Simulation and Experimental Results of Interdigital Capacitor (IDC) Sensors to Monitor Insulation Degradation of Cables

The efficacy of using interdigital capacitor (IDC) sensors to monitor cable insulation aging was studied through electromagnetic simulations and experimental measurements. Simulation results on both planar and conformal dielectric materials indicated that IDCs on thin substrates and with conducting backplanes provide superior performance in terms of higher capacitance. An airgap study showed that even a very small airgap between the sensor and the cable’s insulation results in significant reduction in capacitance; therefore, airgaps should be minimized. Finally, cables that underwent accelerated aging exposure in an oven were tested using fabricated IDC sensors. Measurement results showed a 12.5% increase in capacitance when the IDC was pressed against the insulation versus a 91.3% increase in capacitance when the IDC was pressed against the jackets of the cables for cable specimens ranging from unaged to aged 35 days.

Cable NDE, Interdigital Capacitance↗

Transitioning from Cobalt-60 to X-Ray or E-Beam for Medical Sterilization: Filling Data and Education Gaps

The Office of Radiological Security (ORS) within the U.S. DOE’s National Nuclear Security Administration (NNSA) is charged to “work with government, law enforcement, and businesses across the globe to protect radioactive sources used for medical, research, and commercial purposes; remove and dispose of disused radioactive sources; and reduce the global reliance on high activity radioactive sources through the promotion of viable non-radioisotopic alternative technologies.” In this effort, the NNSA/ORS, along with the Office of Defense Nuclear Nonproliferation R&D, has been working with government and private entities that utilize gamma-ray irradiators in areas that include blood irradiation, radiotherapy, biology research, well logging, and radiation processing to consider alternative technologies that do not depend upon radioactive materials. In the medical device industry, nearly 50% of products are sterilized with ethylene oxide, 40.5% with cobalt-60 gamma-rays, 4.5% with electron-beam (e-beam), and <1% with X-ray.(1,2) The cobalt-60 irradiation facilities use an estimated 150 MCi of isotope to sterilize approximately 200 million cubic feet of product annually.(3) Due to growing safety regulations governing cobalt-60 use, continued advancements in e-beam and X-ray accelerator technology, and the greater irradiation durations and costs for cobalt-60 irradiation compared to e-beam and X-ray, switching to these non-radionuclide modalities is increasingly economically competitive. However, this breakdown of 40.5% cobalt-60 and 5.5% accelerator for product sterilization illustrates the difficulty that market forces and industry players have had in overcoming barriers in transitioning to non-nuclide alternatives. Besides those associated with construction of new e-beam and X-ray facilities, significant financial and regulatory obstacles are also associated with the irradiation and comprehensive testing of product constituent polymers and elastomers. The standards associated with product material performance testing are the Association for the Advancement of Medical Instrumentation (AAMI) Technical Information Report 17 (TIR 17), and its referenced American Society for Testing and Materials (ASTM) polymer testing standards. In the study now underway, and the subject of this article, the NNSA/ORS provided R&D funding to the Pacific Northwest National Laboratory (PNNL) in partnership with university researchers, leading medical product manufacturers, accelerator manufacturers, and contract sterilizers. The resulting Team Nablo (in memory of Sam Nablo) includes individuals representing PNNL, Becton Dickinson (BD), Johnson & Johnson, Stryker, Texas A&M University (TAMU), Steri-Tek, Mevex, Ion Beam Applications (IBA), and Sterigenics. The goals of this study are to 1) Identify specific polymer and/or elastomer-based medical products that are currently sterilized with gamma-rays, and for which there are data gaps and would be of greatest industry impact, 2) Work with relevant ASTM subcommittees for guidance and for potential standard revision, 3) Work with an appropriate Food & Drug Administration (FDA) office for potential collaboration on a guidance document for device manufacturers, 4) Measure the physical effects that product materials exhibit when they are given sterilization-level radiation doses from cobalt-60, e-beam or X-ray, and determine whether these effects would preclude the use of e-beam or X-ray for sterilization, 5) Communicate the resulting scientific datasets and findings via industry conferences, peer-reviewed journals, and relevant trade magazines, and 6) Post the resulting datasets on a publicly accessible website, which can be built on in future years. The end objective is to identify technical barriers preventing the adoption of X-ray and e-beam technologies, and share the results to encourage X-ray and e-beam adoption where feasible.

sterilization, alternate technologies, gamma, X-ra↗

INTER-DIGITAL CAPACITIVE SENSOR FOR EVALUATING CABLE INSULATION THROUGH JACKET

Interdigital capacitive (IDC) sensors have previously been used to measure cable-age/damage indicative dielectric properties of cable insulation when placed in direct contact with the insulation. Often cable insulation is covered by a polymer jacket precluding direct contact with the insulation. As part of a continuing program to develop and evaluate nondestructive examination methods that may be applied to cable condition assessment, an IDC to measure the effect of cable polymer dielectric change through a covering jacket has been developed. The IDC consists of two fork-like electrodes facing each other with the fork tines interspersed and separated by a small gap. On one electrode, the gap is 5 mm while on the other, the gap is 2 mm. Electric field depth-of-field penetrations are similar to the electrode gaps. The electrodes are printed on a flexible substrate that can be conformed to the outside jacketed surface of a cylindrical cable, with tines parallel to the cable axis. The electrodes are connected to a broad frequency-spectral impedance meter that senses the capacitance between the narrowly gapped electrode tines. This capacitance is known to vary as a function of the permittivity of any material in close proximity to the electrodes. For jacketed cable systems, the IDC response is dominated by the jacket but, by analyzing measurements from IDC sensors with different depths-of-field penetration into the cable under test, the influence of the cable jacket material (primarily influenced by the shallow-depth-of field IDC) can be separated from the deeper-depth-of-field IDC sensing the combined effects of both jacket and underlying insulation. No other NDE method is known that is capable of sensing insulation dielectric properties through an overlying jacket.

Cable NDE, Interdigital Capacitance, Insulation Pe↗

Understanding H 2 Evolution from the Decomposition of Dibutylmagnesium Isomers Using in-Situ X-ray Diffraction Coupled with Mass Spectroscopy

Alkylmagnesium compounds such as dibutylmagnesium can be effectively decomposed to produce MgH 2 and Mg metal for applications such as hydrogen storage, single site catalysis, and powder metallurgy or as the last step of comprehensive processes to produce Mg metal from magnesium salts. For these applications it is important to understand the decomposition reactions of dibutylmagnesium and to quantify its decomposition products. In this study, to avoid interference from air and moisture, an in situ X-ray diffraction (XRD) coupled with mass spectroscopy system was developed to investigate phase changes and released products in real time for the decomposition reactions. For the dibutylmagnesium (MgBu 2 n-n ) with two n -butyl groups, transformation to MgH 2 occurred at 250 °C and transformation to Mg metal occurred near 384 °C. The diffraction data suggest the possibility of an intermediate phase with one butyl group formed during the transformation to MgH 2 . Decomposition of MgH 2 under vacuum is accelerated by eliminating H 2 from the system as it is evolved. The sec- butyl n -butylmagnesium (MgBu 2 s-n ) was observed to decompose at as low as 50 °C, indicating the increased lability of the sec -butyl group in the dibutylmagnesium isomer. Thermogravimetric analysis (TGA) for the MgBu 2 n-n and MgBu 2 s-n loaded in air-free conditions recorded higher than 98% conversion to MgH 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Inter-digital capacitive sensor for evaluating cable jacket and insulation aging

An inter-digital capacitive (TDC) sensor has previously been used to measure dielectric properties of cable insulation polymer material when placed in direct contact with the insulation. Often cable insulation is covered by a polymer jacket. The dielectric properties of many cable jacket and insulation polymers are known to change due to thermal and radiation exposure-related damage. These dielectric properties frequently track with other measures of cable aging, such as tensile elongation-at-break and indenter modulus that have been broadly established as cable insulation polymer assessment methods. The external jacket of a cable is likely to have a different permittivity from the underlying insulation, and frequently the jacket material exhibits more severe damage than the insulation material due to environmental exposure. Because the jacket serves primarily to guard the cable during installation, as long as the underlying insulation condition is acceptable, the jacket condition is relatively unimportant in service. As part of a continuing program to develop and evaluate nondestructive examination methods that may be applied to cable condition assessment, a set of tools has been developed including (1) a parallel-plate sensor to directly measure the permittivity spectrum of flat sheet material and (2) an TDC and fixture to measure the effect of cable polymer dielectric property change on the sensor response. The TDC consists of two fork-like electrodes facing each other with the fork tines interspersed and separated by a small gap. The electrodes are printed on one side of a flexible substrate that can be conformed to the surface of a cylindrical cable, with tines parallel to the cable axis. The electrodes are connected to a broad-frequency-spectral impedance meter that senses the capacitance between the narrowly gapped electrode tines. This capacitance is known to vary as a function of the permittivity of any material in close proximity to the electrodes. By finite element modeling (FEM) and experimentation, this study investigates the effect of tine spacing and other design parameters associated with the TDC on the voltage (potential) distribution and electric field depth of penetration. The TDC measurement of an unshielded ethylene-propylene rubber (EPR)-insulated cable is shown to track with the degree of aging and quantities obtained by established methods. For jacketed cable systems, the TDC response is dominated by the jacket but, by analyzing measurements from TDC sensors with different depths-of-field penetration into the cable under test, the influence of the chlorinated polyethylene (CPE) cable jacket material degradation can be separated from an assessment of the cable insulation thereby enabling assessment of the insulation beneath/through the jacket.

Cable NDE, Interdigital Capacitance, Cable test↗

Highly Selective Supported Graphene Oxide Membranes for Water-Ethanol Separation

Polyethersulfone (PES)-supported graphene oxide (GO) membrane has been developed by a simple casting approach. This stable membrane is applied for ethanol/water separation at different temperatures. The 5.0 µm thick GO film coated on PES membrane showed a long-term stability over a testing period of one month and excellent water/ethanol selectivity at elevated temperatures. The water/ethanol selectivity is dependent on the ethanol weight percentage in the water/ethanol feed mixtures and the operating temperature. The water/ethanol selectivity was enhanced with an increase of ethanol weight percentage in water/ethanol mixtures and from below 100 at RT to close to 874 at 90 ºC for 90% ethanol/10% water mixture. Molecular simulations of water-ethanol mixtures in graphene bilayers that are considered to play a key role in transport revealed that molecular transport is negligible for layer spacing below 1 nm. The differences in the diffusion of ethanol and water in the bilayer are not consistent with the large selectivity value experimentally observed. The entry of water and ethanol into the interlayer space may be the crucial step controlling the selectivity.

36 MATERIALS SCIENCE↗

Dielectric and Mechanical Behavior of Thermally Aged EPR/CPE Cable Materials

Power and instrumentation cables play a crucial role in the safe operation of Nuclear Power Plants (NPPs). Thermal and other stressors present in the reactor environment cause the cable materials to degrade. In this work, dielectric and mechanical properties of cable insulation and jacket materials are studied as they are thermally aged, supporting development of non-destructive evaluation sensors for monitoring cable aging. Materials selected for this study are found in certain types of single-core unshielded power cables. These utilize ethylene propylene rubber (EPR)-based insulation material and chlorinated polyethylene (CPE)-based jacket material. Flat mats of these materials were obtained from the cable manufacturer and thermally aged at 140 °C in an air-circulating oven. Elongation-at-break was measured on tensile specimens stamped from the aged mats, and dielectric properties were measured from 100 Hz to 100 kHz using a parallel plate capacitor and precision LCR meter. In the case of aged EPR-based materials, rapid decrease in elongation at break indicating end of useful life was accompanied by a significant increase in dissipation factor, D, measured at 100 kHz. Capacitive measurement of D shows promise, therefore, as a non-destructive indicator of corresponding mechanical property changes in thermally-aged EPR-based insulation materials.

cable aging, nuclear cables, material degradation,↗

Dielectric Response of Cross-Linked Polyethylene (XLPE) Cable Insulation Material to Radiation and Thermal Aging

This work seeks dielectric indicators of the aged state of cross-linked polyethylene (XLPE) that has been simultaneously irradiated and thermally aged. The XLPE samples studied here were of the same material formulation as XLPE insulation found in RSCC I46-0021 instrumentation cable, formed into tapes with dimensions approximately 20 × 0.7 × 100 mm 3 . Aging was conducted by suspending the samples from a rack within an oven and subsequently exposing oven and samples to gamma radiation. Samples were aged at 60, 90, and 115 °C, with gamma-radiation dose rates from 0 to 450 Gy/h with total received doses from 0 to 216 kGy. The dielectric spectra of these samples were measured over the frequency range 1 Hz to 1 MHz using custom electrodes and a Novocontrol dielectric spectrometer before dielectric breakdown strength was measured on the same samples. Dielectric loss tangent was observed to increase as a function of dose, dose rate and exposure time for XLPE samples exposed as described above. Dielectric loss tangent did not, however, show sensitivity to thermal aging for the range of temperatures studied. Dielectric breakdown strength initially increased as the material oxidized, then decreased for more extreme aging, due to chain scission. It is concluded that dielectric loss tangent is a promising indicator of XLPE aging due to gamma radiation exposure.

dielectric losses, dielectric breakdown, cable ins↗

Quantitative analysis of changes in antioxidant in crosslinked polyethylene (XLPE) cable insulation material exposed to heat and gamma radiation

Quantitative analysis of the antioxidant poly(1,2-dihydro-2,2,4-trimethylquinoline) (pTMQ) was conducted on pristine, thermally-aged, and gamma radiation-aged commercial cross-linked polyethylene-(XLPE-)based cable insulation material aged at temperatures 60, 90, and 115?°C, with gamma radiation exposure dose rates of 0, 120, 300, and 540?Gy/h for 15 days. The quantification of antioxidant was performed using pyrolysis gas chromatography-mass spectrometry (Py-GCMS). Oxidation induction time (OIT) was measured using differential scanning calorimetry (DSC) and correlation was made between the quantified depletion of antioxidant and measured OIT. It was observed that, in the case of isothermal aging, the quantity of antioxidant and OIT decreased with increasing gamma radiation dose. In the case of samples exposed to the same gamma radiation dose, the quantity of antioxidant and OIT were observed to decrease with increasing aging temperature. Depletion in the quantity of antioxidant relative to that in the pristine material ranged from 7 to 93% for differently aged samples. The measured decline in OIT ranged from 0 to 80%. Change in the quantity of antioxidant in the material was observed to follow the same trend as the change in OIT when the samples were aged under various conditions. The observations are explained in terms of the reaction between the antioxidant and free radicals created during exposure of the samples to thermal and gamma radiation.

Pyrolysis gas chromatography-mass spectroscopy, an↗

Initiation of Experimental Campaign to Address Knowledge Gaps Related to Simultaneous Thermal and Gamma Radiation Aging of Crosslinked Polyethylene and Ethylene-Propylene Rubber Cable Insulation

Key cable knowledge gaps identified in the Expanded Materials Degradation Assessment (EMDA) volume on Aging of Cables and Cable Systems (Volume 5) specifically relate to the combined effects of thermal and gamma irradiation stresses on cable insulation materials. These include dose rate effects (DRE), inverse temperature effects (ITE), and synergistic effects (S/E). Extent of radiation-induced polymer degradation is proportional to absorbed dose, but DRE describe the phenomenon in which degree of damage is based not only on total dose, but also on the dose rate experienced during dose accumulation. This can be particularly complicated in the presence of thermal stress as a material spends more time at elevated temperature to receive the same total dose at a lower dose rate. Rates of cable polymer degradation generally increases with temperature, but ITE describes the situation in which polymer material damage under irradiation is greater at lower temperatures than at higher temperatures. Finally, S/E describe the concept that the mechanism of polymer material degradation when exposed to thermal aging and radiation aging in succession may be different than when exposed to thermal and radiation aging concurrently. The experimental campaign at the Pacific Northwest National Laboratory (PNNL) described in this report seeks to address these knowledge gaps through investigation of the degradation of relevant cable insulation materials at select conditions using controlled temperatures, dose rates and total doses. Insulation materials considered were chosen to represent those most commonly found in U.S. nuclear power plants in terms of manufacturers and polymer systems. They include products from manufactures including The Rockbestos Company; The Okonite Company; Boston Insulated Wire & Cable Company; Kerite Company; Anaconda Company; Brand Rex, Inc.; and Samuel Moore Company. The products include the most ubiquitous cross-linked polyethylene (XLPE) and ethylene-propylene rubber (EPR) classes of insulation polymer. Circulating air ovens with remote temperature sensing and control are positioned within the gamma irradiation beam to enable controlled temperatures during radiation exposure. Dose rates are controlled through repeatable positioning of specimens at determined distances from the Cobalt-60 gamma source. Total absorbed doses for comparing temperature and dose rate effects are controlled by removing samples from exposure at pre-determined time points. The effects of gamma beam geometry, source decay and attenuation due to samples, ovens and racks are determined and controlled for using local point dosimetry. The temperature, dose and dose rates selected for the experimental campaign described in this report were determined following input from a range of stakeholders and intended to balance the constraints of the experimental capabilities, available material, project timeline and project funding with the value of the effort in narrowing EMDA-identified knowledge gaps. Results from this campaign are anticipated to reduce uncertainty in the understanding of cable material degradation behavior in nuclear power plant environments and thereby support cable aging management in long term operation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Dielectric Spectroscopy for Bulk Condition Assessment of Low Voltage Cable (Interim Report)

This Pacific Northwest National Laboratory milestone report describes progress to date on the investigation of nondestructive test methods focusing on bulk cable insulation testing using a dielectric spectroscopy (DS) approach. This report addresses relevant literature coupled with a discussion of the theory of DS measurements and work on modeling to appreciate the influence of damage/defect profile on the bulk total cable measurement.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Insight into Thermal Aging of Jacket-bonded Ethylene-propylene Rubber Cable Insulation

Electrical cables are integral to nuclear power plant operation and control during power generation, during planned outages, and during design basis events. Polymeric insulation and jacketing used in cable construction does age over time as a function of environmental stresses including heat, moisture, and radiation. Degradation of polymer mechanical properties can lead to breaks in the insulation and consequent electrical shorting. In this work we consider the thermal aging behavior of one of the two most common insulation polymer classes in nuclear power plants, ethylene-propylene rubber (EPR), both as an independent material and within a cable in which the EPR is bonded to a chlorinated polyethylene (CPE) jacket. Understanding the changes in these two materials with aging, both independently and in concert, will allow the establishment of aging lifetime curves and enable the development of effective non-destructive methods for tracking the condition of installed cables composed of similar material systems. Additional and more effective methods for monitoring the condition of installed cables are needed as a technical basis for continued safe use of aging cables in long term operation and to minimize operating costs for cable aging management through better informed retain/repair/replace decisions.

Light Water Reactors, electrical cables, aging, EP↗

Defect Length and Profile Influence on Frequency Domain Reflectometry

Degradation of the cable jacket, electrical insulation, and other cable components of installed cables within nuclear power plants (NPPs) is known to occur as a function of age, temperature, radiation, and other environmental factors. Although system tests verify cable function under normal loads, demonstration of some cable’s ability to perform under exceptional loads associated with design-basis events is essential to assuring plant integrity. The cable’s ability to perform safely over the initial 40 year planned and licensed life has generally been demonstrated and there have been very few age-related cable failures. With greater than 1000 km of power, control, instrumentation, and other cables typically found in an NPP, replacing all the cables would be a severe cost burden. Justification for life extension to 60 and 80 years requires a cable aging management program that includes condition monitoring to justify cable performance under normal operation as well as accident conditions. A variety of tests are available to assess various aspects of electrical and mechanical cable performance, but none are suitable for all cable configurations nor does any single test confirm all features of interest. One particularly promising test that is beginning to be used more and more by utilities is frequency domain reflectometry (FDR). FDR is a nondestructive electrical inspection technique used to detect and localize faults in power and communication system conductors along the length of a cable from a single connection point. FDR detects discontinuities in the electrical impedance that arise due to cable splices or similar changes along the path of the conductor pair. In addition, FDR has the potential to provide sensitivity to insulation degradation by detecting small changes in impedance between the cable conductors being examined. The technique is also sensitive to cable bends, the particular lay of the cable in tray, proximity to other cable, and other factors that bear consideration when interpreting the test results. This paper examines various influences on the FDR approach particularly using FEM modeling methods and focusing on defect length and defect profile.

Cable Inspection, Frequency Domain Reflectometry, ↗

State of Electrical Cable Aging in U.S. Nuclear Power Plants

Nuclear energy has supplied one fifth of the electricity generation in the United States for the last thirty years, but headwinds for continued contribution of nuclear to the US energy mix include the aging state of existing plants and the challenge of remaining cost competitive with energy alternative such as natural gas. As an integral component of the power, control and safety operations of a nuclear power plant, electrical cables are a significant factor in both long term and resource-efficient plant operation. The cost and practical challenge of wholesale replacement of the thousands of miles of cables in each reactor make effective management of the existing cable inventory increasingly important as the cables age in service. Total generation costs for US nuclear reactors have increased in the last decade, due in part to safety and security upgrades. Passive, long-lived structures, systems and components may be subject to aging-related degradation, necessitating increase frequency of inspection and repair/replace decisions. Costs associated with cable aging management in long-term operation can be reduced with effective cable condition monitoring technology and sufficient understanding of material aging behavior. Technical basis for confidence in cable status can reduce the frequency of cable system inspections and align cable replacement decisions with physical need. Knowledge of cable remaining useful life can allow longer term cable maintenance planning and fewer unplanned outages. As methods for relating measurable key indicators of aging with cable status develop, industry has begun to demonstrate how informed cable aging management can help to minimize costs necessary for safe, long-term operation.

light water reactors, electrical cables, nuclear p↗

Interdigital Capacitance Local Non-Destructive Examination of Nuclear Power Plant Cable for Aging Management Programs

This Pacific Northwest National Laboratory milestone report describes progress to date on the investigation of non-destructive test methods focusing on local cable insulation and jacket testing using an interdigital capacitance (IDC) approach. Earlier studies have assessed a number of non-destructive examination (NDE) methods for bulk, distributed, and local cable tests. A typical test strategy is to perform bulk assessments of the cable response using dielectric spectroscopy, Tan , or partial discharge followed by distributed tests like time domain reflectometry or frequency domain reflectometry to identify the most likely defect location followed by a local test that can include visual inspection, indenter modulus tests, or Fourier Transform Infrared Spectroscopy (FTIR) or Near Infrared Spectroscopy FTIR (FTNIR). If a cable is covered with an overlaying jacket, the jacket’s condition is likely to be more severely degraded than the underlying insulation. None of the above local test approaches can be used to evaluate insulation beneath a cable jacket. Since the jacket’s function is neither structural nor electrical, a degraded jacket may not have any significance regarding the cable’s performance or suitability for service. IDC measurements offer a promising alternative or complement to these local test approaches including the possibility to test insulation beneath an overlaying jacket.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Frequency Domain Reflectometry Modeling and Measurement for Nondestructive Evaluation of Nuclear Power Plant Cables

Cable insulation polymers are among the more susceptible materials to age-related degradation within a nuclear power plant. This is recognized by both regulators and utilities, so all plants have developed cable aging management programs to detect damage before critical component failure in compliance with regulatory guidelines. Although a wide range of tools are available to evaluate cables and cable systems, cable aging management programs vary in how condition monitoring and NDE is conducted as utilities search for the most reliable and cost-effective ways to assess cable system condition. Frequency domain reflectometry (FDR) is emerging as one valuable tool to locate and assess damaged portions of a cable system with minimal cost and only requires access in most cases to one of the cable terminal ends. This work examines a physics-based model of a cable system and relates it to FDR measurements for a better understanding of specific damage influences on defect detectability.

cable↗

Simultaneous Thermal and Gamma Radiation Aging of Electrical Cable Polymers

The polymers used for insulation in nuclear power plant electrical cables are susceptible to aging during long term operation. Elevated temperature is the primary contributor to changes in polymer structure that result loss of mechanical and electrical properties, but gamma radiation is also a significant source of degradation for polymers used within relevant plant locations. Despite many years of polymer degradation research, the combined effects of simultaneous exposure to thermal and radiation stress are not well understood. As nuclear operators contemplate and prepare for extended operations beyond initial license periods, a predictive understanding of exposure-based cable material degradation is becoming an increasingly important input to safety, licensing, operations and economic decisions. We are focusing on carefully-controlled simultaneous thermal and gamma radiation accelerating aging and characterization of the most common nuclear cable polymers to understand the relative contributions of temperature, time, dose and dose rate to changes in cable polymer material structure and properties. Improved understanding of cable performance in long term operation will help support continued sustainable nuclear power generation.

Cables, Nuclear, Polymers, Thermal aging, Gamma ag↗

Aging Mechanisms and Nondestructive Aging Indicator of Filled Cross-linked Polyethylene (XLPE) Exposed to Simultaneous Thermal and Gamma Radiation

Aging mechanisms and a nondestructive aging indicator of filled cross-linked polyethylene (XLPE) cable insulation material used in nuclear power plants (NPPs) are studied. Using various material characterization techniques, likely candidates and functions for the main additives in a commercial filled-XLPE insulation material have been identified. These include decabromodiphenyl ether and Sb2O3 as flame retardants, ZnS as white pigment and polymerized 1,2-dihydro-2,2,4-trimethylquinoline as antioxidant. Gas chromatography-mass spectrometry, differential scanning calorimetry, oxidation induction time and measurements of dielectric loss tangent are utilized to monitor property changes as a function of thermal and radiation exposure of the cable material. Small-molecular-weight hydrocarbons are evolve with gamma radiation aging at 90 °C. The level of antioxidant decreases with aging by volatilization and chemical reaction with free radicals. Thermal aging at 90 °C for 25 days or less causes no observable change to the cross-linked polymer structure. Gamma radiation causes damage to crystalline polymer regions and introduces defects. Dielectric loss tangent is shown to be an effective and reliable nondestructive indicator of the aging severity of the filled-XLPE insulation material.

aging mechanisms↗