Search NASA⌕ Search

Engineering topics

Jordan-Sweet, J

Publications and source records attributed to Jordan-Sweet, J.

At least 37 records · Page 2

Texture of CoSi2 Films on Si(111) (110) and (001) Substrates

Synchrotron radiation was used to study the texture of polycrystalline CoSi{sub 2} films that were formed by a solid-state reaction between a 30 nm Co film and Si(111), (110) and (001) substrates. All films were strongly textured, and several texture components were identified. We discuss the simultaneous occurrence of axiotaxy (i.e. alignment of lattice planes across the interface) and several different types of epitaxy in each of the films. Comparison of the different texture components observed on the three substrate orientations suggests a strong preference for the alignment of CoSi{sub 2}{l_brace}110{r_brace} planes in the film with Si{l_brace}110{r_brace} planes in the substrate, and twinning around Si[111] directions.

36 MATERIALS SCIENCE↗

Irreversible altering of crystalline phase of phase-change Ge-Sb thin films

The stability of the crystalline phase of binary phase-change Ge{sub x}Sb{sub 1-x} films is investigated over a wide range of Ge content. From Raman spectroscopy we find the Ge-Sb crystalline structure irreversibly altered after exposure to a laser beam. We show that with increasing beam intensity/temperature Ge agglomerates and precipitates out in the amount growing with x. A simple empirical relation links Ge precipitation temperature T{sub Ge}{sup p} to the rate of change dT{sub cryst}/dx of crystallization, with the precipitation easiest on the mid-range x plateau, where T{sub cryst} is nearly constant. Our findings point to a preferable 15% < or approx. x < 50% window, that may achieve the desired cycling/archival properties of a phase-change cell.

36 MATERIALS SCIENCE↗

Diamond Photodiodes for X-ray Applications

Single crystal high purity CVD diamonds have been metallized and calibrated as photodiodes at the National Synchrotron Light Source (NSLS). Current mode responsivity measurements have been made over a wide range (0.2-28 keV) of photon energies across several beamlines. Linear response has been achieved over ten orders of magnitude of incident flux, along with uniform spatial response. A simple model of responsivity has been used to describe the results, yielding a value of 13.3 {+-} 0.5 eV for the mean pair creation energy. The responsivity vs. photon energy data show a dip for photon energies near the carbon edge (284 eV), indicating incomplete charge collection for carriers created less than one micron from the metallized layer.

43 PARTICLE ACCELERATORS↗

In situ X-ray Diffraction Study of Thin Film Ir/Si Solid State Reactions

The solid state reaction between a thin (30 nm) Ir film and different Si substrates (p-type Si(1 0 0), n- and p-type Si(1 1 1), silicon on insulator (SOI) and polycrystalline Si) was studied using a combination of in situ X-ray diffraction (XRD), in situ sheet resistance and laser light scattering measurements. No significant influence of either the dopants or the substrate orientation was detected as a phase formation sequence of IrSi, Ir{sub 3}Si{sub 4},Ir{sub 3}Si{sub 5} and IrSi{sub 3} was found for all samples. The presence of a thin (<4 nm) amorphous IrSi film at room temperature and its subsequent crystallization could be deduced from the appearance of a broad semi-amorphous diffraction peak in the XRD spectrum around 400 C. The results were verified using ex situ Rutherford Backscattering Spectroscopy, Scanning Electron Microscopy and 4-point probe measurements on quenched samples. The activation energy of the crystallization process and the silicide growth was determined using a Kissinger analysis on ramp anneals with different ramp rates. In addition, the influence of up to 25 volumetric % (20.5 atomic %) of Ir to the silicide formation in the Ni/Si system was studied on SOI and polycrystalline Si substrates. In the presence of Ir, the temperature range over which the low resistivity NiSi exists, is reduced both through an increase in formation temperature and an earlier consumption by the formation of NiSi{sub 2}. After the heat treatment, a continuous distribution of Ir throughout the NiSi{sub 2} phase was detected using X-ray photoelectron spectroscopy depth profiling. A low sheet resistance of < 20 {Omega}/{open_square} was maintained on both substrates up to 900 C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

In Situ Study of the Formation of Silicide Phases in Amorphous Co–Si Mixed Layers

We investigate Co silicide phase formation when extra Si is added within an as deposited 50 nm Co film. The addition of Si is investigated for both the Co/SiO{sub 2} and Co/Si(1 0 0) system. A series of 10 Co-Si mixed films with a Si content varying from 21 to 59 at.% was prepared and investigated during annealing with in situ X-ray diffraction. The oxide system is used as reference system to identify phases that initially crystallize in an amorphous mixture of a given composition. Multiple phases can nucleate, and the temperature of crystallization depends on the Co-Si atomic ratio. Upon heating of the Co(Si)/Si system, the first reaction is a similar crystallization reaction of the Co(Si) mixture. Once the first phase is formed, one has the normal system of a silicide phase in contact with an unlimited amount of Si from the substrate, and the sequential phase formation towards CoSi{sub 2} is established. For deposited layers of composition ranging from 48%Si to 52%Si, the CoSi is the first phase to form and increasing the amount of Si leads to a remarkable improvement of the thermal stability of CoSi on Si(1 0 0). CoSi{sub 2} nucleation was extensively delayed by 150 C compared to the reaction observed from a pure Co film on Si(1 0 0). Electron backscatter diffraction measurements reveal that in this range, the gradual Si increase systematically leads to bigger CoSi grains (up to 20 {micro}m). This shows that the grain size of the CoSi precursor strongly affects the nucleation of the following CoSi{sub 2} phase. Laser-light scattering measurements suggest that adding more than 42%Si reduces the roughness of the CoSi{sub 2} layer.

99 GENERAL AND MISCELLANEOUS↗

Morphological Stability and Specific Resistivity of sub-10 nm Silicide Films of Ni1 xPtx on Si Substrate

This letter studies the morphological stability and specific resistivity of sub-10 nm silicide films of Ni, Ni{sub 0.95}Pt{sub 0.05}, and Ni{sub 0.9}Pt{sub 0.1} formed on Si(100) substrate. When the deposited metal films are below 1 to 4 nm in thickness depending on the Pt content, the resultant silicide films tend to become epitaxially aligned to the Si substrate and hence exhibit an extraordinary morphological stability up to 800 C. The presence of Pt in the silicides increases the film resistivity through alloy scattering, but alleviates, owing to a reduced electron mean free path, the frequently encountered sharp increase in resistivity in the sub-10 nm regime.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Phase Formation and Thermal Stability of Ultrathin Nickel-silicides on Si(100)

The solid-state reaction and agglomeration of thin nickel-silicide films was investigated from sputter deposited nickel films (1-10 nm) on silicon-on-insulator (100) substrates. For typical anneals at a ramp rate of 3 C/s, 5-10 nm Ni films react with silicon and form NiSi, which agglomerates at 550-650 C, whereas films with a thickness of 3.7 nm of less were found to form an epitaxylike nickel-silicide layer. The resulting films show an increased thermal stability with a low electrical resistivity up to 800 C.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Understanding Tunneling Magnetoresistance During Thermal Annealing in MgO-based Junctions with CoFeB Electrodes

The competition between the interface crystallization and diffusion processes, their influence on the onset of symmetry-filtering coherent tunneling of {Delta}{sub 1} band electrons in the MgO-based magnetic tunnel junctions is investigated. Systematic study of the transport and magnetoresistance during thermal annealing of these junctions shows a unique behavior of the tunneling conductance in the parallel state. The optimal annealing time for achieving giant tunneling magnetoresistance at different temperatures is determined. The evolution of magnetoresistance consists of three distinct regions, responsible by different contributions from CoFeB electrodes and the MgO barrier. The whole phenomenon can be understood through an empirical model based on the Landauer tunneling picture.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

In situ X-ray Diffraction Study of Ni–Yb Interlayer and Alloy Systems on Si„100

The phase formation in the ternary Ni/Yb/Si system was studied for Ni-Yb alloy and interlayer structures on Si(100) substrates using in situ x-ray diffraction measurements. Yb was treated as an alloying element in the Ni-Si system with Yb concentrations varying between 0 and 40 at. % of the Ni concentration. Independent of the initial structure of the sample, a Ni-Si or Ni-Yb compound was detected first which suggests that Ni is the dominant diffusing species during the solid state reactions. No pure Yb silicides were identified but a ternary phase (YbNi{sub 2}Si{sub 2}) formed in all samples after the Si atoms became mobile. Information about the distribution of the phases throughout the thin silicide film was obtained using ex situ Rutherford backscattering analysis. Independent of the Yb concentration, the NiSi phase formed at the substrate interface. As a result, the immobile Yb atoms shifted toward the sample surface and no detectable amount of Yb atoms was left at the Ni-silicide/Si interface after annealing.

36 MATERIALS SCIENCE↗

Texture of Cobalt Germanides on Ge(100) and Ge(111) and Its Influence on the Formation Temperature

The phase formation of cobalt germanides on Ge(100) and Ge(111) substrates was investigated using in situ X-ray diffraction, starting from room-temperature sputter-deposited Co films. The formation temperature of the CoGe{sub 2} phase was dependent on the substrate orientation. X-ray pole figures and electron backscatter diffraction measurements were used to identify the texture and microstructure of the CoGe{sub 2} and the preceding Co{sub 5}Ge{sub 7} films. A significant difference in preferential orientation was found in the Co{sub 5}Ge{sub 7} films, depending on the substrate orientation. This influences the formation temperature of the CoGe{sub 2} and results in the coexistence of Co{sub 5}Ge{sub 7} and CoGe{sub 2} on Ge(111) in a large temperature window.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Outstanding Symposium Paper: Stress Gradients Observed in Cu Thin Films Induced by Capping Layers

Glancing-incidence x-ray diffraction (GIXRD) has been applied to the investigation of depth-dependent stress distributions within electroplated Cu films due to overlying capping layers. Cu films, 0.65 {micro}m thick, plated on conventional barrier and seed layers received a chemical vapor deposited (CVD) SiC{sub x} N{sub y} H{sub z} cap, an electrolessly deposited CoWP layer, or a CoWP layer followed by a SiC{sub x} N{sub y} H{sub z} cap. GIXRD and conventional x-ray diffraction measurements revealed that strain gradients were created in Cu films possessing a SiC{sub x} N{sub y} H{sub z} cap, where a greater in-plane tensile stress of approximately 180 MPa was generated near the film/cap interface as a result of constraint imposed by the SiC{sub x} N{sub y} H{sub z} layer during cooling from the cap deposition temperature. Although Cu films possessing a CoWP cap without a SiC{sub x} N{sub y} H{sub z} layer did not exhibit depth-dependent stress distributions, subsequent annealing introduced stress gradients and increased the bulk Cu stress. However, a thermal excursion to liquid-nitrogen temperatures significantly reduced tensile stresses in the Cu films.

36 MATERIALS SCIENCE↗

Phase transitions in Ge-Sb phase change materials

Thin films of the phase change material Ge-Sb with Ge concentrations between 7.3 and 81.1 at. % were deposited by cosputtering from elemental targets. Their crystallization behavior was studied using time-resolved x-ray diffraction, Auger electron spectroscopy, differential scanning calorimetry, x-ray reflectivity, profilometry, optical reflectivity, and resistivity versus temperature measurements. It was found that the crystallization temperature increases with Ge content. Calculations of the glass transition temperature (which is a lower limit for the crystallization temperature T{sub x}) also show an increase with Ge concentration closely tracking the measured values of T{sub x}. For low Ge content samples, Sb x-ray diffraction peaks occurred during a heating ramp at lower temperature than Ge diffraction peaks. The appearance of Ge peaks is related to Ge precipitation and agglomeration. For Ge concentrations of 59.3 at. % and higher, Sb and Ge peaks occurred at the same temperature. Upon crystallization, film mass density and optical reflectivity increase as well as electrical contrast (ratio of resistivity in amorphous phase to crystalline phase) all showed a maximum for the eutectic alloy (14.5 at. % Ge). For the alloy with 59.3 at. % Ge there was very little change in any of these parameters, while the alloy with 81.1 at. % Ge behaved opposite to a typical phase change alloy and showed reduced mass density and reflectivity and increased resistivity.

36 MATERIALS SCIENCE↗

Influence of a Transient Hexagonal Phase on the Microstructure and Morphological Stability of NiSi Films

The morphological stability of NiSi is investigated when 40% of Si is mixed into an as deposited 10 nm Ni film. When annealing at 3?C/s, scanning electron microscopy images and in situ sheet-resistance measurements show that NiSi agglomeration is delayed by more than 100?C. In situ x-ray diffraction reveals that NiSi grows from an unusual transient hexagonal ?-nickel-silicide phase. The significant improvement of the NiSi film's morphological stability can be related to its microstructure, with large grains and a strong texture. This peculiar microstructure is compared to the microstructure of the ?-nickel-silicide precursor by electron backscattering diffraction and pole figures.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Annealing Behavior of Atomic Layer Deposited HfO2 Films Studied by Synchrotron X-ray Reflectivity and Grazing Incidence Small Angle Scattering

New results are presented for the annealing behavior of ultrathin complementary-metal-oxide-semiconductor (CMOS) gate dielectric HfO{sub 2} films grown by atomic layer deposition (ALD). A series of ALD HfO{sub 2} dielectric films has been studied by a combination of x-ray reflectivity (XRR) and grazing-incidence small-angle x-ray scattering (GISAXS) measurements. By using these techniques together, we have shown that the surface, interfaces, and internal structure of thin ALD films can be characterized with unprecedented sensitivity. Changes in film thickness, film roughness, or diffuseness of the film/substrate interface as measured by XRR are correlated with the corresponding changes in the internal film nanostructure, as measured by GISAXS. Although the films are dense, an internal film structure is shown to exist, attributed primarily to {approx} 2 nm 'missing island' porosity features close to the substrate; these are most likely associated with coalescence defects as a result of initial ALD growth, as they are not observed in the upper regions of the film. Some 8-9 nm heterogeneities are also present, which may indicate a widespread modulation in the film density pervading the entire film volume, and which likely also give rise to surface roughness. Comparison of the data between different scattering geometries and among a carefully designed sequence of samples has enabled important insights to be derived for the annealing behavior of the ALD HfO{sub 2} films. The main effects of single, brief, high temperature excursions to above 900C are to anneal out some of the fine voids and reduce the mean roughness and interfacial diffuseness of the film. These changes are indicative of densification. However, depending on the film thickness, the annealing behavior at temperatures between 650 and 800C is quite different for single excursion and cyclic anneals. Particularly for thin, just-coalesced films, XRR indicates marked increases in the film thickness and in the mean roughness/diffuseness dimension for cyclic anneals. GISAXS also shows an increase, rather than a reduction, in the void microstructure under these conditions. These changes in the film microstructure appear sufficient to overcome the expected film densification at elevated temperatures with implications for the gate dielectric performance of the films after extended high temperature exposure and cycling, as may occur during gate dielectric fabrication.

36 MATERIALS SCIENCE↗

Influence of Interfaces and Doping on the Crystallization Temperature of Ge-Sb

The crystallization temperature Tx of the phase change material Ge-Sb as a function of film thickness and cladding material was measured using time-resolved x-ray diffraction. For films >5 nm, a weak influence of the cladding material on Tx was found (increase for Si, SiN, Pt, SiC, and TiN and decrease for Al and W). For very thin films, however, Tx differed up to 200?C. Doping of Ge-Sb with these materials led to an increase in Tx in all cases, up to a maximum of 180?C for SiN. Such a large influence of interfaces and doping on Tx is of great technological importance.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Method to Measure the Viscosity of Nanometer Liquid Films from the Surface Fluctuations

We describe a method to measure the viscosity of polystyrene liquid films with thicknesses {approx} 5 and {approx} 80 nm spin-cast on oxide-coated silicon. In this method, temporal evolution of the film surface is monitored and modeled according to the dynamics of the surface capillary waves. Viscosities obtained from the {approx} 80 nm films display an excellent agreement with those of the bulk polymer, but those from the {approx} 5 nm films are up to 106 times reduced. By modeling the data to the Vogel-Fulcher-Tammann relation, we find that the observations are consistent with the thickness dependence of the glass transition temperature previously reported of these films.

36 MATERIALS SCIENCE↗

In situ Study of the Formation of Silicide Phases in Amorphous Ni-Si Mixed Layers

In this paper, we investigated Ni silicide phase formation when Si is added within an as deposited 50 nm Ni film. A series of 22 samples with a Si content varying from 0 to 50 at.% was prepared and systematically investigated with in situ x-ray diffraction. The inert oxide substrate was used to identify the phases which first crystallize in an amorphous Ni-Si mixture of a given concentration. The noncongruent silicides Ni{sub 3}Si and Ni{sub 3}Si{sub 2} are never observed to crystallize readily out of the mixture. A remarkable observation is the initial crystallization at low temperature of a hexagonal Ni-silicide, observed over a broad mixed layer composition [35-49%Si]; this hexagonal phase nucleates readily as a single phase [39-47%Si] or together with Ni{sub 2}Si [35-38%Si] or NiSi [49%Si]. This low-temperature phase is related to the high temperature {theta}-phase, but covers a wide composition range up to 47%Si. For the same Ni-Si films deposited on Si(100), the initial nucleation of the Ni(Si) mixture is similar as for the samples deposited on SiO{sub 2}, such that the complex sequence of metal-rich Ni-silicide phases typically observed during Ni/Si reactions is modified. For samples containing more than 21%Si, a simpler sequential phase formation was observed upon annealing. From pole figures, the phase formation sequence was observed to have a significant influence on the texture of the technologically relevant NiSi phase. For mixture composition ranging from 38% to 43%Si, the initial transient {theta}-phase appears extremely textured on Si(100). The observed transient appearance of a hexagonal phase is of importance in understanding the phase formation mechanisms in the Ni-Si system.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Phase Transitions in Ge-Te Phase Change Materials Studied by Time-resolved X-ray Diffraction

Resistivity versus temperature measurements and time-resolved x-ray diffraction were used to study Ge-Te phase change materials. Resistivity versus temperature measurements showed one sharp drop in resistivity for films with 30, 50, and 70 at.?% Ge, two steps for films with 40 at.?% Ge, and a gradual transition for films with 60 at.?% Ge. Films with 30, 50, and 70 at.?% Ge crystallized in a single-step process with GeTe and Te, only GeTe, and GeTe and Ge diffraction peaks, respectively. Films with 40 and 60 at.?% Ge crystallized in a two-step process with GeTe peaks appearing first and additional Te or Ge peaks, respectively, appearing at higher temperature.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗