In-Situ Visualization of a Growing Brittle Crack in Aluminum Oxynitride Using Synchrotron X-Rays and the Double-Cleavage Drilled Compression Geometry

Abstract

Brittle fracture is difficult to study in situ due to the speed of a growing crack and the often-catastrophic nature of failure in brittle materials. As a result, the influence of microstructural considerations, such as orientation, grain boundary locations, and strain field, on the crack path remains poorly understood. Presented in this study is a method addressing this knowledge gap, which utilizes the double-cleavage drilled compression geometry to achieve quasi-stable fracture in aluminum oxynitride (AlON). Synchrotron X-ray micro-computed tomography is used to characterize the crack shape and length, while high-energy diffraction microscopy provides information on the strains, orientations, and shapes of grains in the microstructure surrounding the crack tip. During testing, the crack grew in discrete and irregular jumps while the fracture toughness falls within reported ranges. The crack in AlON is found to have no greater tendency to crack intergranularly as compared to transgranularly, and grains which are cracked transgranularly do not display a trend in orientation or stress when compared to those around which the crack followed a grain boundary. The high resolution of the crack path and microstructural data provides a path forward for modeling and understanding 3D brittle fracture.

Keep this discovery

BibTeXRIS

Gorske, Sara F., Park, Jun-Sang, Kenesei, Peter, Sharma, Hemant, Almer, Jonathan (ORCID:0000000219002271), Voorhees, Peter, Faber, Katherine T.. 2026-06-15. In-Situ Visualization of a Growing Brittle Crack in Aluminum Oxynitride Using Synchrotron X-Rays and the Double-Cleavage Drilled Compression Geometry. https://doi.org/10.1016/j.actamat.2026.122213

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related discoveries

Visualizing Crystallization Dynamics and Transformation Pathways of Disordered Rocksalt Oxides During Thermally Activated Sol–Gel Synthesis

Sol–gel synthesis is a wet-chemical processing route for fabricating functional materials with control over composition and microstructure at relatively low temperatures compared to conventional solid-state synthesis. While sol–gel process initiates with intermixed molecular precursors, the early-stage nucleation pathways are insufficiently understood. Here, in this study, the chemical and structural transformation of ion disordered rocksalt (DRX) Li 1.2 Mn 0.4 Ti 0.4 O 2 (LMTO), a promising cathode material for lithium batteries, is studied by multiscale characterizations. In situ heating transmission electron microscopy (TEM) using a liquid cell visualizes and identifies crystallization pathways at the nanoscale. While some regions follow a classical multi-step transition through thermodynamically stable intermediates, others exhibit a kinetic shortcut via a localized amorphous matrix to directly form the DRX structure. Macroscale Fourier transform infrared spectroscopy corroborates the findings and reveals that transition metal ions are more strongly incorporated into the acetate-coordinated network than lithium. Although in situ heating TEM captures diverse local transformation pathways, in situ synchrotron X-ray diffraction indicates that the macroscopic transformation proceeds predominantly through spinel LMTO and lithium titanates toward DRX-LMTO. The findings uncover the spatiotemporal chemical and structural transformations in sol–gel derived DRX-LMTO materials, and call for fine-tuning of such sol–gel chemistries to manipulate the crystallization pathways and achieve target material homogeneity more efficiently.

cathode material

Impact of the Annealing Temperature on the Local Se Distribution and Optical Properties in CdSexTe1-x Solar Cells by Multimodal X-ray Microscopy

The introduction of Se in CdTe solar-cell absorbers has led to multiple beneficial effects in the devices, including an increased short-circuit current and an extended charge-carrier lifetime. A critical manufacturing step of CdSexTe1-x solar cells is CdCl2 annealing at high temperatures, during which Se diffuses through the absorber layer. Understanding the local Se distribution in the absorber and its impact on optical properties of the material is key for the further development of this thin-film solar cell technology. In a multimodal x-ray scanning microscopy approach, we investigated the impact of the annealing temperature of CdSexTe1-x solar cells on the Se distribution and on optical characteristics of the material. For this purpose, we exploited an upgraded x-ray excited optical luminescence (XEOL) detection unit that enables simultaneous spectrally and temporally resolved XEOL mapping at synchrotron facilities that are ideal for studying thin-film solar-cell materials with hard x-rays featuring high penetration depth and lateral resolution.

14 SOLAR ENERGY

Revealing key structures for reversible sulfur redox in amorphous polymeric sulfur

Amorphous polymeric sulfur cathodes, such as sulfurized polyacrylonitrile (SPAN), enable high-energy lithium-sulfur batteries without cobalt or nickel, leveraging abundant sulfur. However, the limited in situ understanding of their synthesis and electrochemistry has impeded targeted optimization. Here, in this study, we integrate operando high-energy total scattering with sulfur K-edge X-ray absorption spectroscopy to monitor SPAN's formation and cycling in real time. Our results show that S-C bond formation halts further fusion of cyclized polyacrylonitrile, fostering π-π stacking and a transition from long-chain to short-chain sulfur-critical for reversible sulfur redox. These features synergistically minimize polysulfide dissolution and charge-transfer resistance, enabling optimized SPAN to achieve high capacity retention over 1,000 cycles. Operando X-ray absorption spectroscopy reveals that residual protons drive thiol-thione tautomerism, with lithium replacement during the first discharge causing ~20% irreversible capacity loss. To enhance performance, minimizing -NH groups and expanding pyridine networks are key. These findings transform SPAN optimization from empirical tuning to mechanism‑guided engineering and point the way towards sulfur loadings and energy densities competitive with state‑of‑the‑art Li‑ion cathodes.

25 ENERGY STORAGE