Janus Membranes via Diffusion-Controlled Atomic Layer Deposition

Abstract

The first use of atomic layer deposition (ALD) to produce Janus membranes is reported, with an example system consisting of a compositional gradient ranging from hydrophilic Al 2 O 3 on one face to hydrophobic poly(propylene) on the opposite face. Alternating pulses of trimethyl aluminum and water vapor lead to the growth of covalently bonded Al 2 O 3 conforming to the membrane pore surfaces. Precise control of ALD parameters significantly affects the surface wetting of the modified membrane face and the depth of Al 2 O 3 infiltration into the porosity. This depth control derives from slow precursor diffusion through the 200 nm membrane pores compared to much faster ALD surface reactions. For a given precursor exposure and purge time, increasing the number of ALD cycles decreases the water contact angle at the modified surface from hydrophobic to hydrophilic, until the water droplet is completely imbibed by the membrane. To demonstrate the utility of these Janus membranes, a hydrophilic/superaerophobic Janus treatment is shown to greatly reduce the size of air bubbles generated through the membrane, enabling faster mixing. This technique represents the first application of vapor-deposited covalently bonded metal oxides to form Janus membranes. Further opportunities are afforded by the ability to laterally pattern Al 2 O 3 across the membrane surface via physical masking.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Waldman, Ruben Z., Yang, Hao-Cheng, Mandia, David J., Nealey, Paul F., Elam, Jeffrey W., Darling, Seth B.. 2018-06-12. Janus Membranes via Diffusion-Controlled Atomic Layer Deposition. https://doi.org/10.1002/admi.201800658. https://searchnasa.com/record/osti%3A1466309/janus-membranes-via-diffusion-controlled-atomic-layer-deposition

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Search NASA by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗