Optical and electronic functionality arising from controlled defect formation in nanoscale complex oxide lateral epitaxy

Epitaxial crystallization of complex oxides provides the means to create materials with precisely selected composition, strain, and orientation, thereby controlling their functionalities. Extending this control to nanoscale three-dimensional geometries can be accomplished via a three-dimensional analog of oxide solid-phase epitaxy, lateral epitaxial crystallization. The orientation of crystals within laterally crystallized SrTiO 3 systematically changes from the orientation of the SrTiO 3 substrate. This evolution occurs as a function of lateral crystallization distance, with a rate of approximately 50° μm -1 . The mechanism of the rotation is consistent with a steady-state stress of tens of megapascal over a 100–nanometer scale region near the moving amorphous/crystalline interface arising from the amorphous-crystalline density difference. Second harmonic generation and piezoelectric force microscopy reveal that the laterally crystallized SrTiO 3 is noncentrosymmetric and develops a switchable piezoelectric response at room temperature, illustrating the potential to use lateral crystallization to control the functionality of complex oxides.

36 MATERIALS SCIENCE↗

Twinning microstructure in the solid-phase epitaxial crystallization of BaTiO 3

Amorphous BaTiO 3 layers deposited on SrTiO 3 (001) substrates at room temperature were subsequently crystallized using solid phase epitaxy (SPE). Heating an initially amorphous BaTiO 3 layer in air at 650 °C for 3 h resulted in crystallization with components in two distinct crystallographic orientation relationships with respect to the substrate. Part of the volume of the BaTiO 3 layer crystallized in a cube-on-cube relationship with the substrate. Other volumes crystallized in four variants of a 70.5° rotation about $\langle$110$\rangle$, resulting in a $\langle$221$\rangle$ surface normal in each case. Each of these four variants forms a Σ = 3 coincident site lattice with respect to the SrTiO 3 substrate and the cube-on-cube oriented BaTiO 3 . Heating for the same duration and temperature in a reducing gas atmosphere resulted in the formation of polycrystalline BaTiO 3 with no preferred crystallographic orientation. The dependence on the gas atmosphere indicates that it may be possible to tune the annealing time, temperature, and atmosphere to produce a single crystalline BTO on STO by SPE or produce a desired distribution of orientations.

36 MATERIALS SCIENCE↗

Growth far from equilibrium: Examples from III-V semiconductors

The development of new applications has driven the field of materials design and synthesis to investigate materials that are not thermodynamically stable phases. Materials which are not thermodynamically stable can be synthesized and used in many applications. These materials are kinetically stabilized during use. The formation of such metastable materials requires both an understanding of the associated thermochemistry and the key surface transport processes present during growth. Phase separation is most easily accomplished at the growth surface during synthesis where mass transport is most rapid. These surface transport processes are sensitive to the surface stoichiometry, reconstruction, and chemistry as well as the growth temperature. The formation of new metastable semiconducting alloys with compositions deep within a compositional miscibility gap serves as model systems for the understanding of the surface chemical and physical processes controlling their formation. The GaAs{sub 1−y}Bi{sub y} system is used here to elucidate the role of surface chemistry in the formation of a homogeneous metastable composition during the chemical vapor deposition of the alloy system.

36 MATERIALS SCIENCE↗

Optimizing AlF{sub 3} atomic layer deposition using trimethylaluminum and TaF{sub 5}: Application to high voltage Li-ion battery cathodes

Atomic layer deposition (ALD) of conformal AlF{sub 3} coatings onto both flat silicon substrates and high-voltage LiNi{sub 0.5}Mn{sub 0.3}Co{sub 0.2}O{sub 2} (NMC) Li-ion battery cathode powders was investigated using a Al(CH{sub 3}){sub 3}/TaF{sub 5} precursor combination. This optimized approach employs easily handled ALD precursors, while also obviating the use of highly toxic HF(g). In studies conducted on planar Si wafers, the film's growth mode was dictated by a competition between the desorption and decomposition of Ta reaction byproducts. At T ≥ 200 °C, a rapid decomposition of the Ta reaction byproducts to TaC led to continuous deposition and high concentrations of TaC in the films. A self-limited ALD growth mode was found to occur when the deposition temperature was reduced to 125 °C, and the TaF{sub 5} exposures were followed by an extended purge. The lower temperature process suppressed conversion of TaF{sub x}(CH{sub 3}){sub 5−x} to nonvolatile TaC, and the long purges enabled nearly complete TaF{sub x}(CH{sub 3}){sub 5−x} desorption, leaving behind the AlF{sub 3} thin films. NMC cathode powders were coated using these optimized conditions, and coin cells employing these coated cathode particles exhibited significant improvements in charge capacity fade at high discharge rates.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Increased bismuth concentration in MBE GaAs{sub 1−x}Bi{sub x} films by oscillating III/V flux ratio during growth

The authors have examined bismuth concentration profiles in GaAs{sub 1−x}Bi{sub x} films grown by molecular beam epitaxy using high angle annular dark field imaging (Z-contrast imaging) in an aberration-corrected scanning transmission electron microscope in conjunction with x-ray diffraction. Samples were grown with a gradient in each of the component fluxes, and therefore, the III/V ratio across the substrate. Rotating the sample during growth exposed the growth surface to an oscillating III/V flux ratio. Sinusoidal [Bi] profiles resulted in the growth direction, the wavelength and number of which were consistent with the growth rate and the rate of substrate rotation. However, the magnitude of [Bi] in the observed fluctuations was greater than the maximum [Bi] achieved using the same Bi flux and Ga/As flux ratios in steady-state conditions on a stationary substrate, suggesting that varying the III/V flux ratio during growth promotes the incorporation of Bi in GaAs{sub 1−x}Bi{sub x} films. A proposed qualitative model for how this enhancement might occur hypothesizes a critical role for alternating growth and shrinkage of Ga-Bi predroplet clusters on the surface as the growing material is rotated through Ga-rich and As-rich flux compositions.