Insulating gallium oxide layer produced by thermal oxidation of gallium-polar GaN: Insulating gallium oxide layer produced by thermal oxidation of gallium-polar GaN

We report the benefits of dry oxidation of n -GaN for the fabrication of metal-oxide-semiconductor structures. GaN thin films grown on sapphire by MOCVD were thermally oxidized for 30, 45 and 60 minutes in a pure oxygen atmosphere at 850 °C to produce thin, smooth GaO x layers. Moreover, the GaN sample oxidized for 30 minutes had the best properties. Its surface roughness (0.595 nm) as measured by atomic force microscopy (AFM) was the lowest. Capacitance-voltage measurements showed it had the best saturation in accumulation region and the sharpest transition from accumulation to depletion regions. Under gate voltage sweep, capacitance-voltage hysteresis was completely absent. The interface trap density was minimum (D it = 2.75×10 10 cm –2 eV –1 ) for sample oxidized for 30 mins. These results demonstrate a high quality GaO x layer is beneficial for GaN MOSFETs.

36 MATERIALS SCIENCE↗

On the electrical and optical properties of oxide nanolayers produced by the thermal oxidation of metal tin

Thin SnO{sub 2–x} layers, 30 nm in thickness, are produced by the thermal oxidation of metal tin nanolayers at a temperature of 450–750°C. The electrical and optical properties of the layers are studied. During the thermal oxidation of tin nanolayers, an unsteady variation in their conductivity is observed. For the oxide films produced at 450 and 550°C, an absorption band at 340 nm (3.65 eV) is detected in the optical spectra. The conductivity-activation energy is determined for samples oxidized to different degrees. On the basis of experimental data and the data reported in publications, an oxidation mechanism controlling the properties of Sn nanolayers is proposed.

36 MATERIALS SCIENCE↗

Progress of Coating Stress Compensation of Silicon Mirrors for Lynx X-ray Telescope Mission Concept Using Thermal Oxide Patterning Method

A thermal oxide patterning method has proven to be effective for correcting coating-stress-induced distortion on flat silicon wafers. We report progress on developing this method for correcting curved silicon mirrors distorted by front-side iridium coatings. Owing to the difference in geometry, a finite element model has been established to calculate the appropriate duty cycle maps in thermal oxide hexagon patterns used for compensation. In addition, a photolithographic process, along with three-dimensional printed equipment, has been developed for creating patterns precisely on the back side of curved mirrors. The developed method has been used to recover the original surface shape of two silicon mirrors which are 100-mm long, 0.5-mm thick, having 312-mm radius of curvature, and 30 deg in azimuthal span (Wolter-I geometry). These mirrors’ front sides are sputter-coated by 20-nm iridium layers with ∼-70 N∕m integrated stress. Measurement results show that the developed method can mitigate coating-induced distortion by a factor of ∼5 in RMS height and ∼4 in RMS slope error, corresponding to ∼0.5 arc sec RMS slope error. Residual errors after correction are dominated by midfrequency ripples created during the annealing process, which will be resolved in the future. The presented method is precise and inexpensive and a potential candidate for resolving the coating stress issue for Lynx optics in the future.

x-ray↗

Surface characterization and mechanical property evaluation of thermally oxidized Ti-6Al-4V

The present study concerns development of a thin and adherent oxide film on the surface of Ti-6Al-4V by thermal oxidation. Thermal oxidation was carried out over a range of temperature between 400 to 600 deg. C and a time from 25 h to 60 h. A detailed characterization of the surface and cross section of the oxidized surface was carried out by optical/scanning electron microscopy and X-ray diffraction techniques. Finally, the mechanical properties of the oxidized surface in terms of microindentation hardness and wear resistance were evaluated as a function of oxidation parameters. Surface oxidation of Ti-6Al-4V at 600 deg. C for 36 h offered a defect free oxide scale with improved hardness and wear resistance.

36 MATERIALS SCIENCE↗

Development of a Thermal Oxidizer for Distributed Microturbine Based Generation

This project concerns the replacement of the catalytic bed in a microturbine with a thermal oxidizer. The advantage of a thermal oxidizer over a traditional combustion chamber is that the length and temperature of the device allows the volatile species to oxidize relatively slowly and without a flame front. With no flame, the temperature increase throughout the unit is spread over a much larger volume so there is no hot spot for thermal NO{sub x} formation, and the gas Btu level does not have to be above the ignition concentration. Project specific objectives included assessment of the materials and performance requirements of the thermal oxidizer, design the thermal oxidizer system, fabrication of the thermal oxidizer, testing of the oxidizer's performance in concert with the microturbine and comparison of the performance of the oxidizer with catalytic beds and traditional combustion chambers. The thermal oxidizer was designed and fabricated with the assistance of High Country Fabrication of Casper, Wyoming. The design consists of a long set of tubes surrounded by a packed bed of loose ceramic material. The outer vessel containing the tubes and packing is a 3-foot diameter steel shell with multiple layers of thermal insulation. After the metal components were fabricated, the vessel was shipped to Denver where the insulation was poured. The unit was shipped to the cosponsor site for integration with the 100 kW microturbine device. Connection of the thermal oxidizer to the Elliot microturbine turned out to be problematic. The high flow rate of gas tended to push the hot zone out of the oxidizer as assembled. The research team identified several approaches to improve the oxidizer performance including a longer gas path, increased residence time, higher surface area packing material and improved combustion catalysts. The cosponsor is working with an engineering form with oxidizer experience to reconfigure the hardware before moving to a field trial on landfill gas.

36 MATERIALS SCIENCE↗

Comparison of thermal oxidation and plasma oxidation of 4H-SiC (0001) for surface flattening

The thermal oxidation and water vapor plasma oxidation of 4H-SiC (0001) were investigated. The initial oxidation rate of helium-based atmospheric-pressure plasma oxidation was six times higher than that of thermal oxidation. The oxide-SiC interface generated by plasma oxidation became flatter with increasing thickness of the oxide, whereas the interface generated by thermal oxidation was atomically flat regardless of the oxide thickness. Many pits were generated on the thermally oxidized surface, whereas few pits were observed on the surface oxidized by plasma. After the oxide layer generated plasma oxidation was removed, an atomically flat and pit-free SiC surface was obtained.

36 MATERIALS SCIENCE↗

Effect of thermal oxidation on helium implanted 316L stainless steel

The effect of thermal oxide layer on He implanted 316L stainless steel was studied to evaluate experimentally how thermal oxidation affects the diffusion and distribution of He in the material. In the case of thermal oxidation of a He implanted sample, with an increase in oxidation time, the max swelling height increases logarithmically as a function of time and finally saturates for all samples except for the lowest dose of implanted He. Concerning TEM results, two void regions are identified. Similar to the calculation, the total irradiated depth was around 250 nm and the large void region was formed around 100–150 nm depth. On the other hand, the small void region was observed immediately under oxide layer from the thermal oxidation. In contrast, there were no voids in the altered zone near the metal/oxide interface in the non-thermal oxidized/He implanted sample. This description of the phenomena was justified using the Kirkendall effect and the Point Defect Model.

36 MATERIALS SCIENCE↗

Multi–length scale characterization of point defects in thermally oxidized, proton irradiated iron oxides

A key for the success of safe nuclear power generation system is to consider structural materials that are economical, meet mechanical property needs, possess good corrosion resistance, and are radiation tolerant. Nevertheless, fundamental insights that elucidate the details of radiation damage on materials corrosion performance are lacking. This includes the behavior of surface oxides which often regulate corrosion. For example, it is unclear how non-equilibrium point defects, oxide structure, mass transport in oxides, and subsequent oxidation behavior are altered by the radiation. Here, in this work, some of the effects of proton irradiation on the attributes of point defects, iron oxide microstructures, and the physical nature of the oxidation product were correlated with corrosion behavior. Iron oxides, fabricated by thermal oxidation in air at 400°C and 800°C for 1 h, were subjected to 200 keV, 0.03 dpa (displacements per atom) of proton irradiation, and subjected to corrosion reactivity assessment using AC and DC electrochemical methods. Experimental methods that target materials information at different length scales, such as positron annihilation spectroscopy (atomistic), transmission electron microscopy (mesoscopic), and electrochemical methods (macroscopic), were coupled to shed light on the impact of radiation-induced defect modifications and structural changes in oxides on corrosion reactivity which ultimately affects durability in harsh environments.

36 MATERIALS SCIENCE↗

Thermal-oxidative Pretreatment and Evaluation of Poly (hexafluoropropene Oxide) Fluids

Two commercial poly(hexafluoropropene oxide) fluids were thermally pretreated at 343 C in pure oxygen. IR and NMR spectra indicate that this pretreatment was effective in removing hydrogen end-capped impurities. Decrease in the quantity of volatile material produced during thermal oxidative decomposition and increase in the thermal decomposition temperature indicated improvement in the stability of the fluids. However, this pretreatment failed to render the fluids completely stable in oxidizing atmospheres at 316 C in the presence of metal alloys.

Paciorek, K. J. L.↗

Thermal-oxidative pretreatment and evaluation of poly(hexafluoropropene oxide) fluids

Two commercial poly(hexafluoropropene oxide) fluids were thermally pretreated at 343 C in pure oxygen. IR and nuclear magnetic resonance(NMR) spectra indicate that this pretreatment was effective in removing hydrogen end-capped impurities. A decrease in the quantity of volatile material produced during thermal oxidative decomposition and increase in the thermal decomposition temperature indicated improvement in the stability of the fluids. However, this pretreatment failed to render the fluids completely stable in oxidizing atmospheres at 316 C in the presence of metal alloys.

Paciorek, K. J. L.↗

Effect of thermal oxidation on helium implanted pure iron

The impact of thermal oxidation on Helium (He) implanted pure iron (Fe) was investigated to experimentally evaluate how thermal oxidation influences the diffusion and distribution of He within the material. In case of the sample with the lowest dose (2 × 10 17 ions/cm 2 ), the thinnest oxide layer was observed compared to the non-implanted pure Fe. It is due to He nano bubbles implanted in the material, which hinder the diffusion of Fe ions necessary for forming the oxide layer. For the medium dose sample (5 × 10 17 ions/cm 2 ), the oxide layer was slightly thicker than that of the lowest dose, however it had more porous structure due to the numerous nano He bubbles. In addition, a large bubble region around 150–200 nm depth was generated. Here, the highest dose sample (1 × 10 18 ions/cm 2 ) was observed that the escape of He was accelerated by the large amount of nano He bubbles from within the metal, forming a porous Fe matrix on the top surface and an oxide layer that is very porous but thicker than those of lower doses.

He implantation↗

Thickness-Dependent Thermal Oxidation of Ni into NiO Thin Films

We report thickness-dependent thermal oxidation in Ni (t = 10–300 nm) thin films exposed to air annealing and the resulting vibrational, magnetic and electrical properties of Ni films deposited directly on thermally oxidized Si substrate using magnetron sputtering technique at ambient temperature. As-deposited Ni films exhibit face-centred cubic structure with fine crystals and large lattice constant (a{sub Ni}) at lower t (< 50 nm). With increasing t, a{sub Ni} decreases and approaches to bulk value. With increasing T{sub A}, a{sub Ni} not only decreases to bulk Ni due to improved crystallization but also reduces below bulk Ni for t > 50 due to formation of NiO. The relative fraction of Ni and NiO in annealed films up to 400 {sup ∘}C strongly depends on t. Annealing Ni films at 500 {sup ∘}C results into complete oxidation of Ni into granular-type NiO. X-ray reflectivity studies reveal that oxidation process occurs from surface of the films converting Ni into NiO possibly through layer by layer process, which is subtle to t. Raman spectra show that intensity ratio between one-phonon longitudinal optical (LO) and two-phonon LO bands decreases and intensity of two-magnon band increases with increasing t for films annealed at particular T{sub A}. This confirms the growth of NiO not only with increasing T{sub A}, but also with t. As-deposited films exhibit ferromagnetism at room temperature. The presence of Ni and NiO in annealed films implies coexistence of ferromagnetic and antiferromagnetic interactions, leading to tunable exchange bias (H{sub E}), whose magnitude strongly depends on the ratio between Ni and NiO. Electrical resistance (R) of the as-deposited Ni films decreases with increasing t and follows the Namba’s model. Upon annealing, R increases largely due to oxidation of Ni. The observed results are explained on the basis of thickness dependent thermal oxidation process with increasing T{sub A}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Operando Study of Thermal Oxidation of Monolayer MoS 2

Abstract Monolayer MoS 2 is a promising semiconductor to overcome the physical dimension limits of microelectronic devices. Understanding the thermochemical stability of MoS 2 is essential since these devices generate heat and are susceptible to oxidative environments. Herein, the promoting effect of molybdenum oxides (MoO x ) particles on the thermal oxidation of MoS 2 monolayers is shown by employing operando X‐ray absorption spectroscopy, ex situ scanning electron microscopy and X‐ray photoelectron spectroscopy. The study demonstrates that chemical vapor deposition‐grown MoS 2 monolayers contain intrinsic MoO x and are quickly oxidized at 100 °C (3 vol% O 2 /He), in contrast to previously reported oxidation thresholds (e.g., 250 °C, t ≤ 1 h in the air). Otherwise, removing MoO x increases the thermal oxidation onset temperature of monolayer MoS 2 to 300 °C. These results indicate that MoO x promote oxidation. An oxide‐free lattice is critical to the long‐term stability of monolayer MoS 2 in state‐of‐the‐art 2D electronic, optical, and catalytic applications.

2-dimensional material↗

Cyclic Thermal Oxidation Evaluation to Improve Ti6Al4V Surface in Applications as Biomaterial

Thermal oxidation treatments are widely used to modify titanium surfaces. Thermally oxidized titanium alloys are used as biomaterials due to their better surface properties, such as corrosion resistance. However, the use of cyclic thermal treatment for this purpose has not yet been reported. This paper’s objective was to compare roughness, microhardness and corrosion resistance after cyclic and conventional isothermal heat treatments in a Ti6Al4V alloy. The heat treatments were performed over a period of 24 h with a maximum temperature of 650 °C, and cyclic conditions were executed from 200 to 400 °C for 48 cycles, each lasting 0.5 h. After the thermal treatments, roughness was measured through profilometer and atomic force microscopy, Vickers microhardness was evaluated, and polarization corrosion tests were performed in simulated body fluid. All treatments increased surface roughness, microhardness and corrosion resistance at 500 mV above open-circuit potential in polarization tests, compared to the material without oxidation. These results are associated with rutile formation, observed through XRD analysis. Although the isothermal and cyclic treatments presented similar behaviors, the 650-200 °C cyclic heat treatment provided an intermediate roughness and produced a slightly better corrosion resistance, demonstrating that cyclic thermal treatments are a viable alternative for improving titanium alloy surface properties.

36 MATERIALS SCIENCE↗

Temperature stability of Al(x)Ga(1-x)As (x = 0-1) thermal oxide masks for selective-area epitaxy

The use of thermal oxides of Al(x)Ga(1-x)As (x = 0-1) as masking materials for selective-area epitaxy by a organometallic chemical-vapor deposition has been investigated. It was found that the thermal oxide of GaAs is only applicable for low growth temperatures (less than or equal to 600 C), and the addition of aluminum significantly improves the thermal stability of the oxide. The oxide of Al(0.4)Ga(0.6)As is suitable for high-temperature deposition, but there are criteria for the thickness and oxidation temperature. Thin layers of AlAs oxidized at 475 C are excellent masks and allow precise thickness control. Promising results of selective-area deposition using these aluminum oxide masks have been obtained. High-quality single crystal grew in mask openings uniformly surrounded by dense and fine-grain polycrystalline deposits, producing a planar duplication of the original pattern.

Jones, Stephen H.↗

Thermal oxidative degradation reactions of perfluoroalkylethers

The mechanisms operative in thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes are investigated. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids is not established. It was determined that this behavior is not associated with hydrogen end groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres is dependent on the surface/volume ratio. Once a limiting ratio is reached, a steady rate appears to be attained. Based on elemental analysis and oxygen consumption data, CF2OCF2CF2O2, no. CF2CF2O, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys is much more drastic in the case of Fomblin Z fluids than that observed for the hexafluoropropene derived materials. The effectiveness of antioxidation anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys is very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appears to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes this takes place to a much lesser degree with M-50.

Paciorek, K. L.↗

Pretreatment effects on the morphology and properties of aluminum oxide thermally grown on NiCoCrAlY

The effect of pretreatments on the morphology and properties of aluminum oxide thermally grown from NiCoCrAlY was investigated. The goal was to optimize process steps to produce a highly adherent, continuous, and insulating aluminum oxide. Two pretreatments were carried out, one in vacuum (about 0.0001 Torr) at 1350 K for 5 h, and the other consisting of deposition of a 1-micron thick Al2O3 film by activated reactive evaporation. Samples were subsequently oxidized thermally at 1000 C for 50 h at 0.5 Torr oxygen pressure. The two pretreatments were carried out on electron-beam evaporation NiCoCrAlY, about 120 microns thick, deposited on a superalloy turbine blade substrate. The results showed that the thermally grown oxide was significantly different in microstructure, surface topography and in its adherence to the NiCoCrAlY for the two pretreatments. Optimum results were obtained by combining the two pretreatments to produce an adherent, continuous, and insulating oxide film on the NiCoCrAlY-coated superalloy substrate.

Prakash, S.↗