Spherical nanoindentation on tungsten single crystal: The transition from source-controlled plasticity to bulk plasticity
Keep this discovery
Explore connections, maps & timelines
Patel, Hetal D., Lee, Seok-Woo. 2020-01-01. Spherical nanoindentation on tungsten single crystal: The transition from source-controlled plasticity to bulk plasticity. https://doi.org/10.1016/j.scriptamat.2019.08.038