Search NASA⌕ Search

Engineering topics

Jones, William R., Jr.

Publications and source records attributed to Jones, William R., Jr..

At least 73 records · Page 4

Interfacial chemistry of a perfluoropolyether lubricant studied by X-ray photoelectron spectroscopy and temperature desorption spectroscopy

The interfacial chemistry of Fomblin Z25, a commercial perfluoropolyether used as lubricant for space applications was studied with different metallic surfaces: 440C steel, gold, and aluminum. Thin layers of Fomblin Z25 were evaporated onto the oxide-free substrates, and the interfacial chemistry was studied using XPS and TDS. The reactions were induced by heating the substrate and by rubbing the substrate with a steel ball. Gold was found to be completely unreactive towards Fomblin at any temperature. Reaction at room temperature was observed only in the case of the aluminum substrate, the most reactive towards Fomblin Z25 of the substrates studied. It was necessary to heat the 440C steel substrate to 190 C to induce decomposition of the fluid. The degradation of the fluid was indicated by the formation of a debris layer at the interface. This debris layer, composed of inorganic and organic reaction products, when completely formed, passivated the surface from further attack to the Fromblin on top. The tribologically induced reactions on 440C steel formed a debris layer of similar chemical characteristics to the thermally induced layer. In all cases, the degradation reaction resulted in preferential consumption of the difluoroformyl carbon (-OCF2O-).

Herrera-Fierro, Pilar↗

Determination of the thermal stability of perfluoropolyalkyl ethers by tensimetry

The thermal decomposition temperatures of several perfluoropolyalkyl ether fluids were determined with a computerized tensimeter. In general, the decomposition temperatures of the commercial fluids were all similar and significantly higher than those for noncommercial fluids. Correlation of the decomposition temperatures with the molecular structures of the primary components of the commercial fluids revealed that the stability of the fluids was not affected by carbon chain length, branching, or adjacent difluoroformal groups. Instead, stability was limited by the presence of small quantities of thermally unstable material and/or chlorine-containing material arising from the use of chlorine containing solvents during synthesis. Finally, correlation of decomposition temperatures with molecular weights for two fluids supports a chain cleavage reaction mechanism for one and an unzipping reaction mechanism for the other.

Helmick, Larry A.↗

Determination of the oxidative stability of perfluoropolyalkyl ethers and correlation with chemical structure

The oxidative stabilities of several perfluoropolyalkyl ethers (PFPAE) with related chemical structures were determined by thermal gravimetric analysis and correlated with their chemical structures. These results show that oxidative stability increases as the number of difluoroformal groups decreases and as trifluoromethyl substituents are added. They are also consistent with a recently proposed intramolecular disproportionation reaction mechanism involving coordination of successive ether oxygens to a Lewis acid. Since polytetrafluoroethylene contains no oxygen, it provides an indication of the upper limit to oxidative stability of PFPAE fluids. These results also show that oxidative decomposition of PFPAE fluids requires the presence of an active metal as well as air. Consequently, it may be possible to minimize decomposition and thus improve oxidative stability by passivating reactive metal surfaces.

Helmick, Larry S.↗

Interfacial chemistry of a perfluoropolyether lubricant studied by XPS and TDS

The interfacial chemistry of Fomblin Z25, a commercial perfluoropolyether used as lubricant for space applications, with different metallic surfaces: 440C steel, gold and aluminum was studied. Thin layers of Fomblin Z25 were evaporated onto the oxide-free substrates and the interfacial chemistry studied using XPS and TDS. The reactions were induced by heating the substrate and by rubbing the substrate with a steel ball. Gold was found to be completely unreactive towards Fomblin at any temperature. Reaction at room temperature was observed only in the case of the aluminum substrate, the most reactive towards Fomblin Z25 of the substrates studied. It was necessary to heat the 440C steel substrate to 190 degree C to induce decomposition of the fluid. The degradation of the fluid was indicated by the formation of a debris layer at the interface. This debris layer, composed of inorganic and organic reaction products, when completely formed, passivated the surface from further attack to the Fromblin on top. The tribologically induced reactions on 440C steel formed a debris layer of similar chemical characteristics to the thermally induced layer. In all cases, the degradation reaction resulted in preferential consumption of the difluoroformyl carbon (-OCF2O-).

Herrera-Fierro, Pilar C.↗

Parched elastohydrodynamic lubrication: Instrumentation and procedure

A counter rotating bearing rig was designed and constructed to study transient elastohydrodynamic lubrication phenomena. New instrumentation is described and test procedures are documented. Ball and race speed measurement systems and the capacitance (film thickness) measurement system were upgraded. Methods for measuring bearing torque and race temperatures were implemented.

Schritz, Bryan↗

Determination of the thermal stability of fluids by tensimetry - Instrumentation and procedure

A computerized tensimeter and experimental procedure for determination of the thermal decomposition temperature (T sub d) of perfluoro alkylethers were developed and tested. Both the apparatus and the procedure are described in detail. Results of testing with bis(2-ethylhexyl) phthalate and trimethylolpropane triheptanoate demonstrate that the reciprocal of the decomposition temperature is a linear function of the logarithm of the gas volume/heated liquid volume ratio. The T sub d obtained for each compound at a gas volume/heated liquid volume ration of one was similar to the value previously reported using an isoteniscope technique. Results of testing with a polymer of hexafluoropropylene oxide demonstrate that this instrument and procedure can be used to determine the T sub d of perfluoro alkylethers.

Helmick, Larry S.↗

Determination of the thermal stability of perfluoroalkylethers

The thermal decomposition temperatures of several commercial and custom synthesized perfluoroalkylether fluids were determined with a computerized tensimeter. In general, the decomposition temperatures of the commercial fluids were all similar and significantly higher than those for custom synthesized fluids. Correlation of the decomposition temperatures with the molecular structures of the primary components of the commercial fluids revealed that the stability of the fluids is not affected by intrinsic factors such as carbon chain length, branching, or cumulated difluoroformal groups. Instead, correlation with extrinsic factors revealed that the stability may be limited by the presence of small quantities of thermally unstable material and/or chlorine-containing material arising from the use of chlorine-containing solvents during synthesis. Finally, correlation of decomposition temperatures with molecular weights for Demnum and Krytox fluids supports a chain cleavage reaction mechanism for Demnum fluids and an unzipping reaction mechanism for Krytox fluids.

Helmick, Larry S.↗

Infrared Pyrometry From Room Temperature To 700 Degrees C

Consistent readings obtained when specimens prepared appropriately. New method largely overcomes limitations. Transmission of infrared increased by replacing customary metal-coated glass viewing port with quartz viewing port covered with tantalum mesh. Commercially available infrared microscope with focal distance of 53 cm focuses on spot only 1 mm wide on specimen. Microscope operated as radiometer. Output of detector varies by several orders of magnitude, processed by logarithmic amplifier before reading.

Wheeler, Donald R.↗

Determination of the thermal stability of perfluoroalkylethers by tensimetry: Instrumentation and Procedure

A computerized tensimeter and experimental procedure for determination of the thermal decomposition temperature (T sub d) of perfluoro alkylethers were developed and tested. Both the apparatus and the procedure are described in detail. Results of testing with bis(2-ethylhexyl) phthalate and trimethylolpropane triheptanoate demonstrate that the reciprocal of the decomposition temperature is a linear function of the logarithm of the gas volume/heated liquid volume ratio. The T sub d obtained for each compound at a gas volume/heated liquid volume ration of one was similar to the value previously reported using an isoteniscope technique. Results of testing with a polymer of hexafluoropropylene oxide demonstrate that this instrument and procedure can be used to determine the T sub d of perfluoroalkylethers.

Helmick, Larry S.↗

Tribology - A Survery Of The Science

Compendium presents six papers on tribology study of adhesion, friction, wear, and lubrication of solid materials in contact: collection of papers covering theory, practice, history, and research.

Buckley, Donald H.↗

Surface temperature determination in surface analytic systems by infrared optical pyrometry

An IR pyrometric technique for measuring the surface temperatures of metal specimens in an ultrahigh-vacuum analytic chamber is described and demonstrated. The experimental setup comprises a commercial IR microscope with a long-working-distance right-angle objective (focal spot diameter 1 mm at 53 cm), a metal-coated glass vacuum chamber with a Ta-mesh-covered quartz viewport, an Mo specimen stub with an internal heating element, and a Ta disk test specimen with a flat side coated with a high-emissivity graphite film. The results of an initial calibration test are presented graphically and briefly characterized. The measurement error at 450 C is found to be less than 10 C.

Wheeler, Donald R.↗

Investigation of PTFE transfer films by infrared emission spectroscopy and phase-locked ellipsometry

When a PTFE sheet was rubbed unidirectionally over a smooth surface of stainless steel an essentially monomolecular transfer film was formed. by ellipsometric and emission infrared spectroscopic techniques it was shown that the film was 10 to 15 A thick and birefringent. From the intensity differences of infrared bands obtained with a polarizer passing radiation polarized in mutually perpendicular planes, it was possible to deduce transfer film orientation with the direction of rubbing. After standing in air for several weeks the transfer films apparently increased in thickness by as much as threefold. At the same time both the index of refraction and the absorption index decreased. Examination of the surfaces by optical and electron microscopies showed that the films had become porous and flaky. These observations were consistent with previous tribological measurements. The coefficients of friction decreased with the formation of the transfer film but increased again as the film developed breaks. The applicability of the ellipsometric and polarized infrared emission techniques to the identification of monomolecular tribological transfer films of polymers such as PTFE has been demonstrated.

Lauer, James L.↗

The preparation of new perfluoro ether fluids exhibiting excellent thermal-oxidative stabilities

A series of low molecular weight perfluoroalkyl ethers (PFAEs) were synthesized by direct fluorination. Viscosity-temperature properties and oxidation stabilities were determined. Viscosity-temperature correlations indicated that increases in branching and increases in the size of the branching substituent caused a deterioration in viscometric properties (i.e., an increase in ASTM slope). In addition, increasing the ratio of carbon to oxygen in these compounds also increased the ASTM slope. Preliminary oxidation stability measurements indicated that highly branched PFAE fluids (i.e., those containing quaternary carbons) may be less stable than either those containing a single trifluoromethyl pendant group or those containing no branching at all.

Jones, William R., Jr.↗

Investigation of PTFE transfer films by infrared emission spectroscopy and phase-locked ellipsometry

When a PTFE sheet was rubbed unidirectionally over a smooth surface of stainless steel an essentially monomolecular transfer film was formed. By ellipsometric and emission infrared spectroscopic techniques it was shown that the film was 10 to 15 A thick and birefringent. From the intensity differences of infrared bands obtained with a polarizer passing radiation polarized in mutually perpendicular planes, it was possible to deduce transfer film orientation with the direction of rubbing. After standing in air for several weeks the transfer films apparently increased in thickness by as much as threefold. At the same time both the index of refraction and the absorption index decreased. Examination of the surfaces by optical and electron microscopies showed that the films had become porous and flaky. These observations were consistent with previous tribological measurements. The coefficients of friction decreased with the formation of the transfer film but increased again as the film developed breaks. The applicability of the ellipsometric and polarized infrared emission techniques to the identification of monomolecular tribological transfer films of polymers such as PTFE has been demonstrated.

Lauer, James L.↗

A preliminary study of ester oxidation on an aluminum surface using chemiluminescence

The oxidation characteristics of a pure ester (trimethyolpropane triheptanoate) were studied by using a chemiluminescence technique. Tests were run in a thin-film micro-oxidation apparatus with an aluminum alloy catalyst. Conditions included a pure oxygen atmosphere and a temperature range of 176 to 206 C. Results indicated that oxidation of the ester (containing 10 to the minus 3rd power M diphenylanthracene as an intensifier) was accompanied by emission of light. The maximum intensity of light emission (I sub max) was a function of the amount of ester, the concentration of intensifier, and the test temperature. The induction period or the time to reach one-half of maximum intensity (t sub 1/2) was an inverse function of test temperature. Decreases in light emission at the later stages of a test were caused by depletion of the intensifier.

Jones, William R., Jr.↗

Improved perfluoroalkyl ether fluid development

The feasibility of transforming a commercial linear perfluoroalkylether fluid into a material stable in the presence of metals and metal alloys in oxidizing atmospheres at 300 C without the loss of the desirable viscosity temperature characteristics was determined. The approach consisted of thermal oxidative treatment in the presence of catalyst to remove weak links, followed by transformation of the created functional groups into phospha-s-triazine linkages. It is found that the experimental material obtained in 66 percent yield from the commercial fluid exhibits, over an 8 hr period at 300 C in the presence of Ti(4Al, 4Mn) alloy, thermal oxidative stability better by a factor of 2.6 x 1000 based on volatiles evolved than the commercial product. The viscosity and molecular weight of the developed fluid are unchanged and are essentially identical with the commercial material. No metal corrosion occurs with the experimental fluid at 300 C.

Jones, William R., Jr.↗

Ester oxidation on an aluminum surface using chemiluminescence

The oxidation characteristics of a pure ester (trimethyolpropane triheptanoate) were studied by using a chemiluminescence technique. Tests were run in a thin film microoxidation apparatus with an aluminum alloy catalyst. Conditions included a pure oxygen atmosphere and a temperature range of 176 to 206 C. Results indicated that oxidation of the ester (containing .001 M diphenylanthracene as an intensifier) was accompanied by emission of light. The maximum intensity of light emission was a function of the amount of ester, the concentration of intensifier, and the test temperature. The induction period, or the time to reach one-half of maximum intensity was inversely proportional to test temperature. Decreases in light emission at the later stages of a test were caused by depletion of the intensifier.

Jones, William R., Jr.↗