Search NASA⌕ Search

SEARCH · Search NASA

Results for “tungsten composite”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Temperature effects of ion irradiation on the nanostructural features in ductile-phase-toughened tungsten composites

Ductile-phase toughened tungsten (DPT W) composites have emerged as promising candidates for load-bearing components behind the plasma-facing tungsten armor in fusion reactors due to their enhanced thermomechanical properties. This study focuses on a composite consisting of W particles embedded in a ductile NiFeW solution matrix, hot-rolled to a thickness reduction of 87% (87R DPT W). Sequential irradiations with Ni2+ and He+ ions were performed to identical doses and helium concentrations at room temperature (RT) and 1273 K. Irradiation at RT produced no discernible nanostructural features due to the immobility of mono-vacancies, whereas cavity formation was observed at 973 K. At 1273 K, the W phase exhibited larger cavities, reduced cavity number density, and lower volumetric swelling compared to 973 K. Notably, nanosized NiFeW precipitates formed within the W phase at 1273 K, a phenomenon absent at 973 K. A new phase of cubic (NiFe)6W6C was also observed at the interphase boundary. In contrast, the NiFeW matrix showed no nanostructural changes at 1273 K, likely due to cavity dissociation. Separate irradiations at 1273 K indicated that Ni2+ ions induced precipitate formation in the W phase, while He+ ions exclusively caused cavity formation. The microstructure of 87R DPT W irradiated at RT and subsequently annealed at 1273 K closely resembled that of material irradiated directly at 1273 K. Like oxide-dispersion-strengthened steels, the observed nanoparticle-embedded W can inhibit dislocation propagation, potentially delaying the ductile-to-brittle transition temperature. These findings highlight the potential of NiFeW nanoparticle-reinforced W composites as irradiation-resistant materials for fusion reactors.

Jiang, Weilin (ORCID:0000000183028313)↗

Factors affecting the thermal shock behavior of yttria stabilized hafnia based graphite and tungsten composites.

Hafnia-based composites containing either graphite or tungsten were investigated as rocket nozzle throat inserts in solid propellant rocket engines. The thermal shock resistance of these materials is considered in terms of macroscopic thermal conductivity, thermal expansion, modulus of elasticity, and compressive fracture stress. The effect of degree of hafnia stabilization, density, and graphite or tungsten content upon these parameters is discussed. The variation of the ratio of elastic modulus to compressive fracture stress with density and its effect upon thermal shock resistance of these materials are discussed in detail.

Lineback, L. D.↗

Thermophysical Properties of a Uranium Nitride–Molybdenum-Tungsten Composite Fuel for Nuclear Thermal Propulsion

The thermal conductivity of a ceramic-metal composite consisting of 60 vol % uranium nitride incorporated into a molybdenum-tungsten matrix has been measured up to a temperature of 1200°C. Compositing nuclear fuel with refractory materials is considered a viable way to improve the thermal and mechanical properties of fuels, and more recently, has been investigated as a way to improve hydrogen compatibility in a nuclear thermal propulsion rocket reactor. Here, we demonstrate that high-density composites can be produced from direct current sintering and that the resulting thermal conductivity is improved compared to the pure.

33 ADVANCED PROPULSION SYSTEMS↗

Creep behavior of tungsten fiber reinforced niobium metal matrix composites

Tungsten fiber reinforced niobium metal matrix composites were evaluated for use in space nuclear power conversion systems. The composite panels were fabricated using the arc-spray monotape technique at the NASA Lewis Research Center. The creep behavior of W/Nb composite material was determined at 1400 and 1500 K in vacuum over a wide range of applied loads. The time to reach 1 percent strain, the time to rupture, and the minimum creep rate were measured. The W/Nb composites exceeded the properties of monolithic niobium alloys significantly even when compared on a strength to density basis. The effect of fiber orientation on the creep strength also was evaluated. Kirkendall void formation was observed at the fiber/matrix interface; the void distribution differed depending on the fiber orientation relative to the stress axis. A relationship was found between the fiber orientation and the creep strength.

Grobstein, T. L.↗

Creep behavior of tungsten fiber reinforced niobium metal matrix composites

Tungsten fiber reinforced niobium metal matrix composites were evaluated for use in space nuclear power conversion systems. The composite panels were fabricated using the arc-spray monotape technique at the NASA Lewis Research Center. The creep behavior of W/Nb composite material was determined at 1400 and 1500 K in vacuum over a wide range of applied loads. The time to reach 1 percent strain, the time to rupture, and the minimum creep rate were measured. The W/Nb composites exceeded the properties of monolithic niobium alloys significantly even when compared creep strength also was evaluated. Kirkendall void formation was observed at the fiber/matrix interface; the void distribution differed depending the fiber orientation relative to the stress axis. A relationship was found between the fiber orientation and the creep strength.

Grobstein, Toni L.↗

Improving the W Coating Uniformity by a COMSOL Model-Based CVD Parameter Study for Denser W f /W Composites

Tungsten (W) has the unique combination of excellent thermal properties, low sputter yield, low hydrogen retention, and acceptable activation. Therefore, W is presently the main candidate for the first wall and armor material for future fusion devices. However, its intrinsic brittleness and its embrittlement during operation bears the risk of a sudden and catastrophic component failure. As a countermeasure, tungsten fiber-reinforced tungsten (W f /W) composites exhibiting extrinsic toughening are being developed. A possible W f /W production route is chemical vapor deposition (CVD) by reducing WF 6 with H 2 on heated W fabrics. The challenge here is that the growing CVD-W can seal gaseous domains leading to strength reducing pores. In previous work, CVD models for W f /W synthesis were developed with COMSOL Multiphysics and validated experimentally. In the present article, these models were applied to conduct a parameter study to optimize the coating uniformity, the relative density, the WF 6 demand, and the process time. A low temperature and a low total pressure increase the process time, but in return lead to very uniform W layers at the micro and macro scales and thus to an optimized relative density of the W f /W composite. High H 2 and low WF 6 gas flow rates lead to a slightly shorter process time and an improved coating uniformity as long as WF 6 is not depleted, which can be avoided by applying the presented reactor model.

36 MATERIALS SCIENCE↗

Hot Isostatic Pressing Control of Tungsten-Based Composites

Metal-oxide composites are commonly used in high temperature environments for their thermal stability and high melting points. Commonly employed with refractory oxides or carbides such as ZrC and HfC, these materials may be improved with the use of a low density, high melting point ceramic such as CeO2. In this work, the consolidation of W-CeO2 metal matrix composites in the high CeO2 concentration regime is explored. The CeO2 concentrations of 50, 33, and 25 wt.%, the CeO2 particle size from nanometer to micrometer, and various hot isostatic pressing temperatures are investigated. Decreasing the CeO2 concentration is observed to increase the composite density and increase the Vickers hardness. The CeO2 oxidation state is observed to be a combination of Ce3+ and Ce4+, which is hypothesized to contribute to the porosity of the composites. The hardness of the metal-oxide composite can be improved more than 2.5 times compared to pure W processed by the same route. This work offers processing guidelines for further consolation of oxide-doped W composites.

36 MATERIALS SCIENCE↗

Mesoporous tungsten oxide composition

The present disclosure relates to tungsten oxide composition. Specifically, the present disclosure relates to mesoporous tungsten oxide composition that is active for multiple reactions, including aromatic alkylation, alkene coupling, alkene cyclization, alkyne oxidation, alcohol dehydrogenation reactions.

Suib, Steven L.↗

Metal carbide-graphite composites

Tungsten used in NbC-C composites as low melting densification additive to improve composite properties and lower fabrication temperatures

Harada, Y.↗

Discovering tungsten-based composites as plasma facing materials for future high-duty cycle nuclear fusion reactors

Abstract Despite of excellent thermal properties and high sputtering resistance, pure tungsten cannot fully satisfy the requirements for plasma facing materials in future high-duty cycle nuclear fusion reactions due to the coupled extreme environments, including the high thermal loads, plasma exposure, and radiation damage. Here, we demonstrated that tungsten-based composite materials fabricated using spark-plasma sintering (SPS) present promising solutions to these challenges. Through the examination of two model systems, i.e., tungsten-zirconium composite for producing porous tungsten near the surface and dispersoid-strengthened tungsten, we discussed both the strengths and limitations of the SPS-fabricated materials. Our findings point towards the need for future studies aimed at optimizing the SPS process to achieve desired microstructures and effective control of oxygen impurities in the tungsten-based composite materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

High temperature tension-compression fatigue behavior of a tungsten copper composite

The high temperature fatigue of a (O)12 tungsten fiber reinforced copper matrix composite was investigated. Specimens having fiber volume percentages of 10 and 36 were fatigued under fully-reversed, strain-controlled conditions at both 260 and 560 C. The fatigue life was found to be independent of fiber volume fraction because fatigue damage preferentially occurred in the matrix. Also, the composite fatigue lives were shorter at 560 C as compared to 260 C due to changes in mode of matrix failure. On a total strain basis, the fatigue life of the composite at 560 C was the same as the life of unreinforced copper, indicating that the presence of the fibers did not degrade the fatigue resistance of the copper matrix in this composite system. Comparison of strain-controlled fatigue data to previously-generated load-controlled data revealed that the strain-controlled fatigue lives were longer because of mean strain and mean stress effects.

Verrilli, Michael J.↗