Electrocatalytic cleavage of lignin model dimers using ruthenium supported on activated carbon cloth

Biomass lignin is the largest natural source of renewable aromatic compounds, creating an opportunity for its use as a feedstock provided that deconstruction and upgrading methods become available. Valorization of lignin is challenging because its complex structure is naturally recalcitrant to biological degradation. Deconstruction of this amorphous cross-linked polymer requires cleavage of aryl ether bonds, which account for more than half of the linkages between lignin's phenylpropanoid building blocks. High temperature cracking of lignin is possible via pyrolysis, but linkages such as 4-O-5 bonds are resistant to thermal degradation. Electrocatalytic hydrogenation offers a mild alternative; operated at low temperature and atmospheric pressure, it cleaves ether bonds while saturating aromatic rings with in situ generated hydrogen. To investigate the use of catalytic ruthenium supported on activated carbon cloth to cleave 4-O-5 bonds, model compounds that exhibit this linkage were selected, including 3-phenoxyphenol, 4-phenoxyphenol, 3-phenoxyanisole, and 3-phenoxytoluene. The two phenols, 3-phenoxyphenol and 4-phenoxyphenol, were cleaved and hydrogenated to form cyclohexanol. 3-Phenoxyanisole and 3-phenoxytoluene were also cleaved but with lower conversion rates and cyclohexanol yields. Alkaline electrolyte solutions showed the highest cyclohexanol yields for both substrates. Increasing substrate concentrations from 10 mM to 40 mM increased faradaic efficiency to 25%, while decreasing current density from 100 mA (33.33 mA cm -2 ) to 20 mA (6.67 mA cm -2 ) greatly improved the faradaic efficiency to 96%.

09 BIOMASS FUELS↗

Fluorescent aggregate structure revealed in bisphenol F epoxy thermoset

Bisphenol F (BPF) epoxy resin is a prepolymer component of thermosets used in construction of reinforced carbon fiber composites (RCFC). The fluorescence of this resin can provide information about chemical and structural alterations of the thermoset from thermal or mechanical damage. While some work has investigated the fluorescence spectra of bisphenol A epoxy resin, a structural analog of BPF, none have studied BPF. The purpose of this study is to investigate the baseline fluorescence spectra of the BPF epoxy resin for features that could be utilized for monitoring damage and structural alterations. Bisphenol F epoxy resin was found to have two emission peaks with a broad peak centered at 410 nm and a sharp peak centered at 550 nm. The broad emission peak was identified as the fluorescence from BPF epoxy monomer while the sharp emission peak was found to be from an aggregate structure present in the epoxy resin. It is hypothesized that this structure is an H-aggregate based on the emission features and structural stability of the aggregate compared to the alternative J-aggregate which was determined via density functional theory calculations. The H-aggregate was found to persist into one of the cured thermoset formulations evaluated but was lost when exposed to elevated temperatures below thermal degradation of the thermoset. This loss of aggregate structure was due to polymer network rearrangement. This new fluorescence signature can be used as an indicator of polymer network rearrangement from thermal exposure which may alter the expected material performance and precede thermal degradation.

36 MATERIALS SCIENCE↗

Synergistic Enzyme Mixtures to Realize Near-Complete Depolymerization in Biodegradable Polymer/Additive Blends

Embedding catalysts inside of plastics affords accelerated chemical modification with programmable latency and pathways. Nanoscopically embedded enzymes can lead to near-complete degradation of polyesters via chain-end mediated processive depolymerization. The overall degradation rate and pathways have a strong dependence on the morphology of semicrystalline polyesters. Yet, most studies to date focus on pristine polymers instead of mixtures that contain additives and other components despite their nearly universal use in plastic production. Here, for this study, additives are introduced to purposely change the morphology of polycaprolactone (PCL) by increasing the bending and twisting of crystalline lamellae. These morphological changes immobilize chain ends preferentially at the crystalline/amorphous interfaces and limit chain-end accessibility by the embedded processive enzyme. This chain-end redistribution reduces the polymer-to-monomer conversion from >95% to less than 50%, causing formation of highly crystalline plastic pieces, including microplastics. By synergizing both random chain scission and processive depolymerization, it is feasible to navigate morphological changes in polymer/additive blends and to achieve near-complete depolymerization. The random scission enzymes in the amorphous domains create new chain ends that are subsequently bound and depolymerized by processive enzymes. Present studies further highlight the importance to consider how the host polymer's morphologies affect the reactions catalyzed by embedded catalytic species.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of an In-Situ Method for Cable Condition Monitoring in Nuclear Power Plants (SBIR Phase IIB Final Report)

This is the final report of a Small Business Innovation Research (SBIR) project that Analysis and Measurement Services Corporation (AMS) has conducted for the U.S. Department of Energy (DOE) over a seven-and-a-half year period (February 2013 through April 2020 with the awards of Phase I, Phase II and Phase IIB projects). The goal of the project was to design, develop, validate, and demonstrate a technique for in-situ testing of cable insulation polymers that will identify, locate, and provide the degree of aging for cables commonly used in nuclear power plants. During the Phase I project, AMS established that the frequency domain reflectometry (FDR) technique can successfully identify and measure cable insulation degradation that can be trended with aging. In Phase II, AMS performed extensive cable aging studies to correlate FDR measurements with other laboratory condition monitoring techniques and developed aging condition categories to quantify the severity of insulation degradation. In Phase IIB, the project expanded the research to include a wider variety of cable polymers that are used in the commercial nuclear power industry. This work also involved developing acceptance criteria to objectively assess age-related cable degradation while sharing the results of this research with industry, academia, and national laboratories to advance the state of the art in cable aging management technologies. The products developed under this research project provide the nuclear industry with an effective condition monitoring tool to support safe and long-term plant operation. Throughout the project, collaborations and support were received from a variety of industry organizations and individuals including DOE National Laboratories as well as nuclear plant utilities and several other industry experts and cable manufacturers. Contributions from these organizations included the donation of new cables, naturally aged cables, and research collaboration. The validation and commercialization of the products of this project were achieved through opportunities to test and demonstrate the technologies’ capabilities on-site at nuclear power generation and research facilities as well as in the laboratory alongside industry peers and cable testing service companies. The research resulted in a technology that can be used to identify, locate, and quantify age-related degradation in several types of cable polymers. This included developing software and hardware as well as the methodology for using the FDR technique to assess age-related degradation of installed cables. The technology developed under this project can provide nuclear plant management, engineers, and technicians with an in-situ electrical test method to determine if in-service cables need to be replaced, monitored on a periodic basis, or show no evidence of significant age-related degradation that may require action. Near the end of this Phase IIB project, the FDR product was sold to a nuclear power utility in South Korea. This sale of a dedicated aging assessment tool is the beginning of a comprehensive contract with the expectation of twelve (12) units sold to that country. Additionally, the FDR technology has been sold to several industry organizations including a nuclear research institute and the Diablo Canyon nuclear power plant. This technology is also being leased by other nuclear industry service companies for incorporation into aging management programs. The cable testing technology that was developed under this project was also integrated into a comprehensive cable aging assessment service that is being offered to the nuclear industry at the request of U.S. nuclear utilities and is currently part of onsite testing services provided by AMS.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Continued Testing and Modeling of the AirSquared All-Metal Tritium Scroll Pump

The implementation of fusion energy requires the processing of the deuterium-tritium mixture used to fuel the reaction. Many gas processing operations require either a gas-motive force or a pressure gradient across a system; both are achieved using vacuum pumps. However, because of the material challenges of working with tritium, specialized pumps are required that use only metal on wetted surfaces. This prevents tritium retention and degradation of materials such as oils and polymers and reduces the generation of tritiated waste. Typical gas handling systems for tritium operations involve metal bellows pumps, all-metal scroll pumps, and metal turbomolecular pumps, depending on the pressure requirements. With the industry standard Normetex Type 15 m 3 /h (typically referred to as the Normetex 15) pump no longer available, the fusion market requires viable alternatives. In this study, we test an American-made pump, the AirSquared V16H034A-C01, and compare its performance to the Normetex. A performance model of the AirSquared pump is also produced, which can be applied to general process models to generate an accurate description of pressures and flows through various unit operations.

08 HYDROGEN↗

Durability evaluation of a Fe–N–C catalyst in polymer electrolyte fuel cell environment via accelerated stress tests

In this work, an “atomically-dispersed” iron-nitrogen-carbon (Fe–N–C) catalyst was used to provide a systematic comparison of platinum group metal (PGM)-free electrocatalyst degradation as a function of accelerated stress tests (ASTs) in an acidic polymer electrolyte fuel cell (PEFC). It was determined that the majority of catalyst degradation was caused by cell operation in presence of O 2 . In contrast, potential cycling of the Fe–N–C-containing cathode under inert atmosphere over typical PEFC cathode operation from 0.95 to 0.6 V had little to no effect. The increase in kinetic overpotential is shown to be the major source of the PEFC performance decrease during the ASTs. These results continue to showcase the need for development of robust PGM-free electrocatalysts in concert with improved electrochemical performance.

25 ENERGY STORAGE↗

Solubility-limited depolymerization kinetics in the glycolysis of carbonyl-containing polymers

Chemical recycling of condensation polymers is often rationalized on the basis of the intrinsic reactivity of ester and carbonate functional groups. However, under heterogeneous conditions relevant to plastic waste processing and environmental degradation, bulk depolymerization rates often diverge from trends predicted by homogeneous chemistry. Here, we investigate how polymer–solvent compatibility, catalyst strength, and phase behavior govern the heterogeneous glycolysis of carbonyl-containing polymers. Using poly(ethylene terephthalate) (PET), glycol-modified PET (PETG), and bisphenol-A polycarbonate (PC) as model systems, we examine depolymerization kinetics at 180 °C with ethylene glycol and bisphenol A as diols under both amphoteric organosalt (TBD : MSA) and strong base (TBD) catalysis. Despite substantial differences in crystallinity and glycol uptake, PET and PETG depolymerize at comparable rates under organosalt catalysis, while PC depolymerizes significantly more slowly under identical conditions. Time-resolved molecular weight analysis and thermal characterization demonstrate that these rate differences do not arise from crystallinity, swelling, or inherent carbonyl reactivity, but instead reflect solubility-limited kinetics that constrain the transition from heterogeneous to homogeneous reaction regimes. When polymer solubility is low, depolymerization remains heterogeneous and slow; when solubility is enhanced—either through increased polymer–diol compatibility or stronger base catalysis—rapid homogeneous depolymerization is observed, reversing apparent reactivity trends. These results establish solubility and phase behavior as primary determinants of depolymerization kinetics in heterogeneous polymer recycling systems. By demonstrating how catalyst selection and solvent compatibility can expose or overcome solubility limitations, this work provides mechanistic insight to design more energy-efficient and selective chemical recycling processes. More broadly, these findings suggest that polymers with limited solvent or water compatibility may resist chemical degradation in the environment, favoring fragmentation and persistence as micro- and nanoplastics. Understanding solubility-controlled depolymerization offers a pathway toward more sustainable polymer design and end-of-life chemical recovery.

Watson-Sanders, Shelby [Department of Chemistry, U↗

A Micro-Mechanical Constitutive Model to Predict Hygrothermal Aging of Cross-Linked Polymers

Abstract A multi-physics material model is presented to describe the effects of temperature, oxygen, and humidity on the constitutive response of cross-linked polymers. The effect of hygrothermal damage on the mechanical integrity of the polymer matrix can be considered as the result of damage accumulation of two independent aging mechanism namely, i) thermo-oxidative, and ii) hydrolytic aging. In order to capture the mutual effects of thermo-oxidative and hydrolytic aging, an assumption has been made that each of the aging phenomenon can be superposed to each other. In fact, each of them works independently and as a result, they can compete with each other. Utilizing the theory of network decomposition, all phenomena and their correlation were modeled and thus, the strain energy function of the polymer matrix is written with respect to four independent mechanisms, i) the shrinking original matrix that has neither been attacked by water nor oxygen, ii) conversion of the first network to two new network due to the reduction and formation of cross-links, and iii) energy loss from network degradation due to attack of the water molecules to polymer active agents. Moreover, the proposed model is micro-mechanically based and is mainly relevant on thin samples due to our underlying assumption of homogeneous diffusion of oxygen and water throughout the matrix. The model has been validated against extensive data-sets obtained from experiments we specifically designed for concept validation.

Bahrololoumi, Amir↗

Tuning the Mechanical Properties of a Polymer Semiconductor by Modulating Hydrogen Bonding Interactions

Conjugation breakers (CBs) with different H-bonding chemistry and linker flexibility are designed and incorporated into a Diketopyrrolopyrrole (DPP)-based conjugated polymer backbone. The effects of H-bonding interactions on polymer semiconductor morphology, mechanical properties and electrical performance are systematically investigated. We observe that CBs with H-bonding self-association constant >0.7 or denser packing tendency are able to induce higher polymer chain aggregation and crystallinity in as-casted thin film, resulting in higher modulus and crack on-set strain. Additionally, the rDoC (relative degree of crystallinity) of the stretched thin film with the highest crack on-set strain only suffers a small decrease, suggesting the main energy dissipation mechanism is the breakage of H-bonding interactions. By contrast, other less stretchable polymer films dissipate strain energy through the breakage of crystalline domains, indicated by drastic decrease in rDoC. Furthermore, we evaluate their electrical performance under mechanical strain in fully stretchable field-effect transistors. The polymer with the highest crack on-set strain has the least degradation in mobility as a function of strain. Overall, these observations suggest that we can aptly tune the mechanical properties in polymer semiconductors by modulating intermolecular interactions, such as H-bonding chemistry and linker flexibility. Such understanding provides molecular design guidelines for future stretchable semiconductors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evolved Gas Analysis–Mass Spectrometry Exposes Polymer Network Structures

Polymer network structures in epoxy thermosets play an important role in the final thermoset material properties. However, analytical characterization of these network structures is difficult due to their amorphous nature. In this work, the application of evolved gas analysis–mass spectrometry (EGA-MS) to characterize the polymer network structures of bisphenol A (BPA)-based thermosets is demonstrated. Analytical characterization of the polymer network structures is accomplished by monitoring the Product-Specific Kinetics (PSK) of BPA monomer formation during thermal degradation investigations. We relate observed differences in the activation energy (E a ) of BPA monomer formation to the local packing environment around the BPA monomer units within the polymer network. Variations in the local environment related to the polymer networks manifest qualitatively as broadening in the thermal profile of the BPA monomer evolution and quantitatively as changes in the activation energy (E a ). Three BPA thermoset formulations were investigated; two amine-cured thermoset with 4,4′-diaminodiphenylmethane (DDM) or poly(propylene glycol) bis(2-amino-propyl ether) (PPG400) and a homopolymerized thermoset via curing with Epikure 3253 catalyst (3253). Results revealed that the 3253 thermoset contained two distinct packing densities in the polymer network, while DDM and PPG400 thermosets had uniform distributions of packing densities. Results from the DDM thermoset revealed a gradually decreasing E a , while the apparent E a of PPG400 was consistent over the entire degradation. Furthermore, these differences in E a were concluded to stem from the flexibility of the corresponding polymer networks and the ability of the network components to rearrange and occupy formed voids. Due to the minimal sample required for analysis (100–200 μg), this EGA-MS technique has great potential for postproduction evaluation of composite parts to identify changes in the polymer networks from use and aging, which could signal compromised performance.

Degradation↗

Influence of temperature on accessible pyrolysis pathways of homopolymerized bisphenol A/F epoxies and copolymers

Understanding the thermal pyrolysis of epoxies and their copolymers is important for identifying structural changes resultant from thermal transients, enabling identification of failure modes of high-performance composite materials. This work expands our understanding of the thermal pyrolysis of cured epoxies and the role of temperature and composition on products, pathways, and relative rates. Numerous researchers have explored the pyrolysis of bisphenol A (BPA) epoxy. Significantly fewer have studied bisphenol F (BPF), and copolymers of BPA and BPF have been neglected. In this work, a pyrolysis gas chromatography mass spectrometer (PY-GC-MS) was used to investigate the degradation mechanism of homopolymerized BPA, BPF epoxies and their copolymers. Additionally, for polymer identification, pyrolysis >450 °C resulted in the most extensive fragmentation and is useful for material identification, though lower temperatures show different degradation product profiles that provide mechanistic insight into thermal degradation pathways. Temperature greatly influences the accessible pyrolysis pathways of BPA, revealing dual mechanisms of formation for products p-isopropylphenol and p-isopropenylphenol. For BPF at low pyrolysis temperature the p,p-bisphenol F isomer is produced at significantly lower relative abundance compared to the abundance at higher temperatures tested, but production of the other two isomers changes little with respect to temperature. This suggests the epoxy components consisting of the p,p-bisphenol F isomer have higher thermal stability. Overall, the copolymer epoxies were found to have similar degradation products in stoichiometric distributions. The major exception was the formation of the p,p-bisphenol F isomer, which shows evidence of thermal stabilizing effects from addition of BPA epoxy.

36 MATERIALS SCIENCE↗

Photooxidative Upcycling of Post-Consumer Polystyrene Plastics into Phenol Using Eosin Y

Phenol is a commodity chemical frequently used in the manufacturing of resins, pharmaceuticals, and polymers. Yet, its industrial production from cumene requires harsh oxidative conditions followed by the Hock rearrangement. Polystyrene (PS) is a widely manufactured commodity polymer; however, it is among the least recycled plastics. Intriguingly, it is composed of contiguous cumene repeats that could serve as a phenol source, enhancing its value as a waste material. In this work, we leverage the similarity between cumene and PS to drive phenol production via a mild photooxidative HAT mechanism. Using Eosin Y under blue light irradiation and atmospheric pressure of oxygen, commercial PS resin was converted into hydroperoxyl PS. Subsequent acid-catalyzed Hock rearrangement afforded up to 21% yield of phenol. The photooxidation system was successfully applied to 8 post-consumer PS plastics, achieving phenol yields up to 23%, comparable to those of the current industrial Hock process. Our method introduces a mild catalytic strategy for converting post-consumer PS into phenol, offering a potential pathway for PS waste valorization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Consequences of utilizing a redox-active polymeric binder in Li-ion batteries

Development of new polymeric binders can help enable the use of silicon-rich anodes in Li-ion batteries, by providing stronger adhesion to the active material particles. The compositional features that improve interfacial interactions and mechanical properties can often impart electronic conductivity and redox activity to these polymers, which are generally seen as beneficial to cell performance. Alternatively, it is also possible that the addition of charge-transferring centers to the electrode can accelerate cell degradation. Here, we use an aromatic polyimide (∼320 mA h/g of reversible capacity) to explore how a redox-active conductive polymer can affect cell performance. We demonstrate that the lithiated polymer is less stable than the traditional binders upon storage, leading to increased rates of calendar aging. Furthermore, we determine that the adhesion properties of the polymer deteriorate upon repeated cycling, to an extent that is proportional to the degree of delithiation of the binder. More critically, we establish that progressive degradation of the redox behavior of the polymer leads to the release of “extra” Li + into the cell, which can give the false perception of good performance even under conditions of poor stability. In conclusion, our work suggests that redox-active conductive binders can sometimes be detrimental to cell performance, and that works evaluating new polymers must include careful experimental validation under realistic conditions.

25 ENERGY STORAGE↗

Improved Stability and Cyclability of Ceramic Solid Electrolyte by Coating Polymer

Rechargeable all-solid-state lithium (Li) metal batteries show better safety and energy density compared to commercial Li-ion batteries using liquid electrolyte. As the key component of Li metal batteries, ceramic solid-state electrolyte has attracted great interest because of its high ion conductivity and great potential in interfacing with Li metal. Ceramic electrolyte has a more stable interface with Li metal than liquid electrolyte, but chemical reaction and Li dendrite growth at the electrolyte/Li interface are still significant, which causes device degradation and failure by cycling of Li plating and stripping. Unlike ceramic electrolyte, polymer electrolyte has a relatively stable interface with Li metal and better mechanical flexibility. Therefore, we introduced a polymer electrolyte coating to protect the ceramic electrolyte from direct contact with Li metal. The galvanotactic cycling Li plating/striping data on the devices with (without) the coating illustrates increased (decreased) overall conductivity and cyclability of the test cell by the cycling. Nanometer-scale ionic-transport imaging, based on atomic force microscopy, shows that cycling degrades the ceramic-only electrolyte by partially blocking ionic transport in areas; in contrast, cycling on the polymer-coated electrolyte improves ionic conductivity. Compared with the ceramic-only electrolyte, this novel polymer electrolyte coating on ceramic electrolyte shows less degradation when in contact with Li metal.

25 ENERGY STORAGE↗

Probing the Kinetic Origin of Varying Oxidative Stability of Ethyl- vs. Propyl-spaced Amines for Direct Air Capture

Amine-based adsorbents are promising for direct air capture of CO 2 , yet oxidative degradation remains a key unmitigated risk hindering wide-scale deployment. Borrowing wisdom from the basic auto-oxidation scheme, insights are gained into the underlying degradation mechanisms of polyamines by quantum chemical, advanced sampling simulations, adsorbent synthesis, and accelerated degradation experiments. The reaction kinetics of polyamines are contrasted with that of typical aliphatic polymers and they elucidate for the first time the critical role of aminoalkyl hydroperoxide decomposition in the oxidative degradation of amino-oligomers. The experimentally observed variation in oxidative stability of polyamines with different backbone structures is explained by the relationship between the local chemical structure and the free energy barrier of aminoalkyl hydroperoxide decomposition, suggesting that its energetics can be used as a descriptor to screen and design new polyamines with improved stability. In conclusion, the developed computational capability sheds light on radical-induced degradation chemistry of other organic functional materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dual-Wavelength Simultaneous Patterning of Degradable Thermoset Supports for One-Pot Embedded 3D Printing

Vat photopolymerization (VP) techniques have enabled the fabrication of complex geometries while balancing high precision and fast processing times. 3D printed objects are traditionally built layer-by-layer with newly cured layers being structurally supported by previous ones. Fabricating unsupported features such as overhangs and arches risks misalignment and sagging, limiting the range of accessible designs. To overcome this issue, support structures are fabricated along with the primary object as temporary scaffolds that provide stability and conserve print fidelity. For VP specifically, patterning dissolvable sacrificial supports is attractive to avoid manual removal after printing. In this study, we demonstrate a base-degradable thermoset to pattern print supports in a one-pot formulation along with the primary structural material. Efficient printing is enabled using a dual-wavelength negative imaging (DWNI) DLP printer that patterns the degradable thermoset with visible light and the permanent network with UV light, which are simultaneously projected using a single digital micromirror device (DMD). Printed objects undergo thermal postprocessing to enhance the final conversion of the primary material, after which thermoset supports are degraded in a basic, aqueous solution. This approach provides a robust method for the dual-wavelength patterning of sacrificial thermoset supports, broadening the range of accessible 3D printable materials and geometries.

3D printing↗

Identification of durable and non-durable FeN x sites in Fe–N–C materials for proton exchange membrane fuel cells

We report that while Fe–N–C materials are a promising alternative to platinum for catalysing the oxygen reduction reaction in acidic polymer fuel cells, limited understanding of their operando degradation restricts rational approaches towards improved durability. Here we show that Fe–N–C catalysts initially comprising two distinct FeN x sites (S1 and S2) degrade via the transformation of S1 into iron oxides while the structure and number of S2 were unmodified. Structure–activity correlations drawn from end-of-test 57 Fe Mössbauer spectroscopy reveal that both sites initially contribute to the oxygen reduction reaction activity but only S2 substantially contributes after 50 h of operation. From in situ 57 Fe Mössbauer spectroscopy in inert gas coupled to calculations of the Mössbauer signature of FeN x moieties in different electronic states, we identify S1 to be a high-spin FeN 4 C 12 moiety and S2 a low- or intermediate-spin FeN 4 C 10 moiety. These insights lay the groundwork for rational approaches towards Fe–N–C cathodes with improved durability in acidic fuel cells.

36 MATERIALS SCIENCE↗