Robust highly durable solid oxide fuel cell cathodes – Improved materials compatibility & self-regulating surface chemistry

Abstract

Solid oxide fuel cells (SOFCs) are electrochemical conversion devices that directly transform hydrogen or hydrocarbon fuels to electricity, with energy efficiencies as high as 90%, coupled with reduced emissions. Several factors, however, remain to be addressed when considering scale-up of SOFC technology, including the need to overcome decreased performance due to sluggish rates of the oxygen reduction reaction (ORR) at the cathode under reduced temperatures and susceptibility to degradation in performance from surface poisoning e.g. from chromia, while limiting the use of critical raw materials (lanthanides and transition metals) present in high performing mixed ionic electronic conducting electrodes like (La,Sr)CoO 3 (LSC). In this project we explored the key descriptors for determining ORR activity in SOFC electrodes and tried to recover performance degradation by applying them to SOFC electrodes. In order to do this, we first selected a model mixed ionic electronic conducting (MIEC) oxide, Pr-doped CeO 2 (Pr 0.1 Ce 0.9 O 2-δ , PCO), which is a chemically stable fluorite and free of inherent poison sources (e.g. Sr segregation in LSC) that potentially react with external impurities such as Cr-species vaporized from the interconnect. The three approaches originally planned in this project are as follows: 1) evaluation of scavenger exsolution characteristics, 2) study of scavengers gettering efficacy following Cr and Si poisoning and 3) integration of new compositions into porous electrodes. Among them, exceptional progress has been made in 2) and 3), especially understanding the role of surface infiltrants in impacting electrode performance and degradation of PCO materials. We found that the Smith acidity scale for binary oxides serves as a powerful descriptor for tuning and predicting the oxygen exchange kinetics on MIEC PCO surfaces. As a result, with infiltration with binary oxides, ranging from strongly basic (Li 2 O) to strongly acidic (SiO 2 ) onto the surface of porous PCO, it was possible to systematically vary the chemical surface exchange coefficient (k chem ) by 6 orders of magnitude! L i2 O increased k chem by nearly 1,000 times over that of pristine PCO, while SiO 2 decreased k chem by nearly the same factor. Strikingly, although the pre-exponential of k chem scales linearly with the acidity of the infiltrated binary oxide, there is nearly no change in the activation energy. With this insight, we attributed the origin of these dramatic changes in k chem values to the systematic increase and decrease in the surface electron density induced by infiltrated binary oxides. More interestingly, although both Cr 2 O 3 and SiO 2 were determined to be acidic by Smith, suggesting that this feature could likely be the primary reason that these compounds serve to poison the ORR on SOFC cathodes, the effect of poisoning could be subsequently tuned by adding multiple infiltrants and controlling their relative surface acidities. We also systematically examined the effect of serial infiltration of basic and acidic oxides. It turned out that serial infiltration of Li not only recovers approximately 20-fold degraded k chem of PCO by acidic Cr 2 O 3 but its k chem is enhanced even beyond that of the non-infiltrated PCO by more than three orders of magnitude. This was further verified with a screen-printing PCO symmetric cell in terms of the electrode performance (area-specific resistance, ASR) related to approach 3). These observations point to acidity as a key descriptor not only in tuning and predicting the ORR activity of SOFC cathodes that largely determines the overall performance of SOFC, but in mitigating and reactivating poisoned electrode performance. This work provides novel guidelines for making the electrode performance much more active and robust in SOFCs, which can further be applied to all applications requiring oxygen exchange reaction, such as electrolyzers, permeation membranes and gas sensors.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Tuller, Harry L., Seo, Han Gil. 2023-03-03. Robust highly durable solid oxide fuel cell cathodes – Improved materials compatibility & self-regulating surface chemistry. https://doi.org/10.2172/1960547

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Engineering Thermally Resilient and Kinetically Active Reversible Protonic Ceramic Cells via Interfacial Design

Achieving concurrent fast electrode kinetics and long-term thermo-mechanical durability remains a critical challenge for reversible protonic ceramic electrochemical cells (R-PCECs). Herein, we report an interfacial engineering strategy that integrates a perovs.kite-type PrBaRu0.1Co1.9O5+δ (PBRC) nanoparticle layer onto a PrBa0.5Sr0.5Co1.5Fe0.5O5+δ (PBSCF) substrate (PBRC-PBSCF), together with a modified pellet-assisted sintering approach to fabricate dense BaZr0.4Ce0.4Y0.1Yb0.1O3-δ (BZCYYb4411) electrolytes. The in situ reconstructed heterointerface enhances oxygen reduction/evolution reaction (ORR/OER) kinetics, promotes H2O adsorption/dissociation, and improves steam tolerance, as verified by electrochemical measurements and interfacial microstructural analyses. Density functional theory reveals that Ru-induced electronic modulation at the PBRC-PBSCF interface lowers the energy of oxygen vacancy formation and optimizes the position of the O 2p band center, thereby accelerating oxygen redox kinetics and stabilizing the interface. The resulting R-PCECs deliver an excellent peak power density of 1.112 W cm−2 and an electrolysis current density of −1.257 A cm−2 at 1.3 V in 3% H2O wet air at 600°C, with a reasonable faradaic efficiency. Furthermore, the cells demonstrate excellent stability, sustaining 100 h of thermal cycling (400–600°C, 200°C h−1) in both fuel cell and electrolysis modes, with 600 h of stability in electrolysis mode (600°C, −0.5 to −2 A cm−2).

30 DIRECT ENERGY CONVERSION↗

Development of a High-Efficiency Hybrid Dry Cooler System for sCO 2 Power Cycles in CSP Applications

This project addressed a major gap in supercritical CO 2 (sCO 2 ) power cycle research by focusing on the pre-cooler, a component that had received little attention despite its significant impact on cycle efficiency and plant economics. The team developed a compact dry cooler using brazed/diffusion-bonded microchannel passages paired with formed air-side fins, advancing the technology from TRL-2 toward commercial readiness. Compared to conventional fin-tube coolers, the design cuts installation footprint by roughly half for 10+ MWth systems while achieving better heat transfer and lower approach temperatures, translating into a projected LCOE reduction from 6.04 ¢/kWh to between 5.85 and 5.94 ¢/kWh. While fabrication of an aluminum MW-scale prototype revealed brazing and sealing challenges at larger scales, lessons learned informed a subsequent 1 MWth unit that was successfully built and delivered for integration into Sandia's Gen3 Particle Pilot Plant, advancing the technology to TRL-7 with a path toward TRL-8 pending successful testing.

30 DIRECT ENERGY CONVERSION↗

Pressurized Gas-Driven Elemental Redistribution Enables Ultrastable PtNi Catalysts for Heavy-Duty Vehicles

Gas-driven element redistribution, characterized by the preferential enrichment of one element at the surface relative to the bulk, is frequently observed in multicomponent alloys. Using L1 0 -ordered PtNi as a model system, we reveal that gas pressure plays a critical role in governing adsorption-driven surface composition during annealing in reducing gases: low pressure favors Pt surface segregation, while high pressure facilitates Ni surface enrichment. In this study, we developed a high-pressure nitriding (HPN) strategy that modulates the surface structure and composition of PtNi catalysts. The resulting HPN-PtNi exhibits enhanced performance and durability in membrane electrode assemblies for heavy-duty fuel cell applications, maintaining a high current density of 1.19 A cm −2 at 0.7 V after 90,000 voltage cycles. Through a combination of experimental and theoretical analyses, we reveal that the HPN process forms additional stabilizing Ni−N bonds and induces elemental redistribution with Ni surface enrichment and a Ni-deficient Pt subsurface. These modifications alter the atomic coordination environment of the ordered PtNi phase. This work presents a generalizable strategy to design robust and high-performing Pt-based catalysts by controlling gas-pressure-driven elemental redistribution and dopant incorporation.

30 DIRECT ENERGY CONVERSION↗