Nickel Base Superalloy Turbine Disk
Abstract
A low solvus, high refractory alloy having unusually versatile processing mechanical property capabilities for advanced disks and rotors in gas turbine engines. The nickel base superalloy has a composition consisting essentially of, in weight percent, 3.0-4.0 N, 0.02-0.04 B, 0.02-0.05 C, 12.0-14.0 Cr, 19.0-22.0 Co, 2.0-3.5 Mo, greater than 1.0 to 2.1 Nb, 1.3 to 2.1 Ta,3.04.OTi,4.1 to 5.0 W, 0.03-0.06 Zr, and balance essentially Ni and incidental impurities. The superalloy combines ease of processing with high temperature capabilities to be suitable for use in various turbine engine disk, impeller, and shaft applications. The Co and Cr levels of the superalloy can provide low solvus temperature for high processing versatility. The W, Mo, Ta, and Nb refractory element levels of the superalloy can provide sustained strength, creep, and dwell crack growth resistance at high temperatures.
Keep this discovery
Explore connections, maps & timelines
Gabb, Timothy P., Gauda, John, Telesman, Ignacy, Kantzos, Pete T.. 2005-12-13. Nickel Base Superalloy Turbine Disk. https://ntrs.nasa.gov/citations/20060009000
Cite the original work for its findings. Save a collection to share your selection of sources.