Superalloy microstructural variations induced by gravity level during directional solidification

Abstract

The Ni-base superalloy MAR-M246 (Hf) was directionally solidified during low gravity maneuvers aboard a NASA KC-135 aircraft. Gravity force variations during this process yielded a concomitant variation in microstructure and microsegregation. Secondary dendrite arm spacings are noted to be larger in the low-g portion; this, in turn, decreases the extent of interdendritic segregation. The amount of Hf in both the carbides and interdendritic eutectic increases as the gravity force diminishes. Fewer carbides are present in the low-g regions.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Johnston, M. H., Curreri, P. A., Parr, R. A., Alter, W. S.. 1985-09-01. Superalloy microstructural variations induced by gravity level during directional solidification. https://searchnasa.com/record/nasa%3A19850066123/superalloy-microstructural-variations-induced-by-gravity-level-during-directional-solidification

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Search NASA by Indiciae: BibTeX · RIS.