Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ceramic fibers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Self-Assembling, Flexible, Pre-Ceramic Composite Preforms

In this innovation, light weight, high temperature, compact aerospace structures with increased design options are made possible by using self-assembling, flexible, pre-ceramic composite materials. These materials are comprised of either ceramic or carbon fiber performs, which are infiltrated with polymer precursors that convert to ceramics upon thermal exposure. The preform architecture can vary from chopped fibers formed into blankets or felt, to continuous fibers formed into a variety of 2D or 3D weaves or braids. The matrix material can also vary considerably. For demonstration purposes, a 2D carbon weave was infiltrated with a SiC polymer precursor. The green or unfired material is fabricated into its final shape while it is still pliable. It is then folded or rolled into a much more compact shape, which will occupy a smaller space. With this approach, the part remains as one continuous piece, rather than being fabricated as multiple sections, which would require numerous seals for eventual component use. The infiltrated preform can then be deployed in-situ. The component can be assembled into its final shape by taking advantage of the elasticity of the material, which permits the structure to unfold and spring into its final form under its own stored energy. The pre-ceramic composites are converted to ceramics and rigidized immediately after deployment. The final ceramic composite yields a high-temperature, high-strength material suitable for a variety of aerospace structures. The flexibility of the material, combined with its high-temperature structural capacity after rigidization, leads to a less complex component design with an increased temperature range. The collapsibility of these structures allows for larger components to be designed and used, and also offers the potential for increased vehicle performance. For the case of collapsible nozzle extensions, a larger nozzle, and thus a larger nozzle exit plane, is possible because interference with surrounding structures can be avoided in the collapsed state. The larger exit plane leads to an increase in expansion area ratio, which has the potential to increase thrust and overall rocket performance. In general, the use of advanced ceramic materials can lead to improved engine and vehicle performance. The ceramics can run hotter, so less cooling is required. Fuel to coolant ratios can be balanced more readily to reduce weight. Engine efficiency can also be increased with hotter combustion and exhaust temperatures. In addition, the ceramic composites themselves can reduce the component weight by as much as 50 percent, which can translate into greater payload for the vehicle

Jaskowiak, Martha H.↗

High Kinetic Energy Penetrator Shielding and High Wear Resistance Materials Fabricated with Boron Nitride Nanotubes (BNNTS) and BNNT Polymer Composites

Boron nitride nanotubes (BNNTs), boron nitride nanoparticles (BNNPs), carbon nontubes (CNTs), graphites, or their combinations, are incorporated into matrices of polymer, ceramic or metals. Fibers, yarns, and woven or nonwoven mates of BNNTs are uses as toughening layers in penetration resistant materials to maximize energy absorption and/or high hardness layers to rebound or deform penetrators. They can be also uses as reinforcing inclusions combining with other polymer matrices to create composite layer like typical reinforcing fibers such as Kevlar (Registered Trademark), Spectra (Registered Trademark) ceramics and metals. Enhanced wear resistance and prolonged usage time, even under harsh conditions, are achieved by adding boron nitride nanomaterials because both hardness and toughness are increased. Such materials can be used in high temperature environments since the oxidation temperature of BNNTs exceeds 800 C in air. Boron nitride based composite materials are useful as strong structural materials for anti-micrometeorite layers for spacecraft and space suits, ultra strong tethers, protective gear for the human body as well as for vehicles, helmets, shields and safety suits/helmets for industry.

Kang, Jin Ho↗

A test for interfacial effects and stress transfer in ceramic matrix composites

A test specimen was devised for measuring stress transfer between a high modulus fiber and a ceramic matrix. Single filaments of SiC were embedded in chemically vapor deposited SiC on a thin plate of molybdenum. The CVD overcoating which encapsulated the fiber was continuous with a coating of SiC on the molybdenum. When placed in a microtensile test device and loaded in the fiber direction, the fiber fracture characteristics provide information on the fiber/matrix adhesion and stress transfer. Problems were encountered due to the formation of a weak boundary between the SiC and the molybdenum which obviated any meaningful tensile tests. Also, the high CVD temperature used in fabricating these specimens restrict the fiber, matrix (and substrate) to materials having similar thermal coefficients of expansion in order to minimize thermal stresses.

Source record↗

Mechanical behaviors of ceramic matrix composites with matrix cracking and fiber debonding

The purpose of this paper is to summarize the current research of the authors on the mechanical behaviors of ceramic matrix composites, including (1) the stress distributions in a composite with matrix cracking and interfacial debonding, (2) the critical strain for matrix cracking, and (3) the effects of fiber/matrix debonding and thermal residual stresses on the critical strain. The stress fields in both bonded and debonded regions are evaluated by taking into account thermal effects. An energy balance approach is followed to determine the critical strain for matrix cracking. From the general equation of the critical strain for matrix cracking, close form solutions have been obtained for two limiting cases: perfect bonding and complete debonding. Numerical solutions are given for the cases of partial fiber debonding and nonzero debonding energy. It is found that thermal residual stresses and the debonding energy have significant effects on the critical strain.

Kuo, Wen-Shyong↗

Challenges and Opportunities in Design, Fabrication, and Testing of High Temperature Joints in Ceramics and Ceramic Composites

Ceramic joining has been recognized as an enabling technology for successful utilization of advanced ceramics and composite materials. A number of joint design and testing issues have been discussed for ceramic joints in silicon carbide-based ceramics and fiber-reinforced composites. These joints have been fabricated using an affordable, robust ceramic joining technology (ARCJoinT). The microstructure and good high temperature mechanical capability (compressive and flexural strengths) of ceramic joints in silicon carbide-based ceramics and composite materials are reported.

Singh, M.↗

CVD silicon carbide monofilament reinforced SrO-Al2O3-2SiO2 (SAS) glass-ceramic composites

Unidirectional CVD SiC fiber-reinforced SrO.Al2O3.2SiO2 (SAS) glass-ceramic matrix composites have been fabricated by hot pressing at various combinations of temperature, pressure and time. Both carbon-rich surface coated SCS-6 and uncoated SCS-0 fibers were used as reinforcements. Almost fully dense composites have been obtained. Monoclinic celsian, SrAl2Si2O8, was the only crystalline phase observed in the matrix from x-ray diffraction. During three point flexure testing of composites, a test span to thickness ratio of approximately 25 or greater was necessary to avoid sample delamination. Strong and tough SCS-6/SAS composites having a first matrix crack stress of approximately 300 MPa and an ultimate bend strength of approximately 825 MPa were fabricated. No chemical reaction between the SCS-6 fibers and the SAS matrix was observed after high temperature processing. The uncoated SCS-0 fiber-reinforced SAS composites showed only limited improvement in strength over SAS monolithic. The SCS-0/SAS composite having a fiber volume fraction of 0.24 and hot pressed at 1400 deg C exhibited a first matrix cracking stress of approximately 231 +/- 20 MPa and ultimate strength of 265 +/- 17 MPa. From fiber push-out tests, the fiber/matrix interfacial debonding strength (tau(sub debond)) and frictional sliding stress (tau(sub friction)) in the SCS-6/SAS system were evaluated to be approximately 6.7 +/- 2.3 MPa and 4.3 +/- 0.6 MPa, respectively, indicating a weak interface. However, for the SCS-0/SAS composite, much higher values of approximately 17.5 +/- 2.7 MPa for tau(sub debond) and 11.3 +/- 1.6 MPa for tau(sub friction) respectively, were observed; some of the fibers were so strongly bonded to the matrix that they could not be pushed out. Examination of fracture surfaces revealed limited short pull-out length of SCS-0 fibers. The applicability of various micromechanical models for predicting the values of first matrix cracking stress and ultimate strength of these composites were examined.

Bansal, Narottam P.↗

Non-steady state cracking in ceramic matrix composites

A micromechanics analytical model based on the consistent shear lag theory is developed for predicting the failure modes in a fiber-reinforced unidirectional ceramic matrix composite. The model accounts for the relatively large matrix stiffness. The fiber and matrix stresses are established as functions of the applied stress, crack geometry, and most importantly, the microstructural properties of the constituents. From the predicted stress, the mode of failure is established based on the point stress criterion. The role of the microstructural properties on the failure mode and ultimate strength is assessed.

Dharani, L. R.↗

Development and Characterization of Hot-Pressed Matrices for Engineered Ceramic Matrix Composites (E-CMCs)

The present research effort was undertaken to develop a new generation of SiC fiber-reinforced engineered ceramic matrix composites (E-CMCs). In contrast to traditional CMCs with a brittle SiC matrix, an E-CMC is designed to consist of a matrix engineered to possess sufficient high temperature plasticity to minimize crack propagation, relatively high fracture toughness, and self-healing capabilities to prevent oxygen ingress to the BN-coated fibers through surface-connected cracks. The present paper discusses the bend strength, isothermal oxidation, microstructures and self-healing properties of several silicide-behaved engineered matrices. Based on the oxidation tests, where it was observed that some of the matrices exhibited either catastrophic oxidation ("pesting") or spalling of the oxide scale, two engineered matrices, CrSi2/SiC/Si3N4 and CrMoSi/SiC/Si3N4, were down-selected for further investigation. Four-point bend tests were conducted on these two engineered matrices between room temperature and 1698 degrees Kelvin. Although these matrices were brittle at low temperatures, it was observed that the bend strengths and bend ductility increased at high temperatures as the silicide particles became more ductile, which was qualitatively consistent with the theoretically expected behavior that crack blunting at these particles should increase the matrix strength. Additional studies were conducted to study the effects of different additives on the self-healing properties of the engineered matrices, which helped to identify the most effective additives.

Composite Materials↗

Elastic crack bridging in ceramic and intermetallic matrix composites

A micromechanics analytical model based on the consistent shear lag theory is developed for predicting the failure modes in a fiber reinforced unidirectional ceramic and intermetallic matrix composite. The model accounts for the relatively large matrix stiffness. The fiber and matrix stresses are established as functions of the applied stress, crack geometry, and most importantly, the microstructural properties of the constituents. From the predicted stress, the mode of failure is established based on the point stress criterion.

Dharani, L. R.↗

The high temperature creep behavior of oxides and oxide fibers

A thorough review of the literature was conducted on the high-temperature creep behavior of single and polycrystalline oxides which potentially could serve as fiber reinforcements in ceramics or metal matrix applications. Sapphire when oriented with the basal plane perpendicular to the fiber axis (c-axis oriented) is highly creep resistant at temperatures in excess of 1600 C and applied loads of 100 MPa and higher. Pyramidal slip is preferentially activated in sapphire under these conditions and steady-state creep rates in the range of 10(exp -7) to 10 (exp -8)/s were reported. Data on the creep resistance of polycrystalline beryllia suggest that C-axiz oriented single crystal beryllia may be a viable candidate as a fiber reinforcement material; however, the issure of fabricability and moisture sensitivity must be addressed for this material. Yttrium aluminum garnet (YAG) also appears to be a fiber candidate material having a high resistance to creep which is due to it's complex crystal structure and high Peierl resistance. The high creep resistance of garnet suggests that there may be other complex ternary oxides such as single crystal mullite which may also be candidate materials for fiber reinforcements. Finally, CVD and single crystal SiC, although not oxides, do possess a high resistance to creep in the temperature range between 1550 and 1850 C and under stresses of 110 to 220 MPa. From a review of the literature, it appears that for high creep resistant applications sapphire, silicon carbide, yttrium aluminum garnet, mullite, and beryllia are desirable candidate materials which require further investigation.

Jones, Linda E.↗

Research on fiber-reinforced composites

Research in materials science - high temperature structural materials, wetting and adherence of nickel alloys to sapphire, boron carbide filaments, and ceramic and graphite fibers

MATERIALS SCIENCE↗

Study of glass preforms for glass fiber optics applications (study of space processing of ceramic materials)

The feasibility, and technical and economic desirability was studied of space processing of glass preforms for optical fiber transmission applications. The results indicate that space processing can produce glass preforms of equal quality at lower cost than earth bound production, and can produce diameter modulation in the glass preform which promotes mode coupling and lowers the dispersion. The glass composition can be modified through the evaporative and diffusion processes, and graded refractive index profiles can be produced. A brief summary of the state of the art in optical fiber transmission is included.

Wang, F. F. Y.↗

Tensile Creep Behavior of SiC(f)/SiC Ceramic Matrix Minicomposites

Single fiber-tow minicomposites represent the major load-bearing element of woven and laminate ceramic matrix composites (CMCs). To understand the effects of fiber type, fiber content, and matrix cracking on tensile creep in SiCf/SiC CMCs, single-tow SiCf/SiC minicomposites with different fiber types and contents were investigated. The minicomposites studied contained either Hi-Nicalon™ or Hi-Nicalon™ Type S SiC fibers with a boron nitride (BN) interphase and a chemical-vapor-infiltrated-silicon-carbide (CVI-SiC) matrix. Tensile creep was performed at 1200 °C in air. A bottom-up creep modeling approach was applied where creep parameters of the fibers and matrix were obtained separately at 1200 °C. Next, a theoretical model based on the rule of mixtures was derived to model the fiber and matrix creep-time-dependent stress redistribution. Fiber and matrix creep parameters, load transfer model results, and numerical modeling were used to construct a creep strain model to predict creep damage evolution of minicomposites with different fiber types and contents.

SiC/SiC Minicomposites Creep↗

Composites review

The properties and applications of composite materials are reviewed. Glass, carbon, Kevlar, ceramic, whisker, and metal fibers are discussed along with polyester, epoxy, polyimide, Peek, carbon, ceramic, and metal matrices. The quantitative distribution of high technology fiber in various applications is given. The role of aerospace industry in the development and promotion of composite utilization is discussed. Consumption trends indicate a rapid development of the composite market.

Hordonneau, A.↗

Effects of CMAS Application on the Isothermal and Gradient Thermal Cycling Behavior of a Yb 2 Si 2 O 7 EBC

Environmental barrier coatings (EBCs) are critical to the continued advancement of gas turbine hot section materials technology. EBCs are required to protect Si-based ceramics such as silicon carbide fiber-reinforced silicon carbide (SiC/SiC) ceramic matrix composites (CMCs) from oxidation and corrosion in the combustion environment. One of the current challenges concerning EBC lifetime is the thermochemical reactions between calcium-magnesium-aluminosilicate (CMAS) deposits and the EBC that leads to changes in both composition and stress state. These changes can severely reduce the integrity of the EBC leading to crack formation, delamination, and spallation. Current techniques for evaluating CMAS in the laboratory rely on the pre-application of CMAS. Two commonly used application methods to deposit CMAS on EBC materials are tape-casting and air spray. In both methods, the CMAS is applied to the EBC surface at ambient temperature, and then subject to a heat treatment process for binder burnout. The purpose of this study is to compare the tape-cast and air spray methods on the CMAS corrosion of an ytterbium disilicate (Yb 2 Si 2 O 7 ) EBC subject to isothermal, and gradient thermal cycling. The results highlight if any differences exist in the CMAS infiltration kinetics between the two application methods.

Environmental barrier coatings (EBCs)↗

Understanding the Durability of SiC Based Ceramic Matrix Composites (CMCs) for Gas Turbine Engine Hot Section Components

Silicon carbide fiber reinforced silicon carbide ceramic matrix composites (SiCf/SiC-CMCs) are being used in the fabrication of gas turbine engine hot section components due to their light weight and excellent thermal and chemical stabilities at high-temperature. These superior properties enable significant enhancements in engine efficiency and reduced fuel burn, emissions, and cooling requirements. In support of NASA’s Aeronautics Mission under various programs at Glenn Research Center, different types of composites have been developed and assessed for a high temperature (2700 °F) SiCf/SiC CMC system for turbine engine applications. These composites have creep-resistant SiC fibers, advanced 3D weaves, 2700 °F-capable hybrid SiC matrices, and durable environmental barrier coatings (EBCs). These efforts have resulted in improvements in the overall CMC thermomechanical and environmental durability. In order to study the role of different constituents and processing variables, a single fiber tow CVI (chemical vapor infiltration) SiC/SiC mini-composite can be considered the basic architectural feature of woven and laminate SiC/SiC CMCs. Moreover, the mini-composite mechanical and tensile creep damage behavior represents the creep behavior of 0° fiber tows in the axial loading direction of a macro-composite or component. In addition, a large number of mini-composite samples can be fabricated at relatively low cost within a short time, which makes them attractive for obtaining a robust set of experimental data and studying constituent behavior. In this presentation, the mini-composite approach to study damage mechanisms that limit CMC life in extreme environments including exposure to steam will be presented. The effects of constituent type and volume fraction on the CMC durability, which will help influence CMC design, will be discussed.

Ceramic Matrix Composites (CMCs)↗

Modeling of Time-Dependent Strength Degradation of SiC/SiC Ceramic Matrix Composites via MAC/GMC Computer Code

Silicon carbide fiber reinforced silicon carbide (SiC/SiC) ceramic matrix composites (CMCs) display time-dependent strength degradation at intermediate temperatures (600 to 900 degrees Centigrade). This is generally believed to be an oxidation induced phenomenon. The understanding of the effect of temperature with environment (oxidation) is key towards development of SiC/SiC CMCs with a reliable load carrying capacity. Various theories have been proposed to explain the strength degradation. One suggests that the boron nitride (BN) coating deposited on the fibers oxidizes causing fusion of fibers. Another theory proposes that the SiC fibers are oxidized forming a silica scale leading to premature fiber failure. A more recent theory suggests that SiC fiber strength is intrinsically time-dependent due to slow crack growth of flaws in the fibers. An empirical model, termed as a "fiber classic model," which is based on a standard slow crack growth type power-law, has been implemented within NASA's micromechanics-based MAC/GMC computer code as a user routine. Model parameters for this "classic model" were calibrated from stress-rupture data of Hi-Nicalon (TM) monofilaments using the maximum likelihood estimation (MLE) technique. This new capability in the MAC/GMC computer code was then used to predict the stress-rupture behavior of Hi-Nicalon (TM) tows as well as 2-D SiC/SiC composites reinforced with Hi-Nicalon (TM) fibers. Results demonstrate that the MAC/GMC with this new capability successfully predicts the time-to-failure vs. applied stress within the intermediate temperature range at various scales as well as laminated composites in an oxidizing environment.

Environmental degradation↗

High-Temperature, Lightweight, Self-Healing Ceramic Composites for Aircraft Engine Applications

The use of reliable, high-temperature, lightweight materials in the manufacture of aircraft engines is expected to result in lower fossil and biofuel consumption, thereby leading to cost savings and lower carbon emissions due to air travel. Although nickel-based superalloy blades and vanes have been successfully used in aircraft engines for several decades, there has been an increased effort to develop high-temperature, lightweight, creep-resistant substitute materials under various NASA programs over the last two decades. As a result, there has been a great deal of interest in developing SiC/SiC ceramic matrix composites (CMCs) due to their higher damage tolerance compared to monolithic ceramics. Current-generation SiC/SiC ceramic matrix composites rely almost entirely on the SiC fibers to carry the load, owing to the premature cracking of the matrix during loading. Thus, the high-temperature usefulness of these CMCs falls well below their theoretical capabilities. The objective of this work is to develop a new class of high-temperature, lightweight, self-healing, SiC fiber-reinforced, engineered matrix ceramic composites.

Raj, Sai V.↗