Small-scale Assessment of Simplified Ceramic Waste Form Processing

The feasibility of directly processing glass-bonded sodalite ceramic waste form materials by heating a mixture of Zeolite 4A, chloride salt, and sodium borosilicate binder glass was demonstrated by generating laboratory-scale materials. This direct processing method eliminates pre-setting the moisture content of the Zeolite 4A, eliminates the step of occluding salt in the prepared Zeolite 4A prior to processing, and can be conducted using larger particle sizes of crushed Zeolite 4A and crushed borosilicate glass than those called for in the current method. These simplifications are expected to facilitate material transfer and handling in a hot cell or controlled atmosphere environment and be more readily implemented at large scale than the current method. Most materials made to assess these simplifications were directly processed at 925 °C for two hours in an argon atmosphere glovebox, but one material was processed at 925 °C for four hours and one material was processed at 880 °C for two hours. Sodalite was generated and became microencapsulated by the binder glass in all materials. The microstructures were uniform throughout each product, were similar in all products, and were similar to the microstructures of materials made previously using the pressureless consolidation or hot isostatic pressing methods. Various formulations showed the efficiency of sodalite generation was not sensitive to the salt-to-Zeolite 4A ratio or salt-to-glass mass ratio, although a greater relative mass of glass is required to encapsulate sodalite generated from large particles of aggregated Zeolite 4A. The upper limit of salt loadings that can be effectively processed remains to be determined. The effectiveness of direct processing provided new insights into the conversion mechanism. The salt was likely dissolved into the glass that transported NaCl into the Zeolite 4A aggregates and sodalite was generated in situ as NaCl migrated from the outside of the aggregate inward. Other salt cations (e.g., potassium, strontium, cesium, and probably lithium) remain dissolved in the glass encapsulating the zeolite/sodalite domains. When the glass solidifies during cooling, small halite inclusion phases form in glass within sodalite domains and large mixed salt inclusions form in glass surrounding the sodalite due to the low solubility of chloride in the (solid) glass. Other salt cations were oxidized during processing and formed inclusions in the bulk glass (e.g., neodymium). Initial degradation tests show the dissolution behavior of directly processed CWF (SCWF) materials is similar to CWF materials made using different methods.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Electrolyte with Low Polysulfide Solubility for Li-S Batteries

Here, Li-S battery is one of the most promising next generation rechargeable battery technologies due to its high theoretical energy density and low material cost. While its success is impeded by the low energy efficiency and fast capacity fade primarily caused by the discharge intermediates, Li-polysulfides (PS), dissolution in the electrolyte. Mitigation of PS dissolution in electrolyte involves the search of new electrolyte solvent system that exhibits poor solvation to the PS while still have good solvation ability to the electrolyte salt for high ionic conductivity. Applying co-solvents with reduced solvating power but compatible with the state of art Li-S battery’s ether-based electrolyte is one of the most promising concepts. This route is also advantageous of having a low scale-up cost. With the aids of Quantum Chemical Calculation, we have identified high carbon-to-oxygen (C/O) ratio ethers as co-solvent in the new electrolytes that effectively impede PS dissolution while still maintaining high ionic conductivity. Significantly improved cycle life and cycling Coulombic efficiency are observed for Li-S cells using the new composite electrolytes. Anode analysis with different methods also demonstrate that reducing electrolyte’s PS solubility results in less sulfur total amount on the lithium anode surface and lower ratio of the longer-chain PS, which is probably a sign of suppressed side reactions between the anode and PS in the electrolyte.

25 ENERGY STORAGE↗

Investigation and Analysis of Dolomite Dissolution in Variable Strength Systems Relevant to the WIPP

The Waste Isolation Pilot Plant (WIPP) was opened in 1999 as a solution to the long-term disposal of the nation's nuclear defense-generated transuranic (TRU) waste. The salt beds were recommended as the ideal location because they are free from flowing fresh water, easily mined, impermeable, and geologically stable. However, for performance assessment modeling, release scenarios must be considered. The most likely release scenario was determined to be human intrusion leading to direct and/or long-term brine release (US DOE 1995, US DOE 1996, Perkins et al., 1999). The focus of this research is the Rustler formation because it is located above the WIPP and is the most transmissive layer (Perkins et al., 1999). Objective: To determine the effect of chelating ligands ( e.g. EDTA) on dissolution of dolomite in high ionic strength systems. Do brines impact dolomite dissolution and how is it affected by EDTA binding with cations? By varying the ionic strengths, different brine conditions can be simulated similar to those in and around the Culebra member and evaluate trends of dissolved Ca and Mg in the aqueous phase from the quantified data. Conclusions: <2% of dolomite dissolved over one week at pH 8.5. Greater dissolution occurred at higher ionic strength and in the presence of NaCl with approximately 0.4 vs. 0.9% of Mg removed from dolomite in 0.1 and 1.0 M Na. Further, 0.3 vs. 0.9% of Mg was removed from dolomite in 1.0 M IS CaCl{sub 2} versus NaCl. EDTA increased dissolution of dolomite at low ionic strength due to its strong complexation affinity for Ca/Mg with slightly greater removal of Ca than Mg. Significant differences were not observed at high ionic strength due to the presence of large concentrations of competing cations (Na, Ca, Mg). Slightly higher concentrations of Ca were removed from dolomite than Mg after one week, suggesting either incongruent dissolution or release through ion exchange of Ca from trace mineral impurities. Further, when EDTA was present, it may have increased Ca removal due to its greater complexation for Ca than Mg. Environmental Implications: High ionic strength brines and low ionic strength solutions with organic ligands increase dissolution of dolomite. Due to the long half-lives of radionuclides in the TRU waste, it may be important to consider the long term impact of dolomite dissolution for potential release scenarios.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Shale-fluid interactions during forced lmbibition and flow-back

One way to minimize the need for disposal of flow-back waters produced during the hydraulic fracturing of unconventional reservoirs is, potentially, to recycle these fluids by recovering and re-injecting them during hydraulic fracturing of nearby new wells. These flow-back waters contain, however, large concentrations of dissolved salts. During hydraulic fracturing of unconventional reservoirs, a well may undergo extended shut-in periods, following the initial hydraulic-fracture stimulation. The concern here, therefore, is that the salts dissolved in the re-injected flow-back waters may precipitate in the subsurface, thus promoting scale formation; or alternately, because of their high salinity, these same fluids may cause the dissolution of various minerals present in the subsurface. Large divalent cations (e.g., Ca²⁺, Ba²⁺ and Sr²⁺) and anions (e.g., CO3²⁻ and SO4²) may chemically interact with and cause the swelling of clay fractions, thus blocking pores in certain pore size ranges. All these phenomena (i.e., scale formation, clay swelling, minerals dissolution) can influence the petrophysical properties of the formation, including its permeability, porosity, contact angle, etc. One way to potentially overcome some of these technical challenges, is to pre-treat these flow-back waters, prior to re-injection (e.g., via chemical precipitation, followed by membrane filtration) in order to remove unwanted salts. However, such pre-treatment is costly, and the degree of salt removal needed to prevent formation damage is important in determining the economic viability of flow-back water recycle via re-injection. A key focus of this work, therefore, is to study the impact that the injection of flow-back waters, that have undergone varying degrees of pre-treatment and clean-up, will have on the flow-through characteristics of a tight-gas reservoir, particularly of the Marcellus Shale formation. To do so, we have carried-out forced-imbibition experiments with shale samples from various depths in the Marcellus formation, whose properties span high to low ranges of TOC, clay content and matrix permeabilities. We have studied the forced-imbibition characteristics, at an injection pressure of 24,233 kPa (3500 psig), of various flow-back fluids into shale cores saturated with methane at a pore pressure of 17,338 kPa (2500 psig) and a confining stress of 27,680 kPa (4000 psig). Following the forced imbibition experiments, we analyzed the cores for potential changes in permeability and porosity. Quantification of the ion content of the injected and recovered fluids was also performed using Ion Chromatography (IC). The IC analysis of the recovered fluids indicates substantial interactions and geochemical reactions between the invading fluids and the shale cores. The injection of flow-back fluids shows significant impact on the flow-through characteristics, with untreated flow-back fluids, which have the highest cation and anion content, also exhibiting the highest observable reductions in permeability (>90%).

defects, mechanical behavior, carbon sequestration↗

Corrosion mechanism of cold forged 316 stainless steel in molten FLiNaK salt

This study examined how cold forging (CF) affects the corrosion of 316 stainless steel (SS) in molten FLiNaK salt at 700 °C for 48 h. CF samples had two corrosion areas: one near the top and another displaying intergranular corrosion (IGC). Samples with lower CF (5–30 %) showed more IGC, while the 50 % CF sample had less IGC but the shallowest corrosion depth. This was due to the increased number of grain boundaries, which raised the potential corrosion initiation sites, and certain grain boundaries promoting chromium dissolution, thus enhancing IGC.

FLiNaK↗

Investigation of historical metal objects using Laser Induced Breakdown Spectroscopy (LIBS) technique

Analysis of metal objects is a necessary step for establishing an appropriate conservation treatment of an object or to follow up the application's result of the suggested treatments. The main considerations on selecting a method that can be used in investigation and analysis of metal objects are based on the diagnostic power, representative sampling, reproducibility, destructive nature/invasiveness of analysis and accessibility to the appropriate instrument. This study aims at evaluating the usefulness of the use of Laser Induced Breakdown Spectroscopy (LIBS) Technique for analysis of historical metal objects. In this study various historical metal objects collected from different museums and excavations in Egypt were investigated using (LIBS) technique. For evaluating usefulness of the suggested analytical protocol of this technique, the same investigated metal objects were investigated by other methods such as Scanning Electron Microscope with energy-dispersive x-ray analyzer (SEM-EDX) and X-ray Diffraction (XRD). This study confirms that Laser Induced Breakdown Spectroscopy (LIBS) Technique is considered very useful technique that can be used safely for investigating historical metal objects. LIBS analysis can quickly provide information on the qualitative and semi-quantitative elemental content of different metal objects and their characterization and classification. It is practically non-destructive technique with the critical advantage of being applicable in situ, thereby avoiding sampling and sample preparations. It is can be dependable, satisfactory and effective method for low cost study of archaeological and historical metals. But we have to take into consideration that the corrosion of metal leads to material alteration and possible loss of certain metals in the form of soluble salts. Certain corrosion products are known to leach out of the object and therefore, their low content does not necessarily reflect the composition of the metal at the time of the object manufacture. Another point should be taken into consideration that the heterogeneity of a metal alloy object that often result from poor mixing of the different metal alloy composition.There is a necessity to carry out further research to investigate and determine the most appropriate and effective approaches and methods for conservation of these metal objects.

36 MATERIALS SCIENCE↗

Correlating Rate-Dependent Transition Metal Dissolution between Structure Degradation in Li-Rich Layered Oxides

Understanding the mechanism of the rate-dependent electrochemical performance degradation in cathodes is crucial to developing fast charging/discharging cathodes for Li-ion batteries. Here, in this work, taking Li-rich layered oxide Li 1.2 Ni 0.13 Co 0.13 Mn 0.54 O 2 as the model cathode, the mechanisms of performance degradation at low and high rates are comparatively investigated from two aspects, the transition metal (TM) dissolution and the structure change. Quantitative analyses combining spatial-resolved synchrotron X-ray fluorescence (XRF) imaging, synchrotron X–ray diffraction (XRD) and transmission electron microscopy (TEM) techniques reveal that low-rate cycling leads to gradient TM dissolution and severe bulk structure degradation within the individual secondary particles, and especially the latter causes lots of microcracks within secondary particles, and becomes the main reason for the fast capacity and voltage decay. In contrast, high-rate cycling leads to more TM dissolution than low-rate cycling, which concentrates at the particle surface and directly induces the more severe surface structure degradation to the electrochemically inactive rock-salt phase, eventually causing a faster capacity and voltage decay than low-rate cycling. These findings highlight the protection of the surface structure for developing fast charging/discharging cathodes for Li-ion batteries.

25 ENERGY STORAGE↗

Allotropic control: How certain fluorinated carbonate electrolytes protect aluminum current collectors by promoting the formation of insoluble coordination polymers

Here, there is a strong incentive for increasing the operation voltage of Li-ion cells above 4.5 V in order to increase the density of stored energy. Aluminum is an inexpensive, lightweight metal that is commonly used as a positive electrode current collector in these cells. Imide LiX salts, such as lithium bis(trifluoromethylsulfonyl)imide (X = TFSI), and lithium bis(fluorosulfonyl)imide (X = FSI), are chemically stable on the energized lithiated transition metal oxide electrodes, but their presence in the electrolyte causes rapid anodic dissolution and pitting of Al current collectors at potentials exceeding 4.0 V versus Li/Li + . For LiBF 4 and LiPF 6 , the release of HF near the energized surfaces passivates the exposed Al metal, inhibiting this pitting corrosion, but it also causes the gradual degradation of the cathode active material, negating this important advantage. Here we report that in certain electrolytes containing fluorinated carbonate solvents and LiX salts, the threshold voltage for safe operation of Al current collectors can be increased to 5.5 V versus Li/Li + . Interestingly, the most efficient solvent also facilitates the formation of an insoluble gel when AlX 3 is introduced into this solvent. We suggest that this solvent promotes the aggregation of coordination polymers of AlX 3 at the exposed Al surface that isolate this surface from the electrolyte, thereby preventing further Al dissolution and corrosion. Other examples of Al collector protection may also involve this mechanism. Our study suggests that such “allotropic control” could be a way of widening the operation window of Li-ion cells without electrode deterioration, Al current collector corrosion, and electrolyte breakdown.

36 MATERIALS SCIENCE↗

Solution chemistry of Mo(III) and Mo(IV): Thermodynamic foundation for modeling localized corrosion.

To investigate the behavior of molybdenum dissolution products in systems that approximate localized corrosion environments, solubility of Mo(III) in equilibrium with solid MoO{sub 2} has been determined at 80 C as a function of solution acidity, chloride concentration and partial pressure of hydrogen. The measurements indicate a strong increase in solubility with acidity and chloride concentration and a weak effect of hydrogen partial pressure. The obtained results have been combined with literature data for systems containing Mo(III), Mo(IV), and Mo(VI) in solutions to develop a comprehensive thermodynamic model of aqueous molybdenum chemistry. The model is based on a previously developed framework for simulating the properties of electrolyte systems ranging from infinite dilution to solid saturation or fused salt limit. To reproduce the measurements, the model assumes the presence of a chloride complex of Mo(III) (i.e., MoCl{sup 2+}) and hydrolyzed species (MoOH{sup 2+}, Mo(OH){sup 2+}, and Mo(OH){sub 3}{sup 0}) in addition to the Mo{sup 3+} ion. The model generally reproduces the experimental data within experimental scattering and provides a tool for predicting the phase behavior and speciation in complex, concentrated aqueous solutions. Thus, it provides a foundation for simulating the behavior of molybdenum species in localized corrosion environments.

08 HYDROGEN↗

EVALUATION OF LOW TEMPERATURE ALUMINUM DISSOLUTION IN TANK 51

Liquid Waste Organization (LWO) identified aluminum dissolution as a method to mitigate the effect of having about 50% more solids in High Level Waste (HLW) sludge than previously planned. Previous aluminum dissolution performed in a HLW tank in 1982 was performed at approximately 85 C for 5 days, which became the baseline aluminum dissolution process. LWO initiated a project to modify a waste tank to meet these requirements. Subsequent to an alternative evaluation, LWO management identified an opportunity to perform aluminum dissolution on sludge destined for Sludge Batch 5, but within a limited window that would not allow time for any modifications for tank heating. A variation of the baseline process, dubbed Low Temperature Aluminum Dissolution (LTAD), was developed based on the constraint of available energy input in Tank 51 and the window of opportunity, but was not constrained to a minimum extent of dissolution, i.e. dissolve as much aluminum as possible within the time available. This process was intended to operate between 55 and 70 C, but for a significantly longer time than the baseline process. LTAD proceeded in parallel with the baseline project. The preliminary evaluation at the completion of LTAD focused on the material balance and extent of the aluminum dissolved. The range of values of extent of dissolution, 56% to 64%, resulted from the variation in liquid phase sample data available at the time. Additional solid phase data is available from a sample taken after LTAD to refine this range. This report provides additional detailed evaluation of the LTAD process based on analytical and field data and includes: a summary of the process chronology; a determination of an acceptable blending strategy for the aluminum-laden supernate stored in Tank 11; an update to the determination of aluminum dissolved using more complete sample results; a determination of the effect of LTAD on uranium, plutonium, and other metals; a determination of the rate of heat loss from a quiescent tank; and an evaluation of the aluminum dissolution rate model and actual dissolution rate. LTAD was successfully completed in Tank 51 with minimal waste tank changes. The following general conclusions may be drawn about the LTAD process: (1) Dissolution at about 60 C for 46 days dissolved 64% of the aluminum from the sludge slurry. (2) The aluminum-laden leach solution decanted to Tank 11 can be blended with a wide variety of supernates without risk of precipitating the dissolved aluminum based on thermodynamic chemical equilibrium models. (3) Uranium and plutonium leached into solution without corresponding leaching of iron or metal other than aluminum, but the total mass leached was a small fraction of the total uranium and plutonium in the sludge. (4) The concentration of uranium and plutonium in the leach solution was indistinguishable from other tank farm supernates, thus, the leach solutions can be managed relative to the risk of criticality like any other supernate. (5) A small amount of mercury leached into solution from the sludge causing the liquid phase concentration to increase 6 to 10 fold, which is consistent with the 4 to 14 fold increase observed during the 1982 aluminum dissolution demonstration. (6) Chromium did not dissolve during LTAD. (7) Chloride concentration increased in the liquid phase during LTAD due to chloride contamination in the 50% sodium hydroxide solution. (8) The rate of heat loss from Tank 51 at temperatures above 45 C appeared linear and predictable at 8E+7 cal/hr. (9) The rate of heat transfer from Tank 51 did not follow a simplified bulk heat transfer model. (10) Prediction of the aluminum dissolution rate was prone to error due to a lack of active specific surface area data of sludge particles. (11) The higher than expected dissolution rate during LTAD was likely due to smaller than expected particle sizes of most of the sludge particles. While evaluating the LTAD process, the dissolved salt solution from Tank 41 that was stored and sampled in Tank 49 was determined to be supersaturated relative to aluminum. Supersaturation in Tank 49 is not a risk to LTAD. However, storing and processing of this supernate carries a risk of solids precipitation, primarily in the form of gibbsite or boehmite. Blending with the supernate in Tank 11 neither increases nor decreases this risk. LTAD was initiated as an opportunity to substantially mitigate the planned increase in canister production and DWPF lifecycle after the realization of more sludge solids stored in the HLW tanks. As determined from the preliminary evaluation of LTAD, the direct benefit of the decanted liquid stored in Tank 11 represents 45 canisters at 34% waste loading with potential indirect benefits for much larger reductions. Application of an aluminum dissolution process to the remaining high aluminum content sludge will potentially reduce the planned canister production by several hundred canisters at 34%-38% waste loading.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Compatibility of Type 304H Stainless Steel in Static Molten FLiBe for Inertial Confinement Fusion Reactors: Role of Impurities and Redox Control

Molten fluoride salts, such as FLiBe (LiF-BeF2), are promising candidates for tritium breeding and heat transfer in fusion reactors, but corrosion of structural materials remains a major challenge. This study investigates the corrosion behavior of austenitic stainless steel 304H in purified and NiF2-containing FLiBe at 500°C and 600°C, focusing on the effects of impurities and redox control. Exposure to purified FLiBe resulted in the concurrent depletion of Cr, Mn, and Fe, with corrosion at 500 °C dominated by the combined oxide formation and elemental dissolution, while at 600°C elemental depletion was predominant. The addition of a controlled NiF2 impurity significantly accelerated corrosion at both temperatures, demonstrating the sensitivity of 304H to the salt redox state. Beryllium additions were effective in mitigating corrosion for both baseline and NiF2-containing FLiBe; minimal depletion of Cr, Mn, and Fe occurred with Be additions as low as 2.5 mg (147 wppm), and no NiBe intermetallics formed at 5 mg (294 wppm), indicating that small Be inventories can provide substantial protection without deleterious phase formation. Thermodynamic equilibrium and coupled thermodynamic-kinetic analyses at the salt-alloy interface suggested low corrosion rates in systems with limited hydrogen fluoride (HF) generation, highlighting the importance of salt redox control. Estimates for a Be addition rate were calculated for the HYLIFE-II fusion reactor that can mitigate corrosion-induced degradation, assuming complete conversion of tritium to tritium fluoride (TF). Overall, 304H shows reasonable compatibility with FLiBe under optimized redox conditions. These results provide quantitative guidance for material selection and salt management in fusion blanket and heat exchanger systems and motivate validation under flowing, nonisothermal, and irradiated conditions.

Pillai, Rishi [ORNL] (ORCID:0000000243688197)↗

Optimizing a chemical cleaning protocol to determine the nickel isotopic composition of ancient seawater from carbonates

Reconstructing the ancient marine cycle of Ni, a trace metal in the oceans essential to enzymes regulating the C, N, and O cycles, would inform how Ni bioavailability shaped early life. The Ni isotopic composition of seawater (δ 60 Ni SW ) through time could provide insight, but this approach requires sedimentary archives that faithfully record δ 60 Ni SW . Carbonates are an often-used record of seawater chemistry, but contaminants could bias the measured δ 60 Ni of bulk sediment. To isolate the true carbonate-bound δ 60 Ni signal, we optimized a chemical cleaning protocol designed to minimize non‑carbonate Ni contributions and maximize carbonate recovery. We analyzed ODP Site 1007 sediments and evaluated oxidative and reductive pre-cleaning steps and carbonate dissolution protocols. Our results show that only reductive cleaning significantly altered the subsequent carbonate leachate composition, lowering Ni/Ca ratios by up to 60% and δ 60 Ni values by as much as 0.4 ‰. In contrast, δ 60 Ni values were largely insensitive to premature carbonate dissolution during pre-cleaning or to partial leaching of silicates during carbonate dissolution, even at higher acid molarities or longer reaction times. We recommend an evidence-based protocol that removes hydro-soluble salts and clays, applies reductive cleaning and oxidative cleaning for certain sample compositions, and dissolves carbonate using 0.5 M acetic acid, adjusted to pH 5. Using these results, we infer a ∼ 0.9 ‰ Ni isotopic fractionation between chemically cleaned deep-water carbonates (+0.4 ± 0.1 ‰) and deep seawater. This method development is a key step toward accurately reconstructing ancient marine Ni cycles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Anion Mobility on Electrochemical Behaviors of Lithium–Sulfur Batteries

The electrolyte is a crucial component of lithium-sulfur (Li-S) batteries, as it controls polysulfide dissolution, charge shuttling processes, and solid-electrolyte interphase (SEI) layer formation. Experimentally, the overall performance of Li-S batteries varies with choice of solvent system and Li-salt used in the electrolyte, and a lack of predictive understanding about the effects of individual electrolyte components inhibits the rational design of electrolytes for Li-S batteries. Here we analyze the role of the counter anions of common Li salts (such as TfO-, FSI-, TFSI-, and TDI-) when dissolved in DOL/DME (1:1 vol.) for use in Li-S batteries. The evolution of ion-ion and ion-solvent interactions due to vari-ous anions was analyzed using 17O NMR and pulsed-field gradient (PFG) NMR and then correlated with electrochemi-cal performance in Li-S cells. These data reveal that the for-mation of the passivation layer on the anode and the loss of active materials from the cathode (evidenced by polysulfide dissolution) are related to anion mobility and affinity with lithium polysulfide, respectively. For future electrolyte de-sign, anions with lower mobility and weaker interactions with lithium polysulfides may be superior candidates for increasing the long-term stability of Li-S batteries.

25 ENERGY STORAGE↗

Industrial Scale-Up of Low-Cost Zero-Emissions Magnesium by INFINIUM Electrolysis

INFINIUM led a project whose goal was at first to produce pure magnesium, and later magnesium-rare earth alloys, directly from oxides. The reduction technology is molten salt electrolysis with a fluoride salt bath, similar to the Hall-Héroult process for aluminum. The pure magnesium component of the project used novel oxygen-producing anodes with a zirconia solid electrolyte tube between the molten salt and anode. The project later shifted to direct production of magnesium-neodymium master alloy for Mg-rare earth alloys. These alloys are typically made by dissolution of rare earth metals into magnesium, and cost over six times the rare earth basis price of the master alloy. The resulting process produced a total of over 30 kg of Mg-Nd master alloy, which was made into nearly 250 kg of AE42 (Mg-4%Al-2%Nd) alloy.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Dissolution of Lithium Metal in Poly(ethylene oxide)

We observe that lithium metal is sparingly soluble in poly(ethylene oxide) (PEO). 7 Li NMR shows that when a PEO sample is placed in contact with lithium metal at elevated temperatures, a lithium species dissolves and diffuses into the bulk polymer. A lithium/PEO/lithium electrochemical cell, containing no lithium salts, shows increasing conductivity over time when annealed at 120 °C. Chronoamperometry shows that the annealed cell obeys Ohm's law, implying that conduction occurs without the development of concentration gradients. To explain the findings, it is proposed that atomic lithium dissolves into PEO, where it exists as a lithium cation and free electron. The dissolution of lithium also affects the phase behavior of block copolymer electrolytes. These determinations explain the strong adhesion between lithium metal and PEO and have important implications for lithium metal battery systems that contain PEO-based electrolytes.

25 ENERGY STORAGE↗

Microscale THMC Modeling of Pressure Solution in Salt Rock: Impacts of Geometry and Temperature

Abstract Pressure solution, a mechanism that involves tight coupling between the geometry and thermal-hydro-mechanical-chemical (THMC) processes, plays an important role in diagenesis. In this study, we make the first attempt to conduct microscale THMC modeling to understand and quantify the impacts of geometry and temperature on pressure solution, taking natural salt rock as an example. This modeling capability is achieved by expanding a novel MC code that we developed previously (Hu et al. J Geophys Res: Solid Earth 126:e2021JB023112, 2021) to include temperature effects. We first conduct a simulation of an example that involves a single brine inclusion within a single halite grain and find that the temperature impact is limited for that case. We then extract geometry from an image of a natural salt rock and conduct simulations with different cases: (A) only temperature and no stress, (B) only stress and no temperature, and (C) with both stress and temperature. These different cases result in quite different phenomena. In case A, dissolution and precipitation occur across the entire system due to isolated pore space reaching a localized mass balance between dissolution, precipitation, and diffusion. In case B, intense geometric features (e.g., major asperities, inclusions) in one area undergo stress concentration, thus dominating pressure solution in that area. In case C, pressure solution is spread out at contacting highly stressed geometric features close to the hotter side. We conclude that geometric features dominate stress distribution, thus dominating pressure solution in a natural salt rock that may be affected by the temperature if a sufficient temperature gradient is applied.

58 GEOSCIENCES↗

SLUDGE HEEL REMOVAL BY ALUMINUM DISSOLUTION AT SAVANNAH RIVER SITE 12390

High Level Waste (HLW) at the Savannah River Site (SRS) is currently stored in aging underground storage tanks. This waste is a complex mixture of insoluble solids, referred to as sludge, and soluble salts. Continued long-term storage of these radioactive wastes poses an environmental risk. Operations are underway to remove and disposition the waste, clean the tanks and fill with grout for permanent closure. Heel removal is the intermediate phase of the waste retrieval and tank cleaning process at SRS, which is intended to reduce the volume of waste prior to treatment with oxalic acid. The goal of heel removal is to reduce the residual amount of radioactive sludge wastes to less than 37,900 liters (10,000 gallons) of wet solids. Reducing the quantity of residual waste solids in the tank prior to acid cleaning reduces the amount of acid required and reduces the amount of excess acid that could impact ongoing waste management processes. Mechanical heel removal campaigns in Tank 12 have relied solely on the use of mixing pumps that have not been effective at reducing the volume of remaining solids. The remaining waste in Tank 12 is known to have a high aluminum concentration. Aluminum dissolution by caustic leaching was identified as a treatment step to reduce the volume of remaining solids and prepare the tank for acid cleaning. Dissolution was performed in Tank 12 over a two month period in July and August, 2011. Sample results indicated that 16,440 kg of aluminum oxide (boehmite) had been dissolved representing 60% of the starting inventory. The evolution resulted in reducing the sludge solids volume by 22,300 liters (5900 gallons), preparing the tank for chemical cleaning with oxalic acid.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗