Effects of long term exposure on optical substrates and coatings (SOO50-2)
Kodak included 12 substrate and coating samples on the Long Duration Exposure Facility (LDEF) structure. There were 3 fused silica and 3 ultra low expansion (ULE(tm)) uncoated glass samples, 2 ULE(tm) samples with a high reflectance silver coating, 2 fused silica samples with an antireflectance coating, and 2 fused silica samples with a solar rejection coating. The sample dimensions were 32 mm diameter by 1 mm thick. A set of duplicate control samples was also manufactured and stored in a controlled environment for comparison purposes. A preliminary evaluation of the flight samples for effects from the 5 year mission showed that a contaminant was deposited on the samples, a micrometeroid impact occurred on one of the samples, and the radiation darkening which was expected for the glass did not occur. The results are presented in more detail.