Search NASA⌕ Search

Engineering topics

Shepherd, Jenna

Publications and source records attributed to Shepherd, Jenna.

Biodegradable waterborne polyurethane-urea dispersion adhesives with high biocontent

Non-biodegradable petroleum-based plastic wastes have become a leading environmental concern, and new efforts are underway to prepare biobased and biodegradable replacements. For this work, we have explored the preparation of adhesives suitable for use in consumer products, and here we report the development of waterborne, biodegradable adhesives from biobased monomers resulting in adhesives exceeding 70% biocontent. Using water as the polymer medium, viscosity challenges and the use of volatile organic solvents are avoided. Material properties of the polyurethane dispersions, resulting films, and laminates produced showed M w ranging between 56,000 and 124,000. Lastly, the biodegradability of films and laminates was evaluated. The resulting metrics indicate that the adhesives produced meet the desired mechanical and biodegradability targets, indicating that high renewability content solvent-free polyurethane dispersions are a viable solution for lamination adhesives.

36 MATERIALS SCIENCE↗

Renewable low viscosity polyester-polyols for biodegradable thermoplastic polyurethanes

In the transition to renewably sourced, biodegradable polymers, the preparation of low viscosity polyester-polyols has posed a challenge for renewable polyurethane (PU) development. Low viscosity polyols not only reduce the requirement for high process temperatures but also decrease manufacturing time. In our efforts to incorporate increasing ratios of bio-based monomers into renewable PUs, we mixed diacids such as even carbon sebacic acid and odd carbon azelaic acid along with a renewable diol. This provided library of 2000 g/mol molecular weight polyester-polyols, and structures were established by 1 H and 13 C NMR analysis. The prepared polyester-polyols offered lower viscosity and enable lower fabrication temperatures to make TPUs, and their structure and material metrics were evaluated. The formation of TPUs is ascertained from FTIR and NMR analysis. The final TPUs displayed good physical and mechanical properties. Further, these TPUs exhibited T g in the range of -56.5 to -39.7°C, corresponding to TPU soft block structure, and T m between 98.3 and 105.1°C originating from the hard segment. Prepared TPUs exhibit excellent biodegradation under compost environmental conditions. These TPUs showed up to 57% decrease in molecular weight by GPC analysis after 9 weeks of biodegradation, and respirometer analysis displayed up to 97% biodegradation over 120 days.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗