Search NASA⌕ Search

Engineering topics

Fifield, Leonard S.

Publications and source records attributed to Fifield, Leonard S..

At least 73 records · Page 4

Application of Principal Component Analysis for the Monitoring of the Aging Process of Nuclear Electrical Cable Insulation

To ensure the safe operation of nuclear power plants (NPPs), it is critical to understand how NPP electrical cable insulation will degrade under different service environments. In this study, various nondestructive examination methods were selected to evaluate degradation of electrical cable insulation after aging. Elongation at break, indenter modulus, relaxation constant, mass change, total color difference, and carbonyl index were collected stepwise on cross-linked polyethylene (XLPE) cable insulations after predetermined exposure intervals. Three different insulation aging scenarios were investigated: 1) simultaneous irradiation and heating at 150°C, 2) heating at 150°C followed by corresponding times of irradiation at ambient temperature, and 3) irradiation at ambient temperature followed by heating at 150°C for the same duration. A constant dose rate of 300 Gy/hr was selected with a total gamma irradiation absorbed dose up to 320 kGy. To gain insight into the long-term performance of NPP electrical cable insulation, principal component analysis (PCA), a data-driven approach, was utilized to identify key indicators of cable insulation degradation. By reducing the dimensionality of the data while retaining degradation information, PCA was used to highlight the changes in the measured properties under gamma irradiation according to total absorbed dose and the different aging scenarios.

Li, Donghui↗

Detection of diffusion limited oxidation in thermally aged ethylene propylene rubber cable insulation material

The lifetime prediction of electrical cable insulation in nuclear power plants (NPPs) is primarily based on accelerated aging. Polymeric insulation exposed to accelerated aging at high temperatures may demonstrate diffusion limited oxidation (DLO) where oxygen within the material is consumed faster than can be supplied by diffusion from the surrounding air. This situation leads to equilibrium oxidation at the exposed surfaces and limited oxidation away from the surfaces. Therefore, DLO results in a heterogeneously aged material which can lead to underestimation of lifetime for in-service cable insulation. In this study, the presence of inhomogeneous aging caused by DLO was evaluated on cross-sectioned cable insulation specimens made of ethylene propylene rubber (EPR). The studies were performed on thermally aged specimens (165 °C, 1 day and 165 °C, 16 days) using local measurement techniques including nanoindentation, micro-Fourier transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM) - energy dispersive spectroscopy (EDS). All the results indicate some degree of heterogenous aging, with 165 °C, 16 days, aging demonstrating highest degree of oxidative degradation on the inside edges presumably caused due to copper catalyzed oxidation.

Pallaka, Madhusudhan Reddy↗

Evaluation of Oxygen Consumption as a Sensitive Measure of Electrical Cable Polymer Insulation Degradation

Polymers used as dielectric materials in nuclear grade electrical cables, such as cross-linked polyethylene (XLPE) and ethylene-propylene rubber (EPR), are long-lived and durable. Estimating the decades-long useful service life of polymers experimentally in a feasible timeframe of weeks or months requires greatly accelerated aging in the laboratory at elevated temperatures and/or gamma dose rates. Many limitations of accelerated aging, such as due to artefacts of the process including diffusion limited oxidation and dose rate effects, have been identified that can make accurate lifetime prediction at service conditions challenging. This can be due to differences in degradation mechanisms between rapid and extended aging or to the presence of induction periods during which early aging is undetectable using common metrics of polymer insulation characterization such as tensile elongation at break. Conceptually, an ideal measure of aging would track clearly and predictably with material changes throughout the lifecycle of the evolving material state from early aging through end of useful life. With such a metric accelerated aging could be performed at much milder conditions, conditions closer to those found in long term service, and end of life calculated from the early data. Oxygen consumption has previously been proposed as a sensitive measure of insulation polymer oxidation that might meet such desirable characteristics. In this work, nuclear cable insulation samples of the two most common types, XLPE and EPR, from two of the most sourced manufacturers, RSCC and The Okonite Company, were subjected to gamma irradiation at dose rates of 100, 200, and 300 Gy/hr for up to 42 days at 26°C. The aged samples were used to evaluate oxygen consumption as a sensitive measure of aging for these materials and these conditions. For comparison and validation, the aged samples were also characterized using the more conventional tests of mass change, density, carbonyl index, and yellowness index. For both materials, oxygen consumption during irradiation was found to track consistently with applied dose—oxygen consumption rate was linear with time. Mass change and carbonyl index were also clearly proportional to exposure dose. Yellowness index, a surface sensitive measure, was observed to increase linearly with dose at low exposure levels before plateauing. Sample density was not observed to change under the conditions explored. Oxygen consumption was found to be a particularly sensitive metric to measure the degradation of polymeric cable insulation exposed to radiation. Oxygen consumption was compared to Arrhenius and time-temperature-superposition methods for activation energy calculation using literature date and found to be a useful and viable alternative for lifetime prediction. The techniques developed in this work are anticipated to be valuable in the estimation of insulation aging rates under mild conditions approaching service conditions. Direction comparison of useful life prediction by oxygen consumption with prediction via Arrhenius methodology for thermal aging and existing methods for radiation and combined thermal/radiation aging would serve to further validate this promising approach and refine our understanding of material-specific aging rates.

36 MATERIALS SCIENCE↗

Nondestructive Evaluation (NDE) of Cable Moisture Exposure using Frequency Domain Reflectometry (FDR)

This Pacific Northwest National Laboratory (PNNL) milestone report assesses the capability of frequency domain reflectometry (FDR) to determine electrical cable submergence using PNNL’s Accelerated and Real-Time Environmental Nodal Assessment (ARENA) cable/motor test bed. This work includes a review of relevant literature as well as experimental tests. Nuclear power facilities have experienced various electrical cable failures related to water exposure. The current industry response involves actions to de-water cable vaults, manholes, and other cable locations. These efforts require considerable expenditure of resources, which makes it desirable for the industry to have information on cable condition and history regarding their submergence and water exposure (Mantey 2012). Two tests that are gaining favor within the nuclear industry are time-domain reflectometry (TDR) and FDR. These are low-voltage nondestructive tests that can be applied at a cable end. Testing from the cable end is important because local inspection along the cable length is very difficult due to cables being routed within trays, conduits, underground, and through walls. Both TDR and FDR techniques have been shown to locate cable insulation damage due to thermal, radiation, and mechanical damage. FDR measurements are also more sensitive than TDR to temperature changes, low-bend radius bends, and cable contact with various materials, including conductive materials like steel and water. This work evaluates the feasibility to extend FDR testing to characterizing whether an electrical cable is submerged or not and where it may be submerged using PNNL’s ARENA cable/motor test bed.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Direct comparison of gamma, electron beam and X-ray irradiation doses on characteristics of low-density polyethylene, polypropylene homopolymer, polyolefin elastomer and chlorobutyl rubber medical device polymers

There is a growing need for increased efficiency in the sterilization of single use medical devices and other products that contain polymer components. Gamma radiation is widely used for devices suited for radiation sterilization; however, safety, throughput and cobalt-60 source availability are challenging the prospect of relying on gamma radiation to meet the anticipated needs of the industry. Use of electron beam (e-beam) and X-rays as alternatives to gamma for radiation sterilization have been hampered in part by a concern that these modalities may adversely affect polymer integrity and performance relative to the gamma method, for which the industry has had much more experience. To address this concern, the effects of sterilization-relevant doses of ebeam, X-ray and gamma radiation were directly compared using common medical device polymers found in two prototypical commercial devices currently sterilized using cobalt-60 gamma irradiation. The Becton, Dickinson and Company (BD) Vacutainer™ Plus tube contains low-density polyethylene and chlorobutyl rubber components, while the BD Vacutainer™ Push Button Blood Collection Set contains polypropylene homopolymer and polyolefin elastomer components. Injection-molded samples prepared from the polymers used in these products were exposed to target doses of 15, 35, 50 and 80 kGy using gamma, e-beam and X-ray radiation. Changes in coloration, tensile properties and hardness were measured for each condition, and the effects of e-beam and X-ray irradiation compared with the effects of gamma irradiation on these properties. Both e-beam and X-ray appear as viable alternatives to gamma irradiation for sterilization of the polymers tested.

sterilization, gamma, X-ray, electron beam, radiat↗

Principal Component Analysis of Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

In nuclear power plants (NPPs), the aging of electrical cable insulation occurs due to elevated temperature, ionizing radiation, and other environmental factors. To ensure the safe and efficient operation of NPPs, determination of key indicators of cable aging is critical to predict the remaining useful lifetime of electrical cable insulation. In this work, the effects of simultaneous and sequential thermal and gamma radiation on the aging of cross-linked polyethylene (XLPE) electrical cable insulation are investigated. The chemical changes of the insulation were monitored non-destructively through the use of Fourier transform infrared (FTIR) spectroscopy. The FTIR spectra were measured stepwise after predetermined exposure intervals, with a total irradiation dose up to 320 kGy at a dose rate of 300 Gy/hr in two exposure scenarios; simultaneously aged samples were heated at 150 °C during irradiation, while sequentially aged samples were heated at 150 °C for designated durations followed by corresponding times of irradiation at ambient temperature. A data-driven approach using principal component analysis (PCA) was developed to highlight changes in the carbonyl region of the infrared spectra of the aged samples due to oxidation and to differentiate oxidation rates under the simultaneous and sequential exposure conditions. Findings indicate that the sequential aging scenario may be more conservative than the simultaneous aging scenario for XLPE electrical cable insulation.

Li, Donghui↗

Monitoring Degradation of Nuclear Cable Insulation Subjected To Sequential and Simultaneous Thermal and Radiation Aging

Predicting useful remaining life of cables in nuclear power plants is a topic of growing interest as plant continue to age. A typical electrical cable consists of polymeric materials, such as the cable jacket and insulation, which are susceptible to degradation due to exposure to both elevated temperatures and gamma irradiation over decades of service. In this work two insulation materials, crosslinked polyethylene (XLPE) and ethylene propylene diene (EPDM) elastomer, were characterized to quantify aging using total color difference and indenter modulus. Since the effects of thermal and gamma radiation are not additive but coupled, the effects of different aging scenarios including sequential and simultaneous aging were also evaluated. In the case of sequential aging, two aging scenarios were explored where the order in which thermal and gamma radiation received were altered. Total color difference of XLPE showed that sequentially aged insulation specimens, which received radiation first, degraded slightly more at maximum exposure than specimens which received thermal first. Similarly, in the case of EPDM, the extent of degradation evaluated using total color difference was found to be most severe in the case of sequentially aged insulation specimens which received radiation first. Indenter modulus was found to be insensitive to aging for XLPE but trended for EPDM. The largest variations were observed for the sequentially aged insulation specimens which received radiation first, similar to what was observed for total color difference.

Pallaka, Madhusudhan Reddy↗

PNNL ARENA Cable Motor Test Bed Update

A major focus of the Light Water Reactor Sustainability (LWRS) Cable Nondestructive Examination (NDE) 2021 research is to acquire new equipment and integrate it with existing NDE instruments for a cable motor test bed which has been dubbed the Accelerated and Real Time Experimental Nodal Analysis or “ARENA”. All the primary components have been received and are being staged in the 2410 Stevens building on PNNL’s Richland campus. Building modifications to support a plug-in 480VAC receptacle have been completed and details of the system operating procedure (SOP) are in review. The approved SOP is required before the system is energized but is expected before July 2021. The ARENA system will support planned cable tests for 2021 and beyond that cannot conveniently be performed with on-site installations of cable test equipment including: (1) NDE Tests including Frequency Domain Reflectometry (FDR), Time Domain Reflectometry (TDR), Tan Delta (TD) Impedance measurements, Low Frequency Dielectric Spectroscopy (DS) measurements, standard multi-meter resistance checks, withstand tests and other bulk and distributed tests from the instrument panel with and without motors connected. (2) Online energized live wire tests using partial discharge instruments and LIVE-WIRE spread-spectrum TDR instruments. (3) Cable tests with partially submerged cable segments (including ability to submerge live cable segments). (4) Cable tests with partially or completely thermally aged segments (including ability to expose energized cable segments to thermal aging and use online monitoring instruments to monitor cable performance. (5) Ability to introduce low resistance simulations of connector or splice faults to off-line and on-line instrument setups.

42 ENGINEERING↗

Aging mechanisms of filled cross-linked polyethylene (XLPE) cable insulation material exposed to simultaneous thermal and gamma radiation

Thermal and simultaneous thermal and gamma radiation aging experiments were conducted on an industry grade cross-linked polyethylene (XLPE) cable insulation material, which is a composite material with XLPE as polymer matrix and various additives and fillers. Reverse engineering was conducted to identify and quantify the material composition given that this information was not revealed by the cable manufacture. Samples were then aged at temperatures of 60, 90, and 115 °C, exposed to gamma radiation for total doses of 0 to 324 kGy, and at dose rates of 0 to 540 Gy/h. Aging mechanisms were studied using various materials characterization techniques including pyrolysis gas chromatography mass spectrometry (Py-GCMS), differential scanning calorimetry (DSC), nuclear magnetic resonance spectroscopy (NMR), and gel-fraction tests. Results show that the flame-retardant components were decomposed into smaller molecules when the material was exposed to gamma radiation, while no changes were observed when the samples were aged thermally without gamma radiation. With exposure to gamma radiation, the crystalline phase of the XLPE were damaged by gamma radiation introducing defects in the crystals, resulting in smaller and less perfect crystals. The dominance of chain scission or chain reformation process largely depends on the chain mobility, which is decided by the aging temperature. Chain scission was seen to dominate when the material was exposed to gamma radiation at 60 °C. Chain cross-linking slightly dominated when the material was exposed to gamma radiation at 90 °C and became more dominant with exposure to gamma radiation at 115 °C. No significant change to the XLPE polymer matrix was observed when the samples were exposed to thermal aging without gamma radiation. Finally, antioxidant is more effective in protecting the XLPE polymer matrix under thermal aging, but less effective with sample exposure to gamma radiation.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Flexible Fabric-Based IDC Sensors for Conformal Curved Surface Applications

Interdigital capacitor (IDC) sensors are attractive in-situ sensors that can be used to measure permittivity variations in materials. Such sensors could be powerful enablers for cable insulation aging detection. Since insulation aging is correlated with a change in its material permittivity an IDC can measure that change via its measured capacitance. A new thin, flexible fabric-based IDC sensor is introduced for application on conformal curved surfaces such as an electrical cable surface. A multielectrode IDC and its backplane were fabricated using conductive copper polyester taffeta fabrics that were adhesively bonded to nonconductive polyester fabric. The sensor because of its soft flexible structure eliminates the problem of sensor conductor damage which is common for printed circuit board (PCB) type sensors when conformed to the surface of a cable. It also significantly reduces the airgap between the electrodes and the surface that they must contact in order to measure the capacitance. Airgap reduction and consistency are important in order to accurately predict permittivity variations in cable insulation material due to aging. Both PCB-based sensors and the new fabric-based sensors were built and tested on unaged cables and cables that underwent accelerated aging. Results demonstrate the proposed advantages of the novel fabric-based IDC sensor.

interdigital capacitor sensor, IDC, NDE, PCB senso↗

Comparative Analysis of Capacitive Sensors with Different Geometrical layouts for Cable Insulation Degradation Detection

This paper presents a comparative analysis between an Interdigital Capacitor (IDC) sensor and a Serpentine Capacitive (SRC) sensor. The effects of electrode layouts on sensor performance are studied by means of finite element simulation where the geometrical dimensions (except electrode length) and material characteristics of both sensors are identical. Conformal IDC and SRC sensors with equal sensor area are modeled on a cable surface. The simulation results show a tradeoff between IDC and SRC sensors in terms of sensitivity and penetration depth. The SRC sensor shows 13.3% increase in sensitivity and 16.8% increase in capacitance compared to the IDC sensor, though the electric field penetration depth of the SRC sensor is 18.8% lower than the IDC sensor. In addition, the effects of change in electrode width, inter-electrode gap, and number of electrodes on SRC and IDC sensor comparative performance are evaluated.

Interdigital Capacitance, Serpentive Capacitive Se↗

Interdigital Capacitance Sensor for Cable Insulation Test and Monitoring

A substantial body of work suggests feasibility to measure cable jacket and insulation conditions using various forms of interdigital capacitance (IDC) sensors. The sensors can either be used to manually test local cable conditions or as permanently installed sensors. Eligible cables subject to these measurements do not include shielded cables but the set of candidate cables is expanded from only unjacketed cables by the ability to assess insulation condition through the jacket. Dual gap IDC sensors are confirmed to be able to sense the insulation condition beneath a polymer jacket and, moreover, the IDC is the only known way to assess the insulation condition through the jacket. PNNL has filed a patent for this approach and is exploring commercial partnerships to exploit IDC technology for actionable field measurements.

NDE, cable, IDC, capacitance, permittivity, insula↗

Sequential versus Simultaneous Aging of EPDM Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

Electrical cables are integral to power, control, and instrumentation systems within nuclear power plants (NPPs). Exposure of cable systems within nuclear containment to elevated temperatures and gamma radiation during decades-long operation of NPPs can lead to degradation of cable polymeric insulation. Prediction of nuclear cable insulation degradation is complicated as thermal and radiation stress are not additive. In this work, we explore the relative effects of simultaneous and sequential thermal and gamma irradiation on the aging of ethylene-propylene-diene (EPDM) elastomer insulation to better understand realistic scenarios of cable insulation degradation. Cable insulation samples of EPDM were subjected to up to 320 kGy of gamma radiation at a dose rate of 300 Gy/hr in two heating scenarios: (1) simultaneously aged samples were heated at 150°C during irradiation and (2) sequentially aged samples were heated at 150°C for designated durations followed by corresponding periods of irradiation at ambient temperature. The mass, tensile elongation at break, and carbonyl index were assessed to quantify aging of the polymers. The simultaneous aging scenario was found to the more severe of the two for EPDM insulation degradation.

ethylene-propylene-diene elastomer, EPDM, nuclear ↗

Malleable Thermosets (Vitrimers) from CO 2 and Plants

Fiber-reinforced composite materials are increasingly used to replace heavy metal components in transportation applications for lightweighting purposes. Polymer matrix materials used in automotive parts, such as epoxies, nylons, and polypropylenes, are almost all produced from fossil fuels. Higher performance thermoset composites are generally not repairable and lower-cost thermoplastic composites do not have enough performance to replace steel. Vitrimers are a new class of polymer materials with long shelf life, low waste in production, ease of processing, and repairability that have the potential to break through the high-cost thermoset/low-performance thermoplastic barrier to vehicle light-weighting. Vitrimers also exhibit easier chemical recyclability than conventional thermosets with reversible chemical crosslinking that enables reprocessing of scrap from production and end of life components. Vitrimers are a new class of engineered plastics that are weldable, repairable and recyclable like thermoplastics but have high mechanical properties like thermosets. Bio-based vitrimers have only recently been reported in the academic and patent literature. These materials represent an unusual opportunity to meet both VTO light-weighting targets for low-density, high performance materials and BETO sustainability targets for value-added high-volume applications of bio-fuel byproducts. Also, PNNL researchers have previously demonstrated a process to convert CO 2 into potential vitrimer precursors. Washington State University (WSU) success in demonstration of bio-based vitrimers and recent steps toward commercialization of petroleum-based vitrimers support the opportunity for PNNL success in development of sustainable vitrimer materials for recyclable, high-performance fiber-reinforced composites for the transportation sectors.

36 MATERIALS SCIENCE↗

Sequential versus Simultaneous Aging of XLPE Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

Electrical cables constitute a critical component of nuclear power generation. The aging behavior of electrical cable insulation under combined exposure to thermal and radiation stress is not additive, complicating lifetime prediction of cable performance based on sequential accelerated aging. In this work we explore the relative effects of simultaneous and sequential thermal and gamma radiation aging on cross-linked polyethylene (XLPE), which is commonly found in commercial nuclear power plants in the United States. Samples of XLPE were subjected to up to 320 kGy of gamma irradiation at a dose rate of 300 Gy/hr in two heating scenarios. In the first, simultaneously-aged samples were heated at 150°C during irradiation. In the second, sequentially aged samples were heated at 150°C for designated durations followed by corresponding periods of irradiation without heating. The mass, total color difference, and density were characterized to quantify aging of the insulation polymer. Sequential aging is hypothesized to be more damaging to XLPE insulation due to an increased trend in mass gain, total color difference, and density.

Cross-linked polyethylene, XLPE, nuclear cable, ac↗

Assessment of EPRI’s Tan Delta Approach to Manage Cables in Submerged Environments: Statistical Review of EPRI Data

Research conducted by the Electric Power Research Institute (EPRI) and other research institutions have concluded that water-trees are one of the leading degradation mechanisms that contribute to the loss of dielectric insulation strength in medium-voltage cable insulating materials in wet or submerged environments. The electrochemical reactions are caused by the combined effect of water presence and relatively high electrical stress. Records of cable failures provided by the licensees in response to Generic Letter (GL) 2007-01 (NRC 2007) have called into question the reliability of medium voltage cables in wetted or submerged environments. EPRI’s dissipation factor or Tan Delta testing guidelines and acceptance criteria have been adopted by most nuclear power plant operators as the primary tool for condition monitoring of medium voltage cables in wet or submerged environments. EPRI has been collecting member data since late 2009 to analyze and provide feedback to members, validate the EPRI-developed acceptance criteria guidelines, support analysis of test results, recommend appropriate actions for the "action required" category, and gather candidate cables for EPRI-sponsored forensic research on causes for insulation degradation. EPRI has collected data from 37 nuclear sites, which represent 44 operating units. The test results have been organized by insulation type, such as cross-linked polyethylene (XLPE); butyl rubber; black, pink, and brown ethylene-propylene rubber (EPR); and compact insulation (black and pink EPR)1. The data have been analyzed, and follow-up information was obtained from members for “action required” test results. EPRI has also performed correlations between Tan Delta tests and the information gathered under the EPRI forensic research on medium-voltage cables. In addition, EPRI has developed guidance by cable insulation type on how to systematically analyze Tan Delta test results. The analysis described here reviewed the two primary EPRI reports (EPRI 3002000557 and EPRI 3002005321) as well as two precedent EPRI reports (EPRI 1028262 and EPRI 1021070) that were cited in the primary reports. The principal results and conclusions from the project analyses are provided.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗