Evaluation of Superalloy 718 Additively Manufactured Lattice Blocks

Abstract

Lattice block structures made up of high temperature superalloys could offer advantages in density, efficiency, and tailored properties. Three candidate lattice designs were screened through additive manufacturing of superalloy 718. Laser powder bed fusion was applied with 718 powder to produce lattice blocks for three-dimensional octahedral unit cell designs of three heights. As-designed versus additively manufactured 718 lattices were compared, including structural dimensions, densities, defects, grain structures, crystallographic texture, and surface residual stresses. Manufactured lattice I diverged the most from its design, with both corner and center nodes merged into continuous columns. Manufactured lattice III came closest to its design, though the actual nodes and struts were still larger in cross section than in the design. Only modest grain coarsening and negligible chemical segregation were observed for all three designs, suggesting uniform thermo-physical and mechanical properties are possible. Significant tensile residual stresses were present at the surface of the manufactured blocks, with highest stresses in the building direction. Current findings indicate this concept could produce useful superalloy structures for high-temperature-capable static components requiring tailored density, and thermo-physical/mechanical properties.

Explore related subjects

Keep this discovery

BibTeXRIS

Timothy P Gabb, Aaron C Thompson, Christopher A Kantzos, Timothy M Smith, Richard B Rogers, Richard W Rauser, Richard E Martin. 2026-03-01. Evaluation of Superalloy 718 Additively Manufactured Lattice Blocks. https://ntrs.nasa.gov/citations/20260001478

Cite the original work for its findings. Save a collection to share your selection of sources.

Discover connections

Connections use source metadata and explicit phrase matches, not verified experimental comparisons.

KEEP EXPLORING

Related reports

A strong and ductile Super Kovar alloy via fully coherent nanoprecipitates

Emerging high-precision technologies demand materials with exceptional dimensional stability and mechanical robustness, as even microscopic thermomechanical deformation can cause functional failure. However, a fundamental trilemma exists: High strength, ductility, and low thermal expansion are mutually exclusive, as strengthening-induced lattice distortions compromise the spin-lattice coupling, which is essential for low thermal expansion. Here, we overcome this trilemma by designing “Super Kovar,” an Fe-Ni-Co-Al-Ta alloy, featuring fully coherent nanoprecipitates. It unifies a 1.0-gigapascal ultimate tensile strength and ∼39% elongation with a Kovar-grade thermal expansion of 3.81 × 10−6 K−1 (100 to 410 K). The key is a dense dispersion of L12 nanoprecipitates that form an almost strain-free coherent interface with the ferromagnetic matrix. Beyond providing precipitation strengthening, these coherent interfaces suppress intrinsic phonons of nanoprecipitates via elastic coupling while avoiding magnetic domain pinning to preserve the Invar effect of the matrix. This reduces the thermal expansion of the precipitates by 56% and achieves a fourfold enhancement in the strength-ductility product, establishing a paradigm for dimensionally stable, ultrastrong alloys.

Yu, Chengyi [University of Science and Technology