An Introduction to Atomic Layer Deposition

Abstract

Atomic Layer Deposition has been instrumental in providing a deposition method for multiple space flight applications. It is well known that ALD is a cost effective nanoadditive-manufacturing technique that allows for the conformal coating of substrates with atomic control in a benign temperature and pressure environment. Through the introduction of paired precursor gases, thin films can be deposited on a myriad of substrates from flat surfaces to those with significant topography. By providing atomic layer control, where single layers of atoms can be deposited, the fabrication of metal transparent films, precise nano-laminates, and coatings of nano-channels, pores and particles is achievable. The feasibility of this technology for NASA line of business applications range from thermal systems, optics, sensors, to environmental protection. An overview of this technology will be presented.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Dwivedi, Vivek H.. 2017-07-18. An Introduction to Atomic Layer Deposition. https://ntrs.nasa.gov/citations/20170006914

Cite the original work for its findings. Save a collection to share your selection of sources.