Hot isostatic compaction of tungsten-uranium dioxide fuels with high-volume fraction of uranium dioxide
Smooth surface coating of molybdenum alloys for cermets by hot isostatic compaction of tungsten-uranium dioxide fuels
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Smooth surface coating of molybdenum alloys for cermets by hot isostatic compaction of tungsten-uranium dioxide fuels
Uranium losses during thermal cycling of tungsten - uranium dioxide composites to 2500° C in flowing purified hydrogen for specimens initially containing 35 volume percent uranium dioxide were reduced by the use of thorium dioxide, calcium oxide, or yttrium oxide as additives in solid solution with the uranium dioxide. The effectiveness of the additives decreased in the order yttrium oxide, calcium oxide, and thorium dioxide. Stabilization of uranium dioxide by calcium oxide or yttrium oxide can be explained in part on the basis of the introduction of oxygen vacancies into the fluorite lattice and the associated lowered partial molar free energy of oxygen. The difference in the effectiveness of calcium oxide and yttrium oxide is discussed, and a possible explanation of the observed behavior is proposed. Of the concentrations of yttrium oxide tested (i.e., 2. 5, 5, and 10 mole percent), 10 mole percent of yttrium oxide was the most effective in pre venting loss of uranium from composities.
Although tungsten-uranium dioxide composites appear very promising, as fuel element materials for high-temperature nuclear rocket reactors, one of the major problems with these materials is the loss of fuel at reactor operating temperatures (near or above 4500 F). Substantial fuel losses occur by vaporization whenever the uranium dioxide is directly exposed to elevated temperature environments and by fuel migration and vaporization when reactor operating conditions that involve thermal cycling are simulated. Several methods of minimizing fuel loss have been evaluated and appear quite promising.
An investigation was undertaken to determine the feasibility of depositing integrally bonded plasma-sprayed tungsten coatings onto 80-volume-percent tungsten - 20-volume-percent uranium dioxide composites. These composites were face clad with thin tungsten foil to inhibit uranium dioxide loss at elevated temperatures, but loss at the unclad edges was still significant. By preheating the composite substrates to approximately 3700 degrees F in a nitrogen environment, metallurgically bonded tungsten coatings could be obtained directly by plasma spraying. Furthermore, even though these coatings were thin and somewhat porous, they greatly inhibited the loss of uranium dioxide. For example, a specimen that was face clad but had no edge cladding lost 5.8 percent uranium dioxide after 2 hours at 4750 dgrees F in flowing hydrogen. A similar specimen with plasma-spray-coated edges, however, lost only 0.75 percent uranium dioxide under the same testing conditions.
Irradiated fuel capsules containing uranium dioxide and uranium carbide
Compatibility of molten uranium dioxide with refractory metals
The plasma spheroidization system (PSS) is the first process in the development of tungsten-uranium dioxide (W-UO2) fuel cermets. The PSS process improves particle spherocity and surface morphology for coating by chemical vapor deposition (CVD) process. Angular fully dense particles melt in an argon-hydrogen plasma jet at between 32-36 kW, and become spherical due to surface tension. Surrogate CeO2 powder was used in place of UO2 for system and process parameter development. Particles range in size from 100 - 50 microns in diameter. Student s t-test and hypothesis testing of two proportions statistical methods were applied to characterize and compare the spherocity of pre and post process powders. Particle spherocity was determined by irregularity parameter. Processed powders show great than 800% increase in the number of spherical particles over the stock powder with the mean spherocity only mildly improved. It is recommended that powders be processed two-three times in order to reach the desired spherocity, and that process parameters be optimized for a more narrow particles size range. Keywords: spherocity, spheroidization, plasma, uranium-dioxide, cermet, nuclear, propulsion
Thermal conductivity measurements on tungsten coated uranium dioxide cermets
Uranium dioxide vent loss in externally fueled thermionic reactor concept
Fission product gas pressure calculated for uranium dioxide ceramic fuel elements
Postirradiation of high temperature, low burnup tungsten uranium dioxide test plates
High temperature creep rupture strength of tungsten uranium dioxide cermets
Furnace brazing butt joints in tungsten-uranium dioxide cermet cylinders at 3000 deg C
Equilibrium carbon monoxide pressures measured by torsion effusion studies of reaction of graphite with hafnium and uranium dioxides at high temperatures
Establishing allowable temperature gradients for tungsten-uranium dioxide fuel elements using experimental cyclic strain data
A fuel pin clad with TZM and containing solid pellets of uranium dioxide was fission heated in a static helium-cooled capsule at a maximum surface temperature of 1700 K for approximately 1000 hr and to a total burnup of 2.0 percent of the uranium-235. The results of the postirradiation examination indicated: (1) A transverse, intergranular failure of the fuel pin occurred when the fuel pin reached 2.0-percent burnup. This corresponds to 1330 kW-hr/cu cm, where the volume is the sum of the fuel, clad, and void volumes in the fuel region. (2) The maximum swelling of the fuel pin was less than 1.5 percent on the fuel-pin diameter. (3) There was no visible interaction between the TZM clad and the UO2. (4) Irradiation at 1700 K produced a course-grained structure, with an average grain diameter of 0.02 centimeter and with some of the grains extending one-half of the thickness of the clad. (5) Below approximately 1500 K, the irradiation of the clad produced a moderately fine-grained structure, with an average grain diameter of 0.004 centimeter.
CERMET fuel materials are being developed at the NASA Marshall Space Flight Center for a Nuclear Cryogenic Propulsion Stage. Recent work has resulted in the development and demonstration of a Compact Fuel Element Environmental Test (CFEET) System that is capable of subjecting depleted uranium fuel material samples to hot hydrogen. A critical obstacle to the development of an NCPS engine is the high-cost and safety concerns associated with developmental testing in nuclear environments. The purpose of this testing capability is to enable low-cost screening of candidate materials, fabrication processes, and further validation of concepts. The CERMET samples consist of depleted uranium dioxide (UO2) fuel particles in a tungsten metal matrix, which has been demonstrated on previous programs to provide improved performance and retention of fission products1. Numerous past programs have utilized hot hydrogen furnace testing to develop and evaluate fuel materials. The testing provides a reasonable simulation of temperature and thermal stress effects in a flowing hydrogen environment. Though no information is gained about radiation damage, the furnace testing is extremely valuable for development and verification of fuel element materials and processes. The current work includes testing of subscale W-UO2 slugs to evaluate fuel loss and stability. The materials are then fabricated into samples with seven cooling channels to test a more representative section of a fuel element. Several iterations of testing are being performed to evaluate fuel mass loss impacts from density, microstructure, fuel particle size and shape, chemistry, claddings, particle coatings, and stabilizers. The fuel materials and forms being evaluated on this effort have all been demonstrated to control fuel migration and loss. The objective is to verify performance improvements of the various materials and process options prior to expensive full scale fabrication and testing. Post test analysis will include weight percent fuel loss, microscopy, dimensional tolerance, and fuel stability.
Radial power tailoring for uranium dioxide-T-111 clad reactor with contained fission product gases