Stress-rupture strength and microstructural stability of W-HF-C wire-reinforced superalloy composites

W-Hf-C superalloy composites were found to be potentially useful for turbine-blade applications on the basis of stress-rupture strength. The 100- and 1000-hour rupture strengths obtained for 70 volume percent fiber composites tested at 1090 C were 420 and 280 MN/sq m. The investigation indicated that with better quality fibers, composites having 100- and 1000-hour rupture strengths of 570 and 370 MN/sq m may be obtained. Metallographic studies indicated sufficient fiber-matrix compatibility for long-term applications at 1090 C for 1000 hours or more.

Petrasek, D. W.↗

Effect of rolling on the high temperature tensile and stress-rupture properties of tungsten fiber-superalloy composites

An investigation was conducted to determine the effects of mechanical working on the 1093 C (2000 F) tensile and stress-rupture strength of tungsten alloy/superalloy composites. Hot pressed composites containing either conventional tungsten lamp filament wire or tungsten-1% ThO2 wire and a nickel base alloy matrix were hot rolled at 1093 C (2000 F). The hot pressed and rolled composite specimens were then tested in tension and stress-rupture at 1093 C (2000 F). Rolling decreased the degree of fiber-matrix reaction as a function of time of exposure at 1093 C (2000 F). The stress-rupture properties of the rolled composites were superior to hot pressed composites containing equivalent diameter fibers. Rolling did not appreciably affect the 1093 C (2000 F) ultimate tensile strength of the composites.

Petrasek, D. W.↗

Stress-rupture strength and microstructural stability of W-HF-C wire reinforced superalloy composites

W-Hf-C/superalloy composites were found to be potentially useful for turbine blade applications on the basis of stress-rupture strength. The 100-and 1000-hour rupture strengths obtained for 70 volume percent fiber composites tested at 1090 C were 420 and 280 MN/sq m (61,000 and 41,000 psi). The investigation indicated that with better quality fibers, composites having 100- and 1000-hour rupture strengths of 570 and 370 MN/sq m (82,000 and 54,000 psi) may be obtained. Metallographic studies indicated sufficient fiber-matrix compatibility for long time applications at 1090 C for 1000 hours or more.

Petrasek, D. W.↗

Effect of rolling on the high temperature tensile and stress-rupture properties of tungsten fiber-superalloy composites

An investigation was conducted to determine the effects of mechanical working on the 1093 C tensile and stress-rupture strength of tungsten alloy/superalloy composites. Hot pressed composites containing either conventional tungsten lamp filament wire or tungsten-1% ThO2 wire and a nickel base alloy matrix were hot rolled at 1093 C. The hot pressed and rolled composite specimens were then tested in tension and stress-rupture at 1093 C. Rolling decreased the degree of fiber-matrix reaction as a function of time of exposure at 1093 C. The stress-rupture properties of the rolled composites were superior to hot pressed composites containing equivalent diameter fibers. Rolling did not appreciably affect the 1093 C ultimate tensile strength of the composites.

Petrasek, D. W.↗

Factors affecting miniature Izod impact strength of tungsten-fiber-metal-matrix

The miniature Izod and Charpy impact strengths of copper, copper-nickel, and nickel-base superalloy uniaxially reinforced with continuous tungsten fibers were studied. In most cases, impact strength was increased by increasing fiber or matrix toughness, decreasing fibermatrix reaction, increasing test temperature, hot working, or heat treating. Notch sensitivity was reduced by increasing fiber content or matrix toughness. An equation relating impact strength to fiber and matrix properties and fiber content was developed. Program results imply that tungsten alloy-fiber/superalloy matrix composites can be made with adequate impact resistance for turbine blade or vane applications.

Winsa, E. A.↗

Production of small diameter high-temperature-strength refractory metal wires

Special thermomechanical techniques (schedules) have been developed to produce small diameter wire from three refractory metal alloys: colombian base alloy, tantalum base alloy, and tungsten base alloy. High strengths of these wires indicate their potential for contributing increased strength to metallic composites.

Petrasek, D. W.↗

High-temperature strength of refractory-metal wires and consideration for composite applications

Tensile and stress-rupture tests were conducted on wires of W-Hf-C, W-Re-Hf-C, ASTAR 811C (a tantalum alloy), and B-88 (a columbium alloy) at room temperature, 1093 C (2000 F), and 1204 C (2200 F). Metallographic examinations were also made of the wire microstructure after testing. Ultimate tensile strength values up to 2170 meganewtons per square meter (314000 psi) at 1093 C (2000 F) and 1940 meganewtons per square meter (281 000 psi) at 1204 C (2200 F) were obtained for W-Re-Hf-C wire. The best strength values obtained for a 100-hour rupture life were, 1410 meganewtons per square meter (205 000 psi) at 1093 C (2000 F) and 910 meganewtons per square meter (132 000 psi) at 1240 C (2200 F) for W-Re-Hf-C wire. The properties obtained suggested that the wires studied showed promise as potential fiber reinforcement in the 1093 to 1204 C (2000 to 2200 F) temperature range.

Petrasek, D. W.↗

Pendulum impact resistance of tungsten fiber/metal matrix composites.

The impact properties of copper, copper-10 nickel, and a superalloy matrix reinforced with tungsten fibers were studied. In most cases the following increased composite impact strength: increased fiber or matrix toughness, decreased fiber-matrix reaction, increased test temperature, hot working and heat treatment. Notch sensitivity was reduced by increasing fiber or matrix toughness. The effect of fiber content depended on the relative toughness of the fibers and matrix. Above 530 K a 60 volume per cent superalloy matrix composite had a greater impact strength than a turbine blade superalloy, whereas below 530 K a hot worked 56 volume per cent composite had a greater impact strength than the superalloy.

Winsa, E. A.↗

Tungsten fiber-reinforced nickel superalloy

Tungsten fiber-reinforced nickel superalloy combines the strength of refractory metals with the oxidation resistance of superalloys. Knowledge of the relationship between fabrication technique, matrix compositions and fiber sizes minimized fiber-matrix reaction. Potential application includes high temperature turbine components.

Petrasek, D. W.↗