Delineating the Factors Impacting the Electrochemical Behavior of Single-Crystal High-Nickel Layered Oxide Cathodes

High-nickel (Ni) (≥80%) single-crystal LiNi 1-x-y Mn x Co y O 2 (NMCs) have garnered recent interest as cathodes in lithium (Li)-ion batteries (LIBs). However, capacity fade at high voltages, particularly after the onset of the H2–H3 phase transition, hampers their viability. In this study, single-crystal LiNi 0.8 Mn x Co 0.2-x O 2 (x = 0.2, 0.1, 0) are synthesized and tested in LiPF 6 in ethyl methyl carbonate-based electrolytes, with and without monofluoroethylene carbonate and LiF 2 PO 2 additives, to clarify the effects of Co/Mn ratio and surface stabilization on high-voltage cycling degradation. By imposing a kinetic barrier to the accessible H2–H3 capacity, surface reconstruction is identified as the primary driver of high-voltage capacity loss, being greater in the Co-free cathode and in the absence of fluorinated electrolyte components. This is attributed to a synergy between increased mechanical stress due to worsened bulk and interfacial H2–H3 kinetics and decreased interfacial stability due to the poor passivating capability of the electrolyte. Here, the findings highlight the importance of limiting cathode impedance growth during high-voltage cycling, which can be achieved by tuning bulk dopants and electrolyte chemistry.

25 ENERGY STORAGE↗

Evaluation of Gas Formation and Consumption Driven by Crossover Effect in High-Voltage Lithium-Ion Batteries with Ni-Rich NMC Cathodes

Gas formation during lithium-ion battery (LIB) cycling impacts the stability and safety of these batteries, especially for those containing Ni-rich NMC cathodes. In this paper, the cycling performance and gassing behavior of NMC811/graphite full cells with 4.2 and 4.4 V upper cutoff voltages were first compared. We report cells with a 4.2 V upper cutoff voltage had good cycling stability, exhibiting a capacity retention of 96.8% after 100 cycles and generated little gas. On the other hand, cells with a 4.4 V upper cutoff voltage lost over 25% of initial capacity after 100 cycles and generated large amounts of gas in the first 10 cycles. Electrochemical cycling of anode and cathode symmetric cells was implemented to isolate gases formed at the electrode. Gas chromatography–mass spectrometry, Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy, and scanning transmission electron microscopy were used to characterize the gas formation and associated material surfaces and structural properties. It was found that CO2 and fluorinated alkanes were the dominant gases evolved on the cathode side during cycling to 4.4 V. Gas crossover to the anode led to the depletion of gaseous products, which stabilized the cell performance to some extent. However, the growing surface reconstruction layer at the cathode, the thickening of the solid electrolyte interphase layer at the anode, and the gradual depletion of lithium inventory collectively contributed to the continuous capacity loss of full cells cycled to 4.4 V.

25 ENERGY STORAGE↗

Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging

Rapid charging of Li-ion batteries is limited by lithium plating on graphite anodes, whereby Li+ ions are reduced to Li metal on the graphite particle surface instead of inserting between graphitic layers, which directly contributes to cell capacity loss because of the low reversibility of the Li plating/stripping process. Furthermore, precisely identifying the onset and amount of Li plating is therefore vital in order to remedy these issues. We demonstrate a titration technique with a detection limit of 20 nmol (5 × 10 –4 mAh) of Li that can be used to quantify inactive Li that remains on the graphite electrode after fast charging. The titration is extended to quantify the total amount of solid carbonate species and lithium acetylide (Li 2 C 2 ) within the solid–electrolyte interphase (SEI), and electrochemical modeling is used to determine the Li plating exchange current density (10 A/m 2 ) and stripping efficiency (65%) of plated Li metal on graphite. These techniques provide a highly accurate measure of the onset of Li plating and quantitative insight into graphite SEI evolution during fast charging.

25 ENERGY STORAGE↗

In Situ and Operando Observation of Zinc Moss Growth and Dissolution in Alkaline Electrolyte for Zinc–Air Batteries

As a promising battery technology, zinc–air batteries still face significant challenges, including the formation of a mossy structure on the zinc metal anode in alkaline electrolyte. Because a similar phenomenon also plagues lithium and sodium metal batteries, elucidating its mechanism has important implications for progress in energy storage. Herein, operando X-ray nanotomography was employed to visualize zinc moss growth and dissolution at the individual colony level. By tracking its microstructure evolution, zinc moss was found to display irreversible plating/stripping behavior. While zinc moss exhibits self-limiting growth and zinc deposition occurs mainly in its outer region, zinc dissolution is more uniformly distributed inside the moss colony upon stripping, leading to the formation of “dead” zinc and capacity loss. A direct correlation is established between the moss amount and zinc plating/stripping efficiency. Finally, results from this study offer new insights into mitigating the unstable zinc plating morphology and improving the cycle life of aqueous zinc–air batteries.

36 MATERIALS SCIENCE↗

Reactive Suspension Electrolytes for Lithium Metal Batteries

Lithium metal batteries (LMBs) suffer from dendrite growth and capacity loss, which compromise safety and cycle life. Here, we present a simple reactive suspension electrolyte (RSE) strategy. When metal oxide (MO x ) nanoparticles are dispersed in the liquid electrolyte, in situ formation of Li 2 O and Li–M phases occurs at the lithium metal anode. By studying two different types of RSEs, Type 1 RSEs (i.e., CuO RSE) without metal-Li alloying and Type 2 RSEs (i.e., ZnO RSE and In 2 O 3 RSE) with metal-Li alloying capability, we elucidate the roles of each reaction compound. Here, we find that Li 2 O can improve reversibility of Li metal anode by stabilizing the interphase while Li–M alloy phases guide uniform Li metal plating. Compared to the carbonate-type reference electrolyte, RSEs demonstrate reduced nucleation overpotential, lower interfacial impedance, and higher Coulombic efficiency, leading to an extended cycle life in Li|Li 1 Ni 0.8 Co 0.1 Mn 0.1 O 2 full cells.

Lee, Junyoung [Stanford Univ., CA (United States)]↗

Effect of Chemical Lithium Intercalation into Rutile TiO2 Nanorods

Rutile TiO2 nanorods were synthesized by hydrolysis of TiCl4 followed by a hydrothermal method. Lithium insertion into the rutile nanorods was achieved by a chemical lithium intercalation process. The structural evolution of nano-structured rutile upon lithium intercalation was characterized by several experimental techniques, namely, XRD, TEM and 6Li MAS NMR. The XRD and TEM studies indicate the formation of a new lithium titanate phase (LixTiO2) during lithium intercalation. Additionally, SAED patterns show that the lithium titanate phase has cubic symmetry. Finally, ultra-high magnetic field (21.1T) 6Li MAS NMR reveals that the lithium titanate phase adopts two different structures depending on lithium content. Taken together, the three techniques consistently show that the intercalation of lithium into rutile TiO2 nanorods causes two consecutive structural phase transformations to lithium titanate phases with spinel (Fd m) and rocksalt (Fm m) structures at x=0.46 and 0.88, respectively. In addition, the broad line widths in the 6Li MAS NMR spectrum of the rocksalt phase are indicative of a disordered structure. Density functional theory calculations of the rutile, spinel and rocksalt bulk phases as a function of lithium content corroborate the observed phase transformations. These phase transitions could account for the large irreversible capacity loss of nano-structured rutile anodes observed in electrochemical cycling experiments.

36 MATERIALS SCIENCE↗

Formation Of The Spinel Phase In The Layered Composite Cathode Used In Li-Ion Batteries

Pristine Li-rich layered cathodes, such as Li1.2Ni0.2Mn0.6O2 and Li1.2Ni0.1Mn0.525Co0.175O2, were identified to exist in two different structures: LiMO2 R-3m and Li2MO3 C2/m phases. Upon charge/discharge cycling, both phases gradually transform to the spinel structure. The transition from LiMO2 R-3m to spinel is accomplished through the migration of transition metal ions to the Li site without breaking down the lattice, leading to the formation of mosaic structured spinel grains within the parent particle. In contrast, transition from Li2MO3 C2/m to spinel involves removal of Li+ and O2-, which produces a large lattice strain and leads to the breakdown of the parent lattice and therefore the newly formed spinel grains show random orientation within the same particle. Cracks and pores were also noticed within some particles, which is believed to be the consequence of the breakdown of the lattice and vacancy condensation upon removal of lithium ions. The presently observed structure transition characteristics provide direct reasons for the observed gradual capacity loss and poor rate performance of the layered composite. Ultimately it also provides clues about how to improve the materials structure with potential improved performance.

Environmental Molecular Sciences Laboratory↗

Mesoporous Silicon Sponge as an Anti-Pulverization Structure for High-Performance Lithium-ion Battery Anodes

Nanostructured silicon is a promising anode material for high performance lithium-ion batteries, yet scalable synthesis of such materials, and retaining good cycling stability in high loading electrode remain significant challenges. Here, we combine in-situ transmission electron microscopy and continuum media mechanical calculations to demonstrate that large (>20 micron) mesoporous silicon sponge (MSS) prepared by the scalable anodization method can eliminate the pulverization of the conventional bulk silicon and limit particle volume expansion at full lithiation to ~30% instead of ~300% as observed in bulk silicon particles. The MSS can deliver a capacity of ~750 mAh/g based on the total electrode weight with >80% capacity retention over 1000 cycles. The first-cycle irreversible capacity loss of pre-lithiated MSS based anode is only <5%. The insight obtained from MSS also provides guidance for the design of other materials that may experience large volume variation during operations.

anode↗

Three-dimensional bicontinuous ultrafast-charge and -discharge bulk battery electrodes

Rapid charge and discharge rates have become an important feature of electrical energy storage devices, but cause dramatic reductions in the energy that can be stored or delivered by most rechargeable batteries (their energy capacity). Supercapacitors do not suffer from this problem, but are restricted to much lower stored energy per mass (energy density) than batteries. A storage technology that combines the rate performance of supercapacitors with the energy density of batteries would significantly advance portable and distributed power technology. Furthermore, we demonstrate very large battery charge and discharge rates with minimal capacity loss by using cathodes made from a self-assembled three-dimensional bicontinuous nanoarchitecture consisting of an electrolytically active material sandwiched between rapid ion and electron transport pathways. Rates of up to 400C and 1,000C for lithium-ion and nickel-metal hydride chemistries, respectively, are achieved (where a 1C rate represents a one-hour complete charge or discharge), enabling fabrication of a lithium-ion battery that can be 90% charged in 2 minutes.

25 ENERGY STORAGE↗

Predictive modeling of battery degradation and greenhouse gas emissions from U.S. state-level electric vehicle operation

Electric vehicles (EVs) are widely promoted as clean alternatives to conventional vehicles for reducing greenhouse gas (GHG) emissions from ground transportation. However, the battery undergoes a sophisticated degradation process during EV operations and its effects on EV energy consumption and GHG emissions are unknown. Here we show on a typical 24 kWh lithium-manganese-oxide–graphite battery pack that the degradation of EV battery can be mathematically modeled to predict battery life and to study its effects on energy consumption and GHG emissions from EV operations. We found that under US state-level average driving conditions, the battery life is ranging between 5.2 years in Florida and 13.3 years in Alaska under 30% battery degradation limit. The battery degradation will cause a 11.5–16.2% increase in energy consumption and GHG emissions per km driven at 30% capacity loss. This study provides a robust analytical approach and results for supporting policy making in prioritizing EV deployment in the U.S.

Science & Technology - Other Topics↗

Parasitic structure defect blights sustainability of cobalt-free single crystalline cathodes

Abstract Recent efforts to reduce battery costs and enhance sustainability have focused on eliminating Cobalt (Co) from cathode materials. While Co-free designs have shown notable success in polycrystalline cathodes, their impact on single crystalline (SC) cathodes remains less understood due to the significantly extended lithium diffusion pathways and the higher-temperature synthesis involved. Here, we reveal that removing Co from SC cathodes is structurally and electrochemically unfavorable, exhibiting unusual voltage fade behavior. Using multiscale diffraction and imaging techniques, we identify lithium-rich nanodomains (LRNDs) as a heterogeneous phase within the layered structure of Co-free SC cathodes. These LRNDs act as critical tipping points, inducing significant chemo-mechanical lattice strain and irreversible structural degradation, which exacerbates the voltage and capacity loss in electrochemical performance. Our findings highlight the considerable challenges of developing Co-free SC cathodes compared to polycrystalline ones and emphasize the need for new strategies to balance the interplay between cost, sustainability, and performance.

36 MATERIALS SCIENCE↗

Chemical factors controlling the behaviour of oxide cathodes in batteries

Oxide cathodes enable high-energy lithium-ion and sodium-ion batteries, with their performances fundamentally governed by three interrelated chemical factors: electronic configuration, chemical bonding, and chemical reactivity. Here, we illustrate how these factors dictate the redox energy, structural stability, ionic and electronic transport, and interfacial behavior in both layered oxide and polyanion oxide cathodes. We discuss how crystal-field effects and octahedral-site stabilization energies influence cation migration, and how inductive effects tune bond covalency and operating voltages. We also explain how chemical bonding governs thermal stability, gas evolution, and first-cycle capacity loss, and how alignment of transition-metal redox band with the oxygen 2p band determines electrolyte reactivity. Comparison between lithium and sodium layered oxides further reveals how differences in Li-O and Na-O bond ionicity affect chemical reactivity. Finally, we outline strategies including compositional tuning, surface doping, and electrolyte optimization, and emphasize how high-throughput, data-driven approaches in guiding the design of next-generation oxide cathodes.

25 ENERGY STORAGE↗

Dynamic spatial progression of isolated lithium during battery operations

The increasing demand for next-generation energy storage systems necessitates the development of high-performance lithium batteries. Unfortunately, current Li anodes exhibit rapid capacity decay and a short cycle life, owing to the continuous generation of solid electrolyte interface and isolated Li (i-Li). The formation of i-Li during the nonuniform dissolution of Li dendrites leads to a substantial capacity loss in lithium batteries under most testing conditions. Because i-Li loses electrical connection with the current collector, it has been considered electrochemically inactive or ‘dead’ in batteries. In this work, contradicting this commonly accepted presumption, we show that i-Li is highly responsive to battery operations, owing to its dynamic polarization to the electric field in the electrolyte. Simultaneous Li deposition and dissolution occurs on two ends of the i-Li, leading to its spatial progression toward the cathode (anode) during charge (discharge). Revealed by our simulation results, the progression rate of i-Li is mainly affected by its length, orientation and the applied current density. Moreover, we successfully demonstrate the recovery of i-Li in Cu–Li cells with >100% Coulombic efficiency and realize LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC)–Li full cells with extended cycle life.

25 ENERGY STORAGE↗

Structural and electronic properties of Li8ZrO6 and its CO2 capture capabilities: an ab initio thermodynamic approach

The structural, electronic, and phonon properties of Li8ZrO6 are investigated with the application of density functional theory and lattice phonon dynamics. Based on the calculated data, the thermodynamics of CO2 absorption?desorption for Li8ZrO6 is analyzed and compared with those of Li2ZrO3 and Li6Zr2O7. The band gap of Li8ZrO6 is indirect along G?L with a value of 4.74 eV. From the calculated thermodynamic properties of Li8ZrO6 reacting with CO2, we found that Li8ZrO6 could be regenerated at high temperatures (>1100 K). Our results indicated that the lithium zirconate with a lower Li2O/ZrO2 ratio has a lower turnover temperature. Hence, by mixing or doping two or more materials to form a new material, it is possible to find or synthesize CO2 sorbents that can fit the industrial needs for optimal performance. Although the CO2 capture capacity of Li8ZrO6 is much higher than that of Li2ZrO3, the high energy required for regeneration, the capacity loss during long absorption?desorption cycles, solid sintering at high temperature, and the material cost may affect its overall capture performance. Our results also provided some general guidelines for designing new CO2 sorbents.

Duan, Y↗

Stackable bipolar pouch cells with corrosion-resistant current collectors enable high-power aqueous electrochemical energy storage

A critical bottleneck in the development of aqueous electrochemical energy storage systems is the lack of viable complete cell designs. Here, we report a metal-free, bipolar pouch cell designed with carbon black/polyethylene composite film (CBPE) current collectors as a practical cell architecture. The light-weight, corrosion-resistant CBPE provides stable operation in a variety of aqueous electrolytes over a ~2.5 V potential range. Because CBPE is heat-sealable, it serves simultaneously as both the pouch cell packaging and seal in addition to its use as a current collector. Although this non-metallic composite has a low electrical conductivity relative to metal foils, current travels only a short distance in the through-plane direction of the current collector in the bipolar cell configuration. This shorter path length lowers the effective electrical resistance, making the design suitable for high-power applications. We test the cell architecture using an aqueous ZnBr 2 battery chemistry and incorporate tetrabutylammonium cations to improve the intrinsic low Coulombic efficiency and fast self-discharge of non-flow ZnBr 2 cells. These devices demonstrate a cell-level energy density of 50 W h L -1 at a 10C rate (0.5 kW L -1 ), with less than 1% capacity loss over 500 cycles. A large-area (>6 cm 2 ) 4-cell stack is built to illustrate that the pouch cells are scalable to practical dimensions and stackable without sacrificing performance. The device operates in the range of 6–7 V and has an internal self-balancing mechanism that prevents any individual cell in the stack from overcharging. The results thus demonstrate both a conceptually new cell architecture that is broadly applicable to many aqueous electrolyte chemistries and a specific high-performance example thereof.

25 ENERGY STORAGE↗

Nanoscale in situ detection of nucleation and growth of Li electrodeposition at various current densities

Li metal batteries can store at least ten times more energy than currently existing Li-ion batteries. However, during routine charging and discharging, Li dendrites grow on the Li metal electrode, which can lead to capacity loss by the consumption of Li salt at the surface of the Li dendrites, and be a safety hazard resulting from the potential for short-circuits. Although past efforts have provided useful information about the morphology and surface area of Li dendrite formation at the microscale, a nanoscale understanding of nucleation and growth of Li nanoparticle electrodeposition is still elusive. In this study, using a new electrochemical cell for transmission mode grazing incidence small angle X-ray scattering, we obtained, for the first time, the primary nucleus size of Li nanoparticles, their size evolution and their fractal structures at various current densities and in real-time. The measured average radius of gyration, R g , at current densities of 0.1, 0.5, and 2.0 mA cm -2 is 5.4 ± 0.4, 4.5 ± 0.3, and 3.5 ± 0.3 nm, respectively. This variation in size with current density is noteworthy when recognizing that the surface area-to-volume ratio of the Li nanoparticles is 3.7 times higher at 2.0 mA cm -2 than at 0.1 mA cm -2 . We also compared a hierarchical fractal structure of Li particles from the nanometer to micrometer scale. Our findings illuminate the role of overpotential in the reactive surface area of Li dendrites at the nanoscale, and provide a novel research platform for suppressing Li dendrite formation in Li metal battery systems.

25 ENERGY STORAGE↗

Suppressing the Voltage Decay of Low-Cost P2-Type Iron Based Cathode Materials for Sodium-ion Batteries

Rechargeable sodium-ion batteries with earth abundant Fe/Mn based cathodes are promising choice for grid-scale applications. However, the important candidate, P2-type Fe based materials suffer from server voltage decay during battery operation, which is due to the Fe 3+ migration to the neighboring tetrahedral sites. Two Fe based layered oxides Na 0.7 [Cu 0.15 Fe 0.3 Mn 0.55 ]O 2 and Na 0.7 [Cu 0.2 Fe 0.2 Mn 0.6 ]O 2 have been prepared. With the combination of in-situ XRD, X-ray PDF, hard and soft X-ray absorption, we demonstrate that the voltage decay in Fe based layered oxides comes from a dynamic origin. Dramatic phase transition can be triggered by higher upper voltage limit and partially irreversible Fe migration lead to voltage fade. With excess Cu doping into crystal lattice, Fe migration can be much mitigated and structural stability can therefore be maintained. Furthermore, Cu introduction brings about extra capacity via the correlation between transition metals elements and ligand oxygen, which may well compensate capacity loss from inert impurity doping. Finally, possible strategies for suppressing the detrimental voltage decay in battery cathodes can be proposed accordingly.