Reducing Operating Temperature in Photovoltaic Modules

Reducing the operating temperature of photovoltaic modules increases their efficiency and lifetime. This can be achieved by reducing the production of waste heat or by improving the rejection of waste heat. We tested, using a combination of simulation and experiment, several thermal modifications in each category. To predict operating temperature and energy yield changes in response to changes to the module, we implemented a physics-based transient simulation framework based almost entirely on measured properties. The most effective thermal modifications reduced the production of waste heat by reflecting unusable light from the cell or the module. Consistent with previous results and verified in this work through year-long simulations, the ideal reflector resulted in an annual irradiance-weighted temperature reduction of 3.8 K for crystalline silicon (c-Si). Our results illustrate that more realistic reflector concepts must balance detrimental optical effects with the intended thermal effects to realize the optimal energy production advantage. Methods improving thermal conductivity or back-side emissivity showed only modest improvements of less than 1 K. We also studied a GaAs module, which uses high-efficiency and high-subbandgap reflectivity to operate at an annual irradiance-weighted temperature 12 K cooler than that of a c-Si module under the same conditions.

14 SOLAR ENERGY↗

Laser lift-off scribing of the CZTSe thin-film solar cells at different pulse durations

Here, the transition to fully sized solar modules requires additional three-step laser structuring processes to preserve small-scale cell efficiencies over the large areas. The adjacent cell isolation (the P3 scribe) was found to be the most sensitive process in the case of laser induced damage. The laser induced layer lift-off mechanism seems to be a very attractive process for the P3 patterning, since almost all the laser affected material is removed by mechanical spallation. However, a laser induced layer spallation behavior together with scribe electrical validation under the different laser pulse durations was not investigated extensively in the past. Therefore, we report our novel results on the P2 and P3 laser lift-off processing of the Cu 2 ZnSn(S, Se 4 ) (CZTSe) thin-film solar cells covering the pulse duration range from 300 fs to 60 ps. Shorter sub-ps pulses enabled us to process smaller P2 and P3 craters, although the lift-off threshold fluences were higher compared to the longer ps pulses. In the case of the layer lift-off, the laser radiation had to penetrate through the layer stack down to the CZTSe/Mo interface. At shorter sub-ps pulses, the nonlinear effects triggered absorption of the laser radiation in the bulk of the material, resulting in increased damage of the CZTSe layer. The Raman measurements confirmed the CZTSe surface stoichiometry changes for shorter pulses. Furthermore, shorter pulses induced higher electrical conductivity of a scribe, resulting in lower photo-electrical efficiency during the mini-module simulation. In the case of the P3 lift-off scribing, the 10 ps pulses were more favorable than shorter femtosecond pulses.

14 SOLAR ENERGY↗

Cu2ZnSnSe4 Photovoltaic Absorber Layers Evaluated by Transmission X-Ray Microscopy Tomography: Composition Fluctuations on the Length Scale of Grains

The origins of open-circuit voltage deficits in Cu2ZnSnS(e)4-based solar cells have been an intense topic of research over the past few years as device efficiencies have never approached those of CuInGaSe2 based cells despite the materials sharing similar crystal and electronic structures. In this work, we use transmission X-ray microscopy tomography to investigate the length scales over which elemental fluctuations occur. We find and show evidence of micron-scale Cu to Zn anti-correlations over a previously inaccessible combination of resolution and sample size that is consistent with the length scale of grains in this material. This result yields further insight into the causes of the large open-circuit voltage deficits regularly seen in these devices as well as the challenges of achieving compositional homogeneity in this material.

composition fluctuations↗

Wild Band Edges: The Role of Bandgap Grading and Band-Edge Fluctuations in High-Efficiency Chalcogenide Devices

Band-edge effects - including grading, electrostatic fluctuations, bandgap fluctuations, and band tails - affect chalcogenide device efficiency. These effects now require more careful consideration as efficiencies increase beyond 20%. Several aspects of the relationships between band-edge phenomena and device performance for NREL absorbers are examined. For Cu(In, Ga)Se2 devices, recent increases in diffusion length imply changes to the optimum bandgap profile. The origin, impact, and modification of electrostatic and bandgap fluctuations are also discussed. The application of the same principles to devices based on CdTe, kesterites, and emerging absorbers (Cu2SnS3, CuSbS2), considering differences in materials properties, is examined.

14 SOLAR ENERGY↗

Development of Cu(In,Ga)Se2 Test Coupons for Potential Induced Degradation Studies

We report on the design, fabrication and accelerated testing of fully encapsulated small area coupons (approximately 7.5cm x 7.5 cm) for the purpose of researching potential induced degradation in Cu(In, Ga)Se2 based PV modules. The fabrication of these coupons enables the study of the solar cells and the materials used in PV module manufacturing such as top and bottom glass covers of different composition (soda-lime glass, high temperature glass, alkaline-free glass, etc), plastic-based top covers, ethylene vinyl acetate and edge seal encapsulation materials. The coupons can also be used to emulate framed and frameless modules that utilize either monolithically interconnected modules or singular cell type of modules. The design of the coupons, their fabrication, the materials used and their testing for 1000 hours under 85 degrees C and 85% RH conditions are presented.

14 SOLAR ENERGY↗

Minority Carrier Electron Traps in CZTSSe Solar Cells Characterized by DLTS and DLOS

We report observations of minority carrier interactions with deep levels in 6-8% efficient Cu2ZnSn(S, Se)4 (CZTSSe) devices using conventional and minority deep level transient spectroscopy (DLTS) and deep level optical spectroscopy (DLOS). Directly observing defect interactions with minority carriers is critical to understanding the recombination impact of deep levels. In devices with Cu2ZnSn(S, Se)4 nanoparticle ink absorber layers we identify a mid-gap state capturing and emitting minority electrons. It is 590+/-50 meV from the conduction band mobility edge, has a concentration near 1015/cm3, and has an apparent electron capture cross section ~10-14 cm2. We conclude that, while energetically positioned nearly-ideally to be a recombination center, these defects instead act as electron traps because of a smaller hole cross-section. In CZTSe devices produced using coevaporation, we used minority carrier DLTS on traditional samples as well as ones with transparent Ohmic back contacts. These experiments demonstrate methods for unambiguously probing minority carrier/defect interactions in solar cells in order to establish direct links between defect energy level observations and minority carrier lifetimes. Furthermore, we demonstrate the use of steady-state device simulation to aid in the interpretation of DLTS results e.g. to put bounds on the complimentary carrier cross section even in the absence its direct measurement. This combined experimental and theoretical approach establishes rigorous bounds on the impact on carrier lifetime and Voc of defects observed with DLTS as opposed to, for example, assuming that all deep states act as strong recombination centers.

14 SOLAR ENERGY↗

Comparison and Interpretation of Admittance Spectroscopy and Deep Level Transient Spectroscopy from Co-Evaporated and Solution-Deposited Cu2ZnSn(Sx, Se1-x)4 Solar Cells

Cu2ZnSn(S, Se)4 (CZTSe) is an earth-abundant semiconductor with potential for economical thin-film photovoltaic devices. Short minority carrier lifetimes contribute to low open circuit voltage and efficiency. Deep level defects that may contribute to lower minority carrier lifetimes in kesterites have been theoretically predicted, however very little experimental characterization of these deep defects exists. In this work we use admittance spectroscopy (AS) and deep level transient spectroscopy (DLTS) to characterize devices built using CZTSSe absorber layers deposited via both coevaporation and solution processing. AS reveals a band of widely-distributed activation energies for traps or energy barriers for transport, especially in the solution deposited case. DLTS reveals signatures of deep majority and minority traps within both types of samples.

14 SOLAR ENERGY↗

Intragrain charge transport in kesterite thin films—Limits arising from carrier localization

Intragrain charge carrier mobilities measured by time-resolved terahertz spectroscopy in state of the art Cu 2 ZnSn(S,Se) 4 kesterite thin films are found to increase from 32 to 140 cm 2 V -1 s -1 with increasing Se content. The mobilities are limited by carrier localization on the nanometer-scale, which takes place within the first 2 ps after carrier excitation. The localization strength obtained from the Drude-Smith model is found to be independent of the excited photocarrier density. This is in accordance with bandgap fluctuations as a cause of the localized transport. Lastly, charge carrier localization is a general issue in the probed kesterite thin films, which were deposited by coevaporation, colloidal inks, and sputtering followed by annealing with varying Se/S contents and yield 4.9%-10.0% efficiency in the completed device.

14 SOLAR ENERGY↗

Special Testing for Modules Deployed in Hot Use Environments - Are We Doing This in a Low-Cost Way?

The proposed new IEC standard will address the test temperature requirements in IEC 61215 (module design), IEC 61730 (module safety), IEC 62790 (junction box safety) and IEC 62852 (connectors), and will provide guidelines to modify temperature limits in four existing standards to better describe module performance in hotter climates. This workshop includes four presentations: Special Testing for Modules Deployed in Hot Use Environments - Are We Doing This in a Low-Cost Way?, Experimental Evidence, Why the highest temperatures are the most stressful to PV modules during thermal cycling, and Safety Aspects for Modules Deployed in Hot Use Environments.

14 SOLAR ENERGY↗

Damage in Monolithic Thin-Film Photovoltaic Modules Due to Partial Shade

The typical configuration of monolithic thin-film photovoltaic modules makes it possible for partial shade to place one or more cells in such a module in reverse bias. Reverse bias operation leads to high voltage, current density, and power density conditions, which can act as driving forces for failure. We showed that a brief outdoor shadow event can cause a 7% permanent loss in power. We applied an indoor partial shade durability test that moves beyond the standard hot spot endurance test by using more realistic mask and bias conditions and by carefully quantifying the permanent change in performance due to the stress. With the addition of a pass criterion based on change in maximum power, this procedure will soon be proposed as a part of the module-type qualification test. All six commercial copper indium gallium diselenide and cadmium telluride modules we tested experienced permanent damage due to the indoor partial shade test, ranging from 4% to 14% loss in maximum power. We conclude by summarizing ways to mitigate partial shade stress at the cell, module, and system levels.

14 SOLAR ENERGY↗

Defect chemistry and chalcogen diffusion in thin-film Cu{sub 2}ZnSnSe{sub 4} materials

Selenium diffusion in polycrystalline thin-film Cu{sub 2}ZnSn(S,Se){sub 4} (CZTSe) on molybdenum-coated soda-lime glass substrates was investigated by in situ monitoring of the molybdenum back-contact resistance during high-temperature selenization treatments. In these measurements, selenium diffusion through the CZTSe layer results in conversion of the molybdenum layer to MoSe{sub 2}, increasing the sheet resistance of the film stack. By monitoring the rate of MoSe{sub 2} formation as a function of annealing temperature, an activation energy of 0.5 ± 0.1 eV has been measured for selenium diffusion in CZTSe. The partial pressure dependence of chalcogen diffusion suggests that chalcogen vacancies are not the defect controlling chalcogen diffusion in thin-film CZTSe.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase identification and control of thin films deposited by co-evaporation of elemental Cu, Zn, Sn, and Se

Kesterite thin films [(i.e., Cu{sub 2}ZnSn(S,Se){sub 4} and related alloys] have been the subject of recent interest for use as an absorber layer for thin film photovoltaics due to their high absorption coefficient (>10{sup 4} cm{sup -1}), their similarity to successful chalcopyrites (like CuInxGa{sub 1-x}Se{sub 2}) in structure, and their earth-abundance. The process window for growing a single-phase kesterite film is narrow. In this work, we have documented, for our 9.15%-efficient kesterite co-evaporation process, (1) how appearance of certain undesirable phases are controlled via choice of processing conditions, (2) several techniques for identification of phases in these films with resolution adequate to discern changes that are important to device performance, and (3) reference measurements for those performing such phase identification. Data from x-ray diffraction, x-ray fluorescence, Raman scattering, scanning electron microscopy, energy dispersive spectroscopy, and current-voltage characterization are presented.