Abstract

High strength superplastic superalloys are produced by extruding a pre-alloyed powder. The cast nickel base superalloy was remelted and converted to pre-alloyed powder by inert gas atomization. The superalloy shows high tensile strength and superplasticity and finds use in hot working and casting.