. Specifically, the effects of the concentration of sulfate solution and temperature on the distribution of sulfate ions in concrete are experimentally investigated and used to demonstrate the accuracy of the modeling framework. Further, the profile of aluminate depletion and the leaching depth numerically are investigated. For all cases the model predictions are in good agreement with the experimental results, showing increases of the concentration of sulfate ions in concrete with higher concentrations of sulfate solution and higher temperatures. It is concluded that higher sulfate solution concentration and temperature enhance the processes involved in the external sulfate attack on concrete, namely diffusion of sulfate ions and their chemical reactions with concrete. It is found that these parameters affect the external sulfate attack predominantly via the chemical reaction process.

36 MATERIALS SCIENCE↗

Developing Machine Learning Interatomic Potential for Fe-Cr-Ni Alloys

Accurate prediction of creep and fatigue behavior of stainless steel at elevated temperatures in hydrogen environment requires fundamental understanding of alloy-hydrogen interaction at cross-scale including bulk lattice and key defects such as vacancies, grain boundaries, surfaces, stacking faults, dislocations, and precipitates. This project aims to predict creep behavior of 347H stainless steel with H using machine learning interatomic potentials based on first-principles density functional theory simulations. The Moment Tensor Potentials platform is adopted for this work since it demonstrates a fine balance between model accuracy and computational efficiency. The potential is well trained based on large amount of high-fidelity density functional theory calculations. The validation is carried out by comparing various important properties including short range order, coefficient of thermal expansion, elastic properties, stacking fault energy, grain boundary energy, and surface energy. This work lays the foundation for reliable atomistic simulation of high temperature hydrogen attack of stainless steel.

density functional theory (DFT)↗

Hydrothermal corrosion behavior of CVD SiC in high temperature water

Here, the hydrothermal corrosion of polished and as-cut high purity chemical vapor deposited (CVD) SiC was studied in a constantly refreshing water loop. Light water reactor (LWR) conditions were simulated at 288, 320, and 350 °C with dissolved gas concentrations between 0.15 and 3 ppm H 2 or between 1 and 4 ppm O 2 . In hydrogenated water, the rate of material loss was low, calculated to be ~1.3 μm of recession after 5 years of service in 320 °C water. Moreover, there was no observed localized attack at any temperature. In oxygenated conditions, the corrosion rate was higher, with a calculated material loss >10 μm after 5 years of service in 1 ppm O 2 , 320 °C water. Mass loss significantly increased when grain fallout became significant (as early as 200h with 4 ppm O 2 at 350 °C or after 1000–2000h with 2 ppm O 2 at 288 °C). Grain fallout more than doubled the corrosion rate and a steady state corrosion rate in the grain fallout regime was not observed but expected to eventually occur once large grains begin to be removed. Polished specimens had lower mass loss than unpolished coupons. A kinetic analysis of the data in this work suggests that the corrosion rates are controlled by a single activation step in both oxygenated and deoxygenated conditions, with the reaction order with respect to oxygen being 1. A resulting reaction rate equation to predict corrosion of SiC (in mg/cm 2 s) in high purity water from 288 to 350 °C and up to 4 ppm O 2 was constructed: Rate = $\frac{0.1458}{1+SA}$ T (1.09(1–10 -3 T)[O 2 ]e– $\frac{1.275x10^4}{T}$ + 7.91x10 -6 e– $\frac{7.39x10^3}{T}$).

36 MATERIALS SCIENCE↗

Effect of surface oxides on tritium entrance and permeation in FeCrAl alloys for nuclear fuel cladding: a review

Abstract Iron-chromium-aluminum (FeCrAl) alloys are being considered for the cladding of uranium dioxide fuel in light water reactors (LWRs). FeCrAl alloys have good mechanical properties at temperatures of 300 °C and higher, and have superlative resistance to attack by steam at temperatures of up to 1000 °C and higher. A concern has been raised that the use of FeCrAl for cladding would result in a higher content of tritium in the reactor coolant as compared with the current system where the cladding is a zirconium based alloy. This review shows that the flux of tritium from the fuel rod cavities to the coolant across the fuel cladding wall will be greatly reduced by the presence of oxides on the surface of the cladding. The review of current literature and permeation data show that (a) protective oxides are expected to be present on both sides of the FeCrAl cladding, and (b) depending on the characteristics of these oxide layers it is reasonable to expect about two–three orders of magnitude reduction in tritium permeation, relative to the permeation response in clean, unoxidized condition for FeCrAl steels of interest, around 277 °C–377 °C temperatures.

Electrochemistry↗

Electric Vehicle Charging Data Falsification Attacks Utilizing Behavioral Models

A charging station (CS) and its associated electric vehicle supply equipment (EVSE) and charging electric vehicle (EV) interactions are potential targets for data falsification attacks since CSs are typically unmanned public facilities that are connected to the internet and EVs incorporate the vulnerable CAN bus network, which are both susceptible to remote attacks. The research question being addressed is how is the EV owner and CS negatively affected by CAN bus EV battery current sensor and battery temperature sensor data falsification attacks. Negative effects include economic losses from reduced life span of the battery, battery thermal runaway and fire (and potential loss of surrounding structure), and reduced utilization of the CS due to delayed departure time (longer charging times).

25 ENERGY STORAGE↗

Deconsolidation and Leach Burn Leach of Seven As Irradiated AGR 5/6/7 TRISO Fuel Compacts from Capsules 2, 3, 4, and 5

Seven as-irradiated Advanced Gas Reactor (AGR) 5/6/7 compacts underwent destructive post-irradiation examination via deconsolidation-leach-burn leach at Idaho National Laboratory (INL). The selection of the compacts extended the upper and lower limits of time-average volume-average (TAVA) temperature for compacts that had gone through deconsolidation-leach-burn leach so far. The measured inventories of fission products and actinides in the compact matrix and outer pyrolytic carbon were reported. Results indicated unexpectedly higher rates of fuel kernel leaching compared to compacts from AGR-1 and AGR-2. These failure rates were attributed to damage during post-irradiation sample handling, rather than irradiation itself. AGR-5/6/7 compacts have little or no matrix coverage for some particles at the top and bottom ends of cylindrical fuel compacts, making them more fragile. Sixty particles were randomly sampled from each compact, and the gamma results were reported. Three SiC shells from were identified, one of which showed signs of chemical attack in the high-irradiation temperature compact.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Physical and Engineering Limits of Coupled In situ TEM Experiments

Almost all future energy systems (advanced nuclear reactors, fusion energy system, concentrating solar-thermal power (CSP), and wind technologies) are limited by degradation of key material systems exposed to multiple environmental stressors. The degradation during exposure to high temperatures, radiation, mechanical loading, and chemical attack is often dictated by mechanisms active at the microstructural level. The nature of these mechanisms and the associated variations between sequential and concurrent interplay can be explored if the transmission electron microscope (TEM) is utilized as a toolbox for exploration [1]. One such tool developed at Sandia National Laboratories to couple several of these environments is the In situ Ion Irradiation TEM (I3TEM) [2]. Several studies over the last decade utilizing this tool have shown that the scientific intuition developed over decades of sequential experiments is not always a good indicator of concurrent mechanisms or failure routes. This presentation will highlight the recent and planned additions into the I3TEM facility of a Waviks gas injection system and Raman system, respectively, as can be seen in Fig. 1, permitting environmental degradation from gas species leaked into the pole piece region during quantitative mechanical loading (indentation, monotonic loading, high temperature creep, irradiation induced creep, and high-cycle fatigue); multi-beam ion irradiation (energies ranging from 1 keV to 48 MeV and species from H to Au); laser exposure (20 W and 1064 nm), or various combinations thereof that are already possible [3]. This addition permits the facility to explore both sequential or concurrently the four axes of stressors: thermal, mechanical, radiation, and chemical. This information can be directly coupled to modeling, expediting the refinement and validation of both atomistic and mesoscale models.

degradation↗

Oxidation Behavior and Property Degradation of Nuclear Graphites

During its multidecade operation in the core of nuclear reactors, graphite components are subjected to aggressive and continuous exposure to a high field of ionizing and neutron irradiation, high temperature, and various types of present and postulated chemical attacks. High density, high crystallinity polygranular synthetic graphite is unique among other materials for its extraordinary capacity of resisting and adapting to the aggression inflicted by high temperature, high energy neutron bombardment and ionizing gamma radiation. But, as a carbonaceous material, even though of very high purity, graphite is reactive towards common oxidizing agents: oxygen, carbon dioxide, water. Safe operation of HTGRs relies, among other aspects, on engineered safeguard systems for efficient and continuous protection of graphite components against oxidation. Graphite oxidation behavior was, and continues to be, an important direction of theoretical and experimental research, engineering analyses, models and simulations, and design and safety regulations. The avalanche of publications, reports, experimental data, computer codes, and regulatory documents related to oxidation behavior of nuclear graphite is now accelerating to new levels, prompted by the increased interest for nuclear energy as a clean, carbon-free energy source. Even though public’s perception of nuclear energy advantages may still be influenced by the memories of past accidents of nuclear reactors from generations II and III, the community of informed scientists and engineers, regulators and statemen knows that generation IV of nuclear reactors is designed at very high safety standards, doubled by great advances of scientific knowledge and technological progress. One of routes of these recent advances is directed at better understanding of graphite oxidation behavior, its relationship with graphite manufacturing and microstructural properties, along with the effects of various environmental factors and process variables. Together, the recent progress in manufacturing, properties characterization, and modeling of intricated physical and chemical processes that concur to the oxidation behavior led to development of powerful simulation codes able to analyze various scenarios of normal operation and hypothetical off-normal events, and thus to clearly specify the allowable parameters envelopes for the designers, constructors, and operators of current and future modular HTGRs. This review begins with an introduction on manufacturing methods, structure, and properties of nuclear graphite, including basic requirements that this specialty graphite type must satisfy for nuclear use. It continues with a chapter on environmental effects on nuclear graphite, where emphasis is placed less on irradiation and much more on oxidation phenomena, their safety implications, and the basic traits of chronic and acute oxidation by air (oxygen) and water (humidity, steam). Particular attention is placed on the three graphite grades of interest for this document (IG-110, NBG-18, PCEA). A chapter on properties degradation induced by oxidation follows, with focus on density, dimensional, and mechanical properties changes. The next chapter is intended as a brief review of various approaches used for modeling of graphite oxidation behavior. It summarizes the progress of oxidation models, from the early attempts to complex computational approaches interfaced with specialized computer codes designed for nuclear reactor simulations. Last, a list is presented of knowledge gaps where more research is needed. A short summary concludes the review.

36 MATERIALS SCIENCE↗

Observed volatilization behavior of silicon carbide in flowing hydrogen above 2000 K

In this work, the intrinsic compatibility of silicon carbide (SiC) and hydrogen (H 2 ) at high temperatures (2000-2473 K) and pressure near one atmosphere was evaluated through a combination of thermodynamic calculations and hot hydrogen exposure testing. Thermodynamic calculations predict the decomposition of SiC in a hydrogen environment to form free silicon (Si) and free carbon (C). Free Si is predicted to vaporize from the surface as a volatile species, while free C may interact with H 2 to form the hydrocarbons CH 4 (T < 2100 K) or C 2 H 2 (T > 2100 K). Coupons of high purity chemical vapor deposition (CVD) β-SiC were exposed to slowly flowing hydrogen at temperatures ranging between 2000 and 2473 K. SiC experienced active attack as the result of H 2 exposure, exhibiting linear weight loss kinetics and an Arrhenius dependence of weight loss on exposure temperature. The linear volatilization constant was experimentally evaluated to correspond with an activation energy of 370 ± 18 kJ/mol. Due to the dependence of observed corrosion rates on gas velocity, corrosion of SiC in flowing H 2 was determined to be governed by external mass transfer of volatile Si species through the boundary layer. Experimentally derived mass losses were in good agreement with mass losses predicted by a boundary layer limited gas diffusion model.

36 MATERIALS SCIENCE↗

Corrosion of 316H Stainless Steel in Flowing FLiBe (LiF-BeF 2 )

This milestone was originally envisioned for completion in FY21 and was delayed due to the COVID-19 response and difficulties in fabricating/obtaining fluoride salts. A monometallic type 316H stainless steel thermal convection loop (TCL) was operated for 1000 h with flowing LiFBeF 2 (i.e. FLiBe) salt and a peak temperature of 650°C. In general, the attack was minimal. However, classic mass transfer was not clearly observed with mass losses in both the hot and cold legs. There was an issue with cleaning the loop with water and specimens may have oxidized, which was not an issue with the previous FLiNaK TCL.

36 MATERIALS SCIENCE↗