Capacity Fading Mechanism and Improvement of Cycling Stability of the SiO Anode for Lithium-Ion Batteries
Not Available
Engineering topics
Publications and source records attributed to Qin, Yan.
Not Available
The application of lithium-ion batteries in electric vehicles calls for decreased cost, increased energy density, increased power density, as well as low-temperature and fast-charging capability. In regard to fast charging, it is generally understood that it is the kinetic overpotential at the graphite anode that limits the cycling rate in modern commercial battery formulations. Here, we study the fast-charging capabilities of a series of graphite samples from commercial suppliers, as part of a materials validation effort at Argonne National Laboratory. Lastly, we combine materials characterization data from the raw samples with electrochemical characterization of graphite laminate electrodes in full-cell configuration to explore the causes of differences in rate performance and its impact on cycle life.
Here, lithium cobalt oxides (LiCoO 2 ) possess a high theoretical specific capacity of 274 mAh/g. However, cycling LiCoO 2 -based batteries to voltages greater than 4.35 V vs. Li/Li + causes significant structural instability and severe capacity fade. Consequently, commercial LiCoO 2 exhibits a maximum capacity of only ~165 mAh/g. Here we develop a doping technique to tackle this long-standing issue of instability and thus increase the capacity of LiCoO 2 . La and Al are concurrently doped into Co-containing precursors, followed by high-temperature calcination with lithium carbonate. The dopants are found to reside in the crystal lattice of LiCoO 2 , where La works as a pillar to increase the c-axis distance and Al as a positively charged center, facilitating Li + diffusion, stabilizing the structure and suppressing the phase transition during cycling, even at a high cut-off voltage of 4.5 V. This doped LiCoO 2 displays an exceptionally high capacity of 190 mAh/g, cyclability with 96% capacity retention over 50 cycles and significantly enhanced rate capability.
Various fluorescent probes have been developed to reveal the biological functions of intracellular labile Zn 2+ . Here we present Green Zinc Probe (GZnP), a novel genetically encoded Zn 2+ sensor design based on a single fluorescent protein (single-FP). The GZnP sensor is generated by attaching two zinc fingers (ZF) of the transcription factor Zap1 (ZF1 and ZF2) to the two ends of a circularly permuted green fluorescent protein (cpGFP). Formation of ZF folds induces interaction between the two ZFs, which induces a change in the cpGFP conformation, leading to an increase in fluorescence. A small sensor library is created to include mutations in the ZFs, cpGFP and linkers between ZF and cpGFP to improve signal stability, sensor brightness and dynamic range based on rational protein engineering and computational design by Rosetta. Using a cell-based library screen, we identify sensor GZnP1 which demonstrates a stable maximum signal, decent brightness (QY = 0.42 at apo state), as well as specific and sensitive response to Zn 2+ in HeLa cells (F max /F min = 2.6, K d = 58 pM, pH 7.4). The subcellular localizing sensors mito-GZnP1 (in mitochondria matrix) and Lck-GZnP1 (on plasma membrane) display sensitivity to Zn 2+ (F max /F min = 2.2). In conclusion, this sensor design provides freedom to be used in combination with other optical indicators and optogenetic tools for simultaneous imaging and advancing our understanding of cellular Zn 2+ function.
The effect of composition on the voltage fade phenomenon was probed using combinatorial synthesis methods. In compositions that have the general formula, (Li 2 MnO 3 ) a (LiNiO 2 ) b (LiMnO 2 ) c (LiCoO 2 ) d , where 0 ≤ a≤0.83, 0.15 ≤ b ≤ 0.42, 0 ≤ c ≤ 0.85, and 0 ≤ d ≤ 0.30 (a + b + c + d = 1), the dependence of features in the x-ray diffraction pattern and of voltage fade on composition were identified and mapped. The observed values of voltage fade indicated that it displayed some sensitivity to composition, but that the sensitivity was not large. The values of voltage fade were found to be amenable to statistical modeling. The model indicated that it may be possible to lower the value of voltage fade below 0.01% by adjusting the composition of the system; however, the composition is not expected to have the layered–layered structure.
Not Available
The migration of transition metal ions in the oxygen framework was recently proposed to be responsible for the continuous loss of average working potential of high energy density layered–layered composite cathodes for lithium-ion batteries. The potential migration pathway in a model material, LiNi 0.5 Mn 1.5 O 4 spinel, was investigated using in situ high-energy X-ray diffraction and in situ neutron diffraction during the solid state synthesis process. It was found that the migration of transition metal ions among octahedral sites is possible by using tetrahedral vacancies as intermediate sites. It was also suggested that the number of electrons in 3d orbitals has a significant impact on their mobility in the hosting oxygen framework.
Infection of Kaposi's sarcoma-associated herpesvirus (KSHV) is commonly occurred in AIDS patients. KSHV and HIV-1 act cooperatively in regulating infection with each other and in human carcinogenesis. Dendritic cells (DCs), as the pivotal cells in host immunity, may be modulated by both viruses, for immunoevasion and dissemination, therefore, the interaction between DCs and each virus has been a prior focus for pathogenesis elucidation. Here, we assessed the potential effect of KSHV on DC–HIV-1 interaction. We found that KSHV stimulation could promote maturation of monocyte-derived DCs (MDDCs) and impaired the ability of MDDCs to drive proliferation of resting CD4{sup +} T cells, demonstrating the immunosuppression induced by KSHV. More importantly, KSHV-stimulated MDDCs could capture more HIV-1 and efficiently transferred these infectious viruses to Hut/CCR5 T cell line. Our results reveal the novel modulation of DC-mediated HIV-1 dissemination by KSHV, and highlight the importance of studying DC–HIV-1 interaction to elucidate HIV/AIDS pathogenesis. - Highlights: ► KSHV impaired the ability of MDDCs to drive proliferation of resting CD4{sup +} T cells. ► KSHV stimulation matured MDDCs and enhanced HIV-1 endocytosis. ► KSHV stimulated MDDCs increased ICAM-1 expression and tighten contact with T cells. ► KSHV-stimulated MDDCs promoted HIV-1 trans-infection of CD4{sup +} T cells.
The successful development of Li-air batteries would significantly increase the possibility of extending the range of electric vehicles. There is much evidence that typical organic carbonate based electrolytes used in lithium ion batteries form lithium carbonates from reaction with oxygen reduction products during discharge in lithium-air cells so more stable electrolytes need to be found. This combined experimental and computational study of an electrolyte based on a tri(ethylene glycol)-substituted trimethylsilane (1NM3) provides evidence that the ethers are more stable toward oxygen reduction discharge species. X-ray photoelectron spectroscopy (XPS) and FTIR experiments show that only lithium oxides and no carbonates are formed when 1NM3 electrolyte is used. In contrast XPS shows that propylene carbonate (PC) in the same cell configuration decomposes to form lithium carbonates during discharge. Density functional calculations of probable decomposition reaction pathways involving solvated oxygen reduction species confirm that oligoether substituted silanes, as well as other ethers, are more stable to the oxygen reduction products than propylene carbonate. These results indicate that the choice of electrolyte plays a key role in the performance of Li-air batteries.