Search NASA⌕ Search

Engineering topics

Novak, Alan M.

Publications and source records attributed to Novak, Alan M..

Novel Segregated Solid Propulsion System with Separately Stored Fuel and Oxidizer

Abstract The development and experimentation of a solid propulsion concept consisting of separate hydrogen‐rich solid propellant and solid oxidizer grains is presented. This system consists of an extremely fuel‐rich solid propellant, which, once ignited, undergoes a self‐sustaining decomposition to release fuel‐rich product gases, which are particularly rich in hydrogen gas. These relatively high‐temperature gases subsequently react with a solid oxidizer grain stored downstream. Progress in high‐nitrogen materials has allowed for the synthesis of fuel‐rich compounds that can store significant amounts of hydrogen, with little or no bound oxygen. With these new developments in propellant chemistry, a unique segregated propulsion system has been developed, creating an all‐solid propulsion system that combusts analogously to a reverse hybrid rocket system. Because of the physical separation of fuel and oxidizer, a higher level of safety is achieved which concurrently allows for the utilization of higher energy ingredients without the penalty of higher sensitivity. Theoretical performance calculations and experimental data have shown the potential for this system to compete with existing composite rocket propellants while having significant benefits in terms of safety, toxicity, and mission space. This paper presents a detailed overview of the conception, development, and testing of this propulsion system.

42 ENGINEERING↗

Wedding Cake Experiments Design and Data Packages (V.2)

This report documents the design and data for four related experiments known as the Wedding Cake shots. It is a revised version of LA-UR-17-28352. The basic designs of these four shots are the same. A high-explosive plane-wave lens launches a flyer towards an acceptor material with a smaller diameter. This acceptor is either another piece of high-explosive or a piece of polyethylene. A detonation or shock wave propagates through this material and launches a second flyer. The velocities of both flyers are recorded using Photon Doppler Velocimetry (PDV). The overall shape of the shots is reminiscent of a tiered wedding cake and, consequently, these shots are know as the Wedding Cake shots. Details of the shot assembly are shown in the Wedding Cake Assembly Drawing and component drawings that accompany this report.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Proof Testing of Small-Scale HE Press Shielding

High explosives pressing activities at Los Alamos National Laboratory have played a critical role in meeting the core missions of the lab since its early days. Small scale pressing (25 grams of energetic material or less) constitutes a significant portion of current production and much of this occurs as an attended operation. Workers that are present during HE pressing operations are to be protected from blast and fragment dangers associated with the potential violent reaction of the energetic material being pressed. Safety is paramount in all HE operations, and the ongoing evolution of analysis and mitigation of hazards contributes strongly to the development of adequate protections for personnel. Attended pressing operations satisfying Class 1 Level Protection criteria, until recently, have been allowed for small scale pressing activities on the basis of an undocumented design of shielding enclosures used at LANL. Recent review of the shield design has determined the necessity of proof testing an adequate enclosure and thoroughly documenting the test results and fabrication specifications. This will provide a basis for continuing attended operations and guidance for future design iterations. The results of the testing described in this report provide sufficient assurance that the new shield design is adequate to protect attendant workers against injury from direct blast and fragments resulting from full detonation of the maximum allowable mass of explosives (less than 25 grams) confined in a uniaxial pressing configuration typical for Los Alamos National Laboratory.

42 ENGINEERING↗

PBX 9502 air-gap tests

A small number of simple air-gap tests were performed on 1-inch diameter PBX 9502 cylinders to determine an approximate threshold for detonation failure. The primary diagnostics were streak imaging and dent measurements in a steel witness plate. Relight was found to occur, with negligible excess transit time, for air gaps up to 1 mm. Relight did not occur with a 3-mm air gap.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Isolator fragmentation and explosive initiation tests

Three tests were conducted to evaluate the effects of firing an isolator in proximity to a barrier or explosive charge. The tests with explosive were conducted without a barrier, on the basis that since any barrier will reduce the shock transmitted to the explosive, bare explosive represents the worst-case from an inadvertent initiation perspective. No reaction was observed. The shock caused by the impact of a representative plastic material on both bare and cased PBX 9501 is calculated in the worst-case, 1-D limit, and the known shock response of the HE is used to estimate minimum run-to-detonation lengths. The estimates demonstrate that even 1-D impacts would not be of concern and that, accordingly, the divergent shocks due to isolator fragment impact are of no concern as initiating stimuli.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Isolator fragmentation and explosive initiation tests

Three tests were conducted to evaluate the effects of firing an isolator in proximity to a barrier or explosive charge. The tests with explosive were conducted without barrier, on the basis that since any barrier will reduce the shock transmitted to the explosive, bare explosive represents the worst-case from an inadvertent initiation perspective. No reaction was observed. The shock caused by the impact of a representative plastic material on both bare and cased PBX9501 is calculated in the worst-case, 1-D limit, and the known shock response of the HE is used to estimate minimum run-to-detonation lengths. The estimates demonstrate that even 1-D impacts would not be of concern and that, accordingly, the divergent shocks due to isolator fragment impact are of no concern as initiating stimuli.

36 MATERIALS SCIENCE↗

The violence of reaction from a fast projectile fired into heated PBX 9502

The shock sensitivity of hot PBX 9502 is of concern in abnormal combined insult situations. A series of fragment impacts into thin aluminum cased PBX 9502 heated to various temperatures was performed. The explosive was tightly radially confined but effectively unconfined axially. A 15.5 mm diameter by 3 mm thick heavy tungsten fragment (17.5 g/cc) fired at a velocity of approximately 1.4 km s –1 imparted an initial shock pressure of ≈15 GPa into the explosive. Under one dimensional shock conditions, the run to detonation in PBX 9502 at ambient temperature and at this pressure is ≈5 mm, however, given the small dimensions of the fragment in this insult, the pressure is quickly released from the edge so that a dying reaction is created. The situation is very different at higher explosive temperatures when the shock sensitivity of lightly confined PBX 9502 is much greater. Under these specific insult conditions, detonations were not observed at 22 and 70°C, but were observed at 170 and 108°C. The significance of these results is discussed.

36 MATERIALS SCIENCE↗

The Effect of Grit on Frictional Heating During Oblique Impacts with PBX 9501

Technicians working at the Pantex Plant routinely perform assembly/disassembly operations on weapons containing plastic-bonded explosives (PBXs). With high explosives (HE) operations comes the potential for high consequence accidents. As a result, a process for hazard analysis has been developed within the DOE-NNSA complex to identify and prevent HE-related accidents. Part of this process is to perform research to support or reject the safety basis upon which plant operations are authorized. Understanding the physics of HE response to a variety of mechanical and thermal insults is valuable to this process to: 1) assess risk probability to rank scenarios for the purpose of focusing resources to maximize benefit; 2) define screening thresholds to minimize risk for when an accident does occur; and 3) to develop engineered controls and administrative strategies to mitigate consequences when an accident occurs.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Projectile containing metastable intermolecular composites and spot fire method of use

A method for altering the course of a conflagration involving firing a projectile comprising a powder mixture of oxidant powder and nanosized reductant powder at velocity sufficient for a violent reaction between the oxidant powder and the nanosized reductant powder upon impact of the projectile, and causing impact of the projectile at a location chosen to draw a main fire to a spot fire at such location and thereby change the course of the conflagration, whereby the air near the chosen location is heated to a temperature sufficient to cause a spot fire at such location. The invention also includes a projectile useful for such method and said mixture preferably comprises a metastable intermolecular composite.

36 MATERIALS SCIENCE↗

Summary of Booster Development and Qualification Report

This report outlines booster development work done at Los Alamos National Laboratory from 2007 to present. The booster is a critical link in the initiation train of explosive assemblies, from complex devices like nuclear weapons to conventional munitions. The booster bridges the gap from a small, relatively sensitive detonator to an insensitive, but massive, main charge. The movement throughout the explosives development community is to use more and more insensitive explosive components. With that, more energy is needed out of the booster. It has to initiate reliably, promptly, powerfully and safely. This report is divided into four sections. The first provides a summary of a collaborative effort between LANL, LLNL, and AWE to identify candidate materials and uniformly develop a testing plan for new boosters. Important parameters and the tests required to measure them were defined. The nature of the collaboration and the specific goals of the participating partners has changed over time, but the booster development plan stands on its own merit as a complete description of the test protocol necessary to compare and qualify booster materials, and is discussed in its entirety in this report. The second section describes a project, which began in 2009 with the Department of Defense to develop replacement booster formulations for PBXN-7. Replacement of PBXN-7 was necessary because it contained Triaminotrinitrobenzene (TATB), which was becoming unavailable to the DoD and because it contained Cyclotrimethylenetrinitramine (RDX), which was sensitive and toxic. A LANL-developed explosive, Diaminoazoxyfurazan (DAAF), was an important candidate. This project required any replacement formulation be a drop-in replacement in existing munitions. This project was timely, in that it made use of the collaborative booster development project, and had the additional constraint of matching shock sensitivity. Additionally it needed to be a safety improvement, and a performance improvement, especially at cold temperatures. The requirements of this project necessitated novel test development and a different approach to ranking booster qualities. Results of this project have been documented to the DoD and the relevant portions are included within. The third section of this booster report outlines testing related to main charge initiation merit. Initiability can be evaluated by looking at critical diameter, run distance, and shock sensitivity. Once a booster is initiated, it needs to be powerful enough to initiate the main charge symmetrically and evenly. Main charge initiability is evaluated directly by observing detonation wave symmetry, curvature, and first break out over the surface of a charge. Furthermore it must be insensitive to accidents and insults, and safe and reliable across a range of temperatures. These effects, tests, and results will be discussed individually in the context of DAAF and other explosives similarly tested. The last section provides a conclusion and summary of our experimental work and recommendations for the path forward. References and additional supporting documentation and results are provided in the appendices at the end of this report.

36 MATERIALS SCIENCE↗