Abstract

All neutron radiography (NRAD) images of fuel pins in Argonne’s collection were originally generated using the NRAD imaging facility established in the Hot Fuel Examination Facility (HFEF) at Idaho National Laboratory (INL). The NRAD reactor facility was built in 1977 and has been operating since. The reactor is a TRIGA-type reactor operating at a power level of 250 kWth to provide a neutron source for radiography imaging. The reactor is equipped with two beam tubes (i.e., east beam tube and north beam tube) to guide the neutron beams to two radiography stations. The east radiography station is directly under the HFEF main cell and is dedicated for specimens already in the HFEF hot cell. The north radiography station is outside of the main HFEF hot cell and allows NRAD imaging of non-irradiated items. The NRAD images of EBR-II irradiated metallic fuel pins were taken in the east radiography station. Thermal neutrons have the capability to transmit through most materials and are ideal for NRAD imaging. However, because of their high thermal neutron absorption cross-section, fissile materials (e.g., highly-enriched nuclear fuels) may not be as transmissible to thermal neutrons. This is also the case for oversize specimens with extraneous thickness. Epithermal neutron imaging is therefore used as a complement to thermal neutron NRAD imaging. At HFEF’s NRAD facility, both thermal and epithermal neutrons can be used for NRAD imaging. Irradiated nuclear fuels emit high levels of γ radiation that can easily darken X-ray films, so direct exposure NRAD cannot be used to image them. Instead, an indirect NRAD imaging method was developed at HFEF’s NRAD facility. In this method, foils made of materials that can be activated by neutrons (i.e., with large neutron absorption cross section) are used to collect transmitted neutron signals. Then the activated foils are then placed against X-ray films and enclosed in a vacuum cassette so that the γ decay from the activated foils can produce images on the X-ray films. Then, general X-ray film processing procedures are used to digitize and store the images. By using different foil materials, different energy neutrons can be used for NRAD imaging. At the HFEF NRAD station, two types of films are commonly used: dysprosium (Dy) foils with thickness of 130 microns are used to capture thermal neutron signal, while indium (In) foils with thickness of 130 microns are used to capture epithermal neutron signal. A cadmium or gadolinium foil is put before the indium foil to work as a thermal neutron filter. The thermal and epithermal NRAD images can be taken simultaneously by using a Dy/Cd/In sandwiched foil combination. The typical NRAD exposure time is approximately 20 minutes. Then the exposed foils are transferred to film vacuum cassettes. The vacuum ensures that there is no gap between the foil and the film. The foil-to-film exposure time is at least three half-lives of the corresponding radioisotopes, which are 3 hours for In and 7.5 hours for Dy, respectively. Exposed films are processed using an automatic film processor to produce completed NRAD images.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Miao, Yinbin, Mo, Kun, Oaks, Aaron, Tomchik, Carolyn, Mei, Zhi-Gang. 2022-09-30. Specifications of EBR-II Neutron Radiography Method Description and Digitization Approach. https://doi.org/10.2172/1973262

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Evaluating transient fission gas release in high burnup light water reactor fuel during loss of coolant accident conditions via new capabilities

In this work, the role of transient fission gas release (tFGR) in the cladding burst behavior of high burnup fuel during a loss-of-coolant accident (LOCA) in commercial light water reactors was further investigated via the use of a new apparatus. During the LOCA-related temperature ramps of high burnup fuel, the release of fission gases exceeds the steady-state release observed under normal operating conditions. An enhancement was made to the Oak Ridge National Laboratory Severe Accident Test Station (SATS) to probe the various factors influencing tFGR. Experiments were performed on commercially irradiated, zirconium-clad uranium dioxide fuel, and this paper details the design of the experimental setup, the initial test results, and the subsequent post-test analyses. Notably, the first test on high burnup fuel demonstrated a LOCA-relevant tFGR of 5.3% from an unpressurized fuel segment. The ultimate tFGR was 10.7% for beyond LOCA conditions. A follow-up test on similar fuel revealed a tFGR of 12.6% under comparable conditions. Microstructural analysis and an analysis of the released gas provide some insight regarding the source of tFGR in the fuel. Finally, a grain boundary bubble model may aid in the interpretation of the results and offer a guide for future work.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of ceramic fuel powder packing fractions to support INFLUX

Triply periodic minimal surface (TPMS)-based structures show marked potential in novel nuclear reactor fuel designs, as their high surface area-to-volume ratio increases the efficiency of heat transfer out of the fuel, enabling safer, more innovative reactor designs. This milestone report addresses the role of dUO 2 powder processing route on the fill behavior of TPMS-based cladding shells to understand and advance the feasibility of manufacturing TPMS-based nuclear fuel forms. dUO 2 powder was processed through either a dry granulation route, varying consolidation pressure, or through milling, varying milling time, milling method and milled size distribution. The lowest tapped bulk densities (TBD), but best powder flowabilities, were obtained when testing unprocessed dUO 2 powder which was prone to self-agglomeration and formed low-density spheroids. The highest TBD and lowest flowabilities were obtained when using powder produced by hammer-milling dUO 2 powder to pass through a 200-mesh sieve, which led to particles with angular morphologies. Powder produced by dry granulation exhibited TBD that varied according to the consolidation pressure used to form the initial pellets and exhibited improved flowabilities when compared to hammer-milled material. Because of the large span of granule sizes formed as well as the irregular shape associated with the granules, a packing fraction of 0.69 was achieved, exceeding the analytical solution for random close packing of mono-sized spheres. TPMS polymer shells were loaded with unprocessed, granulated, and hammer-milled dUO 2 powders, and their qualitative packing behaviors were analyzed using x-ray computed tomography (xCT). TBDs calculated after loading TPMS polymer shells were 10-20% lower when compared to tapped bulk density measurements taken in a glass graduated cylinder, indicating a non-trivial impact on the tapped bulk density of either the TPMS channel size, TPMS channel surface material, powder cohesiveness, or a combination of the two parameters. A metallic zircaloy-4 TPMS shell will be loaded with hammer-milled dUO 2 powder upon receipt of the shell from Oak Ridge National Laboratory (ORNL) and shipped to Idaho National Labs (INL) for subsequent hot isostatic pressing (HIP) densification experiments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗