Improved high-temperature-strength nickel-base superalloy

Abstract

Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the strength of the strongest available cast nickel-base alloys. It is not subject to the formation of embrittling phases upon long time exposure at intermediate temperatures.