Search NASA⌕ Search

SEARCH · Search NASA

Results for “ABRASIVES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

The subsurface structure of abraded Al–Zn–Mg–Cu alloy

Surface abrasion has been shown to introduce heavy shear stress and produce a few hundred nanometers thick altered surface layer (ASL) on Al alloys. Such ASLs exhibit microstructural changes at room temperature and different corrosion resistance than the underlying substrate. Here, we report how sample dimensions and temperature affect the deformed subsurface microstructure evolution on an abraded Al–Zn–Mg–Cu alloy using transmission electron microscopy (TEM) and atom probe tomography. The ASL microstructure evolves differently in the bulk sample than in the thin TEM specimen. In the freshly abraded ASL, the original η'/η precipitates and grain boundaries were deformed toward the abrasion direction. After 7-day natural aging of the freshly abraded bulk sample, well-defined subgrains formed locally in the ASL, and unusual Al 2 Cu (θ) and Mg x Zn y phases precipitated at the subgrain boundaries. However, during natural aging of this TEM specimen taken from the abraded and aged bulk samples, much faster changes occurred, including the continued formation of subgrains and θ particles in the entire ASL, and the diffusion of Zn atoms out of Mg x Zn y particles to form a Zn particle. On the other hand, no obvious microstructural changes occurred in the ASL during 3-month natural aging of the TEM specimen immediately taken from the freshly abraded sample. Finally, this work advances the understanding of how Al alloy microstructures respond during and following any shear deformation, and complex and unexpected effects of sample dimensions on the behavior.

36 MATERIALS SCIENCE↗

The characterization of wear-causing particles and silica sand in particular

Erodants and abradants are two types of wear-causing particles (WCP). Despite their effects on the severity and rate of wear, WCP are inadequately characterized in a surprising number of publications, especially those involving impingement erosion and three-body abrasion. That shortfall makes it difficult to correlate features of WCP with the details of worn surfaces, or to develop wear models that account for those features. It is argued that the documentation of WCP should go beyond simply reporting their composition and mean particle size. In late 1985, ASTM Committee G2 on Wear and Erosion established a task group on the characterization of WCP. At that time, image analysis was slower and less sophisticated than it is today. While that ASTM task group failed to produce a consensus standard, computerized particle characterization methods were developing in fields other than tribology, fields like geoscience, heavy sand mining, materials processing, and pharmaceuticals. A notable exception to this is ferrography, which is a widely-used diagnostic for lubricated tribosystems. In the context of dry wear, it is useful to identify which features of WCP would be beneficial to document, and to identify some techniques and scales of detail appropriate to particular tribosystems. In this paper, examples are presented for the morphological and mechanical characterization of silica sand grains, as prompted by a triboanalysis of the abrasive and erosive wear of biomass pre-processing equipment. The authors propose a minimum level of documentation for WCP, one that can enrich tribosystem analysis both in laboratory tests and field studies.

36 MATERIALS SCIENCE↗

Laser interference structuring of Cu for adhesive joining of HVAC equipment

Due to potential energy and cost savings benefits, adhesive joining has been recently considered for heating, ventilation, air conditioning, and refrigeration (HVAC&R) systems. HVAC adhesive bonding requires cost-effective and adequate surface preparations of adherents. Here, this article investigates the use of abrasion, traditional single-beam laser, and a laser-interference technique as surface preparations of copper surfaces. Surface morphology is characterized using scanning electron microscopy (SEM) and atomic force microscopy (AFM). Effective submicrometer peak-to-valley structuring with a periodicity of ∼2.7μ⁢m was demonstrated for laser-interference processing. Single-lap shear tests were conducted for 89 joints made with bondline thicknesses of 0.15 and 0.3 mm. Data on process variables and measured variables included open-time, bond length, maximum load, displacement at failure, shear lap strength, and failure mode. A statistical analysis was conducted on each lot to determine the lower limit with 95% confidence intervals for displacements at failure and shear lap strengths. A comparison is presented between the properties of laser-structured joints with respect to those prepared by abrasion, which is considered the baseline surface preparation technique. Based on this comparison, one single-beam laser technique and two laser-interference techniques were shown to exhibit vastly superior performance over the joints made with abraded specimens.

Sabau, Adrian S. [Oak Ridge National Laboratory (O↗

Fabrics coated with lubricated nanostructures display robust omniphobicity

The development of a stain-resistant and pressure-stable textile is desirable for consumer and industrial applications alike, yet it remains a challenge that current technologies have been unable to fully address. Traditional superhydrophobic surfaces, inspired by the lotus plant, are characterized by two main components: hydrophobic chemical functionalization and surface roughness. While this approach produces water-resistant surfaces, these materials have critical weaknesses that hinder their practical utility, in particular as robust stain-free fabrics. For example, traditional superhydrophobic surfaces fail (i.e., become stained) when exposed to low-surface-tension liquids, under pressure when impacted by a high-velocity stream of water (e. g., rain), and when exposed to physical forces such as abrasion and twisting. We have recently introduced slippery lubricant-infused porous surfaces (SLIPS), a self-healing, pressure-tolerant and omniphobic surface, to address these issues. Herein we present the rational design and optimization of nanostructured lubricant-infused fabrics and demonstrate markedly improved performance over traditional superhydrophobic textile treatments: SLIPS-functionalized cotton and polyester fabrics exhibit decreased contact angle hysteresis and sliding angles, omni-repellent properties against various fluids including polar and nonpolar liquids, pressure tolerance and mechanical robustness, all of which are not readily achievable with the state-of-the-art superhydrophobic coatings.

Shillingford, C↗

Investigation on nanoscale material removal process of BK7 and fused silica glass during chemical‐mechanical polishing

Abstract Understanding the nanoscale material removal process in chemical mechanical polishing (CMP) is of fundamental importance for the operation and further development of CMP. In this study, the nanoscale material removal processes of both fused silica glass and BK7 glass were investigated based on single‐pad‐asperity polishing experiments. The results indicate that the material removal characteristics are highly dependent on the composition and structure of glass materials. In the mechanically induced chemical bonding removal mode, only atoms locate near the outermost several layers can participate in the formation and breakage of interfacial bridge bonds. Moreover, the force on the abrasive particle must exceed a threshold value to induce significant removal of Si atoms from the glass substrate, because as the breakage of Si glass –O backbonds does not occur in low‐stress conditions. We reveal for the first time that the chemical and mechanical properties of the topmost layer, which is recognized as densification, hydrated, or redeposition layer, have not been significantly affected by the mechanical action of the abrasive particles when polishing in this kind of material removal mode. The results are expected to provide a deeper insight into the nanoscale material removal mechanism during glass CMP.

Wang, Lin↗

Zirconia-coated carbonyl-iron-particle-based magnetorheological fluid for polishing optical glasses and ceramics

We report on magnetorheological finishing (MRF) spotting experiments performed on glasses and ceramics using a zirconia-coated carbonyl-iron (CI)-particle-based magnetorheological (MR) fluid. The zirconia-coated magnetic CI particles were prepared via sol-gel synthesis in kilogram quantities. The coating layer was {approx}50-100 nm thick, faceted in surface structure, and well adhered. Coated particles showed long-term stability against aqueous corrosion. ''Free'' nanocrystalline zirconia polishing abrasives were cogenerated in the coating process, resulting in an abrasive-charged powder for MRF. A viable MR fluid was prepared simply by adding water. Spot polishing tests were performed on a variety of optical glasses and ceramics over a period of nearly three weeks with no signs of MR fluid degradation or corrosion. Stable material removal rates and smooth surfaces inside spots were obtained.

36 MATERIALS SCIENCE↗

Process Parameter Effects on Material Removal in Magnetorheological Finishing of Borosilicate Glass

We investigate the effects of processing parameters on material removal for borosilicate glass. Data are collected on a magnetorheological finishing (MRF) spot taking machine (STM) with a standard aqueous magnetorheological (MR) fluid. Normal and shear forces are measured simultaneously, in situ, with a dynamic dual load cell. Shear stress is found to be independent of nanodiamond concentration, penetration depth, magnetic field strength, and the relative velocity between the part and the rotating MR fluid ribbon. Shear stress, determined primarily by the material mechanical properties, dominates removal in MRF. The addition of nanodiamond abrasives greatly enhances the material removal efficiency, with the removal rate saturating at a high abrasive concentration. The volumetric removal rate (VRR) increases with penetration depth but is insensitive to magnetic field strength. The VRR is strongly correlated with the relative velocity between the ribbon and the part, as expected by the Preston equation. A modified removal rate model for MRF offers a better estimation of MRF removal capability by including nanodiamond concentration and penetration depth.

Miao, C↗

Wear behavior of Al 0.6 CoCrFeNi high-entropy alloys: Effect of environments

Environment can impact the wear behavior of metals and alloys substantially. The tribological properties of Al 0.6 CoCrFeNi high-entropy alloys (HEAs) were investigated in ambient air, deionized water, simulated acid rain, and simulated seawater conditions at frequencies of 2–5 Hz. The as-cast alloy was composed of simple face-centered cubic and body-centered cubic phases. The wear rate of the as-cast HEA in the ambient air condition was significantly higher than that in the liquid environment. The wear resistance in seawater was superior to that in ambient air, deionized water, and acid rain. Both the friction coefficient and wear rate in seawater were the lowest due to the formation of oxidation film, lubrication, and corrosion action in solution. The dominant wear mechanism in the ambient air condition and deionized water was abrasive wear, delamination wear, and oxidative wear. Here by contrast, the wear mechanism in acid rain and seawater was mainly corrosion wear, adhesive wear, abrasive wear, and oxidative wear.

36 MATERIALS SCIENCE↗

Ultra-fast Boriding for Improved Energy Efficiency and Reduced Emissions in Materials Processing Industries (Final Report)

High-temperature treatment processes (such as nitriding, carburizing, and boronizing) are well-established and used widely by numerous industrial sectors to achieve superior mechanical and tribological properties on all kinds of engineering components made out of ferrous materials. Unfortunately, these traditional processes are very slow and energy intensive, and they produce large amounts of CO 2 emissions and liquid/solid wastes to deal with during and after each process run. From economic and environmental points of views, it is highly desirable to develop and implement novel surface treatment technologies that are quick, cheap, clean, and energy efficient. The main objective of this project was to develop an industrial-scale ultra-fast boriding process that realizes all of these desirable attributes. The other objectives of the project were to demonstrate the superior performance, properties, and durability of borided surfaces under relevant test conditions and to transfer optimized technology to industry for large-scale practice. Major research activities included process design, modeling, product optimization, and scale-up. This project has achieved all of its stated objectives, and the industrial-scale boriding process has been successfully transferred to industry. Specifically, all of the original tasks have been completed, and the milestones have been met by scaling up from a small proof-of-concept system (which could only handle about 0.25 kg melt) to a commercial-scale boriding unit that can handle up to 4,000 kg melt. Mechanical and tribological testing of borided test samples and industrial parts has also been carried out, and their superior performance over a broad range of test conditions has been validated. With the large-scale, ultra-fast boriding process, we could achieve thick, hard, and uniform boride layers on all kinds of steel components, even after only 5 min of treatment time. We could also attain excellent uniformity in thickness over the entire exposed surfaces — even in the very sharp corners or interior sections of odd-shaped workpieces. Boriding of numerous nonferrous materials was also demonstrated, and thick boride layers (up to 300 µm in thickness) were achieved on their outer surfaces. With the use of a large-scale boriding unit at Argonne National Laboratory, our research team has successfully treated large numbers of industrial components in a batch-to-batch operation without creating any in-house gaseous emissions or producing solid and/or liquid wastes. With the use of this large unit, our team achieved surface hardness values of 15 to 45 GPa, depending on the type of metal or alloy being treated. The thick boride layers attained on steel components consisted of FeB, Fe 2 B, and Fe 3 B phases, and their hardness values ranged from 16 to 22 GPa. Layers consisting of Fe 2 B phase alone are also possible with this process, and in the case of nonferrous materials. Overall, because of the much superior property and performance improvements in treated products, much lower energy consumption, and nearly zero environmental waste and emissions, the demonstrated boriding technology may find broad applications in many cross-cutting industries. Mechanical wear, abrasion, erosion, corrosion, and scuffing are often life-limiting factors in mechanical systems that are used in manufacturing, transportation, aerospace, agricultural, earth-moving, and mining equipment; but the machine components treated by ultra-fast boriding can effectively prevent such degradations. In this project, the ultra-fast boriding was proven to be most ideal for the treatment of iron and many other ferrous alloys, like stainless steel. We have shown through our experimental studies that our method can also be used for the treatment of many nonferrous metals and alloys. In the case of superalloys and Ni 3 Al intermetallic materials, more than a 300-µm thick boride layer can be achieved with our boriding furnace within 15 to 30 min (which results in five times the hardness of the base materials). Pre-carburized steels and nonferrous alloys can also be treated by the new boriding technique. Overall, very thick (more than a quarter millimeter) and hard surface layers produced by ultra-fast boriding are expected to have a positive impact on the performance and durability of all types of machine components that are subject to corrosive, erosive, abrasive, and adhesive wear. Since the focus of our project was primarily on the large-scale boriding of ferrous materials, in this report, we will broadly cover the results from various ferrous materials that were used in our experiments. Another transformational feature of ultra-fast boriding is that it does not create any greenhouse gas emissions or solid and/or liquid wastes to deal with during or after the treatment; hence, it is an ultra-green technology (no need for expensive waste disposal and/or treatment facilities). It may eliminate the use of natural gas and other carbon-based fuels as the primary energy source in the heat treatment industry (which is the most common practice at present), thus, minimizing the CO 2 , NO x , CO, and SO x emissions that are generated in large quantities by current heat treatment practices. The main ingredient used during boriding is borax, which is a natural mineral. Our demonstrated and scaled-up technology can now be used in a wide range of manufacturing and transportation applications. It can deliver thick and uniform boride layers of more than 200 µm in steels, if needed, over the entire exposed surfaces — even in the very sharp corners or interior sections of workpieces (which are typical of gears, tools, pipes, and other components). Beneath the distinct boride layers is an equally-thick boron diffusion layer or zone, which is comparable to the diffusion zones achieved by carburizing and nitriding processes. In the cases of traditional boriding, nitriding, and/or carburizing methods, achieving such layer thickness and case depths would have taken several hours, and these surfaces would not have achieved the same levels of hardness and other desirable properties as they do with ultra-fast boriding. Some of the key stakeholders of ultra-fast boriding technology include companies that are active in heat-treatment, thermal-diffusion, and hard-coating processes; metal-forming, machining, and other manufacturing processes; and technologies related to transportation (including original equipment manufacturers for autos), mining and oil exploration, agricultural and heavy equipment. Bodycote Thermal Processing was the cost-sharing industrial partner and licensee in this project. They also provided test components and technical and commercial information pertaining to industrial components that are most suitable for ultra-fast boriding. Bodycote also coordinated some of the field tests and metallurgical examinations. Overall, ultra-fast boriding is a transformational technology that can complement, if not replace, many of the energy- and carbon-intensive surface treatment processes that are in use today, such as conventional boriding, carburizing, nitriding, carbo-nitriding, and physical and chemical vapor deposition. In our project, the developed technology was scaled-up and proven to be an ultra-green, ultra-efficient process that can drastically reduce costs, increase productivity, and improve the performance and reliability of machine components used in cross-cutting industrial applications.

Erdemir, Ali↗

Simulant Development for Hanford Tank Farms Double Valve Isolation (DVI) Valves Testing

Leakage testing of a representative sample of the safety-significant isolation valves for Double Valve Isolation (DVI) in an environment that simulates the abrasive characteristics of the Hanford Tank Farms Waste Transfer System during waste feed delivery to the Waste Treatment and Immobilization Plant (WTP) is to be conducted. The testing will consist of periodic leak performed on the DVI valves after prescribed numbers of valve cycles (open and close) in a simulated environment representative of the abrasive properties of the waste and the Waste Transfer System. The valve operations include exposure to cycling conditions that include gravity drain and flush operation following slurry transfer. The simulant test will establish the performance characteristics and verify compliance with the Documented Safety Analysis. Proper simulant development is essential to ensure that the critical process streams characteristics are represented, National Research Council report “Advice on the Department of Energy's Cleanup Technology Roadmap: Gaps and Bridges”

DVI Simulant↗

Preliminary photovoltaic arc-fault prognostic tests using sacrificial fiber optic cabling.

Through the New Mexico Small Business Assistance Program, Sandia National Laboratories worked with Sentient Business Systems, Inc. to develop and test a novel photovoltaic (PV) arc-fault detection system. The system operates by pairing translucent polymeric fiber optic sensors with electrical circuitry so that any external abrasion to the system or internal heating causes the fiber optic connection to fail or detectably degrade. A periodic pulse of light is sent through the optical path using a transmitter-receiver pair. If the receiver does not detect the pulse, an alarm is sounded and the PV system can be de-energized. This technology has the unique ability to prognostically determine impending failures to the electrical system in two ways: (a) the optical connection is severed prior to physical abrasion or cutting of PV DC electrical conductors, and (b) the polymeric fiber optic cable melts via Joule heating before an arc-fault is established through corrosion. Three arc-faults were created in different configurations found in PV systems with the integrated fiber optic system to determine the feasibility of the technology. In each case, the fiber optic cable was broken and the system annunciated the fault.

Johnson, Jay Dean↗

Abradable Sealing Materials for Emerging IGCC-Based Turbine Systems (Final Report)

Reducing the gap between rotating and stationary parts in gas turbine engines, and mitigating gas leakage via these paths, can significantly increase the performance and attendant efficiency. One approach to reducing such gaps is to deploy abradable coatings on the stationary shroud components as seals, to reduce the blade-tip clearances under operational conditions. Abradable coatings must be able to withstand high temperature oxidation, thermal cycling, and erosion, while providing optimal controlled abrasion and associated shape retention. Existing abradable seals utilized in power generation turbines have generally been optimized for use with natural gas-fired systems; however, preliminary testing of syngas and high-hydrogen-content (HHC) fired turbines has shown that the stability of hot-section materials (and presumably abradable sealing materials) may be substantially altered due to characteristic changes in the combustion by-products (partial pressures of water vapor, etc.) as well as characteristic impurities and particulate matter entrained in the fuel. The primary focus of this research program has been to develop a mechanistic understanding of how the altered combustion environments modify the thermo-mechanical stability and performance of the sealing materials, including the requisite abradable sealing behavior. A key component of the research program carried out has been an exploration of mechanisms underpinning observed degradation processes, and an assessment of connections to the combustion environments and characteristic non-combustible constituents. The ultimate goal of the project has been to advance the goals of the Advanced Turbine Program by developing materials design protocols leading to turbine hot-section components with improved resistance to service lifetime degradation under advanced fuels exposures. This research program has evaluated the performance and degradation of ceramic abradable seals used in the high-temperature turbine sections of gas turbine engines. The focus has been two-fold: (1) to understand performance of such materials in relation to the turbines operating on coal-derived syngas and high hydrogen content (HHC) fuels, ultimately seeking an improved understanding of factors that control performance and durability of abradable seal materials for these combustion environments (and play into materials design protocols); and (2) to evaluate the potential of alternative materials as abradable seals for the higher temperatures expected with IGCC and HHC fueled turbine systems. In particular, we carried out an initial assessment of multi-layered systems of existing abradable seal materials (YSZ) and other ceramics. The research program also investigated several classes of abradable coatings under simulated exposures to syngas-based combustion environments, evaluating the relevant wear behavior, hardness, stability under cyclic oxidation, and general thermo-mechanical behavior. The research also attempted to develop alternatives to carrying out full-scale combustion-based abradability test rig exposures to evaluate materials system performance. The research has been focused on correlating the measured thermo-mechanical behavior, and controlled abrasive wear, with the intrinsic properties of the multilayer coatings and processing-controlled microstructural features that have shown attractive machinability characteristics based on weak interfacial bonding between the constituent phases at elevate temperatures (while maintaining thermochemical stability). This program has resulted in an improved mechanistic understanding of factors governing performance of high temperature abradable seals, and degradation mechanisms unique to IGCC-based power generation turbine systems and the realization of coal-derived syngas and HHC-based combustion environments – ultimately with the goal of developing a knowledge base upon which the design of coatings that retain optimal sealing characteristics and are more resistant to the observed wear/attack mechanisms, important aspects of advancing the goals of the DOE Advanced Turbine Program.

36 MATERIALS SCIENCE↗

Neptunium(IV) Diffusion through Bentonite Clay

DOE Fellow, Silvina A. Di Pietro, completed a 10-week internship at Lawrence Livermore National Laboratory (LLNL) in Livermore, California. The objective of the study was to determine the diffusion profile of neptunium (Np) in bentonite clay (potential geo-engineered barrier for nuclear waste repositories). Under the mentorship of Drs. Claudia Joseph (Karlsruhe Institute of Technology, Germany) and Mavrik Zavarin, she prepared a series of core abrasion peeling samples. This procedure was a continuation of a Np diffusion experiment conducted by Dr. Joseph during her post-doc residency at LLNL in the year 2016. The second part of the experiment (from now on will be referred as abrasive peeling) focuses on understanding (1) the Np movement through the clay core and (2) the influence of temperature (25°C, 65°C, and 85°C) for the Np transport across the clay core under anaerobic conditions. End of 2016, the diffusion core samples were embedded in epoxy resin to stabilize them for long-term. The abraded core powder samples vary in material (epoxy vs. clay), Np activity and concentration, temperature exposed during the diffusion experiment, and mass, or amount of clay peeled off. Throughout the course of the 10-week internship program at LLNL, the experiments implemented and discussed in this report aimed to answer the questions: (1) How is the Np(IV) diffusion profile through bentonite influenced by the temperature? and (2) Will Np(IV) migrate through the geoengineered barrier of a nuclear waste repository? In addition, Ph.D. candidate Di Pietro received invaluable guidance in experimental design and development that will benefit her ongoing research endeavors.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Saltstone Grout Line Samples

During a prestart recirculation operation in the Saltstone Processing Facility (SPF), operations staff noticed hardened scaling falling into the hopper. As a result, SPF operators and Saltstone Engineering decided to postpone operation and conduct a process room hopper cleanout. During the cleanout effort personnel noted greater than normal buildup of damp solid material in the transfer line. A borescope investigation was conducted and confirmed buildup was present throughout the transfer line to the downstream valves. Savannah River National Laboratory personnel were asked to characterize the scale material and samples collected from the saltstone grout line and provide recommendations and/or further guidance as to whether additional corrosion testing is needed for useful equipment operating life information. Based on the samples characterized results, the plug material contained only the 60:40 slag:fly ash saltstone. Portland cement in the original 10:45:45 Portland cement:slag:fly ash mix may result in a less abrasive slurry compared to the 60:40 slag:fly ash mix because the slag is > 95 % crushed angular, sharp edged glass. Saltstone grout erosion and corrosion testing of A36 carbon steel is needed to determine if the 60:40 mix is more abrasive and corrosive for A36 carbon steel than the 10:45:45 mix.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

GEN3D Experimental and Numerical Development of GEN3 Durability Models

Understanding of the high temperature durability of particles and the materials that contain them is critical to next generation of concentrating solar power (CSP) technology. Here we studied the durability of particles and their containment materials under extreme UV cycling, thermal cycling, and in low-speed high temperature mechanical wear situations. The optical stability of seven candidate particles has been determined following exposure to the high temperature conditions present in a generation 3 particle-based CSP technology. Particle solar weighted absorptance and emittance measured periodically during 10,000 high solar irradiance exposure cycles and up to 400 hours of isothermal aging has been documented. The particle aging due to repeated exposure to concentrated solar flux represented the 30-year lifetime of a power plant. Models were fit to the absorptivity and emissivity data following the isothermal aging provides the projected optical degradation of the particles as a function of temperature. Mechanical wear was studied through the use of custom developed wear testing facilities for measuring high temperature impact wear, abrasion wear, and particle attrition. Additionally, a novel technique for measuring the high temperature mechanical properties of single particles was developed. Through these tests it was observed that high nickel alloys generally showed lower wear than comparable iron based steels, particularly at elevated temperatures of 800°C. Mechanical wear at these temperatures is a highly complex phenomenon combining both mechanical wear and oxidation. Additionally, the containment materials wear rates are influenced by the particles (both hardness and roundness), making the wear mechanisms complex. The initial wear test conducted in the abrasion test rig revealed a substantial amount of oxide materials in the particle bed after testing (in relative to later tests), and substantially more wear, likely indicating a need for concern in startup operation of particle facilities to not incur high wear from the presence of oxides. Particle attrition experiments have only been conducted for a single material but increase size distribution, reduction in circularity, and particle diameter is observed. Efforts to develop predictive models was limited due to a testing campaign that prioritized testing materials for particle pathway developers over building a comprehensive design of experiments. The results discussed in this report inform future CSP developers and researchers further de risking the technology and assisting in its future development. ParticleBased CSP development provides a path to dispatchable solar power generation with storage at a price competitive in the current energy market. Lowering the cost of CSP technology provides a carbon free power generation solution that can assist in the transition from fossil fuels to renewable sources of electricity.

14 SOLAR ENERGY↗

Examining Graphite Degradation in Molten Salt Environments: A Chemical, Physical, and Material Analysis

Molten-salt reactors (MSRs) are Generation IV nuclear reactors that use liquid salt as a coolant and/or fuel. In several MSR designs, graphite serves as a moderator and/or reflector. However, due to limited experimental data and operational experience, our understanding of graphite behavior in molten salt environments remains incomplete. This report aims to identify the degradation mechanisms of nuclear graphite in MSRs, detail the mechanisms of each factor, and provide an initial assessment of their impact on the structural integrity of graphite components. This assessment is based on an extensive literature review and insights from subject matter experts. Furthermore, given the limited data, a modeling strategy using existing Grizzly software is proposed for a more thorough analysis where appropriate. Additionally, it presents mitigation strategies where applicable. The report covers physical degradation mechanisms such as infiltration, erosion, and abrasion, as well as chemical degradation mechanisms including fluorination, intercalation, corrosion, and oxidation. Molten salt can infiltrate the porous structure of graphite, leading to several detrimental effects. Entrapment of fissile products within the graphite pores can cause radiation damage and could pose challenges in the handling and disposal of contaminated components. The differential thermal expansion between the infiltrated salt and graphite, along with internal stress from pressurized molten salt and volumetric heating, can compromise the structural integrity of graphite. To mitigate these effects, employing ultra-fine graphite grades and applying sealants and coatings are effective strategies. A computational model based on coupled solid mechanics and heat transfer phenomena could be used to predict the internal stresses using Grizzly software. In pebble-bed MSRs, graphite fuel pebbles can cause abrasion against reactor components due to friction and wear. The severity of wear is influenced by various factors such as temperature, environment, and the presence of lubricants. Tribological studies reveal that higher temperatures and molten salt environments, such as FLiBe, significantly reduce wear rates compared to dry conditions. Additionally, the chemical composition of the salt can further optimize graphite's tribological performance. Long-term wear effects can be modeled by incorporating surface defects into the geometry and predict stresses under thermal and radiation effects using Grizzly software. Chemical degradation of graphite in a molten salt environment can occur through fluorination and intercalation. Fluorination can occur via replacement of hydrogen or oxygen atoms, or at the active sites, but does not cause structural degradation. Intercalation, on the other hand, can lead to exfoliation, where layers of graphite separate and peel away, damaging the graphite. Protective coatings can enhance graphite's resistance to intercalation. Graphite generally exhibits good chemical stability in molten salt environments, though it can corrode under specific conditions, particularly in the presence of impurities or oxidants. Studies have shown that protective coatings, such as plasma-sprayed partially stabilized zirconia (PSZ), can effectively prevent such degradation. Corrosion behavior varies significantly with different graphite grades and coating applications, underscoring the need for detailed studies on uncoated and coated graphite to understand and mitigate corrosion mechanisms in MSRs. Research indicates that the presence of oxidants and impurities can accelerate graphite degradation in molten salts, making it essential to explore acceptable impurity limits. Oxidation is another critical degradation mechanism, leading to weight loss and structural damage due to the formation of CO and CO 2 from the reaction of carbon atoms with oxygen. This process creates new porosity and compromises graphite's integrity. While extensive research on graphite oxidation has been conducted for gas-cooled reactors, studies specific to MSRs are limited. Findings from the coal industry suggest that molten alkali metal salts can significantly accelerate graphite oxidation, a hypothesis worth exploring for fluoride salts in MSRs. Understanding oxidation behavior in MSRs is vital for developing protective measures. The analysis of post-irradiated graphite from the MSRE experiment demonstrated exceptional chemical compatibility with molten fluoride salt, suggesting that the extent of chemical attack on graphite largely depends on the salt's infiltration capability. Therefore, the use of ultra-fine grade graphite could help mitigate chemical degradation effects. Existing oxidation modeling capabilities in Grizzly, which use reaction-diffusion equations to model graphite-air interactions, could be adapted to simulate the chemical degradation effects of graphite in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Dynamics of solid lubrication as observed by optical microscopy

A bench metallograph was converted into a micro contact imager by the addition of a tribometer employing a steel ball in sliding contact with a glass disk. The sliding contact was viewed in real time by means of projection microscope optics. The dynamics of abrasive particles and of solid lubricant particles within the contact were observed in detail. The contact was characterized by a constantly changing pattern of elastic strain with the passage of surface discontinuities and solid particles. Abrasive particles fragmented upon entering the contact, embedded in one surface and scratched the other; in contrast, the solid lubricant particles flowed plastically into thin films. The rheological behavior of the lubricating solids gave every appearance of a paste-like consistency within the Hertzian contact.

Sliney, H. E.↗

Slicing of silicon into sheet material: Silicon sheet growth development for the large area silicon sheet task of the low cost silicon solar array project

Multiblade slurry sawing is used to slice 10 cm diameter silicon ingots into wafers 0.024 cm thick using 0.050 cm of silicon per slice (0.026 cm kerf loss). Total slicing time is less than twenty hours, and 143 slices are produced simultaneously. Productivity (slice area per hour per blade) is shown as a function or blade load and thickness, and abrasive size. Finer abrasive slurries cause a reduction in slice productivity, and thin blades cause a reduction of wafer accuracy. Sawing induced surface damage is found to extend 18 microns into the wafer.

Holden, S. C.↗