Search NASA⌕ Search

SEARCH · Search NASA

Results for “wire”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Effect of electrode polarity on wire explosion in vacuum

This paper presents experimental results on electrical explosions of thin tungsten wires at wire currents of 0.04-0.4 kA and current rise times of several tens of nanoseconds. The experiment was performed for both negative and positive polarity of the high-voltage electrode. In addition to conventional current and voltage measurements, the current to a grounded cylindrical collector placed between the exploded wire and the return conductor was measured. The collector current was observed only for a 6 {mu}m wire exploded with the high-voltage electrode being at a negative potential. In all other test modes (a 6 {mu}m wire exploded with electrode positive polarity, 6 {mu}m wire exploded with electrodes enclosed in ceramic tubes, 30 {mu}m wires exploded with electrode negative and positive polarities) no collector current was detected. A model of the discharge initiation during a wire explosion (WE) in vacuum has been proposed which is based on the supposition that a surface discharge develops over the electrodes. The presence of plasma-emitted electrons at the cathode surface makes it possible to interpret the experimental results on WEs at different electrode polarities reported both in this paper and in previous publications.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Soldered Contact and Current Risetime Effects on Negative Polarity Wire Array Z-pinches

The Cornell University COBRA pulser is a nominal 1 MA machine, capable of driving up to 32 wire cylindrical Z-pinch arrays. COBRA can operate with variable current risetimes ranging from 100 ns to 200 ns (short and long pulse, respectively). Wires are typically strung with a 'press' contact to the electrode hardware, where the wire is loosely pulled against the hardware and held there to establish electrical contact. The machine is normally negative, but a bolt-on convolute can be used to modify the current path and effectively produce positive polarity operation at the load.Previous research with single wires on a 1-5 kA pulser has shown that soldering the wire, thereby improving the wire/electrode contact, and operating in positive polarity can improve the energy deposition into the wire and enhance wire core expansion. Negative polarity showed no difference. Previous experiments on the negative polarity, 20 MA, 100 ns Z accelerator have shown that improving the contact improved the x-ray yield.Cornell data were collected on 16-wire Aluminum Z-pinch arrays in negative polarity. Experiments were conducted with both short and long current pulses with soldered and no-soldered wire/electrode contacts. The initiation, ablation, implosion and stagnation phases were compared for these four conditions. Time dependent x-ray signals were measured using diodes and diamond detectors. An inductive voltage monitor was used to infer minimum current radius achieved, as defined by a uniform shell of current moving radially inward, producing a time dependent inductance. Total energy data were collected with a metal-strip bolometer. Self-emission data were collected by an XUV 4-frame camera and an optical streak camera.In negative polarity and with short pulses, soldering appeared to produce a smaller radius pinch and decrease variations in the x-ray pulse shape. The bolometer, laser backlighter, 4-frame and streak cameras showed negligible differences in the initiation ablation and implosion phases. X-ray yield was increased with soldered arrays in negative polarity with long pulses. The bolometer also showed a 50% increase in radial power emitted for soldered arrays. 4-frame images showed soldered arrays have a more pronounced 'Christmas Tree' effect originating from the cathode. The inductive voltage monitor showed, with both long and short pulses, that soldered and no-solder arrays reached the same minimum current radius at the same time. However, with long pulses soldered arrays radiate x-rays at the time of minimum current radius while no-solder array x-ray output is delayed by {approx}20 ns, resulting in decreased x-ray yield.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Study of transparent and nontransparent regimes of implosion in star wire arrays

Star wire arrays were used to control the imploding plasma flows and study plasma interpenetration. These arrays consisted of linear 'rays' aligned azimuthally and extending from the vertical axis. Star arrays with two close located wires ('gates') instead of a single wire on the inner cylinder were studied for transparent and nontransparent regimes of propagation of imploding plasma through the gates. Nontransparent mode of collision is typical for regular star wire arrays and it was also observed in Al stars with gate wires of regular length and with the gate width of 0.3-2 mm. The cascade process of implosion in stars and trapping of imploding plasma in 1-2 mm gates were modeled with the three-dimensional resistive magnetohydrodynamics code. The intermediate semitransparent mode of collision was observed in Al stars with long Al 'gate' wires. A transparent mode was observed in Al stars with long stainless steel or W gate wires. Applications of wire arrays with controlled plasma flows are discussed.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Experimental study of surface insulated-standard hybrid tungsten planar wire array Z-pinches at “QiangGuang-I” facility

The experimental results of the insulated-standard hybrid wire array Z pinches carried out on “QiangGuang-I” facility at Northwest Institute of Nuclear Technology were presented and discussed. The surface insulating can impose a significant influence on the dynamics and radiation characteristics of the hybrid wire array Z pinches, especially on the early stage (t/t{sub imp} < 0.6). The expansion of insulated wires at the ablation stage is suppressed, while the streams stripped from the insulated wires move faster than that from the standard wires. The foot radiation of X-ray is enhanced by increment of the number of insulated wires, 19.6 GW, 33.6 GW, and 68.6 GW for shots 14037S, 14028H, and 14039I, respectively. The surface insulation also introduces nonhomogeneity along the single wire—the streams move much faster near the electrodes. The colliding boundary of the hybrid wire array Z pinches is bias to the insulated side approximately 0.6 mm.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Influence of twist pitch on hysteretic losses and transport J c in overpressure processed high J c Bi-2212 round wires

Abstract Bi-2212 is the only high field, high-temperature superconductor (HTS) available in the macroscopically isotropic, multifilament high J c round wire (RW) form capable of generating high uniformity fields with minimum-screening current errors. However, the heat treatment that enables impressively high J c (4.2 K, 30 T) values that can attain ∼5000 A mm −2 also produces significant filament bonding (bridging). Filament bridging appears to significantly enhance hysteretic losses of the filaments themselves by coupling neighboring, nominally independent filaments, enabling shielding currents to flow across multiple filaments as though they were one filament of much larger diameter. Wire twisting can be employed to reduce filament-to-filament eddy current coupling losses due to induced currents flowing across the matrix, but twisting is less effective in reducing increased losses from bridging. Here, we compare the twist-pitch dependence of the losses of overpressure processed (OP) high J c Bi-2212 RWs with partially bridged filaments to those found in OP Bi-2212 RWs with discrete, not-bridged filaments. We show that filament sub-bundles in standard, partially-bridged wires that have some superconducting connections between filaments can exhibit significant coupling (much larger effective filament diameter), but twisting still reduces their hysteretic losses to values close to or below the ITER Nb 3 Sn wire loss specification, even though Bi-2212 wires have significantly larger J c values. Although it has been reported that twisting can reduce wire J c by damaging filaments, we found no reduction in transport J c , even for nominal twist pitches of 12 mm in 0.8 mm diameter wires. Evaluation of more-recent, higher J c Engi-Mat powder wires showed that their reduced filament bridging and improved longitudinal connectivity significantly improved transport J c and reduced the J c normalized losses, signaling that J c can be further improved without commensurate increase in losses. This important result strengthens the argument for production of high field, low loss HTS magnets made with Bi-2212 RWs.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High critical current STAR ® wires with REBCO tapes by advanced MOCVD

RE–Ba–Cu–O (REBCO, RE = rare earth) symmetric tape round (STAR ® ) wires of 1.5–2.5 mm diameter have been fabricated with 4–12 strands of symmetric REBCO tape made by advanced metal organic chemical vapor deposition (MOCVD). 1.5 mm diameter STAR ® wires made with just four advanced MOCVD tape strands are able to sustain nearly the same critical current (I c ) as 2.5 mm diameter wires made with 12 commercial-grade tape strands. An I c of 1070 A, corresponding to an engineering current density (J e ) of 597 A mm –2 , has been demonstrated at 4.2 K, 30 T in 1.5 mm diameter, four-strand wire at a bend radius of 15 mm. This I c value exactly matches the Ic expected from the lift factor of the tape strands used in the wire. The 2.5 mm diameter STAR ® wires made with 12 advanced MOCVD tape strands exhibit an I c of 1075 A at 77 K, self-field and sustained currents of 2500–2750 A at 4.2 K, 30 T before burnout, corresponding to a J e greater than 500 A mm –2 . Finally, these results show that the cost of STAR ® wires can be substantially reduced using fewer tape strands of high-performance advanced MOCVD tapes and that the superior bend performance of STAR ® wires can be maintained, even using 12 strands of advanced MOCVD tapes with 4 μm thick REBCO films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Atom-wide Co Wires on Cu(775) at Room Temperature

We report on a surface phase of the Co-vicinal-Cu(111) system which exhibits self-assembled uniform Co quantum wires that are stable at 300 K. Scanning tunneling microscopy (STM)-imaging measurements show that wires will self-assemble within a narrow range of Co coverage and, within this range, the wires increase in length as coverage is increased. The STM images show that the wires form along the leading edge of the step rise, differentiating it from previously theoretically predicted atomic-wire phases. The formation of relatively long laterally unencapsulated one- and two-atom wires also differentiates it from past experimentally observed step-island formation. Furthermore, our experiments also show directly that the Co wires coexist with another Co phase that had been previously predicted for growth on Cu(111). Our observations allow us to comment on the formation kinetics of the atomic-wire phase and on the fit of our data to a recently developed lattice-gas model.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Understanding Irreversible Degradation of Nb3Sn Wires with Fundamental Fracture Mechanics

Irreversible performance degradation of advanced Nb3Sn superconducting wires subjected to transverse or axial mechanical loading is a critical issue for the design of large-scale fusion and accelerator magnets such as ITER and LHC. Recent SULTAN tests indicate that most cable-in-conduit conductors for ITER coils made of Nb3Sn wires processed by various fabrication techniques show similar performance degradation under cyclic loading. The irreversible degradation due to filament fracture and local strain accumulation in Nb3Sn wires cannot be described by the existing strand scaling law. Fracture mechanic modeling combined with X-ray diffraction imaging of filament micro-crack formation inside the wires under mechanical loading may reveal exciting insights to the wire degradation mechanisms. We apply fundamental fracture mechanics with a singularity approach to study influence of wire filament microstructure of initial void size and distribution to local stress concentration and potential crack propagation. We report impact of the scale and density of the void structure on stress concentration in the composite wire materials for crack initiation. These initial defects result in an irreversible degradation of the critical current beyond certain applied stress. We also discuss options to minimize stress concentration in the design of the material microstructure for enhanced wire performance for future applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Spectroscopic properties of colloidal indium phosphide quantum wires

Colloidal InP quantum wires are grown by the solution-liquid-solid (SLS) method, and passivated with the traditional quantum dots surfactants 1-hexadecylamine and tri-n-octylphosphine oxide. The size dependence of the band gaps in the wires are determined from the absorption spectra, and compared to other experimental results for InP quantum dots and wires, and to the predictions of theory. The photoluminescence behavior of the wires is also investigated. Efforts to enhance photoluminescence efficiencies through photochemical etching in the presence of HF result only in photochemical thinning or photo-oxidation, without a significant influence on quantum-wire photoluminescence. However, photo-oxidation produces residual dot and rod domains within the wires, which are luminescent. The results establish that the quantum-wire band gaps are weakly influenced by the nature of the surface passivation, and that colloidal quantum wires have intrinsically low photoluminescence efficiencies.

36 MATERIALS SCIENCE↗

Effects of Chromium Additions upon Microstructure and Mechanical Properties of Cold Drawn Pearlitic Steel Wires

Cr-containing pearlitic steel wires were prepared through cold drawing and simulated galvanization process. Effect of chromium microalloying on microstructural and mechanical properties of the steel wires was investigated. Experimental results show that size of pearlitic colonies of the steel rods decreased as Cr content increased from 0.2 to 0.6 wt.%; meanwhile, interlamellar spacing was little affected because of isothermal phase transition in salt bath. The tensile strength of the pearlitic steel rods was increased from 1480 to 1550 MPa. The tensile strength of the Cr-containing cold drawn wires (ε = 1.58) was increased about 33%, and the torsion circle of the wires were about 15 with cleavage fracture. After annealing at 450 °C for 2 min, tensile strength of the wires increased, but torsion circle was decreased to less than 5. As the annealing time increased, the torsion circle of the steel wires with 0.2 wt.% Cr was improved to about 10 with cleavage fracture, while the torsion performance of the wires having high Cr contents remained low because of delamination fracture. The cementite platelets in Cr-containing wires turned into cementite crystal particles during cold drawing. Microstructure observation and thermal analysis have confirmed that thermal stability of cementite was enhanced with the increase of Cr content.

36 MATERIALS SCIENCE↗

Drawing Direction Effect on Microstructure and Mechanical Properties of Twinning-Induced Plasticity Steel During Wire Drawing

The effect of drawing direction on microstructure and mechanical properties in twinning-induced plasticity (TWIP) steel during wire drawing has been investigated to improve drawability for wire rod applications. The steel wires subjected to unidirectional (UD) and reverse-directional (RD) wire drawing were analyzed. The yield and tensile strength processed by the RD were slightly higher than those by the UD, whereas the ductility and drawability have inverse features, which is totally different from the results of plain carbon steel and Al wire. Although final shear strain of wires deformed by the RD is lower than that by the UD, the RD wires had a more complex stress history and a higher <111> texture component at the surface area, which encouraged twinning rate, resulting in fast exhaustion of ductility, finally earlier fracture of wires. In contrast to the materials deformed by mainly slip mechanism, the RD process cannot improve the ductility and drawability in TWIP steel due to the stress state dependency of twinning mechanism. Also, based on the different strengthening behaviors between pearlitic and TWIP steels during UD and RD, it is induced that microstructure and applied stress state simultaneously control the mechanical properties.

36 MATERIALS SCIENCE↗

A bi-layer barrier design for 122-type iron-based superconducting wires and tapes

Iron-based superconducting wires and tapes hold great promise for high-field magnet applications. A promising design for 122-type wires and tapes based on the powder-in-tube method is using silver and copper double-layer sheaths. For this design a heat treatment temperature below ~ 779 °C is required to prevent Ag-Cu liquid formation. However, this may be below the optimal heat treatment temperature for the critical current density, and still cannot prevent Ag-Cu interdiffusion occurring in the solid state. In this work we propose adding a niobium or tantalum or vanadium (or their alloys) barrier layer between the Ag and Cu to solve the Ag-Cu interdiffusion issue, given that the group-VB metals (vanadium, niobium, tantalum) are relatively inert to both Ag and Cu. To investigate the effectiveness of this design, BaFe 1.84 Co 0.16 As 2 wires and tapes with Ag/Cu and Ag/Ta/Cu sheaths, as well as Ba 0.6 K 0.4 Fe 2 As 2 wires and tapes with Ag/Cu and Ag/Nb/Cu sheaths, were fabricated. It was found that both the Ta and Nb layers kept integral after wire drawing, but after a large flat-rolling reduction the Ta layer broke while the Nb layer kept integral. In the tapes with Ag/Cu sheaths (without the Ta or Nb layer) Cu diffused through the Ag layer and into the powder cores during 740 °C heat treatment, while in the tapes with Ag/Nb/Cu sheaths the Nb layer effectively blocked Ag-Cu interdiffusion even at 900 °C. Further, this work demonstrates that Ta is a suitable barrier material for 122-type wires, while Nb is suitable for both wires and tapes. In this design using Ag/Nb (or Ta)/Cu sheaths, we can regard the outer Cu as the conductor matrix while the Ag and Nb (or Ta) serve as two layers of barriers that suppress reactions between the components. Thus, we call this design a “bi-layer barrier” design for 122-type wires and tapes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Highly Conductive Ag Paste for Recoverable Wiring and Reliable Bonding Used in Stretchable Electronics

Stretchable wiring and stretchable bonding between rigid chip/component and stretchable substrate are two of the key factors for stretchable electronics. Here, a low cost and highly stretchable paste is developed with Ag micro flakes and PDMS, which can be used to fabricate stretchable wirings and bondings under a low curing temperature of 100 °C with printing method. Recoverabilities as recovery time and recovery resistance of the wirings and bondings are defined and discussed. The wiring with a low resistivity of 8.7 × 10-5 ·cm shows much better recoverability than nanowire based wirings due to the flake nature of the Ag particles. When stretched to 50% and 100% of strain, the resistance of the patterned wiring increases to only 1.1 and 2.1 times, respectively. Moreover, the resistance of the wiring during 20% tensile cyclic test remains within 1.1 times even after 1000 cycles, showing long time durability. On the other hand, the paste is also used as a bonding material to assemble a zero-Ohm chip on the stretchable substrate to fabricate a stretchable demo, whose resistance increased to only 1.9 times when stretched to 50% of strain. The developed pastes can be expected to make various stretchable wirings, bondings and packaging structures by simple printing process, enabling mass production of stretchable electronic devices.

Li, Cai Fu↗

Increased electron, positron, and x-ray production from high intensity laser interactions using micro-wire targets

We report increases in energetic electrons, positrons, and x-rays emitted from high-intensity laser interactions (10 18−20 W/cm 2 ) with structured silicon micro-wires on the surface of a 1 mm gold converter target using a 10 ps laser pulse. A total of four different wire configurations are tested, where the gaps (7–28 μm) between the wires and the thicknesses (3–6 μm) of the wires are varied, while the height remains constant (⁠ ~25 μm). We observe the largest enhancement in electrons, positrons, and x-rays with the sparsest wire configurations. The electron temperature (T e ≈6 MeV) remains consistent across all shots, regardless of whether wires or planar targets are used. This suggests that the observed enhancement is due to increased laser light absorption by the accelerated electrons over a long scale length. Two-dimensional particle-in-cell simulations confirm that absorption is significantly enhanced with the wire target. Additionally, specific simulations examining laser pointing on different parts of the wire structure reveal that, while the final electron spectrum remains largely insensitive, the angular distribution is highly sensitive to these variations.

Bremsstrahlung↗

Oxide Dispersion Strengthened Ferritic Steel Wire Feedstock Development for Larger Format Additive Manufacturing (CRADA Final Report)

This CRADA project funded through DOE’s INFUSE program sought to demonstrate the viability of fabricating large, complex parts from oxide dispersion strengthened (ODS) steel with advanced manufacturing. Exhibiting excellent radiation tolerance and high mechanical performance at elevated temperatures, ODS steel is a promising structural material candidate for near-plasma components in fusion energy systems. Its use, however, has been limited by a lack of manufacturability. This project sought to produce ODS steel wire through a solid-state shear assisted extrusion process and then demonstrate that the wire can undergo controlled local melting while being welded with the final part sufficiently retaining the beneficial properties of ODS steel. This would allow the use of wire-arc additive manufacturing (WAAM) to manufacture large-scale ODS parts, even though ODS is currently only available as a powder. WAAM is a promising technique for producing components like the replaceable ARC vacuum vessel in CFS’ fusion reactor design. Meanwhile, this project will also expand PNNL’s capability in producing custom wire feedstock with friction extrusion, enabling downstream large-scale manufacturing with WAAM and solid-state based additive manufacturing. The project achieved its goals of developing tooling and fixturing to produce ODS wire at smaller diameters than previous projects. Several small lengths of wire of 1.5 mm and 2.5 mm diameter in the range of 2.5-30 mm long were produced at tool temperatures that are known to cause ODS particle coarsening (~1200 °C). Fixtures and tooling for longer (>1 m) wires were developed but further process development is needed reduce tool temperature during extrusions and to increase wire length needed for WAAM testing and development.

36 MATERIALS SCIENCE↗

The Calculated and Measured Performance Characteristics of a Heated-Wire Liquid-Water-Content Meter for Measuring Icing Severity

Ground tests have been made of an instrument which, when assembled in a more compact form for flight installation, could be used to obtain statistical flight data on the liquid-water content of icing clouds and to provide an indication of icing severity. The sensing element of the instrument consists of an electrically heated wire which is mounted in the air stream. The degree of cooling of the wire resulting from evaporation of the impinging water droplets is a measure. of the liquid-water content of the cloud. Determination of the value of the liquid-water content from the wire temperature at any instant requires a knowledge of the airspeed, altitude, and air temperature. An analysis was made of the temperature response of a heated wire exposed to an air stream containing water drops. Comparisons were made of the liquid-water content as measured with several heated wires and absorbent cylinders in an artificially produced cloud. For one of the wires, comparative tests were made with a rotating-disk icing-rate meter in an icing wind tunnel. From the test results, it was shown that an instrument for measuring the concentration of liquid water in an air stream can be built using an electrically heated wire of known temperatureresistance characteristics, and that the performance of such a device can be predicted using appropriate theory. Although an instrument in a form suitable for gathering statistical data in flight was not built, the practicability of constructing such an instrument was illustrated. The ground-test results indicated that a flight heated-wire instrument would be simple and durable, would respond rapidly to variations in liquid-water content, and could be used for the measurement of water content in clouds which are above freezing temperature, as well as in icing clouds.

Neel, Carr B.↗

Experimental comparison of two hot-wire techniques for resolution of turbulent mass flux and local stagnation temperature in supersonic flow

The performance of two constant-temperature normal hot-wire techniques in a supersonic flow is examined. The first technique uses a single-wire and rapid scanning of multiple overheat ratios. Time averages of the signals at all overheats are used to separate the mean and rms mass flux, stagnation temperature and their cross-correlation. The second technique uses a dual-wire probe with each wire operating at different overheat ratios, giving instantaneous mass flux and stagnation temperature. Preliminary results indicate that the separation distance (0.18 mm) between the two hot wires in the dual-wire probe does not introduce significant error. However, the rms mass flux inferred from the dual-wire technique is a factor of two higher than that from the single-wire technique.

Walker, D. A.↗

Tensile and stress-rupture behavior of hafnium carbide dispersed molybdenum and tungsten base alloy wires

The tensile strain rate sensitivity and the stress-rupture strength of Mo-base and W-base alloy wires, 380 microns in diameter, were determined over the temperature range from 1200 K to 1600 K. Three molybdenum alloy wires; Mo + 1.1w/o hafnium carbide (MoHfC), Mo + 25w/o W + 1.1w/o hafnium carbide (MoHfC+25W) and Mo + 45w/o W + 1.1w/o hafnium carbide (MoHfC+45W), and a W + 0.4w/o hafnium carbide (WHfC) tungsten alloy wire were evaluated. The tensile strength of all wires studied was found to have a positive strain rate sensitivity. The strain rate dependency increased with increasing temperature and is associated with grain broadening of the initial fibrous structures. The hafnium carbide dispersed W-base and Mo-base alloys have superior tensile and stress-rupture properties than those without HfC. On a density compensated basis the MoHfC wires exhibit superior tensile and stress-rupture strengths to the WHfC wires up to approximately 1400 K. Addition of tungsten in the Mo-alloy wires was found to increase the long-term stress rupture strength at temperatures above 1400 K. Theoretical calculations indicate that the strength and ductility advantage of the HfC dispersed alloy wires is due to the resistance to recrystallization imparted by the dispersoid.

Yun, Hee Mann↗