As-Deposited Thin-Film Battery Cathode Layers
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Thin film batteries employing sputtered LiCoPO4 cathode layers, LiPON electrolyte and Li anode films have been successfully fabricated and tested.
Crystalline solid solutions of 1:1 Li3PO4/SiO4 were synthesized and tested electrochemically using thin film, physical vapor deposited electrodes. After cathode deposition, the electrolyte/cathode structures were annealed at 700 degrees Celsius for 2 hours, a process that resulted in cathode crystallization without encouraging deleterious interfacial reactions. Results indicate that the electrolyte functioned well in this configuration.
High-nickel layered oxide cathodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) are critical for next-generation lithium-ion batteries (LIBs) due to their superior energy density and reduced reliance on cobalt. However, many Ni-rich cathodes suffer from rapid capacity fade and structural instability originating from complex interfacial reactions at the cathode-electrolyte interface. Traditional composite electrodes exhibit degradation mechanisms that are challenging to quantitatively understand due to additives, including binders and carbon black. In this study, we demonstrate a new synthesis approach for binder- and additive-free NMC811 thin films using polymer-assisted deposition (PAD). PAD-NMC811 are model thin-film cathodes for investigating interfacial phenomena that can be obscured in composite cathodes. Structural and chemical characterization by X-ray diffraction, soft X-ray absorption spectroscopy, and atomic force microscopy show that PAD-NMC811 films possess high phase purity, crystallinity, chemical homogeneity, and morphological uniformity. Electrochemical analyses using cyclic voltammetry and galvanostatic cycling revealed electrochemical behavior consistent with that of composite electrodes, along with a moderate capacity fade indicative of cathode-electrolyte interphase (CEI) formation. Our findings illustrate the effectiveness of PAD synthesis of thin films tailored for detailed mechanistic studies, which offer critical insights into CEI evolution and cathode degradation pathways.
Here, the plasma enhanced atomic layer deposition (PEALD) process for MnO 2 was demonstrated, exhibiting self-limiting growth as well as stable composition and stable growth rate over a temperature window of 205–265 °C. The PEALD process for MnO 2 was combined with the thermal ALD process for LiOH to synthesize Li 1+x Mn 2-x O 4 thin film cathodes, where the stoichiometry was effectively controlled to allow for crystallization in the electrochemically active spinel phase. A 3D nanostructure consisting of an Li 1+x Mn 2-x O 4 cathode layer, ALD Li x Al y Si z O solid electrolyte, and SiGe nanowire anode was fabricated and characterized via TEM. The Li 1+x Mn 2-x O 4 thin films maintained 66% of the areal capacity upon a 100× increase in the rate (4–360 μ A cm -2 ) as well as 97% capacity retention over 100 cycles at ~5C. The ALD Li 1+x Mn 2-x O 4 thin films exhibited a volumetric capacity of 52 μ Ah cm -2 μ m -1 at a C-rate of ~0.5C and, coupled with the high operating voltage (4.0 V), offer some of best areal energy densities for ALD thin film cathodes, making it a viable material for integration with 3D lithium-ion microbatteries.
Navitas teamed up with UMD and ORNL to establish a reliable scientific research team. The project addressed processing limitations of state-of-the-art solid electrolytes by extending solvent-free electrode fabrication technology to the scalable production of cathode/solid electrolyte laminates. The innovation started with a solid-state sulfide electrolyte (LiPS) with Cl stabilization able to meet the keystone conductivity challenge in a film of practical thickness (μ 50 µm). The electrolyte was based on a composite of PTFE, and stabilized LiPSCl. With optimization, the ionic conductivity reached 3.3 ×10 -3 S/cm. The solid electrolyte with as low as 0.4% binder allowed long term cycling (> 500 cycles) of Li/SSE/Li cell at > 4 mA/cm 2 with the utilization of Li > 80%. The Li and SSE interfaces were successfully protected with LiF-rich SEI layer. NCM811cathode active materials were coated with a thin layer of Al 2 O 3 (5 nm). The free standing cathode film was fabricated through dry-process with Al2O3-coated NCM811, LiPSCl, active carbon, and small amount PTFE. The all-solid-state batteries were laminated with free standing surface coated NCM811 cathode film, free standing LiPSCl SSE film, and surface protected Li anode together in a single lamination step, and demonstrated high specific capacity (> 200 mAh/g) with coulombic efficiency > 99.5%. The all-solid-state batteries through solvent-free and no-sintering process are promising for large format cell with 500 Wh/Kg specific energy density.
Abstract The severe capacity loss of spinel LiMn 2 O 4 (LMO) limits the utility of this otherwise promising lithium ion battery cathode material. One of the strategies to mitigate capacity fade is applying a coating on LMO particle surfaces. While this approach yields promising results, there is limited understanding of mechanisms whereby coatings improve LMO capacity retention. Herein, the effects of a new protective coating material, La 0.5 Sr 0.5 CoO 3 (LSCO), in a thin‐film battery geometry that is amenable to fundamental studies of electrode processes, are reported. RF sputtering deposition is used to produce high quality 25–100 nm LMO cathodes on Al 2 O 3 substrates with an intervening Pt/Ti back‐side contact layer. Cycling of the un‐coated cathodes results in capacity loss of 18% over 300 cycles. Adding a 2 nm LSCO layer reduces the capacity loss to 3%. While this may be due in part to reduced Mn dissolution, scanning transmission electron microscopy results indicate that the coating helps to preserve crystallinity and reduce lattice structure distortion due to inhibited formation of defect tetragonal spinel. Three‐electrode electrochemical impedance spectroscopy results reveal that the LSCO coating increases charge transfer and ohmic resistances, but the increases are generally too small to significantly impact cell performance even at high C‐rates.
Lithium-ion batteries (LIBs) have been the focus of research for decades owing to their superior energy storage potential and wide range of applications. However, long-term stability issues still persist in LIB cathodes as the result of the formation of a solid electrolyte interface (SEI), structural transformations, or the loss of active cathode materials. In nanoscale cathodes, it is often impossible to isolate, let alone mitigate the causes of the observed capacity loss. Herein, a novel approach is presented to synthesizing LIB cathode model systems using thin-film molecular beam epitaxy (MBE). Specifically, 100 nm thick LiMn 2 O 4 (LMO) thin-film cathodes are grown on SrRuO 3 /SrTiO 3 (100) single-crystal substrates and characterized in their pristine and cycled states. The pristine thin films exhibit the electro-chemical cycling behavior and structural evolution previously seen in bulk LMO cathodes. The formation of surface-layer rocksalt MnO and spinel Mn 3 O 4 along with the mass-loss associated with the corrosion of active Mn ions is also reported. It is, therefore, demonstrated that these MBE-grown model systems can be used for detailed studies of their surface structures and the electrode/electrolyte interfacial evolution in LIB cathodes, leading to the development of materials for rechargeable batteries with higher capacity and better stability.
Abstract Spinel‐type LiNi 0.5 Mn 1.5 O 4 (LNMO) is one of the most promising 5 V‐class cathode materials for Li‐ion batteries that can achieve high energy density and low production costs. However, in liquid electrolyte cells, the high voltage causes continuous cell degradation through the oxidative decomposition of carbonate‐based liquid electrolytes. In contrast, some solid‐state electrolytes have a wide electrochemical stability range and can withstand the required oxidative potential. In this work, a thin‐film battery consisting of an LNMO cathode with a solid lithium phosphorus oxynitride (LiPON) electrolyte is tested and their interface before and after cycling is characterized. With Li metal as the anode, this system can deliver stable performance for 600 cycles with an average Coulombic efficiency >99%. Neutron depth profiling indicates a slight overlithiated layer at the interface prior to cycling, a result that is consistent with the excess charge capacity measured during the first cycle. Cryogenic electron microscopy further reveals intimate contact between LNMO and LiPON without noticeable structure and chemical composition evolution after extended cycling, demonstrating the superior stability of LiPON against a high voltage cathode. Consequently, design guidelines are proposed for interface engineering that can accelerate the commercialization of a high voltage cell with solid or liquid electrolytes.
Graphite fluoride fiber/polymer composite materials consist of graphite fluoride fibers in epoxy, polytetrafluoroethylene, or polyimide resin. Combines high electrical resistivity with high thermal conductivity and solves heat-transfer problems of many electrical systems. Commercially available in powder form, for use as dry lubricant or cathode material in lithium batteries. Produced by direct fluorination of graphite powder at temperature of 400 to 650 degree C. Applications include printed-circuit boards for high-density power electronics, insulators for magnetic-field cores like those found in alternators and transformers, substrates for thin-film resistors, and electrical-protection layers in aircraft de-icers.
Chemo-mechanical degradation of layered oxide electrodes is strongly influenced by crystallographic anisotropy, local stress evolution, and ion insertion, yet the intrinsic mechanical response of layered materials remains incompletely understood. Indeed, most prior studies have focused on polycrystalline materials but single crystals enable direct observation of coupling between anisotropic ion diffusion and mechanical response. This study aims to determine how crystallographic anisotropy and lithiation affect deformation, fracture, and mechanical properties in single-crystal V 2 O 5 , and compares this behavior with polycrystalline counterparts. Polycrystalline V 2 O 5 thin films and single-crystal α-V 2 O 5 were studied using nanoindentation, scanning electron microscopy, focused ion beam cross-sectioning, and Raman spectroscopy. Single crystals were tested in pristine and chemically lithiated states, including experiments in which crystals were first plastically deformed via nanoindentation and subsequently lithiated. Polycrystalline films exhibited significantly higher hardness and elastic modulus than single crystals. Single crystals indented normal to the exposed (001) basal plane exhibited pronounced anisotropic deformation, including directional slip, crystallographically-guided cracking, anisotropic crack propagation, interlayer separation, and shear localization. Lithiation caused substantial softening, reduced hardness and modulus, and suppressed displacement bursts during nanoindentation, while previously indented regions showed crack formation and growth upon lithiation. Mechanical behavior of α-V 2 O 5 is strongly governed by crystallographic anisotropy and further altered by lithiation, with pre-existing deformation serving as a strong driver of fracture during ion insertion. These findings illuminate the coupling among ion insertion, deformation, and fracture in layered oxides and provide a basis for understanding and mitigating mechanical failure in electrochemical energy-storage materials.
The integration of organic electrode materials (OEMs) with solid-state electrolytes (SSEs) is expected to build an all-solid-state battery (ASSB) with long-term sustainability, high safety, and high energy density. Despite this great promise, the cell-level energy density is still far from practically applicable, which stems from the ultrathick SSE layer and thin cathode layer used in a pellet-type ASSB design. Here, a cost-effective polyimide (PI) material was first exploited as an organic cathode for sulfide-based ASSBs. A capacity of ~190 mAh g -1 was delivered with almost no capacity decay over 300 cycles. Moreover, for the first time, a dry-film approach was introduced to manufacture a sheet-type Li–organic ASSB with an ultrathin SSE layer and a high-areal-loading PI cathode. Notably, PI is a perfect candidate for dry-film technology due to its high thermal stability and extraordinary chemical inertness toward sulfide SSEs. Remarkably, the free-standing SSE membrane was merely 46 μm thick, and an ultralow areal resistance of 3.3 Ω cm 2 was achieved, more than tenfold lower than that of reported SSE pellets. One order of magnitude boost in the cell-level energy density was achieved. This work presents a significant leap in transferring organic ASSB technology from laboratory research to factory manufacturing.
Composite polymer electrolytes (CPEs) for solid-state Li-metal batteries (SSLBs) still suffer from gradually increased interface resistance and unconstrained Li-dendrite growth. Herein, we addressed the challenges by designing a LiF-rich inorganic solid-electrolyte interphase (SEI) through introducing a fluoride-salt-concentrated interlayer on CPE film. The rigid but flexible CPE helps accommodate the volume change of electrodes, while the polymeric highly concentrated electrolyte (PHCE) surface-layer regulates Li-ion flux due to the formation of a stable LiF-rich SEI via anion reduction. The designed CPE-PHCE presents enhanced ionic conductivity and high oxidation stability of >5.0 V (versus Li/Li + ). Furthermore, it dramatically reduces the interfacial resistance and achieves a high critical current density of 4.5 mA cm –2 . The SSLBs, fabricated with thin CPE-PHCE membranes (<100 μm) and Co-free LiNiO 2 cathodes, exhibit exceptional electrochemical performance and long cycling stability. Lastly, this approach of SEI design can also be applied to other types of batteries.
Solid state lithium-ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid-electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO), with the high voltage cathode, spinel Li x Mn 2 O 4 (LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x-ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer-by-layer deposition of LLZTO and Li 3 N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li 2 MnO 3 , which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn 2 O 4 has a voltage of ≈3.7 V versus Li+/Li, the observation of a well-defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.
Abstract Solid‐state batteries promise higher energy densities and better safety than Li‐ion batteries with liquid electrolytes. However, the interface between solid electrolyte and cathode is unstable at the elevated temperatures that are needed while sintering to achieve good bonding between ceramic components. Here, the hypothesis is that, the gas environment, especially the presence of CO 2, is critical in determining the stability of the solid electrolyte–cathode interface. The effect of gas species on the interface is systematically probed, by a using Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte with a thin film LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode as a model system to enable interface sensitivity. Detrimental phases formed at the interface and their onset conditions are identified by X‐ray absorption spectroscopy, X‐ray diffraction, and Gibbs free energy analysis. As a result, removing CO 2 and minimizing H 2 O(g) during sintering is necessary to obtain good contact at the LLZO|cathode interface without forming secondary phases. Sintering in O 2 is ideal, yielding excellent chemical stability and low interfacial resistance. Secondary phases also do not form in N 2, but oxygen loss occurs at elevated temperatures. The interfacial resistance obtained upon sintering in pure O 2 is comparable to the lowest values at LLZO interfaces with protective coatings, but here without the need for interface coatings.
The high operating voltage of a spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode leads to electrolyte decomposition and accelerated deterioration of the electrode/electrolyte interface in lithium-ion cells. Aggressive side reactions prevent long-term cycling and hinder its practical application. Advanced characterization shows that the high-voltage operation makes the graphite anode react with the electrolyte, particularly with the lithium salt in the electrolyte, resulting in massive active lithium inventory loss and capacity fade. The side reactions at the graphite are identified as the main culprit for the LNMO/graphite full cell decay. Here, we demonstrate that an artificial solid-electrolyte interface layer consisting of an ultra-thin Al 2 O 3 film, generated via atomic layer deposition (ALD) at the graphite surface, can successfully isolate the graphite from the electrolyte and inhibit the undesired reactions. Consequently, the capacity and cycling stability of the LNMO/graphite cell are drastically improved. After 300 cycles, the capacity retention of LNMO/graphite cell increases from 57.7% to 98.6% with the ALD-coated graphite. Furthermore, our findings provide valuable insights into the LNMO/graphite cell degradation and suggest a simple and robust, yet highly effective, approach for the practical viability of high-voltage lithium-ion batteries.
Lithium primary and lithium ion secondary batteries provide high specific energy and energy density. The use of these batteries also helps to reduce launch weight. Both primary and secondary cells can be packaged as high-rate cells, which can present a threat to crew and equipment in the event of external or internal short circuits. Overheating of the cell interior from high current flows induced by short circuits can result in exothermic reactions in lithium primary cells and fully charged lithium ion secondary cells. Venting of the cell case, ejection of cell components, and fire have been reported in both types of cells, resulting from abuse, cell imperfections, or faulty electronic control design. A switch has been developed that consists of a thin layer of composite material made from nanoscale particles of nickel and Teflon that conducts electrons at room temperature and switches to an insulator at an elevated temperature, thus interrupting current flow to prevent thermal runaway caused by internal short circuits. The material is placed within the cell, as a thin layer incorporated within the anode and/or the cathode, to control excess currents from metal-to-metal or metal-to-carbon shorts that might result from cell crush or a manufacturing defect. The safety of high-rate cells is thus improved, preventing serious injury to personnel and sensitive equipment located near the battery. The use of recently available nanoscale particles of nickel and Teflon permits an improved, homogeneous material with the potential to be fine-tuned to a unique switch temperature, sufficiently below the onset of a catastrophic chemical reaction. The smaller particles also permit the formation of a thinner control film layer (<50 m), which can be incorporated into commercial high-rate lithium primary and secondary cells. The innovation permits incorporation in current lithium and lithium-ion cell designs with a minimal impact on cell weight and volume. The composite thermal switch (CTS(TradeMark)) coating can be incorporated in either the anode or cathode or both. The coating can be applied in a variety of different processes that permits incorporation in the cell and electrode manufacturing processes. The CTS responds quickly and halts current flow in the hottest parts of the cell first. The coating can be applied to metal foil and supplied as a cell component onto which the active electrode materials are coated.