Scalable, low-cost synthesis of high volumetric capacity LiMn 0.5 Fe 0.5 PO 4 cathode for lithium-ion batteries

Abstract

A facile, scalable, wastewater-free synthesis of high energy density LiMn0.5Fe0.5PO4 (LMFP) cathodes with high electrode press density is achieved by employing the spinel LiMnFeO4 (LMFO) as a precursor.

Keep this discovery

BibTeXRIS

Reed, Seth [Materials Science and Engineering Program, Texas Materials Institute, The University of Texas at Austin, Austin, Texas 78712, USA], Scanlan, Kevin [Materials Science and Engineering Program, Texas Materials Institute, The University of Texas at Austin, Austin, Texas 78712, USA], Manthiram, Arumugam [Materials Science and Engineering Program, Texas Materials Institute, The University of Texas at Austin, Austin, Texas 78712, USA] (ORCID:0000000302379563). 2024-01-01. Scalable, low-cost synthesis of high volumetric capacity LiMn 0.5 Fe 0.5 PO 4 cathode for lithium-ion batteries. https://doi.org/10.1039/d4ta03438d

Cite the original work for its findings. Save a collection to share your selection of sources.

Discover connections

Connections use source metadata and explicit phrase matches, not verified experimental comparisons.

KEEP EXPLORING

Related discoveries

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Significant capacity loss has been observed across extended cycling of lithium-ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid-electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. Here, in this work, X-ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1-x) LiNi a Mn b Co c O 2 , with a+b+c=1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma-mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

25 ENERGY STORAGE

Single-crystal NMC622 from combustion-assisted solid-state synthesis: Tunable particle size, voltage-dependent stability, and Li-ion diffusion

Cost-effective and scalable synthesis of single-crystal lithium–metal-oxide cathodes with controlled size and morphology remains challenging for advancing high-performance lithium-ion batteries. Here, we demonstrate a solution combustion–assisted solid-state method for producing single-crystal NMC622 with tunable particle size at various lithium stoichiometries. Structural and electronic characteristics were probed using synchrotron-XANES, EXAFS, XRD and XPS, confirming well-defined coordination environments and phase purity up to Li ≈ 1.3. The electrochemical behavior of LixNMC (x = 1.0 and 1.3) single crystals was evaluated across 2.8–4.3 V and 2.8–4.7 V windows to elucidate the effects of lithium content and operating voltage. At 2.8–4.3V, Li1.3NMC exhibits higher initial capacity due to its larger lithium inventory, while Li1.0NMC shows superior long-term retention driven by its larger crystal size and reduced structural distortion. Increasing the cutoff voltage to 4.7 V enhances the initial capacity of both compositions by 17–25%, but long-term capacity retention ultimately converges to values comparable to those at 4.3 V due to voltage-induced degradation, where Li+ diffusion constant remains lying ranging from 10−12 –10−11 cm2s−1. Overall, this study establishes a scalable combustion-assisted route for synthesizing tunable single-crystal NMC622 and highlights the interplay between lithium stoichiometry, particle size, and voltage window in governing cathode stability.

Roy, Subrata C [Jackson State University]

Rinse-Free, Sodium-Efficient Synthesis of O3-Type Layered Oxide Materials Enabled by Acetate Precursors

Sodium-ion batteries (SIBs) are a sustainable alternative to lithium-ion systems for global electrification, with O3-type layered oxide cathodes offering high specific capacity and feasibility of scalable synthesis. Industrial co-precipitation synthesis of these cathodes typically uses transition metal sulfates, requiring extensive water rinsing to remove Na 2 SO 4 impurities, a process that consumes significant water and risks residual inactive phases if incomplete. Here, this work introduces a rinse-free, resource-efficient approach using metal acetate precursors. Residual sodium acetate in non-rinsed precursors decomposes during sintering to generate Na 2 CO 3 in situ, partially substituting an external sodium resource (e.g., NaOH and Na 2 CO 3 ) and reducing its consumption by ∼18–20%. Phase-pure O3-Na 1.0 Ni 1/3 Fe 1/3 Mn 1/3 O 2 (NFM111) cathodes synthesized via this method exhibit microstructure and electrochemical performance comparable to rinsed sulfate-derived counterparts, with initial capacities of 141 mAh g −1 at C/20 (7.5 mA g −1 ). By eliminating rinsing and minimizing sodium reagent use, this acetate-based route enhances sustainability and scalability of layered oxide production for SIBs.

acetate vs. sulfate