Mechanical testing of advanced coating system, volume 1

The Electron Beam Physical Vapor Deposition (EBPVD) coating material has a highly columnar microstructure, and as a result it was expected to have very low tensile strength. To be able to fabricate the required compression and tensile specimens, a substrate was required to provide structural integrity for the specimens. Substrate and coating dimensions were adjusted to provide sufficient sensitivity to resolve the projected loads carried by the EBPVD coating. The use of two distinctively different strain transducer systems, for tension and compression loadings, mandated two vastly different specimen geometries. Compression specimen and tensile specimen geometries are given. Both compression and tensile test setups are described. Data reduction mathematical models are given and discussed in detail as is the interpretation of the results. Creep test data is also given and discussed.

Cruse, T. A.↗

Influences of Introduced Yttrium Oxide Particles on Superalloy 718

Additive manufacturing has proven useful for introducing oxide particles into superalloys, to provide oxide dispersion strengthening (ODS) at high temperatures. This study screened how such an approach can influence microstructure and failure modes for superalloy 718. The objective of this study was to compare tensile and creep failure modes for additively manufactured superalloy 718 having introduced oxide particles. Fine yttrium-oxide (yttria) particles were introduced into 718 powder using two different powder mixing methods. Additive manufacturing by laser powder bed fusion was then used to prepare specimen blanks for each case, oriented parallel and transverse to the building direction. These were subsequently given consistent stress relief, hot isostatic pressurization, and final heat treatments, then subjected to tensile and creep tests at varied temperatures. Additively manufactured 718 without ODS (“no-ODS”) had nearly equiaxed grains at 50 μm in width. Roll-mixed ODS material had a bimodal grain size distribution, with fine grains at 9 μm and coarse grains at 66 μm in average width. The fine grains were elongated about 5x in the building direction. Acoustic-mixed ODS materials had grains at 10 μm in width that were elongated about 10x in the build direction. Compared to no-ODS, roll-mixed and acoustic mixed ODS materials did not show improved tensile strengths at room temperature, 760 °C, and 1093 °C. The tensile failure strains parallel to the building direction of roll-mixed ODS material were lowest in these tests. Flattened clumps of yttria had formed transverse to the building direction in roll-mixed material, which were easily cracked. Creep rupture response at 760 °C in the building direction was highest for acoustic-mixed material test. Creep tests at 1093 °C showed varied results, with low rupture lives associated with enhanced cavitation at grain boundaries and surface oxidation. Transverse to the building direction, all three materials had low failure strains in tests at 760 °C. The elongated grain boundaries failed readily in all transverse specimens tested at 760 °C and 1093 °C.

oxide dispersion strengthening↗

System integration and demonstration of adhesive bonded high temperature aluminum alloys for aerospace structure, phase 2

Adhesive bonding materials and processes were evaluated for assembly of future high-temperature aluminum alloy structural components such as may be used in high-speed civil transport aircraft and space launch vehicles. A number of candidate high-temperature adhesives were selected and screening tests were conducted using single lap shear specimens. The selected adhesives were then used to bond sandwich (titanium core) test specimens, adhesive toughness test specimens, and isothermally aged lap shear specimens. Moderate-to-high lap shear strengths were obtained from bonded high-temperature aluminum and silicon carbide particulate-reinforced (SiC(sub p)) aluminum specimens. Shear strengths typically exceeded 3500 to 4000 lb/in(sup 2) and flatwise tensile strengths exceeded 750 lb/in(sup 2) even at elevated temperatures (300 F) using a bismaleimide adhesive. All faceskin-to-core bonds displayed excellent tear strength. The existing production phosphoric acid anodize surface preparation process developed at Boeing was used, and gave good performance with all of the aluminum and silicon carbide particulate-reinforced aluminum alloys investigated. The results of this program support using bonded assemblies of high-temperature aluminum components in applications where bonding is often used (e.g., secondary structures and tear stoppers).

Falcone, Anthony↗

Energy Absorbing Protective Shroud

The present invention is a dissipating protection energy system designed to receive and safely dissipate the kinetic energy from high energy fragments. The energy dissipation system dissipates energy transferred to it by the incremental and progressive rupturing at an approximately constant force of strategically placed sacrificial stitching applied to a number of high strength straps, such as an aromatic polyimide fiber of extremely high tensile strength. Thus, the energy dissipation system provides a lightweight device for controlling and dissipating the dangerous and destructive energy stored in high strength fragments released by catastrophic failures of machinery minimizing damage to other critical components.

Schneider, William C.↗

Biaxial prestressing of brittle materials

Strengthening of chemically consolidated zirconia with tungsten fibers, graphite fibers, sapphire whiskers, and silicon carbide whiskers is investigated. Addition of silicon carbide whiskers gives the highest increase in strength of zirconia at room and elevated temperatures. Prestressing with tungsten cables increases tensile strength and ductility

Greszczuk, L.↗

Fundamental mechanisms of tensile fracture in aluminum sheet undirectionally reinforced with boron filament

Results are presented from an experimental study of the tensile-fracture process in aluminum sheet unidirectionally reinforced with boron filament. The tensile strength of the material is severely limited by a noncumulative fracture mechanism which involves the initiation and sustenance of a chain reaction of filament fractures at a relatively low stress level. Matrix fracture follows in a completely ductile manner. The minimum filament stress for initiation of the fracture mechanism is shown to be approximately 1.17 GN/sq m (170 ksi), and appears to be independent of filament diameter, number of filament layers, and the strength of the filament-matrix bond. All the commonly observed features of tensile fracture surfaces are explained in terms of the observed noncumulative fracture mechanism.

Herring, H. W.↗

High-Hot-Strength Ceramic Fibers

Continuous fibers consisting of laminae of alumina and yttrium aluminum garnet offer exceptionally high strength, resistance to creep, and chemical stability at high temperatures. These fibers exceed tensile strength of sapphire fibers. Leading candidates for reinforcement of intermetallic-matrix composites in exhaust nozzles of developmental high-speed civil transport aircraft engines. Other applications are in aerospace, automotive, chemical-process, and power-generation industries.

Sayir, Ali↗

Aluminum-Alloy-Matrix/Alumina-Reinforcement Composites

Isotropic composites of aluminum-alloy matrices reinforced with particulate alumina have been developed as lightweight, high-specific-strength, less-expensive alternatives to nickel-base and ferrous superalloys. These composites feature a specific gravity of about 3.45 grams per cubic centimeter and specific strengths of about 200 MPa/(grams per cubic centimeter). The room-temperature tensile strength is 100 ksi (689 MPa) and stiffness is 30 Msi (206 GPa). At 500 F (260 C), these composites have shown 80 percent retention in strength and 95 percent retention in stiffness. These materials also have excellent fatigue tolerance and tribological properties. They can be fabricated in net (or nearly net) sizes and shapes to make housings, pistons, valves, and ducts in turbomachinery, and to make structural components of such diverse systems as diesel engines, automotive brake systems, and power-generation, mining, and oil-drilling equipment. Separately, incorporation of these metal matrix composites within aluminum gravity castings for localized reinforcement has been demonstrated. A composite part of this type can be fabricated in a pressure infiltration casting process. The process begins with the placement of a mold with alumina particulate preform of net or nearly net size and shape in a crucible in a vacuum furnace. A charge of the alloy is placed in the crucible with the preform. The interior of the furnace is evacuated, then the furnace heaters are turned on to heat the alloy above its liquidus temperature. Next, the interior of the furnace is filled with argon gas at a pressure about 900 psi (approximately equal to 6.2 MPa) to force the molten alloy to infiltrate the preform. Once infiltrated, the entire contents of the crucible can be allowed to cool in place, and the composite part recovered from the mold.

Kashalikar, Uday↗

Tension Strength, Failure Prediction and Damage Mechanisms in 2D Triaxial Braided Composites with Notch

The unnotched and notched (open hole) tensile strength and failure mechanisms of two-dimensional (2D) triaxial braided composites were examined. The effect of notch size and notch position were investigated. Damage initiation and propagation in notched and unnotched coupons were also examined. Theory developed to predict the normal stress distribution near an open hole and failure for tape laminated composites was evaluated for its applicability to 2D triaxial braided textile composite materials. Four different fiber architectures were considered; braid angle, yarn and braider size, percentage of longitudinal yarns and braider angle varied. Tape laminates equivalent to textile composites were also constructed for comparison. Unnotched tape equivalents were stronger than braided textiles but exhibited greater notch sensitivity. Notched textiles and tape equivalents have roughly the same strength at large notch sizes. Two common damage mechanisms were found: braider yarn cracking and near notch longitudinal yarn splitting. Cracking was found to initiate in braider yarns in unnotched and notched coupons, and propagate in the direction of the braider yarns until failure. Damage initiation stress decreased with increasing braid angle. No significant differences in prediction of near notch strain between textile and tape equivalents could be detected for small braid angle, but the correlations were weak for textiles with large braid angle. Notch strength could not be predicted using existing anisotropic theory for braided textiles due to their insensitivity to notch.

Norman, Timothy L.↗

High-temperature tensile tester for ceramics

Apparatus measures tensile strength of rigid, low-density ceramic materials at temperatures up to 1375 K. Tensile grips mate with tensile specimen and form top and bottom of lightweight furnace. Apparatus can only be used with rigid materials and grips must be stronger than material under test.

Smith, M.↗

A nickel base alloy, NASA WAZ-16, with potential for gas turbine stator vane application

A nickel-base superalloy based on the nickel-aluminum-tungsten system designated WAZ-16 was developed for high strength in the 1095 C (2000 F) to 1205 C (2200 F) range. Its tensile strength at the latter temperature is approximately 186 MN/m2 (27,000 psi). The combination of properties of the alloy suggest that it has potential as a stator vane material in advanced gas turbine engines.

Waters, W. J.↗

Fundamental studies on the nature and properties of ceramic fiber insulation

Silica and mullite fibers used to fabricate reusable surface insulation (RSI) for the space shuttle orbiter may devitrify/recrystallize within the temperature range anticipated upon reentry. This is shown to be dependent upon impurity level, temperature, and time at temperature. It is determined that the effects of the material improvement and optimization program are positive. The degree of crystallinity is shown to have a predominant effect upon the strength of fabricated RSI tile, and limits are determined. Models are developed to predict tensile strengths and shrinkage rates of silica tile based upon readily measurable parameters. Thermal cycling which simulates reentry results in an increase in the crystallinity and in the porosity of tile coatings.

Mueller, J. I.↗

Thermally induced transverse cracking in graphite-epoxy cross-ply laminates

Thermally induced transverse cracking in T300/5208 graphite-epoxy cross-ply laminates was investigated experimentally and theoretically. The six laminate configurations studied were: 0/90(3)s, 0(2)/90(2)s, 0(3)/90s, 90/0(3)s, 90(2)/0(2)s, and 90(3)/0s. The thermal load required to initiate transverse cracking was determined experimentally and compared to a theoretical prediction. Experimental results for the accumulation of transverse cracks under cyclic thermal loading between - 250 and 250 F for up to 500 thermal cycles are presented. The calculated in situ transverse-lamina strength was determined to be at least 1.9 times the unidirectional-lamina transverse tensile strength. All laminate configurations exhibited an increase in crack density with increasing thermal cycles.

Adams, D. S.↗

Relationship of Cure Temperature to Mechanical, Physical, and Dielectric Performance of PDMS Glass Composite for Electric Motor Insulation

Achieving NASAs aggressive fuel burn and emission reduction for N-plus-3 aircraft will require hybrid electric propulsion system in which electric motors driven by either power generated from turbine or energy storage system will power the fan for propulsion. Motors designed for hybrid electric aircraft are expected to operate at medium to high voltages over long durations in a high altitude service environment. Such conditions have driven research toward the development of wire insulation with improved mechanical strength, thermal stability and increased breakdown voltage. The silicone class of materials has been considered for electric wire insulation due to its inherent thermal stability, dielectric strength and mechanical integrity. This paper evaluates the dependence of these properties on the cure conditions of a polydimethyl-siloxane (PDMS) elastomer; where both cure temperature and base-to-catalyst ratio were varied. The PDMS elastomer was evaluated as a bulk material and an impregnation matrix within a lightweight glass veil support. The E-glass support was selected for mechanical stiffness and dielectric strength. This work has shown a correlation between cure conditions and material physical properties. Tensile strength increased with cure temperature whereas breakdown voltage tended to be independent of process variations. The results will be used to direct material formulation based on specific insulation requirements.

insulation↗

Multiscale Modeling of Fracture Strength in Fibrous Thermal Protection System Materials

This work presents a multiscale modeling approach to predict the fracture strength of fibrous Thermal Protection System (TPS) materials. The model assumes that system failure is initiated at the joints between individual fibers. We investigated three distinct TPS compositions: amorphous silica, alumina and aluminosilicate fibers. Molecular dynamics (MD) simulations were employed to determine the fracture strength values of these fiber joints for both material systems. These fracture strength values were then integrated into simulations of 3D randomly populated fiber structures, where tensile load transfer occurs through the fiber joints. These microscale properties are upscaled through a renormalization approach [1] to predict macroscale tensile strength of 3D random fiber networks, accounting for joint-dominated failure and effective load-bearing area. The study concludes by demonstrating the resulting strength variation as a function of material composition, fiber density, and morphology. We also show validation of results by comparing them against explicit fiber finite element (FE) modeling [2] where fiber joint fracture is represented by cohesive elements.

Jaehyun Cho↗